CN109776834A - 一种防腐抑菌的保鲜膜 - Google Patents
一种防腐抑菌的保鲜膜 Download PDFInfo
- Publication number
- CN109776834A CN109776834A CN201811499679.8A CN201811499679A CN109776834A CN 109776834 A CN109776834 A CN 109776834A CN 201811499679 A CN201811499679 A CN 201811499679A CN 109776834 A CN109776834 A CN 109776834A
- Authority
- CN
- China
- Prior art keywords
- parts
- preservative film
- antiseptic
- raw material
- inhibiting bacteria
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明提出了一种防腐抑菌的保鲜膜,其制备方法为:(1)按重量份数计称取聚丙烯80‑112份、氧化铜5‑7份、氧化锌20‑28份、石墨烯1‑3份、醋酸5‑8份、甘油3‑5份和壳聚糖5‑10份作为原材料;(2)将原材料混合均匀后,挤出机中,熔融挤出后吹塑成基膜;(3)在基膜的上表面和下表面上分别喷涂一层保护膜即可得到保鲜膜。本发明能够有效延长水果,蔬菜的保鲜时间。
Description
技术领域
本发明涉及一种保鲜膜,特别涉及一种防腐抑菌的保鲜膜。
背景技术
塑料保鲜袋是我们大家所常使用的一种用来防止食品受外界的污染,延长食品的保鲜时间的产品。但是通常我们所使用的保鲜塑料袋只是将塑料袋内的蔬菜,水果等食品与外面空气加以隔绝。而保鲜袋内水果,蔬菜成熟时候生产的乙醇如果不加以分解,释放,会加速水果,蔬菜的成熟乃至腐败。同时放入保鲜袋前的水果,蔬菜,以及熟食等食品,在放入保鲜袋之前已经粘又细菌,霉菌,在保鲜袋内可以继续繁殖,加速了食品的腐败。
发明内容
针对上述问题,本发明提出了一种防腐抑菌的保鲜膜,能够有效延长水果,蔬菜的保鲜时间。
具体的技术方案如下:
一种防腐抑菌的保鲜膜,其制备方法为:
(1)按重量份数计称取聚丙烯80-112份、氧化铜5-7份、氧化锌20-28份、石墨烯1-3份、醋酸5-8份、甘油3-5份和壳聚糖5-10份作为原材料;
(2)将原材料混合均匀后,挤出机中,熔融挤出后吹塑成基膜;
(3)在基膜的上表面和下表面上分别喷涂一层保护膜即可得到保鲜膜。
进一步的,聚丙烯和铜粉的重量份数比为16:1。
进一步的,聚丙烯与氧化锌的重量份数比为4:1。
进一步的,挤出机的各段加热温度为:第一段250-260℃、第二段260-280℃、第三段280-290℃、第四段290-310℃。
进一步的,保护膜的制备方法为:
(1)按重量份数计称取水80-100份、生姜提取液10-20份、食用酒精8-16份、硫酸亚铁3-8份、柠檬酸10-15份、羟甲基纤维素6-18份和三聚磷酸钠1-8份作为原材料;
(2)将原材料混合搅拌均匀后得到喷涂液;
(3)将喷涂液均匀喷涂在基膜上、烘干后即可得到保护膜。
本发明的有益效果为:
本发明氧化铜和氧化锌可将乙烯分解成为水以及二氧化碳,乙烯是造成水果,蔬菜快速成熟并腐烂的元凶,因此,本发明能够延长水果,蔬菜的保鲜时间。
具体实施方式
为使本发明的技术方案更加清晰明确,下面对本发明进行进一步描述,任何对本发明技术方案的技术特征进行等价替换和常规推理得出的方案均落入本发明保护范围。
实施例一
一种防腐抑菌的保鲜膜,其制备方法为:
(1)按重量份数计称取聚丙烯96份、氧化铜6份、氧化锌24份、石墨烯2份、醋酸7份、甘油4份和壳聚糖8份作为原材料;
(2)将原材料混合均匀后,挤出机中,熔融挤出后吹塑成基膜;
(3)在基膜的上表面和下表面上分别喷涂一层保护膜即可得到保鲜膜。
进一步的,聚丙烯和铜粉的重量份数比为16:1。
进一步的,聚丙烯与氧化锌的重量份数比为4:1。
进一步的,挤出机的各段加热温度为:第一段255℃、第二段270℃、第三段285℃、第四段300℃。
进一步的,保护膜的制备方法为:
(1)按重量份数计称取水90份、生姜提取液15份、食用酒精12份、硫酸亚铁6份、柠檬酸12份、羟甲基纤维素12份和三聚磷酸钠4份作为原材料;
(2)将原材料混合搅拌均匀后得到喷涂液;
(3)将喷涂液均匀喷涂在基膜上、烘干后即可得到保护膜。
实施例二
一种防腐抑菌的保鲜膜,其制备方法为:
(1)按重量份数计称取聚丙烯80份、氧化铜5份、氧化锌20份、石墨烯1份、醋酸5份、甘油3份和壳聚糖5份作为原材料;
(2)将原材料混合均匀后,挤出机中,熔融挤出后吹塑成基膜;
(3)在基膜的上表面和下表面上分别喷涂一层保护膜即可得到保鲜膜。
进一步的,聚丙烯和铜粉的重量份数比为16:1。
进一步的,聚丙烯与氧化锌的重量份数比为4:1。
进一步的,挤出机的各段加热温度为:第一段250℃、第二段260℃、第三段280℃、第四段290℃。
进一步的,保护膜的制备方法为:
(1)按重量份数计称取水80份、生姜提取液10份、食用酒精8份、硫酸亚铁3份、柠檬酸10份、羟甲基纤维素6份和三聚磷酸钠1份作为原材料;
(2)将原材料混合搅拌均匀后得到喷涂液;
(3)将喷涂液均匀喷涂在基膜上、烘干后即可得到保护膜。
实施例三
一种防腐抑菌的保鲜膜,其制备方法为:
(1)按重量份数计称取聚丙烯112份、氧化铜7份、氧化锌28份、石墨烯3份、醋酸8份、甘油5份和壳聚糖10份作为原材料;
(2)将原材料混合均匀后,挤出机中,熔融挤出后吹塑成基膜;
(3)在基膜的上表面和下表面上分别喷涂一层保护膜即可得到保鲜膜。
进一步的,聚丙烯和铜粉的重量份数比为16:1。
进一步的,聚丙烯与氧化锌的重量份数比为4:1。
进一步的,挤出机的各段加热温度为:第一段260℃、第二段280℃、第三段290℃、第四段310℃。
进一步的,保护膜的制备方法为:
(1)按重量份数计称取水100份、生姜提取液20份、食用酒精16份、硫酸亚铁8份、柠檬酸15份、羟甲基纤维素18份和三聚磷酸钠8份作为原材料;
(2)将原材料混合搅拌均匀后得到喷涂液;
(3)将喷涂液均匀喷涂在基膜上、烘干后即可得到保护膜。
对实施例一、实施例二和实施例三制备得到的保鲜膜进行检测,结果如下:
实施例一 | 实施例二 | 实施例三 | |
抑菌率 | 95% | 92% | 93% |
保鲜贮存期 | 40d | 35d | 42d |
Claims (5)
1.一种防腐抑菌的保鲜膜,其特征为,其制备方法为:
(1)按重量份数计称取聚丙烯80-112份、铜粉5-7份、氧化锌20-28份、石墨烯1-3份、醋酸5-8份、甘油3-5份和壳聚糖5-10份作为原材料;
(2)将原材料混合均匀后,挤出机中,熔融挤出后吹塑成基膜;
(3)在基膜的上表面和下表面上分别喷涂一层保护膜即可得到保鲜膜。
2.如权利要求1所述的一种防腐抑菌的保鲜膜,其特征为,聚丙烯和铜粉的重量份数比为16:1。
3.如权利要求1所述的一种防腐抑菌的保鲜膜,其特征为,聚丙烯与氧化锌的重量份数比为4:1。
4.如权利要求1所述的一种防腐抑菌的保鲜膜,其特征为,挤出机的各段加热温度为:第一段250-260℃、第二段260-280℃、第三段280-290℃、第四段290-310℃。
5.如权利要求1所述的一种防腐抑菌的保鲜膜,其特征为,保护膜的制备方法为:
(1)按重量份数计称取水80-100份、生姜提取液10-20份、食用酒精8-16份、硫酸亚铁3-8份、柠檬酸10-15份、羟甲基纤维素6-18份和三聚磷酸钠1-8份作为原材料;
(2)将原材料混合搅拌均匀后得到喷涂液;
(3)将喷涂液均匀喷涂在基膜上、烘干后即可得到保护膜。