CN1563127A CN 200410014454 CN200410014454A CN1563127A CN 1563127 A CN1563127 A CN 1563127A CN 200410014454 CN200410014454 CN 200410014454 CN 200410014454 A CN200410014454 A CN 200410014454A CN 1563127 A CN1563127 A CN 1563127A
Authority
CN
China
Prior art keywords
pentadiene
raw material
condition
under
petroleum resin
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 200410014454
Other languages
English (en)
Inventor
倪才国
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 200410014454 priority Critical patent/CN1563127A/zh
Publication of CN1563127A publication Critical patent/CN1563127A/zh
Pending legal-status Critical Current

Links

Landscapes

  • Addition Polymer Or Copolymer, Post-Treatments, Or Chemical Modifications (AREA)

Abstract

本发明涉及化工领域,尤其是一种间戊二烯石油树脂的制备方法,具有如下工艺流程:a.催化聚合,以间戊二烯、C5为原料,以C5轻油为溶剂,用三氯化铝作催化剂在70℃~80℃,压力1~2Kg条件下催化聚合,催化剂三氯化铝与原料的重量比为0.7~0.8wt%;b.脱除催化剂,用片碱在150℃~160℃条件下脱除催化剂三氯化铝,片碱与原料的重量比为0.6~0.7wt%;c.合成,在220℃~240℃,真空条件下汽提合成间戊二烯石油树脂;d.造粒,用本发明的间戊二烯石油树脂的制备方法,制得产品软化点高,熔融粘度高。

Description

间戊二烯石油树脂的制备方法
技术领域
本发明涉及化工领域,尤其是一种间戊二烯石油树脂的制备方法。
背景技术
碳五系列石油树脂为由石油裂解副产品,碳五馏份中间戊二烯等组份而成。碳五系列石油树脂用途广泛,可用于制造压敏粘合剂、热熔胶熔剂、热熔涂料封装材料、热熔交通标志涂料、橡胶增粘剂、油漆和清漆、印刷油墨等。中国专利CN1448417A公开了一种高软化点、强熔融粘度C5间戊二烯石油树脂的制备方法,以C5间戊二烯富集物为原料,C5间戊二烯含量为65~80wt%,以苯、甲苯或二甲苯为反应溶剂,在催化剂三氯化铝的存在下聚合制得间戊二烯石油树脂产品,聚合反应在密闭的反应器中进行,聚合温度为40℃~80℃,优选聚合温度45℃~70℃,聚合时间为4~8小时,优选聚合时间为6~8小时,反应原料在整个反应时间内匀速加入反应器中。我们通过反复试验计算,在压力在1~2Kg,聚合温度70℃~80℃条件下,聚合时间5~6小时,制得产品软化点更高,熔融粘度更强。
发明内容
为了克服现有工艺的不足,本发明提供了一种间戊二烯石油树脂的制备方法,利用该工艺所制得的间戊二烯石油树脂,熔融粘度强、软化点高。
本发明解决其技术问题所采用的技术方案是:一种C5间戊二烯石油树脂的制备方法,具有如下工艺流程:a、催化聚合,以C5间戊二烯为原料,以C5轻油为溶剂,用三氯化铝作催化剂在70℃~80℃,压力1~2Kg条件下催化聚合,催化剂三氯化铝与原料的重量比为0.7~0.8wt%;b、脱除催化剂,用片碱在150℃~160℃条件下脱除催化剂三氯化铝,片碱与原料的重量比为0.6~0.7wt%;c、合成,在220℃~240℃,真空条件下汽提合成C5间戊二烯石油树脂;d、造粒。
本发明的有益效果是,用本发明的间戊二烯石油树脂的制备方法,制得产品软化点高,熔融粘度高。
具体实施方式
C5间戊二烯石油树脂的制备方法:
先将三氯化铝15Kg与200Kg C5轻油溶剂在反应釜混合均匀,开始间戊二烯、C5 2100Kg滴加反应升温,其中间戊二烯含量65~70wt%,保持温度在70℃~80℃,压力在1~2Kg条件下反应4~6小时,保温1小时,把反应好的半成品压到中和釜,加碱液水(片碱13Kg)中和釜反应沉淀,开始脱去催化剂三氯化铝,经过三次水洗到PH值6-7止,水洗完毕,把中和釜的半成品树脂液压到树脂计量管,开始树脂液回入蒸馏釜,脱去溶剂,温度在150℃~160℃,后自动流入到汽提釜,经过通蒸汽,真空,温度在220℃~240℃自动出成品树脂,造粒包装。

Claims (1)

1.一种间戊二烯石油树脂的制备方法,其特征在于具有如下工艺流程:a、催化聚合,以间戊二烯、C5为原料,以C5轻油为溶剂,用三氯化铝作催化剂在70℃~80℃,压力1~2Kg条件下催化聚合,催化剂三氯化铝与原料的重量比为0.7~0.8wt%;b、脱除催化剂,用片碱在150℃~160℃条件下脱除催化剂三氯化铝,片碱与原料的重量比为0.6~0.7wt%;c、合成,在220℃~240℃,真空条件下汽提合成间戊二烯石油树脂;d、造粒。
CN 200410014454 2004-03-23 2004-03-23 间戊二烯石油树脂的制备方法 Pending CN1563127A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 200410014454 CN1563127A (zh) 2004-03-23 2004-03-23 间戊二烯石油树脂的制备方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 200410014454 CN1563127A (zh) 2004-03-23 2004-03-23 间戊二烯石油树脂的制备方法

Publications (1)

Publication Number Publication Date
CN1563127A true CN1563127A (zh) 2005-01-12

Family

ID=34478377

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 200410014454 Pending CN1563127A (zh) 2004-03-23 2004-03-23 间戊二烯石油树脂的制备方法

Country Status (1)

Country Link
CN (1) CN1563127A (zh)

Cited By (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN100404568C (zh) * 2005-06-28 2008-07-23 中国石油天然气集团公司 一种碳五加氢石油树脂的制备方法
CN101134797B (zh) * 2006-09-01 2010-05-12 上海江鸟实业有限公司 一种高档间戊二烯石油树脂生产工艺
CN102010481A (zh) * 2010-11-18 2011-04-13 中国海洋石油总公司 一种浅色度间戊二烯石油树脂的制备方法
CN101497677B (zh) * 2008-12-11 2012-01-11 宁波职业技术学院 一种用甲基四氢苯酐生产废液制备c5石油树脂的方法
CN103881027A (zh) * 2012-12-19 2014-06-25 抚顺伊科思新材料有限公司 间戊二烯石油树脂的合成方法

Cited By (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN100404568C (zh) * 2005-06-28 2008-07-23 中国石油天然气集团公司 一种碳五加氢石油树脂的制备方法
CN101134797B (zh) * 2006-09-01 2010-05-12 上海江鸟实业有限公司 一种高档间戊二烯石油树脂生产工艺
CN101497677B (zh) * 2008-12-11 2012-01-11 宁波职业技术学院 一种用甲基四氢苯酐生产废液制备c5石油树脂的方法
CN102010481A (zh) * 2010-11-18 2011-04-13 中国海洋石油总公司 一种浅色度间戊二烯石油树脂的制备方法
CN103881027A (zh) * 2012-12-19 2014-06-25 抚顺伊科思新材料有限公司 间戊二烯石油树脂的合成方法
CN103881027B (zh) * 2012-12-19 2017-03-29 抚顺伊科思新材料有限公司 间戊二烯石油树脂的合成方法

Similar Documents

Publication Publication Date Title
CN101899157B (zh) 一种mq硅树脂的制备方法
CN111154071B (zh) 多官能环氧植物油基uv固化预聚物及其制备方法和应用
CN104140763B (zh) 浅色松香季戊四醇酯的制备方法
CN107793319A (zh) 一种2,6‑二乙基苯胺的制备工艺
CN101503495B (zh) 一种α-蒎烯改性C5石油树脂的制备方法
CN101659733A (zh) 浅色度c9石油树脂的合成方法
CN1563127A (zh) 间戊二烯石油树脂的制备方法
CN101759559A (zh) 一种制备低含水量、低酸度高纯乳酸正丙酯的方法
CN102718927A (zh) 一种古马隆树脂的生产方法
CN101724174A (zh) 一种制备防老剂rd的方法
CN103254073B (zh) 高纯(双)季戊四醇丙烯酸非完全酯化产物的制备方法
CN106188400B (zh) 一种苯乙烯系多元共聚高分子材料的制备工艺
CN102344751A (zh) 以松脂为原料同时制备萜烯松香树脂和聚合松香的方法
CN102382261A (zh) 浅色度芳香族石油树脂的制备方法
CN102382221A (zh) 水芹烯树脂的生产工艺
CN109956849B (zh) 一种制备乙二醇二乙酸酯和仲丁醇的方法及催化体系和装置
CN101735052B (zh) 一种制备衣康酸二正丁酯的方法
CN201999878U (zh) 新型古马隆树脂生产装置
CN102351990A (zh) 一种间戊二烯石油树脂的制备方法
CN101735051B (zh) 一种制备衣康酸二异辛酯的方法
CN100482704C (zh) 一种双环戊二烯酚型树脂的脱色方法
CN104072666A (zh) 一种液体间戊二烯石油树脂的制备方法
CN111072484A (zh) 受阻酚抗氧剂1010的优化制备方法
CN1256354C (zh) 一种用于聚氯乙烯悬浮聚合反应釜的防粘釜剂的制造方法
CN1156152A (zh) 石油树脂生产中的非水脱除三氟化硼方法

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C02 Deemed withdrawal of patent application after publication (patent law 2001)
WD01 Invention patent application deemed withdrawn after publication