CN108513460A - 一种多层pcb板的铆合方法 - Google Patents
一种多层pcb板的铆合方法 Download PDFInfo
- Publication number
- CN108513460A CN108513460A CN201810339094.3A CN201810339094A CN108513460A CN 108513460 A CN108513460 A CN 108513460A CN 201810339094 A CN201810339094 A CN 201810339094A CN 108513460 A CN108513460 A CN 108513460A
- Authority
- CN
- China
- Prior art keywords
- rivet
- hole
- internal layer
- core plate
- pcb board
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明的目的是提供一种多层PCB板的铆合方法:对芯板用数控钻床进行钻铆合孔,内层芯板采用四角最外侧的四个铆合孔做曝光定位,用来制作内层线路,层压前不需要打靶标,此方法生产效率高,不会产生内层铜屑,不需要采用昂贵的熔接机,而且对准度很高,压合时不容易发生移动。
Description
技术领域
本发明涉及PCB (Printed Circuit Board, 简称 :PCB 板 )制造技术领域,具体涉及一种多层 PCB 板的铆合方法。
背景技术
多层 PCB 板由芯板、半固化片 (Prepreg,简称 :PP)、铜箔通过压合而成。
六层及以上 PCB 板包括至少两张芯板和多张半固化片压合而成,各层芯板的走线要对正。
目前通常的做法是在做完芯板的线路之后,采用CCD打靶机捕捉线路层上的靶标,然后钻出靶标孔,在层压前用铆钉把各芯板对准铆合在一起,这种方法需要打铆合孔比较多,生产效率比较低,精度不高。
还有一种方法是采用熔合的方法,不需要打铆合孔,但是熔合的设备比较贵,熔合点比较少,在压合时容易移动发生层间移动。
发明内容
本发明提供一种用于多层 PCB 板的铆合方法,生产效率高,不需要采用昂贵的熔接机,而且对准度很高,压合时不容易发生移动。
为实现以上目的,本发明采用的方法步骤为 :
A、对芯板用数控钻床进行钻铆合孔。
B、内层芯板采用四角最外侧的四个铆合孔做定位,用来制作内层线路。
C、用铆钉把多层芯板和PP铆合起来,然后正常层压。
本发明不同于常规铆合步骤:
制作内层线路→钻铆合孔→铆合后层压。
也不同于熔合步骤:
制作内层线路→对准熔合→层压。
本发明的有益效果在于 :
铆合孔位置精度高,铆合孔的位置精度就是数控钻机的精度,一般达到0.05mm;而采用普通方法的进行钻铆合孔,存在曝光对准度、打铆合孔的精度的双重影响,排除菲林、板变形的影响,铆合孔的位置精度为0.075mm。
加工速度非常快,一般数控钻机有六轴,每轴可以一次叠板10片以上,相对于CCD打孔机有60倍以上的效率提升。
对于薄板更适合,薄板在常规钻铆合孔的时候,靶标会产生披锋和铜屑,造成内层短路和偏位,而本发明的方法不会产生这些问题。
具体实施方式
下面具体阐明本发明的实施方式。
实施例 1:
制作一个普通六层板的步骤如下:
A、对两个芯板用数控钻床进行钻铆合孔:
长边上有4个孔,短边上3个孔,共14个孔,其中四角最外侧的四孔要求不对称,钻孔时在一叠芯板上放置一块酚醛垫板,以保证芯板的钻孔位置的稳定一致。
B、内层芯板曝光:
采用四角最外侧的四个铆合孔做定位孔,优先采用LDI(激光直接曝光)机用来制作内层线路,因为LDI机可以保证芯板曝光时的平整性,也可以采用定位孔自动补偿功能。
C、用铆钉把多层芯板和PP铆合起来,然后正常层压。
实施例 2:
制作一个L1-2\L5-6盲孔六层板的步骤如下:
A、对L1-2\L5-6两个盲孔芯板在钻盲孔时同时钻出铆合孔,并根据L1-2\L5-6的铆合孔数据在L3-4层钻出铆合孔:
长边上有4个孔,短边上3个孔,共14个孔,其中四角最外侧的四孔要求不对称,钻孔时在一叠芯板上放置一块酚醛垫板,以保证芯板的钻孔位置的稳定一致。
B、盲孔、内层芯板曝光:
采用四角最外侧的四个铆合孔做定位孔,优先采用LDI(激光直接曝光)机用来制作盲孔芯板、内层线路,因为LDI机可以保证芯板曝光时的平整性,也可以采用定位孔自动补偿功能。
C、用铆钉把多层芯板和PP铆合起来,然后正常层压。
如上述实施例为本发明较佳的实施方式,但本发明的实施方式并不受上述实施例的限制,其他的任何未背离本发明的精神实质与原理下所作的改变、修饰、替代、组合、简化,均应为等效的置换方式,都包含在本发明的保护范围之内。
Claims (4)
1.一种多层PCB板的铆合方法,其特征在于采用以下步骤实现:
A、对芯板用数控钻床进行钻铆合孔;
B、内层芯板采用四角最外侧的四个铆合孔做定位,用来制作内层线路;
C、用铆钉把多层芯板和PP铆合起来,然后正常层压。
2.根据权利要求1所述的方法步骤A,其特征在于铆合孔是用数控钻床钻出。
3.根据权利要求1所述的方法步骤B,其特征在于用最外侧的四个铆合孔作为内层线路曝光的靶标。
4.根据权利要求1所述的方法步骤C,其特征在于使用铆钉铆合预先在芯板上钻出的孔。