JP2010177187A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2010177187A5 JP2010177187A5 JP2009274262A JP2009274262A JP2010177187A5 JP 2010177187 A5 JP2010177187 A5 JP 2010177187A5 JP 2009274262 A JP2009274262 A JP 2009274262A JP 2009274262 A JP2009274262 A JP 2009274262A JP 2010177187 A5 JP2010177187 A5 JP 2010177187A5
- Authority
- JP
- Japan
- Prior art keywords
- layer
- ysz
- volume
- sintering
- porosity
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
- 229910001233 yttria-stabilized zirconia Inorganic materials 0.000 description 6
- 229910052760 oxygen Inorganic materials 0.000 description 4
- 239000001301 oxygen Substances 0.000 description 4
- 238000005245 sintering Methods 0.000 description 3
- QVGXLLKOCUKJST-UHFFFAOYSA-N atomic oxygen Chemical compound [O] QVGXLLKOCUKJST-UHFFFAOYSA-N 0.000 description 2
- 230000006698 induction Effects 0.000 description 2
- 229910002075 lanthanum strontium manganite Inorganic materials 0.000 description 2
- 239000000463 material Substances 0.000 description 2
- -1 oxygen ion Chemical class 0.000 description 2
- 239000000843 powder Substances 0.000 description 2
- FVROQKXVYSIMQV-UHFFFAOYSA-N [Sr+2].[La+3].[O-][Mn]([O-])=O Chemical compound [Sr+2].[La+3].[O-][Mn]([O-])=O FVROQKXVYSIMQV-UHFFFAOYSA-N 0.000 description 1
- 239000002131 composite material Substances 0.000 description 1
- 239000003792 electrolyte Substances 0.000 description 1
- 239000002002 slurry Substances 0.000 description 1
- 239000007787 solid Substances 0.000 description 1
- 238000005507 spraying Methods 0.000 description 1
- 239000000725 suspension Substances 0.000 description 1
Applications Claiming Priority (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| DKPA200801704 | 2008-12-03 | ||
| DKPA200801704 | 2008-12-03 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JP2010177187A JP2010177187A (ja) | 2010-08-12 |
| JP2010177187A5 true JP2010177187A5 (enExample) | 2013-01-24 |
| JP5591526B2 JP5591526B2 (ja) | 2014-09-17 |
Family
ID=41698263
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2009274262A Expired - Fee Related JP5591526B2 (ja) | 2008-12-03 | 2009-12-02 | 固体酸化物セル及び固体酸化物セルスタック |
Country Status (10)
| Country | Link |
|---|---|
| US (1) | US8304128B2 (enExample) |
| EP (1) | EP2194597B1 (enExample) |
| JP (1) | JP5591526B2 (enExample) |
| KR (1) | KR20100063667A (enExample) |
| CN (1) | CN101752586B (enExample) |
| AU (1) | AU2009243474B2 (enExample) |
| CA (1) | CA2686846A1 (enExample) |
| DK (1) | DK2194597T3 (enExample) |
| ES (1) | ES2456821T3 (enExample) |
| RU (1) | RU2521874C2 (enExample) |
Families Citing this family (21)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| WO2007145015A1 (ja) * | 2006-06-16 | 2007-12-21 | Sharp Kabushiki Kaisha | 正極、その製造方法及びその正極を用いたリチウム二次電池 |
| KR101253956B1 (ko) | 2010-12-28 | 2013-04-16 | 주식회사 포스코 | 금속지지체형 고체산화물 연료전지의 제조방법 |
| ES2655543T3 (es) * | 2011-10-07 | 2018-02-20 | Saint-Gobain Ceramics & Plastics Inc. | Método para formar una celda combustible de un óxido sólido |
| JP5622754B2 (ja) * | 2012-01-05 | 2014-11-12 | 三菱重工業株式会社 | 固体電解質型燃料電池の製造方法及び固体電解質型燃料電池 |
| WO2014012673A1 (en) | 2012-07-19 | 2014-01-23 | Technical University Of Denmark | Solid oxide cell oxygen electrode with enhanced durability |
| KR20140131441A (ko) * | 2013-05-03 | 2014-11-13 | 한국생산기술연구원 | 고체산화물 연료전지용 고체전해질의 제조방법 및 단위셀의 제조방법 |
| JP2015213050A (ja) * | 2014-04-14 | 2015-11-26 | パナソニックIpマネジメント株式会社 | 固体酸化物燃料電池および電気分解デバイス |
| CN104037425B (zh) * | 2014-05-23 | 2016-07-20 | 景德镇陶瓷学院 | 一种中温sofc平板阳极支撑型单电池阳极结构及其制备方法 |
| GB2524638B (en) * | 2015-02-06 | 2016-04-06 | Ceres Ip Co Ltd | Electrolyte forming process |
| KR102054537B1 (ko) * | 2015-08-26 | 2019-12-10 | 주식회사 엘지화학 | 고체 산화물 연료전지의 제조방법, 고체 산화물 연료전지 및 이를 포함하는 전지 모듈 |
| DE112017005364T5 (de) | 2016-10-24 | 2019-07-18 | Precision Combustion, Inc. | Regenerativer festoxidstapel |
| JP6290471B1 (ja) * | 2017-02-16 | 2018-03-07 | 日本特殊陶業株式会社 | 電気化学反応単セルおよび電気化学反応セルスタック |
| KR102158619B1 (ko) * | 2018-08-31 | 2020-09-25 | 대전대학교 산학협력단 | 전기화학식 산소발생기를 위한 산화물 전극이 도포된 고체전해질 멤브레인 및 이의 제조방법 |
| CN109768292B (zh) * | 2019-03-15 | 2021-09-28 | 福州大学 | 一种固体氧化物燃料电池电化学极化原位制备阳极的方法 |
| CN114127339B (zh) | 2019-07-17 | 2024-10-22 | 托普索公司 | 对用于固体氧化物电池堆应用的铁素体钢互连件进行铬升级的方法 |
| AU2021255897A1 (en) * | 2020-04-15 | 2022-11-03 | Fundació Institut Català D'investigació Química (Iciq) | Method of preparation of electrode for electrocatalysis |
| US11837766B2 (en) | 2020-11-09 | 2023-12-05 | Advanced Manufacturing LLC | System and method for continuous fabrication of graded structured units using additive manufacturing |
| CN112751041B (zh) * | 2021-01-17 | 2021-12-03 | 大连理工大学 | 一种制备NiO/磷灰石型硅酸镧亚微-纳米多孔阳极功能层的方法 |
| AU2022268645A1 (en) | 2021-05-06 | 2023-10-12 | Topsoe A/S | Interconnect for solid oxide cell (soc) |
| CN116072892B (zh) * | 2023-01-16 | 2024-04-30 | 福州大学 | 表面重构改进含Ba复合氧电极的方法 |
| CN115939419B (zh) * | 2023-02-09 | 2025-02-11 | 华中科技大学 | 一种固体氧化物电池修饰电极的原位合成方法 |
Family Cites Families (16)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH03112057A (ja) * | 1989-09-27 | 1991-05-13 | Osaka Gas Co Ltd | 固体電解質燃料電池 |
| JPH05190183A (ja) | 1992-01-13 | 1993-07-30 | Ngk Insulators Ltd | 固体電解質型燃料電池 |
| DK171621B1 (da) * | 1993-03-01 | 1997-02-24 | Risoe Forskningscenter | Fastoxidbrændselscelle med katode af LSM og YSZ |
| US5543239A (en) * | 1995-04-19 | 1996-08-06 | Electric Power Research Institute | Electrode design for solid state devices, fuel cells and sensors |
| US6682842B1 (en) | 1999-07-31 | 2004-01-27 | The Regents Of The University Of California | Composite electrode/electrolyte structure |
| RU2280297C2 (ru) * | 2000-11-09 | 2006-07-20 | Трастиз Оф Дзе Юниверсити Оф Пенсильвания | Применение серосодержащих топлив для прямоокислительных топливных элементов |
| KR100424194B1 (ko) | 2001-11-01 | 2004-03-24 | 한국과학기술연구원 | 다공성 이온 전도성 세리아 막 코팅으로 삼상 계면이 확장된 미세구조의 전극부 및 그의 제조방법 |
| US6958196B2 (en) | 2003-02-21 | 2005-10-25 | Trustees Of The University Of Pennsylvania | Porous electrode, solid oxide fuel cell, and method of producing the same |
| CN1802769A (zh) * | 2003-06-09 | 2006-07-12 | 圣戈本陶瓷及塑料股份有限公司 | 堆叠支撑的固态氧化物燃料电池 |
| RU2356132C2 (ru) * | 2004-06-10 | 2009-05-20 | Текникал Юниверсити Оф Денмарк | Твердооксидный топливный элемент |
| RU2403655C9 (ru) | 2005-04-21 | 2011-04-20 | Члены Правления Университета Калифорнии | Инфильтрация исходного материала и способ покрытия |
| JP2006344543A (ja) * | 2005-06-10 | 2006-12-21 | Tokyo Electric Power Co Inc:The | 固体酸化物形燃料電池用セルの製造方法 |
| JP5190183B2 (ja) | 2006-06-09 | 2013-04-24 | 三井農林株式会社 | 茶飲料のフロック発生抑制剤 |
| EP1928049A1 (en) | 2006-11-23 | 2008-06-04 | Technical University of Denmark | Thin solid oxide cell |
| EP1930974B1 (en) * | 2006-11-23 | 2012-03-21 | Technical University of Denmark | Method for the manufacture of reversible solid oxide cells |
| KR100793155B1 (ko) * | 2006-12-20 | 2008-01-10 | 주식회사 포스코 | 고체산화물 연료전지용 단위전지의 제조방법 |
-
2009
- 2009-11-23 DK DK09014539.2T patent/DK2194597T3/da active
- 2009-11-23 EP EP09014539.2A patent/EP2194597B1/en not_active Not-in-force
- 2009-11-23 ES ES09014539.2T patent/ES2456821T3/es active Active
- 2009-11-30 US US12/627,082 patent/US8304128B2/en not_active Expired - Fee Related
- 2009-12-02 AU AU2009243474A patent/AU2009243474B2/en not_active Ceased
- 2009-12-02 RU RU2009144531/07A patent/RU2521874C2/ru not_active IP Right Cessation
- 2009-12-02 KR KR1020090118487A patent/KR20100063667A/ko not_active Withdrawn
- 2009-12-02 JP JP2009274262A patent/JP5591526B2/ja not_active Expired - Fee Related
- 2009-12-02 CA CA2686846A patent/CA2686846A1/en not_active Abandoned
- 2009-12-03 CN CN200910252698.5A patent/CN101752586B/zh not_active Expired - Fee Related
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP2010177187A5 (enExample) | ||
| JP6800297B2 (ja) | 電気化学素子、固体酸化物形燃料電池セル、およびこれらの製造方法 | |
| AU2004216002B2 (en) | Porous electrode, solid oxide fuel cell, and method of producing the same | |
| TWI577077B (zh) | 高溫燃料電池用的陽極及其製造方法 | |
| JP6671132B2 (ja) | 電気化学素子、固体酸化物形燃料電池セル、およびこれらの製造方法 | |
| JP2011518416A5 (enExample) | ||
| JP5895108B1 (ja) | 燃料電池 | |
| CN103828098B (zh) | 存储元件以及用于制造存储元件的方法 | |
| TW200905950A (en) | Interlocking structure for high temperature electrochemical device and method for making the same | |
| JP6644363B2 (ja) | 電気化学素子、固体酸化物形燃料電池セル、およびこれらの製造方法 | |
| CN102917806A (zh) | 制造具有多孔金属层的电化学装置的方法 | |
| WO2009031036A3 (en) | Metal oxide-coated positive electrode active material, lithium secondary battery, and manufacture method therefor | |
| JP2014510014A5 (enExample) | ||
| WO2017002559A1 (ja) | 燃料電池 | |
| Choi et al. | Low temperature preparation and characterization of solid oxide fuel cells on FeCr-based alloy support by aerosol deposition | |
| JP5486748B2 (ja) | 燃料電池セル | |
| JP2008004422A (ja) | 固体酸化物形燃料電池用電極及び固体酸化物形燃料電池並びにその製造方法 | |
| Choi et al. | Low temperature fabrication of nano-structured porous LSM–YSZ composite cathode film by aerosol deposition | |
| JP2004532499A (ja) | 高圧酸素製造のための酸化物イオン導電性セラミック膜構造/微細構造 | |
| Son et al. | Effect of fabrication parameters on coating properties of tubular solid oxide fuel cell electrolyte prepared by vacuum slurry coating | |
| US20140193743A1 (en) | Method for the densification of ceramic layers, especially ceramic layers within solid oxide cell (soc) technology, and products obtained by the method | |
| JP2011510432A (ja) | 電流コレクタ構造 | |
| CN109478651A (zh) | 电化学电池 | |
| WO2014126716A8 (en) | Electrolyte formation for a solid oxide fuel cell device | |
| JP6134085B1 (ja) | 電気化学セル |