DE324919C - Verfahren zur Darstellung von Pinakon - Google Patents
Verfahren zur Darstellung von PinakonInfo
- Publication number
- DE324919C DE324919C DE1917324919D DE324919DD DE324919C DE 324919 C DE324919 C DE 324919C DE 1917324919 D DE1917324919 D DE 1917324919D DE 324919D D DE324919D D DE 324919DD DE 324919 C DE324919 C DE 324919C
- Authority
- DE
- Germany
- Prior art keywords
- pinacon
- representation
- parts
- acetone
- electrodes
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
- Verfahren zur Darstellung von Pinakon. Durch das Patent 3o6523- ist ein Verfahren zur Darstellung von Pinakon geschützt. Es besteht darin, daß man bei der elektrolytischen Reduktion von Aceton in saurer Lösung als Elektrodenmaterial Blei mit einem Kupfergehalt von etwa zwei Prozent und mehr verwendet.
- Es wurde nun die bemerkenswerte Beobachtung gemacht, daß ganz allgemein Mischungen oder Verbindungen zweier oder mehrerer Metalle miteinander sich als Elektrodenmaterial für diese Behandlung vorzüglich eignen. Ihre @Terwendung hat den Vorteil, daß sie leichter herstellbar sind und größere Homogenität und damit eine gleichrnäßigere Wirkung als die Elektroden des Patents 3o6523 besitzen. Beispiel. ioo Teile Aceton werden mit ioo Teilen 25prozentiger Schwefelsäure gemischt und an einer Kathode aus 9o Teilen Blei und zo Teilen Zinn elektrolytisch behandelt. Es wird zehnmal mehr Pinakon als Isopropylalkohol gebildet. Die Bildung von metallorganischen Verbindungen unterbleibt vollkommen.
- Ähnlich verhalten sich - Messing- oder Bronzeelektroden oder andere -.,\!hetallleg ierungen.
Claims (1)
- PATRNT-ANsPRUCH Abänderung des durch das Patent 3o6523, Zusatz zum Patent 252759 geschützten- Verfahrens zur katalytischen Reduktion von Aceton zu Pinakon in saurer Lösung, dadurch gekennzeichnet, daß man als Elektroden andere als die in dem Patent 3o6523 erwähnten Metalllegierungen verwendet.