CN102240742A - 一种锁环截料折弯模具设计方法 - Google Patents

一种锁环截料折弯模具设计方法 Download PDF

Info

Publication number
CN102240742A
CN102240742A CN2011101129552A CN201110112955A CN102240742A CN 102240742 A CN102240742 A CN 102240742A CN 2011101129552 A CN2011101129552 A CN 2011101129552A CN 201110112955 A CN201110112955 A CN 201110112955A CN 102240742 A CN102240742 A CN 102240742A
Authority
CN
China
Prior art keywords
bending
cut
punch
lock ring
designing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2011101129552A
Other languages
English (en)
Inventor
许秋海
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
YANTAI HONGLIN ELECTRONIC MOLD CO Ltd
Original Assignee
YANTAI HONGLIN ELECTRONIC MOLD CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by YANTAI HONGLIN ELECTRONIC MOLD CO Ltd filed Critical YANTAI HONGLIN ELECTRONIC MOLD CO Ltd
Priority to CN2011101129552A priority Critical patent/CN102240742A/zh
Publication of CN102240742A publication Critical patent/CN102240742A/zh
Pending legal-status Critical Current

Abstract

一种锁环截料折弯模具设计方法,属冲压模具领域,是将锁环截料及锁环折弯工序融为一道工序的设计方法,降低了加工成本,减少加工工序,提高了生产效率,改善了零件外观质量。

Description

一种锁环截料折弯模具设计方法
技术领域
本发明涉及冲压模具领域,尤其是一种锁环类零件截料折弯模具设计方法。
背景技术
目前,锁环的生产,需要两道工序,锁环的截料和锁环的折弯墩型,由于需截料折弯的锁环为圆柱形,截料折弯时,在折弯位置附近处会有刮伤变形现象,造成零件局部不能满足直径要求。
发明内容
本发明的目的就是为了解决现有锁环截料折弯技术的不足,提供一种将锁环截料及锁环折弯工序融为一道工序设计方法,降低了加工成本,减少加工工序,提高了生产效率,改善了零件外观质量。
本发明解决其技术问题所采用的技术方案是:一种锁环截料折弯模设计方法,当锁环截料折弯时,冲床行程向下运行至折弯冲头开始接触原材料,且顶块开始接触切断镶块,由于折弯冲头上面为弹性结构,在冲床行程继续向下的过程中,原材料并未开始折弯,而是切断冲头和切断镶块在顶块的作用下开始工作将原材料冲切;冲床行程下行到一定程度,在顶块的作用下,切断镶块与切断冲头已完全将原材料切断,且切断镶块下部为弹性结构,故在顶块下压的过程中继续向下运动,此时,折弯冲头上面弹性结构的行程运行完,折弯冲头开始随着冲床行程向下运动而向下运动,原材料在折弯冲头及折弯滚轮的作用下,开始折弯;冲床下行至下固定点,零件在折弯冲头及折弯滚轮、弹料芯的作用下完成折弯及成型,冲床开始向上运动,模具随着冲床向上运动,折弯好的零件在模具脱料装置作用下脱离折弯冲头,完成一个切断折弯过程。
本发明的有益效果是:一种锁环截料折弯模设计方法,是将锁环截料及锁环折弯工序融为一道工序的设计方法,降低了加工成本,减少加工工序,提高了生产效率,改善了零件外观质量。
附图说明
下面结合附图和实施例对本发明进一步说明。
图1锁环的示意图。
图2、图3、图4是截料折弯过程的状态示意图。
图中1.顶块,2.切断镶块,3.原材料,4.折弯滚轮,5.切断冲头,6.折弯冲头,7.弹料芯,8.顶杆。
具体实施方式
在图2中,冲床行程向下运行至折弯冲头(6)开始接触原材料(3),且顶块(1)开始接触切断镶块,由于折弯冲头(6)上面为弹性结构,且其弹簧力量小于顶杆(8)传递的优力胶的力量,故在冲床行程继续向下的过程中,原材料(3)并未开始折弯,而是切断冲头(5)和切断镶块(2)在顶块(1)的作用下开始工作将原材料(3)冲切。
在图3实施例中,冲床行程下行到一定程度,在顶块(1)的作用下,切断镶块(2)与切断冲头(5)已完全将原材料(3)切断,且切断镶块(2)下部为弹性结构,故在顶块(1)下压的过程中继续向下运动。此时,折弯冲头(6)上面弹性结构的行程运行完,折弯冲头(6)开始随着冲床行程向下运动而向下运动,原材料(3)在折弯冲头(6)及折弯滚轮(4)的作用下,开始折弯。
在图4实施例中,冲床下行至下固定点,零件在折弯冲头(6)及折弯滚轮(4)、弹料芯(7)的作用下完成折弯及成型,冲床开始向上运动,模具随着冲床向上运动,折弯好的零件在模具脱料装置作用下脱离折弯冲头,完成一个切断折弯过程。

Claims (6)

1.一种锁环截料折弯模设计方法,其特征是:将锁环截料及锁环折弯工序融为一道工序。
2.根据权利要求1所述的锁环截料折弯模设计方法,其特征是:冲床行程向下运行至折弯冲头(6)开始接触原材料(3),且顶块(1)开始接触切断镶块,由于折弯冲头(6)上面为弹性结构,且其弹簧力量小于顶杆(8)传递的优力胶的力量,故在冲床行程继续向下的过程中,原材料(3)并未开始折弯,而是切断冲头(5)和切断镶块(2)在顶块(1)的作用下开始工作将原材料(3)冲切。
3.根据权利要求1所述的锁环截料折弯模设计方法,其特征是:冲床行程下行到一定程度,在顶块(1)的作用下,切断镶块(2)与切断冲头(5)已完全将原材料(3)切断,且切断镶块(2)下部为弹性结构,故在顶块(1)下压的过程中继续向下运动。此时,折弯冲头(6)上面弹性结构的行程运行完,折弯冲头(6)开始随着冲床行程向下运动而向下运动,原材料(3)在折弯冲头(6)及折弯滚轮(4)的作用下,开始折弯。
4.根据权利要求1所述的锁环截料折弯模设计方法,其特征是:冲床下行至下固定点,零件在折弯冲头(6)及折弯滚轮(4)、弹料芯(7)的作用下完成折弯及成型,冲床开始向上运动,模具随着冲床向上运动,折弯好的零件在模具脱料装置作用下脱离折弯冲头,完成一个切断折弯过程。
5.根据权利要求2所述的锁环截料折弯模设计方法,其特征是:折弯冲头(6)上面为弹性结构,且其弹簧力量小于顶杆(8)传递的优力胶的力量。
6.根据权利要求3所述的锁环截料折弯模设计方法,其特征是:切断镶块(2)下部为弹性结构。
CN2011101129552A 2011-04-19 2011-04-19 一种锁环截料折弯模具设计方法 Pending CN102240742A (zh)