CN103273668B - 芳纶纤维室内光缆加强芯的制备方法 - Google Patents

芳纶纤维室内光缆加强芯的制备方法 Download PDF

Info

Publication number
CN103273668B
CN103273668B CN201310224468.4A CN201310224468A CN103273668B CN 103273668 B CN103273668 B CN 103273668B CN 201310224468 A CN201310224468 A CN 201310224468A CN 103273668 B CN103273668 B CN 103273668B
Authority
CN
China
Prior art keywords
mass parts
strengthening core
aramid fiber
carry out
heating
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201310224468.4A
Other languages
English (en)
Other versions
CN103273668A (zh
Inventor
陆志强
仇宝鑫
赵荣兵
陆卫强
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nantong Hetai Communication Technology Co. Ltd.
Sichuan Jiusheng Communications Technology Co., Ltd.
Original Assignee
SICHUAN JIUSHENG COMMUNICATIONS TECHNOLOGY Co Ltd
NANTONG HETAI COMMUNICATION EQUIPMENT CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SICHUAN JIUSHENG COMMUNICATIONS TECHNOLOGY Co Ltd, NANTONG HETAI COMMUNICATION EQUIPMENT CO Ltd filed Critical SICHUAN JIUSHENG COMMUNICATIONS TECHNOLOGY Co Ltd
Priority to CN201310224468.4A priority Critical patent/CN103273668B/zh
Publication of CN103273668A publication Critical patent/CN103273668A/zh
Application granted granted Critical
Publication of CN103273668B publication Critical patent/CN103273668B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了芳纶纤维室内光缆加强芯的制备方法,其特征在于:包括以下步骤:芳纶纤维用导纱板进行导纱,多股纱并为一股,进入温度为200-250℃的烘箱进行预加热1-2min,然后进入浸槽中进行浸料,浸槽中的浸液包括100质量份的乙烯基树脂、1-3质量份的过氧化二苯甲酰、1-3质量份的过氧化苯甲酸叔丁酯、2-4质量份的脱模剂和10-20质量份的填料,然后用预热成型孔进行成型处理,然后进入加热温度为150-250℃的加热模具内进行加热固化1-5min,然后通过牵引机将加强芯从模具中拉出,再进行收卷。本发明的优点是:所制得的加强芯着密度小,强度高,柔韧性好,且具有一定的刚性,折断后其拉伸强度仍然保持在1400Mpa以上。

Description

芳纶纤维室内光缆加强芯的制备方法
技术领域
本发明涉及光缆技术领域,尤其涉及一种芳纶纤维室内光缆加强芯的制备方法。
背景技术
蝶形引入光缆作为入户光缆多数情况下是敷设在室内的,这就对蝶形引入光缆中使用加强芯提出了更高的要求。现有技术中加强芯存在着密度大,强度低,柔韧性差等缺点。基于市场的需求,急需一种改进的技术来解决现有技术中所存在的多种问题。
发明内容
本发明的目的是提供一种芳纶纤维室内光缆加强芯的制备方法。
本发明采用的技术方案是:
芳纶纤维室内光缆加强芯的制备方法,包括以下步骤:芳纶纤维用导纱板进行导纱,多股纱并为一股,进入温度为200-250℃的烘箱进行预加热1-2min,然后进入浸槽中进行浸料,浸槽中的浸液包括100质量份的乙烯基树脂、1-3质量份的过氧化二苯甲酰、1-3质量份的过氧化苯甲酸叔丁酯、2-4质量份的脱模剂和10-20质量份的填料,然后用预热成型孔进行成型处理,然后进入加热温度为150-250℃的加热模具内进行加热固化1-5min,然后通过牵引机将加强芯从模具中拉出,再进行收卷。
所述填料为氢氧化铝。
所述脱模剂为聚四氟乙烯、氟树脂涂料、硅树脂或硅橡胶。
所述牵引机采用间隙停机法,每2-4min停5-10s,所述牵引机的牵引速度为4-6m/min。
本发明的优点是:所制得的加强芯着密度小,强度高,柔韧性好,且具有一定的刚性,折断后其拉伸强度仍然保持在1400Mpa以上。
具体实施方式
下面的实施例可以使本专业技术人员更全面地理解本发明,但不以任何方式限制本发明。
实施例1
本发明的芳纶纤维室内光缆加强芯的制备方法,包括以下步骤:芳纶纤维用导纱板进行导纱,多股纱并为一股,进入温度为200℃的烘箱进行预加热2min,然后进入浸槽中进行浸料,浸槽中的浸液包括100kg的乙烯基树脂、1kg的过氧化二苯甲酰、2kg的过氧化苯甲酸叔丁酯、3kg的硅橡胶和10kg的氢氧化铝,然后用预热成型孔进行成型处理,然后进入加热温度为150℃的加热模具内进行加热固化5min,然后通过牵引机将加强芯从模具中拉出,牵引机采用间隙停机法,每2min停7s,所述牵引机的牵引速度为4m/min,防止堵膜,再进行收卷,所制得的加强芯着密度小,强度高,柔韧性好,且具有一定的刚性,折断后其拉伸强度仍然保持在1400Mpa以上。
实施例2
本发明的芳纶纤维室内光缆加强芯的制备方法,包括以下步骤:芳纶纤维用导纱板进行导纱,多股纱并为一股,进入温度为230℃的烘箱进行预加热2min,然后进入浸槽中进行浸料,浸槽中的浸液包括100kg的乙烯基树脂、2kg的过氧化二苯甲酰、3kg的过氧化苯甲酸叔丁酯、2kg的硅树脂和15kg的氢氧化铝,然后用预热成型孔进行成型处理,然后进入加热温度为200℃的加热模具内进行加热固化4min,然后通过牵引机将加强芯从模具中拉出,牵引机采用间隙停机法,每3min停5s,所述牵引机的牵引速度为5m/min,防止堵膜,再进行收卷,所制得的加强芯着密度小,强度高,柔韧性好,且具有一定的刚性,折断后其拉伸强度仍然保持在1400Mpa以上。
实施例3
本发明的芳纶纤维室内光缆加强芯的制备方法,包括以下步骤:芳纶纤维用导纱板进行导纱,多股纱并为一股,进入温度为250℃的烘箱进行预加热1min,然后进入浸槽中进行浸料,浸槽中的浸液包括100kg的乙烯基树脂、3kg的过氧化二苯甲酰、2kg的过氧化苯甲酸叔丁酯、4kg的聚四氟乙烯和20kg的氢氧化铝,然后用预热成型孔进行成型处理,然后进入加热温度为250℃的加热模具内进行加热固化2min,然后通过牵引机将加强芯从模具中拉出,牵引机采用间隙停机法,每4min停10s,所述牵引机的牵引速度为6m/min,防止堵膜,再进行收卷,所制得的加强芯着密度小,强度高,柔韧性好,且具有一定的刚性,折断后其拉伸强度仍然保持在1400Mpa以上。

Claims (3)

1.芳纶纤维室内光缆加强芯的制备方法,其特征在于:包括以下步骤:芳纶纤维用导纱板进行导纱,多股纱并为一股,进入温度为200-250℃的烘箱进行预加热1-2min,然后进入浸槽中进行浸料,浸槽中的浸液包括100质量份的乙烯基树脂、1-3质量份的过氧化二苯甲酰、1-3质量份的过氧化苯甲酸叔丁酯、2-4质量份的脱模剂和10-20质量份的填料,然后用预热成型孔进行成型处理,然后进入加热温度为150-250℃的加热模具内进行加热固化1-5min,然后通过牵引机将加强芯从模具中拉出,再进行收卷,所述牵引机采用间隙停机法,每2-4min停5-10s,所述牵引机的牵引速度为4-6m/min。
2.根据权利要求1所述的芳纶纤维室内光缆加强芯的制备方法,其特征在于:所述填料为氢氧化铝。
3.根据权利要求1所述的芳纶纤维室内光缆加强芯的制备方法,其特征在于:所述脱模剂为聚四氟乙烯、氟树脂涂料、硅树脂或硅橡胶。
CN201310224468.4A 2013-06-07 2013-06-07 芳纶纤维室内光缆加强芯的制备方法 Active CN103273668B (zh)