CN101671956A - 一种吸水性画布涂层及其制作方法 - Google Patents

一种吸水性画布涂层及其制作方法 Download PDF

Info

Publication number
CN101671956A
CN101671956A CN200910153479A CN200910153479A CN101671956A CN 101671956 A CN101671956 A CN 101671956A CN 200910153479 A CN200910153479 A CN 200910153479A CN 200910153479 A CN200910153479 A CN 200910153479A CN 101671956 A CN101671956 A CN 101671956A
Authority
CN
China
Prior art keywords
coating
water absorbent
add
canvas
carbonic acid
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN200910153479A
Other languages
English (en)
Other versions
CN101671956B (zh
Inventor
陈卫宏
陈祎
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiangsu Fenghuang painting material technology Co.,Ltd.
Original Assignee
WUXI PHOENIX DRAWING MATERIALS CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by WUXI PHOENIX DRAWING MATERIALS CO Ltd filed Critical WUXI PHOENIX DRAWING MATERIALS CO Ltd
Priority to CN2009101534791A priority Critical patent/CN101671956B/zh
Publication of CN101671956A publication Critical patent/CN101671956A/zh
Application granted granted Critical
Publication of CN101671956B publication Critical patent/CN101671956B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明涉及一种吸水性画布涂层,其特征在于由下述重量配比的原料制成:水30-33、丙烯酸乳液18-23、聚乙烯醇8-13、钛白粉12-15、滑石粉10-12、碳酸轻钙7-10、碳酸重钙7-10、白炭黑2-4、分散剂0.3-0.4、消泡剂0.2-0.3,增稠剂1-2;具有该涂层的画布特别适用于丙烯画,与丙烯颜料相同的涂层使颜料与画布的结合非常牢固,并且根据需要可以在画布上用丙烯颜料调和成水彩、水粉效果,使丙烯颜料的宽容度更好,表现力更强。

Description

一种吸水性画布涂层及其制作方法
技术领域
本发明涉及一种吸水性画布涂层,本发明还涉及该涂层的制作方法。
背景技术
传统丙烯画所采用的画布因为吸水性的问题致使绘画所使用丙烯颜料与画布的结合力比较差,使用丙烯颜料作画时不能实现直接在画布上将其调和成水彩、水粉效果,使丙烯颜料的宽容度及表现力都受到制约。因此为了更好的突出丙烯颜料绘画时的宽容度及表现力,需要一种新的画布可以使丙烯颜料在画布上依据需要调和出水彩、水粉效果,同时能增强丙烯颜料与画布的结合力。
发明内容
本发明的目的在于提供一种能使丙烯颜料与画布结合更为牢固且能使丙烯颜料的宽容度更好,表现力更强的一种吸水性画布涂层及该涂层的制作方法。
为实现上述目的,本发明采用如下技术方案:一种吸水性画布涂层,其由下述重量配比的原料制成:水30-33、丙烯酸乳液18-23、聚乙烯醇8-13、钛白粉12-15、滑石粉10-12、碳酸轻钙7-10、碳酸重钙7-10、白炭黑2-4、分散剂0.3-0.4、消泡剂0.2-0.3,增稠剂1-2。
所述的吸水性画布涂层的制备方法:依次包括以下步骤(1)首先打开搅拌机做低速运行,逐步加入水、分散剂、消泡剂、碳酸轻钙、碳酸重钙,逐渐提速使物料充分混合,搅拌速度达到分散盘圆周速度20m/s以上;(2)加入钛白粉、滑石粉及白炭黑,加完后混合搅拌40分钟;(3)加入聚乙烯醇及丙烯酸乳液,此时分散盘圆周速度控制为8-10m/s,搅拌时间为10分钟;(4)加入增稠剂,此时分散盘圆周速度控制为10-12m/s,搅拌时间为5分钟。
与现有技术相比,本发明具有如下有益效果:能有效使丙烯颜料与画布的结合非常牢固,并且根据需要可以在画布上用丙烯颜料调和成水彩、水粉效果,使丙烯颜料的宽容度更好,表现力更强。
具体实施方式
本发明一种吸水性画布涂层,其由下述重量配比的原料制成:水30-33、丙烯酸乳液18-23、聚乙烯醇8-13、钛白粉12-15、滑石粉10-12、碳酸轻钙7-10、碳酸重钙7-10、白炭黑2-4、分散剂0.3-0.4、消泡剂0.2-0.3,增稠剂1-2。
所述的丙烯酸乳液的主要成分为:丙烯酸丁脂35%、甲基丙烯酸甲脂13%、去离子水52%。
分散剂为多己内配多元醇与多乙烯亚胺嵌段共聚物,增稠剂为有机纤维素,消泡剂为聚乙烯基异丁基醚。
所述涂层的细度为50um,所述涂层的PH值为8.5-9.0,所述涂层的黏度为2-3Pa.S。
所述的吸水性画布涂层的制备方法:依次包括以下步骤:(1)首先打开搅拌机做低速运行,逐步加入水、分散剂、消泡剂、碳酸轻钙、碳酸重钙,逐渐提速使物料充分混合,搅拌速度达到分散盘圆周速度20m/s以上;(2)加入钛白粉、滑石粉及白炭黑,加完后混合搅拌40分钟;(3)加入聚乙烯醇及丙烯酸乳液,此时分散盘圆周速度控制为8-10m/s,搅拌时间为10分钟;(4)加入增稠剂,此时分散盘圆周速度控制为10-12m/s,搅拌时间为5分钟。
实施例1
(1)首先打开搅拌机做低速运行,逐步加入水33kg、分散剂0.35kg、消泡剂0.2kg、碳酸轻钙8kg、碳酸重钙8kg,逐渐提速使物料充分混合,搅拌速度达到分散盘圆周速度20m/s以上;(2)加入钛白粉13kg、滑石粉10kg及白炭黑3kg,加完后混合搅拌40分钟;(3)加入聚乙烯醇10kg及丙烯酸乳液21kg,此时分散盘圆周速度控制为8-10m/s,搅拌时间为10分钟;(4)加入增稠剂1.5kg,此时分散盘圆周速度控制为10-12m/s,搅拌时间为5分钟。
实施例2
(1)首先打开搅拌机做低速运行,逐步加入水1kg、分散剂10g、消泡剂8g、碳酸轻钙270g、碳酸重钙270g,逐渐提速使物料充分混合,搅拌速度达到分散盘圆周速度20m/s以上;(2)加入钛白粉390g、滑石粉310g及白炭黑100g,加完后混合搅拌40分钟;(3)加入聚乙烯醇300g及丙烯酸乳液610g,此时分散盘圆周速度控制为8-10m/s,搅拌时间为10分钟;(4)加入增稠剂30g,此时分散盘圆周速度控制为10-12m/s,搅拌时间为5分钟。

Claims (7)

1、一种吸水性画布涂层,其特征在于由下述重量配比的原料制成:水30-33、丙烯酸乳液18-23、聚乙烯醇8-13、钛白粉12-15、滑石粉10-12、碳酸轻钙7-10、碳酸重钙7-10、白炭黑2-4、分散剂0.3-0.4、消泡剂0.2-0.3,增稠剂1-2。
2、如权利要求1所述的吸水性画布涂层,其特征在于:所述的丙烯酸乳液的主要成分为:丙烯酸丁脂35%、甲基丙烯酸甲脂13%、去离子水52%。
3、如权利要求2所述的吸水性画布涂层,其特征在于:分散剂为多己内配多元醇与多乙烯亚胺嵌段共聚物,增稠剂为有机纤维素,消泡剂为聚乙烯基异丁基醚。
4、如权利要求1所述的吸水性画布涂层,其特征在于:所述涂层的细度为50um。
5、如权利要求4所述的吸水性画布涂层,其特征在于:所述涂层的PH值为8.5-9.0。
6、如权利要求5所述的吸水性画布涂层,其特征在于:所述涂层的黏度为2-3Pa.S。
7、如权利要求1所述的吸水性画布涂层的制备方法:依次包括以下步骤:(1)首先打开搅拌机做低速运行,逐步加入水、分散剂、消泡剂、碳酸轻钙、碳酸重钙,逐渐提速使物料充分混合,搅拌速度达到分散盘圆周速度20m/s以上;(2)加入钛白粉、滑石粉及白炭黑,加完后混合搅拌40分钟;(3)加入聚乙烯醇及丙烯酸乳液,此时分散盘圆周速度控制为8-10m/s,搅拌时间为10分钟;(4)加入增稠剂,此时分散盘圆周速度控制为10-12m/s,搅拌时间为5分钟。
CN2009101534791A 2009-10-10 2009-10-10 一种吸水性画布涂层及其制作方法 Active CN101671956B (zh)