JP2011070892A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2011070892A5 JP2011070892A5 JP2009220519A JP2009220519A JP2011070892A5 JP 2011070892 A5 JP2011070892 A5 JP 2011070892A5 JP 2009220519 A JP2009220519 A JP 2009220519A JP 2009220519 A JP2009220519 A JP 2009220519A JP 2011070892 A5 JP2011070892 A5 JP 2011070892A5
- Authority
- JP
- Japan
- Prior art keywords
- active material
- mass
- sealed
- current collector
- buffer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
- 239000011149 active material Substances 0.000 description 5
- 239000002131 composite material Substances 0.000 description 5
- 239000000463 material Substances 0.000 description 5
- 239000011230 binding agent Substances 0.000 description 3
- 239000011248 coating agent Substances 0.000 description 3
- 238000000576 coating method Methods 0.000 description 3
- 239000011888 foil Substances 0.000 description 3
- 239000007773 negative electrode material Substances 0.000 description 3
- 239000004020 conductor Substances 0.000 description 2
- 239000011255 nonaqueous electrolyte Substances 0.000 description 2
- 229920001296 polysiloxane Polymers 0.000 description 2
- 239000000843 powder Substances 0.000 description 2
- 239000011347 resin Substances 0.000 description 2
- 229920005989 resin Polymers 0.000 description 2
- OKTJSMMVPCPJKN-UHFFFAOYSA-N Carbon Chemical compound [C] OKTJSMMVPCPJKN-UHFFFAOYSA-N 0.000 description 1
- RYGMFSIKBFXOCR-UHFFFAOYSA-N Copper Chemical compound [Cu] RYGMFSIKBFXOCR-UHFFFAOYSA-N 0.000 description 1
- 229910052799 carbon Inorganic materials 0.000 description 1
- 239000002482 conductive additive Substances 0.000 description 1
- 239000011889 copper foil Substances 0.000 description 1
- 239000011863 silicon-based powder Substances 0.000 description 1
Priority Applications (7)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2009220519A JP5035313B2 (ja) | 2009-09-25 | 2009-09-25 | リチウムイオン二次電池用負極及びその製造方法 |
| CN2010800420879A CN102576859A (zh) | 2009-09-25 | 2010-09-01 | 锂离子二次电池用负极及其制造方法 |
| EP14164918.6A EP2762523A1 (en) | 2009-09-25 | 2010-09-01 | Lithium-ion secondary battery comprising a binder |
| EP10818689.1A EP2482369A4 (en) | 2009-09-25 | 2010-09-01 | ANODE FOR USE IN A LITHIUMION SECONDARY BATTERY AND METHOD OF MANUFACTURING THEREOF |
| PCT/JP2010/065447 WO2011037013A1 (ja) | 2009-09-25 | 2010-09-01 | リチウムイオン二次電池用負極及びその製造方法 |
| US13/497,717 US8822083B2 (en) | 2009-09-25 | 2010-09-01 | Negative electrode for lithium-ion secondary battery and manufacturing process for the same |
| KR1020127005778A KR101294228B1 (ko) | 2009-09-25 | 2010-09-01 | 리튬 이온 2차 전지용 부극 및 그의 제조 방법 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2009220519A JP5035313B2 (ja) | 2009-09-25 | 2009-09-25 | リチウムイオン二次電池用負極及びその製造方法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JP2011070892A JP2011070892A (ja) | 2011-04-07 |
| JP2011070892A5 true JP2011070892A5 (enExample) | 2012-04-05 |
| JP5035313B2 JP5035313B2 (ja) | 2012-09-26 |
Family
ID=43795764
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2009220519A Expired - Fee Related JP5035313B2 (ja) | 2009-09-25 | 2009-09-25 | リチウムイオン二次電池用負極及びその製造方法 |
Country Status (6)
| Country | Link |
|---|---|
| US (1) | US8822083B2 (enExample) |
| EP (2) | EP2762523A1 (enExample) |
| JP (1) | JP5035313B2 (enExample) |
| KR (1) | KR101294228B1 (enExample) |
| CN (1) | CN102576859A (enExample) |
| WO (1) | WO2011037013A1 (enExample) |
Families Citing this family (19)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP5130273B2 (ja) * | 2009-10-14 | 2013-01-30 | 株式会社豊田自動織機 | 非水系二次電池用負極およびその製造方法 |
| JP2012221824A (ja) * | 2011-04-12 | 2012-11-12 | Sony Corp | リチウムイオン二次電池、電子機器、電動工具、電動車両および電力貯蔵システム |
| JP5664942B2 (ja) * | 2011-05-12 | 2015-02-04 | 株式会社豊田自動織機 | リチウムイオン二次電池用電極、その製造方法及びその電極を用いたリチウムイオン二次電池 |
| WO2013114788A1 (ja) * | 2012-02-02 | 2013-08-08 | Jsr株式会社 | 蓄電デバイス用電極の製造方法 |
| JP2013175315A (ja) * | 2012-02-24 | 2013-09-05 | Toyota Industries Corp | リチウムイオン二次電池および車両 |
| JP2013191331A (ja) * | 2012-03-13 | 2013-09-26 | Toyota Industries Corp | 非水電解質二次電池および車両 |
| JP5525003B2 (ja) | 2012-05-07 | 2014-06-18 | 古河電気工業株式会社 | 非水電解質二次電池用負極及びそれを用いた非水電解質二次電池 |
| JP6267910B2 (ja) * | 2012-10-05 | 2018-01-24 | 株式会社半導体エネルギー研究所 | リチウムイオン二次電池用負極の製造方法 |
| US11322745B2 (en) * | 2014-10-15 | 2022-05-03 | Semiconductor Energy Laboratory Co., Ltd. | Electrode, power storage device, electronic device, and manufacturing method of electrode |
| JP2016139521A (ja) * | 2015-01-27 | 2016-08-04 | 日産自動車株式会社 | 非水電解質二次電池 |
| US11094933B2 (en) * | 2016-07-18 | 2021-08-17 | University Of Kentucky Research Foundation | Polysiloxane binders |
| JP6874860B2 (ja) * | 2017-01-27 | 2021-05-19 | 日本電気株式会社 | シリコーンボールを含む電極及びそれを含むリチウムイオン電池 |
| CN107732156A (zh) * | 2017-11-28 | 2018-02-23 | 安徽零度新能源科技有限公司 | 一种提高锂电池负极低温性能的加工方法 |
| CN107959019A (zh) * | 2017-12-13 | 2018-04-24 | 南京红太阳新能源有限公司 | 一种石墨烯锡基硅基电池负极材料的制备 |
| CN109860562A (zh) * | 2019-02-15 | 2019-06-07 | 柔电(武汉)科技有限公司 | 一种电极浆料、柔性极片及其制备方法、柔性电池 |
| DE102019118207A1 (de) * | 2019-07-05 | 2021-01-07 | Bayerische Motoren Werke Aktiengesellschaft | Elektrode mit Abstandshaltern |
| CN110649209B (zh) * | 2019-09-26 | 2022-09-27 | 佛山科学技术学院 | 一种锂离子电池隔膜的处理方法及锂离子电池 |
| CN111584835A (zh) * | 2020-04-30 | 2020-08-25 | 汉腾新能源汽车科技有限公司 | 一种锂离子电池负极及其制备方法 |
| US11532818B2 (en) | 2020-05-29 | 2022-12-20 | Uchicago Argonne, Llc | Solvents and slurries comprising a poly(carboxylic acid) binder for silicon electrode manufacture |
Family Cites Families (10)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2832143B2 (ja) * | 1993-12-28 | 1998-12-02 | 信越化学工業株式会社 | シリコーン微粒子およびその製造方法 |
| ATE423800T1 (de) | 1999-07-15 | 2009-03-15 | Arakawa Chem Ind | Enthaltend glycidylethergruppe partielles alkoxysilan-kondensat, silanmodifiziertes harz, zusammensetzung daraus und verfahren zu deren herstellung |
| CN100367542C (zh) * | 2002-05-24 | 2008-02-06 | 日本电气株式会社 | 充电电池用的负极及使用其的充电电池 |
| JP5073167B2 (ja) * | 2004-12-27 | 2012-11-14 | 三星エスディアイ株式会社 | リチウム二次電池 |
| KR100759556B1 (ko) * | 2005-10-17 | 2007-09-18 | 삼성에스디아이 주식회사 | 음극 활물질, 그 제조 방법 및 이를 채용한 음극과 리튬전지 |
| JP2007165079A (ja) * | 2005-12-13 | 2007-06-28 | Matsushita Electric Ind Co Ltd | 非水電解質二次電池用負極とそれを用いた非水電解質二次電池 |
| KR100766967B1 (ko) * | 2006-11-20 | 2007-10-15 | 삼성에스디아이 주식회사 | 리튬 이차 전지용 전극, 및 이로부터 제조된 리튬 이차전지 |
| JP5128873B2 (ja) * | 2007-08-10 | 2013-01-23 | 株式会社豊田自動織機 | 二次電池用電極及びその製造方法 |
| CN102007627B (zh) | 2008-04-18 | 2014-04-09 | 株式会社丰田自动织机 | 锂离子二次电池用负极及其制造方法 |
| JP5130273B2 (ja) * | 2009-10-14 | 2013-01-30 | 株式会社豊田自動織機 | 非水系二次電池用負極およびその製造方法 |
-
2009
- 2009-09-25 JP JP2009220519A patent/JP5035313B2/ja not_active Expired - Fee Related
-
2010
- 2010-09-01 KR KR1020127005778A patent/KR101294228B1/ko not_active Expired - Fee Related
- 2010-09-01 US US13/497,717 patent/US8822083B2/en not_active Expired - Fee Related
- 2010-09-01 EP EP14164918.6A patent/EP2762523A1/en not_active Withdrawn
- 2010-09-01 WO PCT/JP2010/065447 patent/WO2011037013A1/ja not_active Ceased
- 2010-09-01 EP EP10818689.1A patent/EP2482369A4/en not_active Withdrawn
- 2010-09-01 CN CN2010800420879A patent/CN102576859A/zh active Pending
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP2011070892A5 (enExample) | ||
| TWI591875B (zh) | 用於薄膜電池之電芯 | |
| JP5867044B2 (ja) | 絶縁性接着層およびそれを用いた蓄電デバイス | |
| JP2011520214A5 (enExample) | ||
| JP2016517618A5 (enExample) | ||
| CN102947905B (zh) | 电化学器件用蓄电元件及其制造方法、使用了该蓄电元件的电化学器件及其制造方法 | |
| JP6522494B2 (ja) | 全固体蓄電デバイスおよびその製造方法 | |
| JP2017539051A5 (enExample) | ||
| JP2012048973A5 (enExample) | ||
| JP2010257838A5 (enExample) | ||
| WO2011090779A3 (en) | Low-cost, high power, high energy density, solid-state, bipolar metal hydride batteries | |
| RU2015144284A (ru) | Аноды для литий-ионного аккумулятора, содержащие частицы графенового углерода | |
| WO2012075423A3 (en) | Heat-resistant layer for non-aqueous and solid state battery and method of manufacturing the same | |
| CN101894937A (zh) | 锂离子电池及其正极片 | |
| JP5163026B2 (ja) | 非水電解質二次電池 | |
| CN110416630B (zh) | 全固体电池 | |
| CN206432317U (zh) | 电芯及电池 | |
| JP2016184496A5 (enExample) | ||
| CN105098249A (zh) | 柔性电池和具有其的柔性电池组 | |
| TW201248977A (en) | Battery electrode and battery | |
| CN102969539A (zh) | 一种超薄锂离子二次电池 | |
| JP2015220102A (ja) | 電池実装基板 | |
| JP2001015152A (ja) | 全固体積層電池 | |
| JP3228671U (ja) | フレキシブル電池 | |
| JP6861016B2 (ja) | リチウムイオン電池 |