JP2006318929A5 - - Google Patents

Download PDF

Info

Publication number
JP2006318929A5
JP2006318929A5 JP2006199631A JP2006199631A JP2006318929A5 JP 2006318929 A5 JP2006318929 A5 JP 2006318929A5 JP 2006199631 A JP2006199631 A JP 2006199631A JP 2006199631 A JP2006199631 A JP 2006199631A JP 2006318929 A5 JP2006318929 A5 JP 2006318929A5
Authority
JP
Japan
Prior art keywords
positive electrode
electrode active
active material
secondary battery
granulation
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2006199631A
Other languages
English (en)
Other versions
JP2006318929A (ja
JP4919147B2 (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP2006199631A priority Critical patent/JP4919147B2/ja
Priority claimed from JP2006199631A external-priority patent/JP4919147B2/ja
Publication of JP2006318929A publication Critical patent/JP2006318929A/ja
Publication of JP2006318929A5 publication Critical patent/JP2006318929A5/ja
Application granted granted Critical
Publication of JP4919147B2 publication Critical patent/JP4919147B2/ja
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Links

Claims (4)

  1. 少なくともリチウム塩と遷移金属酸化物、酸化コバルト及び/又は水酸化アルミニウム、酸化アルミニウム等を溶媒中へ分散させ、メジアン粒径D50が1μm以下となるよう粉砕混合し、この原料スラリーを乾燥させ、造粒し顆粒状にした後、大気中、窒素雰囲気中あるいは酸素雰囲気中にて800℃〜1050℃の温度で焼成を行い、組成式Li a Mn x Ni y z 2 (X=Co、Alのうち少なくとも一種)で表され、1≦a≦1.2、0≦x≦0.65、0.35≦y≦1、0≦z≦0.65の範囲でかつx+y+z=1の層状岩塩構造を有する複合酸化物を得て、(タップ密度/真密度)×100[%]で表される充填性が25%以上55%未満、且つX線回折パタ−ンから得られる各回折ピ−クの積分幅からHall法によって測定した結晶子の大きさが400Å以上、850Å以下である正極活物質を得ることを特徴とする非水系リチウム二次電池用正極活物質の製造方法。
  2. 少なくともリチウム塩と遷移金属酸化物、酸化コバルト及び/又は水酸化アルミニウム、酸化アルミニウム等を溶媒中へ分散させ、メジアン粒径D50が0.5〜1μmとなるよう粉砕混合し、この原料スラリーを乾燥させ、造粒し顆粒状にした後、大気中、窒素雰囲気中あるいは酸素雰囲気中にて900℃〜1000℃の温度で焼成を行い、組成式Li a Mn x Ni y z 2 (X=Co、Alのうち少なくとも一種)で表され、1≦a≦1.2、0.2≦x≦0.5、0.35≦y≦0.8、0≦z≦0.45の範囲でかつx+y+z=1の層状岩塩構造を有する複合酸化物を得て、(タップ密度/真密度)×100[%]で表される充填性が25%以上50%未満、且つX線回折パタ−ンから得られる各回折ピ−クの積分幅からHall法によって測定した結晶子の大きさが600Å以上、760Å以下である正極活物質を得ることを特徴とする非水系リチウム二次電池用正極活物質の製造方法。
  3. 前記焼成の後、解砕し、その後大気中、窒素雰囲気中あるいは酸素雰囲気中にて400℃〜900℃の温度で熱処理を行うことを特徴とする請求項1または2に記載の非水系リチウム二次電池用正極活物質の製造方法。
  4. 前記解砕は、有機材料でコ−トしたボ−ルをメディアに用いて行うことを特徴とする請求項1〜3の何れか1項に記載の非水系リチウム二次電池用正極活物質の製造方法。
JP2006199631A 2003-03-25 2006-07-21 非水系リチウム二次電池用正極活物質の製造方法 Expired - Lifetime JP4919147B2 (ja)