CN105102383A - 对具有表面氧化的氮化钛-铝玻璃脱模涂层的玻璃成形模具进行重整 - Google Patents
对具有表面氧化的氮化钛-铝玻璃脱模涂层的玻璃成形模具进行重整 Download PDFInfo
- Publication number
- CN105102383A CN105102383A CN201280057186.3A CN201280057186A CN105102383A CN 105102383 A CN105102383 A CN 105102383A CN 201280057186 A CN201280057186 A CN 201280057186A CN 105102383 A CN105102383 A CN 105102383A
- Authority
- CN
- China
- Prior art keywords
- glass
- release coating
- coating
- mold
- reforming
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C03—GLASS; MINERAL OR SLAG WOOL
- C03B—MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03B11/00—Pressing molten glass or performed glass reheated to equivalent low viscosity without blowing
- C03B11/06—Construction of plunger or mould
- C03B11/08—Construction of plunger or mould for making solid articles, e.g. lenses
- C03B11/084—Construction of plunger or mould for making solid articles, e.g. lenses material composition or material properties of press dies therefor
- C03B11/086—Construction of plunger or mould for making solid articles, e.g. lenses material composition or material properties of press dies therefor of coated dies
-
- C—CHEMISTRY; METALLURGY
- C09—DYES; PAINTS; POLISHES; NATURAL RESINS; ADHESIVES; COMPOSITIONS NOT OTHERWISE PROVIDED FOR; APPLICATIONS OF MATERIALS NOT OTHERWISE PROVIDED FOR
- C09K—MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C09K13/00—Etching, surface-brightening or pickling compositions
- C09K13/04—Etching, surface-brightening or pickling compositions containing an inorganic acid
- C09K13/08—Etching, surface-brightening or pickling compositions containing an inorganic acid containing a fluorine compound
-
- C—CHEMISTRY; METALLURGY
- C03—GLASS; MINERAL OR SLAG WOOL
- C03B—MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03B2215/00—Press-moulding glass
- C03B2215/02—Press-mould materials
- C03B2215/08—Coated press-mould dies
- C03B2215/10—Die base materials
- C03B2215/11—Metals
-
- C—CHEMISTRY; METALLURGY
- C03—GLASS; MINERAL OR SLAG WOOL
- C03B—MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03B2215/00—Press-moulding glass
- C03B2215/02—Press-mould materials
- C03B2215/08—Coated press-mould dies
- C03B2215/14—Die top coat materials, e.g. materials for the glass-contacting layers
- C03B2215/22—Non-oxide ceramics
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Organic Chemistry (AREA)
- Manufacturing & Machinery (AREA)
- Inorganic Chemistry (AREA)
- Re-Forming, After-Treatment, Cutting And Transporting Of Glass Products (AREA)
- Surface Treatment Of Glass (AREA)
- Cleaning By Liquid Or Steam (AREA)
- Glass Compositions (AREA)
Applications Claiming Priority (3)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US201161563192P | 2011-11-23 | 2011-11-23 | |
| US61/563,192 | 2011-11-23 | ||
| PCT/US2012/064914 WO2013078038A1 (en) | 2011-11-23 | 2012-11-14 | Reconditioning glass - forming molds having a surface oxidized titanium -aluminum -nitride glass release coating |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| CN105102383A true CN105102383A (zh) | 2015-11-25 |
Family
ID=47279060
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| CN201280057186.3A Pending CN105102383A (zh) | 2011-11-23 | 2012-11-14 | 对具有表面氧化的氮化钛-铝玻璃脱模涂层的玻璃成形模具进行重整 |
Country Status (6)
| Country | Link |
|---|---|
| US (1) | US20130125590A1 (https=) |
| JP (1) | JP6023818B2 (https=) |
| KR (1) | KR20140143738A (https=) |
| CN (1) | CN105102383A (https=) |
| TW (1) | TWI549917B (https=) |
| WO (1) | WO2013078038A1 (https=) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN114605058A (zh) * | 2022-03-28 | 2022-06-10 | 维达力实业(深圳)有限公司 | 热转印模具和防眩光玻璃的制备装置 |
| CN114702235A (zh) * | 2022-03-28 | 2022-07-05 | 维达力实业(深圳)有限公司 | 防眩光玻璃及其制备方法和显示装置 |
Families Citing this family (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US20140224958A1 (en) * | 2013-02-11 | 2014-08-14 | Corning Incorporated | Coatings for glass-shaping molds and glass-shaping molds comprising the same |
| KR102385315B1 (ko) | 2014-03-13 | 2022-04-11 | 코닝 인코포레이티드 | 유리 제품 및 이의 형성 방법 |
| TW201739704A (zh) * | 2016-01-20 | 2017-11-16 | 康寧公司 | 塑形玻璃基材料之具高溫用途之塗層之模具 |
| KR102558050B1 (ko) * | 2016-08-05 | 2023-07-21 | 엘지전자 주식회사 | 3차원 형상 글래스 제조방법 |
Citations (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2001335340A (ja) * | 2000-05-23 | 2001-12-04 | Toyo Glass Co Ltd | ガラス成型用金型 |
| CN1676477A (zh) * | 2004-03-31 | 2005-10-05 | 柯尼卡美能达精密光学株式会社 | 光学元件成形用模具的制造方法 |
| CN101215099A (zh) * | 2008-01-16 | 2008-07-09 | 京东方科技集团股份有限公司 | 平板玻璃基板减薄蚀刻液 |
| US20110256807A1 (en) * | 2010-04-15 | 2011-10-20 | Jiangwei Feng | Method for stripping nitride coatings |
Family Cites Families (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US3015589A (en) * | 1959-07-16 | 1962-01-02 | Diamond Alkali Co | Chemical method |
| US3859222A (en) * | 1971-07-19 | 1975-01-07 | North American Rockwell | Silicon nitride-silicon oxide etchant |
| JP2898142B2 (ja) * | 1992-06-30 | 1999-05-31 | キヤノン株式会社 | 成形用型の再生方法 |
| US6436859B1 (en) * | 1999-03-25 | 2002-08-20 | Central Glass Company, Limited | Glass composition and ion exchange strengthened glass article produced from same |
| EP1295690A1 (en) * | 2001-05-21 | 2003-03-26 | SACMI COOPERATIVA MECCANICI IMOLA Soc. Coop. a r.l. | A process for the functional regeneration of the porosity of moulds used for moulding ceramic objects |
| JP2009073693A (ja) * | 2007-09-20 | 2009-04-09 | Fujinon Corp | 光学素子成形用金型及びその製造方法 |
-
2012
- 2012-11-01 US US13/666,321 patent/US20130125590A1/en not_active Abandoned
- 2012-11-14 KR KR1020147017203A patent/KR20140143738A/ko not_active Withdrawn
- 2012-11-14 JP JP2014543494A patent/JP6023818B2/ja not_active Expired - Fee Related
- 2012-11-14 WO PCT/US2012/064914 patent/WO2013078038A1/en not_active Ceased
- 2012-11-14 CN CN201280057186.3A patent/CN105102383A/zh active Pending
- 2012-11-23 TW TW101143957A patent/TWI549917B/zh not_active IP Right Cessation
Patent Citations (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2001335340A (ja) * | 2000-05-23 | 2001-12-04 | Toyo Glass Co Ltd | ガラス成型用金型 |
| CN1676477A (zh) * | 2004-03-31 | 2005-10-05 | 柯尼卡美能达精密光学株式会社 | 光学元件成形用模具的制造方法 |
| CN101215099A (zh) * | 2008-01-16 | 2008-07-09 | 京东方科技集团股份有限公司 | 平板玻璃基板减薄蚀刻液 |
| US20110256807A1 (en) * | 2010-04-15 | 2011-10-20 | Jiangwei Feng | Method for stripping nitride coatings |
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN114605058A (zh) * | 2022-03-28 | 2022-06-10 | 维达力实业(深圳)有限公司 | 热转印模具和防眩光玻璃的制备装置 |
| CN114702235A (zh) * | 2022-03-28 | 2022-07-05 | 维达力实业(深圳)有限公司 | 防眩光玻璃及其制备方法和显示装置 |
| CN114605058B (zh) * | 2022-03-28 | 2024-01-26 | 维达力实业(深圳)有限公司 | 热转印模具和防眩光玻璃的制备装置 |
| CN114702235B (zh) * | 2022-03-28 | 2024-01-26 | 维达力实业(深圳)有限公司 | 防眩光玻璃及其制备方法和显示装置 |
Also Published As
| Publication number | Publication date |
|---|---|
| TW201331144A (zh) | 2013-08-01 |
| US20130125590A1 (en) | 2013-05-23 |
| KR20140143738A (ko) | 2014-12-17 |
| JP2015516928A (ja) | 2015-06-18 |
| TWI549917B (zh) | 2016-09-21 |
| JP6023818B2 (ja) | 2016-11-09 |
| WO2013078038A1 (en) | 2013-05-30 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN105102383A (zh) | 对具有表面氧化的氮化钛-铝玻璃脱模涂层的玻璃成形模具进行重整 | |
| KR100828112B1 (ko) | 다성분을 가지는 글라스 기판용 미세가공 표면처리액 | |
| JP2019043841A (ja) | リン酸リチウム化合物を含有する残留物を表面から除去する方法 | |
| JP5721348B2 (ja) | ガラスの製造方法 | |
| JP2013536153A (ja) | ガラス製品の端面を強化する方法 | |
| Mellott et al. | Evaluation of surface preparation methods for glass | |
| JP6395723B2 (ja) | ガラス板の製造方法及びガラス板 | |
| US20110081785A1 (en) | Solution for the selective removal of metal from aluminum substrates | |
| JP6360064B2 (ja) | ガラス板の製造方法 | |
| JP6275206B2 (ja) | 向上した品質の多スペクトル硫化亜鉛 | |
| CN109095789A (zh) | 化学强化玻璃的制造方法 | |
| TWI643824B (zh) | 用於玻璃成形模具之塗層及包含該塗層之玻璃成形模具 | |
| JP2597931B2 (ja) | 高速度工具鋼のチタンコーティング被膜の除去剤 | |
| JP2006096658A (ja) | ディスプレイ用平板ガラスの強化方法 | |
| CN101189192B (zh) | 玻璃条的制造方法 | |
| JP6544043B2 (ja) | 化学強化ガラスの製造方法 | |
| JP2008031038A (ja) | 石英ガラス表面の洗浄方法 | |
| JP2005213091A (ja) | ガラス光学素子の製造方法 | |
| JP4540361B2 (ja) | 凹凸のある表面を有するガラス基材の製造方法 | |
| US6126997A (en) | Method for treating magnesium die castings | |
| TW201040318A (en) | Selective etching of reactor surfaces | |
| CN113955950A (zh) | 锂铝硅玻璃的强化方法 | |
| JPH11100627A (ja) | 巨大結晶粒を表面に析出させたチタン又はチタン合金 製品 | |
| JP2002193634A (ja) | プラズマ耐食性に優れた石英ガラス及び石英ガラス治具 | |
| CN121420093A (zh) | 用于铝表面的碱性清洁剂 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| C06 | Publication | ||
| PB01 | Publication | ||
| C10 | Entry into substantive examination | ||
| SE01 | Entry into force of request for substantive examination | ||
| RJ01 | Rejection of invention patent application after publication | ||
| RJ01 | Rejection of invention patent application after publication |
Application publication date: 20151125 |