JP2013185239A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2013185239A5 JP2013185239A5 JP2012053410A JP2012053410A JP2013185239A5 JP 2013185239 A5 JP2013185239 A5 JP 2013185239A5 JP 2012053410 A JP2012053410 A JP 2012053410A JP 2012053410 A JP2012053410 A JP 2012053410A JP 2013185239 A5 JP2013185239 A5 JP 2013185239A5
- Authority
- JP
- Japan
- Prior art keywords
- ceramic film
- alloy
- film
- ceramic
- molten aluminum
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Priority Applications (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2012053410A JP5931516B2 (ja) | 2012-03-09 | 2012-03-09 | アルミニウム溶湯接触部材の製造方法 |
| CN201310073959.3A CN103305826B (zh) | 2012-03-09 | 2013-03-08 | 接触铝金属熔液的构件和其制造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2012053410A JP5931516B2 (ja) | 2012-03-09 | 2012-03-09 | アルミニウム溶湯接触部材の製造方法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JP2013185239A JP2013185239A (ja) | 2013-09-19 |
| JP2013185239A5 true JP2013185239A5 (https=) | 2015-01-29 |
| JP5931516B2 JP5931516B2 (ja) | 2016-06-08 |
Family
ID=49131535
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2012053410A Expired - Fee Related JP5931516B2 (ja) | 2012-03-09 | 2012-03-09 | アルミニウム溶湯接触部材の製造方法 |
Country Status (2)
| Country | Link |
|---|---|
| JP (1) | JP5931516B2 (https=) |
| CN (1) | CN103305826B (https=) |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN116970944A (zh) * | 2023-08-15 | 2023-10-31 | 苏州博创熠鑫智造科技有限责任公司 | 一种铝合金的表面改性方法 |
Family Cites Families (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CH621952A5 (https=) * | 1977-09-01 | 1981-03-13 | Bbc Brown Boveri & Cie | |
| JPH1034311A (ja) * | 1996-07-26 | 1998-02-10 | Hitachi Metals Ltd | 溶融金属用部材及びその製造方法 |
| ATE235036T1 (de) * | 1999-04-16 | 2003-04-15 | Moltech Invent Sa | Schutzbeschichtung für komponenten, die durch erosion während des frischens von geschmolzenen metallen angegriffen werden |
| JP4409067B2 (ja) * | 2000-08-03 | 2010-02-03 | 東洋鋼鈑株式会社 | 溶融金属に対する耐食性に優れた溶融金属用部材およびその製造方法 |
| JP2002146509A (ja) * | 2000-11-09 | 2002-05-22 | Asahi Glass Co Ltd | 溶融金属用部材およびその製造方法 |
| JP2003166027A (ja) * | 2001-11-30 | 2003-06-13 | Toshiba Mach Co Ltd | Ni基耐食耐摩耗合金、この合金を用いた複合部材およびダイカストマシン用の部材、並びにこの合金用の原料粉末 |
| JP4354315B2 (ja) * | 2004-03-22 | 2009-10-28 | 東芝機械株式会社 | アルミニウム溶湯接触部材およびその製造方法 |
-
2012
- 2012-03-09 JP JP2012053410A patent/JP5931516B2/ja not_active Expired - Fee Related
-
2013
- 2013-03-08 CN CN201310073959.3A patent/CN103305826B/zh not_active Expired - Fee Related
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| WO2010053687A3 (en) | Thermal spray coatings for semiconductor applications | |
| CN102345093A (zh) | 壳体及其制作方法 | |
| CN106498355A (zh) | 一种高温薄膜传感器用抗氧化复合防护层及其制造方法 | |
| CN106463360B (zh) | 用于薄膜沉积设备的内部材料及其制造方法 | |
| CN108048839A (zh) | 一种钨铼热电偶高温抗氧化涂层及其应用 | |
| CN104487403B (zh) | 具有热喷涂被覆层的碳材料 | |
| TWI526412B (zh) | 抗腐蝕膜、形成有抗腐蝕層之金屬基材以及其製備方法 | |
| TW201236876A (en) | Vacuum depositing articles and method for making same | |
| CN102465258A (zh) | 镀膜件及其制备方法 | |
| JPWO2015173843A1 (ja) | 溶融めっき金属浴用部材 | |
| JP2013185239A5 (https=) | ||
| CN104854253B (zh) | 金属陶瓷熔射粉末、熔融金属镀浴用辊和熔融金属镀浴中部件 | |
| JP2004346428A (ja) | ケイ素基材とボンド層とを含む物品 | |
| JP2011153230A5 (https=) | ||
| CN112941458B (zh) | 一种铬改性钛及钛合金原位自生Ti-Al-Si梯度涂层及其制备方法 | |
| CN113891953B (zh) | 防腐蚀的方法 | |
| JP6895259B2 (ja) | Mo−Si−B層およびそれを製造する方法 | |
| CN107385374A (zh) | 一种原位镶嵌式的金属间化合物‑陶瓷双涂层及其制备方法 | |
| JP2014012873A5 (https=) | ||
| CN103614698B (zh) | 一种高温抗氧化铌合金复合涂层及其制备方法 | |
| JP2007175881A (ja) | スーパーエンプラ積層膜及び複合による溶射成膜法 | |
| JP2020519763A5 (https=) | ||
| Li et al. | Zinc-Aluminum Corrosion Resistance and Inactivation Process of NiCr-Cr3C2 Cermet oating | |
| JP6731613B2 (ja) | 複合材料及びこれが用いられる硫酸分解器、水素製造装置 | |
| JP2012201893A (ja) | 耐食性材料 |