JP3079902B2 - 原子炉炉内構造物の溶接補修方法 - Google Patents
原子炉炉内構造物の溶接補修方法Info
- Publication number
- JP3079902B2 JP3079902B2 JP06153300A JP15330094A JP3079902B2 JP 3079902 B2 JP3079902 B2 JP 3079902B2 JP 06153300 A JP06153300 A JP 06153300A JP 15330094 A JP15330094 A JP 15330094A JP 3079902 B2 JP3079902 B2 JP 3079902B2
- Authority
- JP
- Japan
- Prior art keywords
- welding
- crack
- weld
- crack defect
- reactor
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K31/00—Processes relevant to this subclass, specially adapted for particular articles or purposes, but not covered by any single one of main groups B23K1/00 - B23K28/00
- B23K31/02—Processes relevant to this subclass, specially adapted for particular articles or purposes, but not covered by any single one of main groups B23K1/00 - B23K28/00 relating to soldering or welding
Landscapes
- Engineering & Computer Science (AREA)
- Mechanical Engineering (AREA)
- Butt Welding And Welding Of Specific Article (AREA)
- Arc Welding In General (AREA)
Priority Applications (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP06153300A JP3079902B2 (ja) | 1994-07-05 | 1994-07-05 | 原子炉炉内構造物の溶接補修方法 |
| US08/498,485 US5674419A (en) | 1994-07-05 | 1995-07-05 | Method for weld repairing of structures in nuclear reactors |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP06153300A JP3079902B2 (ja) | 1994-07-05 | 1994-07-05 | 原子炉炉内構造物の溶接補修方法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH0815481A JPH0815481A (ja) | 1996-01-19 |
| JPH0815481A5 JPH0815481A5 (enExample) | 1999-12-24 |
| JP3079902B2 true JP3079902B2 (ja) | 2000-08-21 |
Family
ID=15559469
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP06153300A Expired - Fee Related JP3079902B2 (ja) | 1994-07-05 | 1994-07-05 | 原子炉炉内構造物の溶接補修方法 |
Country Status (2)
| Country | Link |
|---|---|
| US (1) | US5674419A (enExample) |
| JP (1) | JP3079902B2 (enExample) |
Families Citing this family (16)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US5762727A (en) * | 1997-04-14 | 1998-06-09 | General Electric Company | Weld repair process and article repaired thereby |
| JP3459193B2 (ja) * | 1999-05-26 | 2003-10-20 | 株式会社日立製作所 | 摩擦攪拌接合部の補修方法および鉄道車両の製作方法 |
| JP4490608B2 (ja) * | 2001-08-09 | 2010-06-30 | 株式会社東芝 | 構造物の補修方法 |
| FR2866148B1 (fr) * | 2004-02-06 | 2006-07-21 | Framatome Anp | Procede de fixation d'un tube dans un alesage traversant une paroi spherique et dispositif de depot metal d'apport dans un lamage. |
| US20050199591A1 (en) * | 2004-03-09 | 2005-09-15 | Westinghouse Electric Co. Llc | Method of forming a weld pad |
| JP4346564B2 (ja) * | 2005-02-10 | 2009-10-21 | 株式会社東芝 | クラッド溶接方法及びその装置 |
| FR2902569B1 (fr) * | 2006-06-16 | 2008-09-12 | Areva Np Sas | Procede de reparation d'une penetration de fond de cuve d'un reacteur nucleaire |
| DE102009016260A1 (de) * | 2009-04-03 | 2010-10-07 | Fraunhofer-Gesellschaft zur Förderung der angewandten Forschung e.V. | Verfahren beim Schweißen und Bauteil |
| CN102275042A (zh) * | 2010-06-08 | 2011-12-14 | 上海振华重工(集团)股份有限公司 | 一种高强钢焊接工艺 |
| US8726610B2 (en) * | 2012-08-29 | 2014-05-20 | General Electric Company | Crack-resistant member, a method of preventing crack propagation, and a method of assembling a tower |
| EP2774715A1 (de) * | 2013-03-06 | 2014-09-10 | Siemens Aktiengesellschaft | Verfahren zur Reparatur einer äußeren Oberfläche oder einer freistehenden Wand eines Bauteils |
| US9962797B2 (en) * | 2014-02-13 | 2018-05-08 | The Chugoku Electric Power Co., Inc. | Repair method for cast steel member |
| CN104526249B (zh) * | 2014-11-14 | 2017-01-04 | 中广核工程有限公司 | 一种核电站密封焊返修方法及系统 |
| US10625361B2 (en) * | 2017-06-14 | 2020-04-21 | General Electric Company | Method of welding superalloys |
| BE1026209B1 (fr) * | 2018-11-15 | 2019-11-07 | Westinghouse Electric Belgium | Procédé de réparation par dépôt de poudre métallique au laser |
| KR20210099595A (ko) * | 2018-11-15 | 2021-08-12 | 웨스팅하우스 일렉트릭 벨기에 | 레이저 금속 분말 퇴적을 이용한 복구 프로세스 |
Family Cites Families (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5431062A (en) * | 1977-08-12 | 1979-03-07 | Hitachi Ltd | Manufacture of structure superior in stress corrosion cracking resistivity |
| JPS5921711B2 (ja) * | 1978-07-11 | 1984-05-22 | 株式会社日立製作所 | ステンレス鋼材の溶接方法 |
| US4562332A (en) * | 1984-03-26 | 1985-12-31 | Rockwell International Corporation | Surface crack healing with high-energy beam |
| JPH0655268A (ja) * | 1992-08-10 | 1994-03-01 | Yamaha Shatai Kogyo Kk | 溶接ロボット |
| US5494539A (en) * | 1993-08-30 | 1996-02-27 | Hitachi, Ltd. | Metal member quality improving method by spot welding |
| US5515589A (en) * | 1994-12-27 | 1996-05-14 | General Electric Company | In situ method for remotely operated, automatic contour mapping, machining and welding of piping |
-
1994
- 1994-07-05 JP JP06153300A patent/JP3079902B2/ja not_active Expired - Fee Related
-
1995
- 1995-07-05 US US08/498,485 patent/US5674419A/en not_active Expired - Fee Related
Also Published As
| Publication number | Publication date |
|---|---|
| US5674419A (en) | 1997-10-07 |
| JPH0815481A (ja) | 1996-01-19 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| Blondeau | Metallurgy and mechanics of welding: processes and industrial applications | |
| JP4246878B2 (ja) | レーザ補修方法 | |
| US5674419A (en) | Method for weld repairing of structures in nuclear reactors | |
| JPH0775893A (ja) | 構造物の補修方法および予防保全方法 | |
| JP2003053533A (ja) | 構造物の補修方法および補修溶接装置 | |
| JPH0815481A5 (enExample) | ||
| US20100217060A1 (en) | Method of Decontaminating Radioisotope-Contaminated Surface Vicinity Region by Use of Nonthermal Laser Peeling Without Re-Melting, Without Re-Diffusion and Without Re-Contamination, and Apparatus Therefor | |
| US5022936A (en) | Method for improving property of weld of austenitic stainless steel | |
| JP4304913B2 (ja) | 亀裂状欠陥の補修方法 | |
| JP7228346B2 (ja) | 溶接補修方法 | |
| JP3272853B2 (ja) | 亀裂の溶融補修方法 | |
| CN109332897A (zh) | 一种中厚板激光焊接方法 | |
| US10363631B2 (en) | Neutron irradiated material repair | |
| JPH06289183A (ja) | 原子炉炉内構造物の補修方法 | |
| Wang et al. | The effect of an applied stress on the welding of irradiated steels | |
| JP3970469B2 (ja) | テンパービード工法 | |
| JP2000254776A (ja) | 原子炉内部配管溶接部の応力腐食割れ防止方法 | |
| JP2002219585A (ja) | 構造物とその補修方法 | |
| Kawano et al. | Weldability of helium-containing stainless steels using a YAG laser | |
| Tamura et al. | Development of underwater laser cladding and underwater laser seal welding techniques for reactor components (II) | |
| JP3530325B2 (ja) | 管台溶接部の補修方法 | |
| JP2000230996A (ja) | 原子炉構造物の補修方法 | |
| JP4412533B2 (ja) | 高ニッケル合金の応力腐食割れ改善方法及び補修方法 | |
| JPH06335792A (ja) | 亀裂補修方法 | |
| Miyazaki et al. | Welding techniques for tailored blanks |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20080623 Year of fee payment: 8 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20080623 Year of fee payment: 8 |
|
| S531 | Written request for registration of change of domicile |
Free format text: JAPANESE INTERMEDIATE CODE: R313531 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20080623 Year of fee payment: 8 |
|
| R350 | Written notification of registration of transfer |
Free format text: JAPANESE INTERMEDIATE CODE: R350 |
|
| S111 | Request for change of ownership or part of ownership |
Free format text: JAPANESE INTERMEDIATE CODE: R313111 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20080623 Year of fee payment: 8 |
|
| R371 | Transfer withdrawn |
Free format text: JAPANESE INTERMEDIATE CODE: R371 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20080623 Year of fee payment: 8 |
|
| S111 | Request for change of ownership or part of ownership |
Free format text: JAPANESE INTERMEDIATE CODE: R313111 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20080623 Year of fee payment: 8 |
|
| R350 | Written notification of registration of transfer |
Free format text: JAPANESE INTERMEDIATE CODE: R350 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20080623 Year of fee payment: 8 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20090623 Year of fee payment: 9 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20100623 Year of fee payment: 10 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20100623 Year of fee payment: 10 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20110623 Year of fee payment: 11 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20110623 Year of fee payment: 11 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20120623 Year of fee payment: 12 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20120623 Year of fee payment: 12 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20130623 Year of fee payment: 13 |
|
| LAPS | Cancellation because of no payment of annual fees |