CN111516409A - 电梯门套的表面修复工艺 - Google Patents
电梯门套的表面修复工艺 Download PDFInfo
- Publication number
- CN111516409A CN111516409A CN202010374124.1A CN202010374124A CN111516409A CN 111516409 A CN111516409 A CN 111516409A CN 202010374124 A CN202010374124 A CN 202010374124A CN 111516409 A CN111516409 A CN 111516409A
- Authority
- CN
- China
- Prior art keywords
- elevator door
- door pocket
- transfer medium
- repaired
- pattern
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明提出一种电梯门套的表面修复工艺,所述电梯门套的表面修复工艺包括以下步骤:涂胶,在作为待修复件的电梯门套的表面的修复区域和/或转印介质的表面涂抹粘接剂;以及加压,使所述转印介质覆盖所述修复区域的表面,并且按压所述转印介质,使所述转印介质紧密贴合所述修复区域,使所述转印介质表面的纹理或图案转印到所述待修复件,从而在所述待修复件形成纹理或图案;分离,使所述转印介质与所述待修复件分离。通过采用上述技术方案,采用转印的方式在修复区域形成花纹,可以方便地进行表面修复,覆盖电梯门套表面的划痕等缺陷。
Description
技术领域
本发明属于表面修复领域,具体涉及一种电梯门套的表面修复工艺
背景技术
在现有技术中,例如电梯门套、门板等部件的表面在使用过程中容易磕碰产生划痕,这些划痕会影响美观。在现有技术中,采用抛光的方式对划痕进行修复,修复过程复杂修复所用的时间较长,而且操作难度较高需要专业人员操作。
发明内容
基于上述现有技术的问题,本发明旨在提出一种电梯门套的表面修复工艺,可以方便快捷地修复电梯门套表面的划痕等缺陷。
本发明提出一种电梯门套的表面修复工艺,所述电梯门套的表面修复工艺包括以下步骤:
涂胶,在作为待修复件的电梯门套的表面的修复区域和/或转印介质的表面涂抹粘接剂;以及
加压,使所述转印介质覆盖所述修复区域的表面,并且按压所述转印介质,使所述转印介质紧密贴合所述修复区域,使所述转印介质表面的纹理或图案转印到所述待修复件,从而在所述待修复件形成纹理或图案;
分离,使所述转印介质与所述待修复件分离。
优选地,所述电梯门套的表面修复工艺还包括打磨,即,将所述待修复件的修复区域打磨平整,去除毛刺。
优选地,所述电梯门套的表面修复工艺还包括清洁,即,将所述修复区域的打磨后的表面清理干净。
优选地,所述电梯门套的表面修复工艺还包括:在所述转印介质中选择表面的纹理或图案与修复区域的纹理或图案吻合的部分并将其剪裁下来以供使用。
优选地,所述梯门套的表面修复工艺在常温环境中进行。
优选地,按压所述转印介质的时间大于60秒。
优选地,按压所述转印介质的压力均匀地施加于所述转印介质的表面各处。
优选地,所述转印介质为转印纸或者转印膜。
优选地,所述电梯门套的表面由大理石、人造大理石或瓷砖形成。
优选地,所述转印介质包括基底和附着于所述基底的纹理或图案,
所述基底与所述纹理或图案的附着力小于所述纹理或图案与所述粘接剂的附着力。
通过采用上述技术方案,采用转印的方式在修复区域形成花纹,可以方便地进行表面修复,覆盖电梯门套表面的划痕等缺陷。
具体实施方式
下面描述本发明的示例性实施方式。应当理解,这些具体的说明仅用于示教本领域技术人员如何实施本发明,而不用于穷举本发明的所有可行的方式,也不用于限制本发明的范围。
本发明提出一种电梯门套的表面修复工艺,该表面修复工艺可以用于修复特别是电梯门套的待修复件的例如磕碰产生的划痕等缺陷,电梯门套可以包括由大理石、人造大理石或瓷砖等材料形成的表面。
该表面修复工艺可以包括以下步骤:
(1)打磨,将例如电梯门套的待修复件的修复区域打磨平整,去除毛刺。
(2)清洁,将修复区域的表面的异物清除干净,例如使用纸巾或布将打磨时残留的碎屑或颗粒擦拭干净。
(3)涂胶,在待修复件的修复区域和/或转印介质的表面涂抹粘接剂。转印介质可以是转印纸或者转印膜。转印介质包括由纸或塑料膜等制成的基底,附着于该基底的例如油墨可以印刷或喷涂形成纹理或图案,纹理或图案与基底的附着力小于纹理或图案与粘接剂的附着力。粘接剂能够将转印介质上的油墨粘附到待修复件上,从而使待修复件上形成纹理或图案,覆盖待修复件划痕等缺陷。
优选地,在转印介质中选择表面的纹理或图案与修复区域的纹理或图案吻合的部分并将其剪裁下来使用。能够保证转印形成的纹理或图案和修复区域周围的纹理或图案是连续的。应当理解,这里的修复区域的纹理或图案是指修复区域损伤之前具有的纹理或图案。在一种方式中,可以通过修复区域周围的纹理或图案来推测或得出修复区域的纹理或图案。
(4)加压,使转印介质覆盖修复区域的表面,并且按压转印介质,使转印介质紧密贴合于待修复件。按压转印介质和待修复件的时间优选大于60秒,例如按压时间为3分钟,按压转印介质的压力优选大于5kg,例如按压压力为10kg。通过加压使转印介质上的纹理或图案转印至待修复件。按压转印介质的压力均匀地施加于转印介质的表面各处,使转印介质上的纹理或图案能够完整地转印至待修复件。按压转印介质时候,如果转印介质的面积较小可以直接用手按压,如果转印介质的面积较大可以借助工件例如平板来进行按压。
可以理解,按压可以使转印介质紧密贴合在待修复件的表面,转印介质上的纹理或图案能够完整地转印到待修复件上,在待修复件上形成纹理或图案。
修复的过程中,例如加压在常温环境中进行即可,例如10摄氏度至40摄氏度,无需进行加热就可以使转印介质上的纹理或图案转印至待修复件,从而方便进行修复。
(5)分离,使转印介质与待修复件分离,完成表面修复的工作。
通过上述表面修复工艺来修复例如电梯门套的待修复件可以方便快捷地修复待修复件表面的划痕等缺陷,不需要专业人员也可以完成。
Claims (10)
1.一种电梯门套的表面修复工艺,其特征在于,所述电梯门套的表面修复工艺包括以下步骤:
涂胶,在作为待修复件的电梯门套的表面的修复区域和/或转印介质的表面涂抹粘接剂;以及
加压,使所述转印介质覆盖所述修复区域的表面,并且按压所述转印介质,使所述转印介质紧密贴合所述修复区域,使所述转印介质表面的纹理或图案转印到所述待修复件,从而在所述待修复件形成纹理或图案;
分离,使所述转印介质与所述待修复件分离。
2.根据权利要求1所述的电梯门套的表面修复工艺,其特征在于,所述电梯门套的表面修复工艺还包括打磨,即,将所述待修复件的修复区域打磨平整,去除毛刺。
3.根据权利要求2所述的电梯门套的表面修复工艺,其特征在于,所述电梯门套的表面修复工艺还包括清洁,即,将所述修复区域的打磨后的表面清理干净。
4.根据权利要求1所述的电梯门套的表面修复工艺,其特征在于,所述电梯门套的表面修复工艺还包括:在所述转印介质中选择表面的纹理或图案与修复区域的纹理或图案吻合的部分并将其剪裁下来以供使用。
5.根据权利要求1所述的电梯门套的表面修复工艺,其特征在于,所述梯门套的表面修复工艺在常温环境中进行。
6.根据权利要求1所述的电梯门套的表面修复工艺,其特征在于,按压所述转印介质的时间大于60秒。
7.根据权利要求1所述的电梯门套的表面修复工艺,其特征在于,按压所述转印介质的压力均匀地施加于所述转印介质的表面各处。
8.根据权利要求1所述的电梯门套的表面修复工艺,其特征在于,所述转印介质为转印纸或者转印膜。
9.根据权利要求1所述的电梯门套的表面修复工艺,其特征在于,所述电梯门套的表面由大理石、人造大理石或瓷砖形成。
10.根据权利要求1所述的电梯门套的表面修复工艺,其特征在于,所述转印介质包括基底和附着于所述基底的纹理或图案,
所述基底与所述纹理或图案的附着力小于所述纹理或图案与所述粘接剂的附着力。