JP2011173236A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2011173236A5 JP2011173236A5 JP2011023445A JP2011023445A JP2011173236A5 JP 2011173236 A5 JP2011173236 A5 JP 2011173236A5 JP 2011023445 A JP2011023445 A JP 2011023445A JP 2011023445 A JP2011023445 A JP 2011023445A JP 2011173236 A5 JP2011173236 A5 JP 2011173236A5
- Authority
- JP
- Japan
- Prior art keywords
- peening
- glass bead
- glass
- intensity
- diameter
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
- 239000011324 bead Substances 0.000 claims 13
- 239000011521 glass Substances 0.000 claims 13
- 238000000034 method Methods 0.000 claims 11
- 238000009499 grossing Methods 0.000 claims 1
Applications Claiming Priority (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US12/702,534 US8468862B2 (en) | 2010-02-09 | 2010-02-09 | Peening process for enhancing surface finish of a component |
| US12/702,534 | 2010-02-09 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JP2011173236A JP2011173236A (ja) | 2011-09-08 |
| JP2011173236A5 true JP2011173236A5 (enExample) | 2014-03-20 |
| JP5778935B2 JP5778935B2 (ja) | 2015-09-16 |
Family
ID=43856133
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2011023445A Active JP5778935B2 (ja) | 2010-02-09 | 2011-02-07 | 部品の表面仕上りを改善するピーニング処理 |
Country Status (4)
| Country | Link |
|---|---|
| US (1) | US8468862B2 (enExample) |
| EP (1) | EP2353782B1 (enExample) |
| JP (1) | JP5778935B2 (enExample) |
| CN (1) | CN102189491A (enExample) |
Families Citing this family (17)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| WO2012014542A1 (ja) * | 2010-07-27 | 2012-02-02 | 新東工業株式会社 | ショットピーニング方法及びショットピーニング装置 |
| US20130084190A1 (en) * | 2011-09-30 | 2013-04-04 | General Electric Company | Titanium aluminide articles with improved surface finish and methods for their manufacture |
| CN104204710A (zh) * | 2012-03-28 | 2014-12-10 | 开利公司 | 用于铝的耐腐蚀性的表面处理 |
| EP2801443B1 (en) | 2013-05-07 | 2015-11-04 | Phibo Industries BVBA | Processing medium for processing stainless steel or other metallic surfaces, method for processing stainless steel or other metallic surfaces using such a processing medium and nozzle arranged to be fitted on a process gun |
| WO2015065747A1 (en) | 2013-10-29 | 2015-05-07 | United Technologies Corporation | Systems and methods for finishing flow elements |
| GB201320501D0 (en) * | 2013-11-20 | 2014-01-01 | Element Six Gmbh | Strike constructions,picks comprising same and methods for making same |
| JP2015214738A (ja) * | 2014-05-13 | 2015-12-03 | 株式会社東芝 | 耐食性金属部材、パワーデバイス用ヒートシンク、発電機用回転翼及び耐食性金属部材の製造方法 |
| PL420430A1 (pl) * | 2017-02-09 | 2018-08-13 | General Electric Company | Kwalifikacja procesów obróbki plastycznej na zimno i polerowania |
| CN108193153A (zh) * | 2018-01-30 | 2018-06-22 | 上海核工程研究设计院有限公司 | 一种锆合金复合喷丸表面改性方法 |
| JP2019210502A (ja) * | 2018-06-01 | 2019-12-12 | 大同特殊鋼株式会社 | プリフォーム及びTiAl系タービンホイールの製造方法 |
| US12173652B2 (en) * | 2018-09-20 | 2024-12-24 | Safran Aircraft Engines | Acoustic management, on a turbomachine or a nacelle |
| JP7319784B2 (ja) * | 2019-01-29 | 2023-08-02 | 住友重機械工業株式会社 | 偏心揺動型減速装置、外歯歯車の製造方法 |
| CN111070104A (zh) * | 2019-12-27 | 2020-04-28 | 安庆谢德尔汽车零部件有限公司 | 一种变速器压缩弹簧抛丸处理方法 |
| CN113246030A (zh) * | 2021-05-27 | 2021-08-13 | 无锡航亚科技股份有限公司 | 一种整体叶盘的叶片喷丸方法 |
| CN114559057B (zh) * | 2022-01-27 | 2023-11-10 | 上海工程技术大学 | 一种改善增材制造金属构件疲劳性能的复合装置及方法 |
| GB202212898D0 (en) * | 2022-09-05 | 2022-10-19 | Rolls Royce Plc | Component and method of manufacturing thereof |
| CN117358778B (zh) * | 2023-12-08 | 2024-03-08 | 成都先进金属材料产业技术研究院股份有限公司 | 一种钛合金无缝管及其制备方法 |
Family Cites Families (15)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US3073022A (en) * | 1959-04-03 | 1963-01-15 | Gen Motors Corp | Shot-peening treatments |
| US4514469A (en) * | 1981-09-10 | 1985-04-30 | United Technologies Corporation | Peened overlay coatings |
| US4454740A (en) * | 1981-09-10 | 1984-06-19 | United Technologies Corporation | Method for simultaneous peening and smoothing |
| JP2994508B2 (ja) * | 1991-11-26 | 1999-12-27 | 株式会社東郷製作所 | コイルばねの製造方法 |
| KR20040083545A (ko) * | 2002-04-02 | 2004-10-02 | 가부시키가이샤 고베 세이코쇼 | 피로강도 및 내 새그성이 우수한 경인발스프링용 강선 및경인발스프링 |
| JP3857213B2 (ja) * | 2002-10-30 | 2006-12-13 | 本田技研工業株式会社 | 鋳造用金型およびその表面処理方法 |
| US7384244B2 (en) * | 2004-12-16 | 2008-06-10 | General Electric Company | Fatigue-resistant components and method therefor |
| WO2006135520A1 (en) * | 2005-06-09 | 2006-12-21 | The Regents Of The University Of California | Volumetric induction phase shift detection system for determining tissue water content properties |
| US7516547B2 (en) * | 2005-12-21 | 2009-04-14 | General Electric Company | Dovetail surface enhancement for durability |
| US8024846B2 (en) * | 2006-01-27 | 2011-09-27 | General Electric Company | Preparation of an article surface having a surface compressive texture |
| US20080221688A1 (en) * | 2007-03-09 | 2008-09-11 | Warsaw Orthopedic, Inc. | Method of Maintaining Fatigue Performance In A Bone-Engaging Implant |
| JP2009018370A (ja) * | 2007-07-11 | 2009-01-29 | Honda Motor Co Ltd | ショットピーニング処理方法及びその装置 |
| US8347683B2 (en) * | 2008-03-14 | 2013-01-08 | Varel International Ind., L.P. | Texturing of the seal surface for a roller cone rock bit |
| JP2010196817A (ja) * | 2009-02-25 | 2010-09-09 | Ntn Corp | 動力伝達軸およびその製造方法 |
| CN101530985A (zh) * | 2009-04-09 | 2009-09-16 | 上海交通大学 | 兼顾表面强化和抛光的复合喷丸处理方法 |
-
2010
- 2010-02-09 US US12/702,534 patent/US8468862B2/en active Active
-
2011
- 2011-02-07 JP JP2011023445A patent/JP5778935B2/ja active Active
- 2011-02-07 EP EP11153601.7A patent/EP2353782B1/en active Active
- 2011-02-09 CN CN2011100780086A patent/CN102189491A/zh active Pending
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP2011173236A5 (enExample) | ||
| JP2019502056A5 (enExample) | ||
| WO2012167136A3 (en) | Expandable crack inhibitors and methods of using the same | |
| TW200951295A (en) | Method for repairing turbine rotor blade | |
| JP2009134867A5 (enExample) | ||
| EP2963144A3 (en) | Abrasive coating and manufacture and use methods | |
| IN2012DE00295A (enExample) | ||
| WO2011133674A3 (en) | Changing the composition and/or density of gases inside of assemblies during manufacturing | |
| WO2013083123A8 (de) | Radfelge mit einem felgenbett aus faserverbundwerkstoff und verfahren zur herstellung | |
| JP2014529704A5 (enExample) | ||
| CN103060528A (zh) | 一种激光复合强化工艺 | |
| EP2535520A3 (en) | Method and apparatus to repair a turbomachine rotor wheel | |
| WO2013010141A3 (en) | Method and apparatus for joining screen material for minimal optical distortion | |
| JP2015534062A5 (enExample) | ||
| JP2014109274A5 (enExample) | ||
| CN205362551U (zh) | 一种芯盒排气结构 | |
| WO2013012189A3 (ko) | 로봇의 주행면 주행 가능 영역 확인 방법, 로봇 및 기록 매체 | |
| CN204054791U (zh) | 一种轻质约束阻尼板 | |
| MX388274B (es) | Metodo, proceso y planta para controlar la fabricacion de llantas para ruedas de vehiculo. | |
| JP2016503961A5 (enExample) | ||
| WO2015036917A3 (en) | Methods and kits for quantifying the removal of mock virus particles from a purified solution | |
| JP2010128987A5 (ja) | シミュレーション方法、システム、プログラム及び記憶媒体 | |
| FR2970663B1 (fr) | Finition par sablage des pieces frittees par fusion laser | |
| WO2013019732A3 (en) | Surface contouring of a weld cap and adjacent base metal using ultrasonic impact treatment | |