CN101538790A - 腈棉混纺毛毯的生产工艺 - Google Patents

腈棉混纺毛毯的生产工艺 Download PDF

Info

Publication number
CN101538790A
CN101538790A CN200810019891A CN200810019891A CN101538790A CN 101538790 A CN101538790 A CN 101538790A CN 200810019891 A CN200810019891 A CN 200810019891A CN 200810019891 A CN200810019891 A CN 200810019891A CN 101538790 A CN101538790 A CN 101538790A
Authority
CN
China
Prior art keywords
blankets
temperature
typing
cloth
acrylic
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN200810019891A
Other languages
English (en)
Inventor
姚寿昌
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN200810019891A priority Critical patent/CN101538790A/zh
Publication of CN101538790A publication Critical patent/CN101538790A/zh
Pending legal-status Critical Current

Abstract

本发明向人们公开了一种既提高产品质量、又有效降低成本的腈棉混纺毛毯的生产工艺,其工艺流程:印花后直接蒸化,蒸化温度为100-105℃,蒸化时间20-25分钟,进行水洗温度为40-50℃,水洗布速为9-10米/分钟,水洗结束后直接定型,定型温度控制在110-120℃,定型布速根据坯布的克重而定,定型后整理成品;本发明的有益效果:既有晴纶毛毯的风格又有棉毯的手感,给人的皮肤带来一种既舒适又柔软的感觉;由本发明制成的产品是人们日常生活的必需品。

Description

腈棉混纺毛毯的生产工艺
技术领域
本发明涉及人们日常生活使用的一种毛毯,具体地说,涉及一种腈棉混纺毛毯的生产工艺。
背景技术
在生产单独的棉毯时,其工艺流程要先印花再焙烘(焙烘温度为110-130℃),而且布面一定要充分的烘干后才能去蒸化固色(蒸化温度为105℃、蒸化时间为25-30分钟)。在水洗时棉毯要升温至90-95℃皂洗,水洗布速为5-6米/分钟,反复水洗。水洗结束后松式烘干(烘干温度为110-130℃)烘干后定型(定型温度为160-170℃)定型布速根据坯布的克重而定)。定型后整理成品。工艺流程图:印花——焙烘——蒸化——水洗——烘干——定型——整理。以上工艺流程多而且复杂造成了生产成本的提高。比如:以上工艺是印好花后必须焙烘后再蒸化,水洗速度慢而且还要反复水洗造成了生产成本的提高。
发明内容
针对上述存在的技术问题,本发明的目的是提出了既提高产品质量、又有效降低成本的一种腈棉混纺毛毯的生产工艺。
本发明的技术方案是:一种腈棉混纺毛毯的生产工艺,其工艺流程:
1、蒸化:印花后直接蒸化,蒸化温度为100-105℃,蒸化时间20-25分钟;
2、水洗:水洗温度为40-50℃,水洗布速为9-10米/分钟;
3、定型:水洗结束后直接定型,定型温度控制在110-120℃,定型布速根据坯布的克重而定;
4、整理:定型后整理成品。
本发明中,棉花是新疆优质棉,晴纶散纤是日本三菱公司,印花机是奥地利齐玛印花机,蒸化机是意大利的它的保温性能好,水洗机和定型机国产的我们公司用的是苏州四海纺织机械。
本发明的有益效果:既有晴纶毛毯的风格又有棉毯的手感,给人的皮肤带来一种即舒适又柔软的感觉。带来的视觉效果是雾里看花。
附图说明
附图为本发明的工艺流程图。
具体实施方案
从附图中可知,一种腈棉混纺毛毯的生产工艺,其工艺过程如下:
1、印花后只要直接蒸化不需要焙烘(蒸化温度为100-105℃,蒸化时间20-25分钟);
2、水洗(水洗温度为40-50℃水洗布速为9-10米/分钟,不需要反复水洗);
3、水洗结束后不需要松式烘干直接定型(定型温度110-120℃,定型布速根据坯布的克重而定);
4、定型后整理成品。
棉花和晴纶散纤是在纺纱时放入进行配比,配比时棉花和晴纶散纤各占50%,印花机最是前道工序其次是蒸化机、水洗机,定型机在最后一道工序。它们起到的作用是印花机是给毛毯白坯印上花型,蒸化机是用来固色使毛毯的纤维得到膨化,水洗机是用来洗干净毛毯表面的浮色,定型机是用来固定毛毯的规格不让毛毯产生纬斜的现象。

Claims (1)

1.一种腈棉混纺毛毯的生产工艺,其特征是:所述工艺流程为,
A、蒸化:印花后直接蒸化,蒸化温度为100-105℃,蒸化时间20-25分钟;
B、水洗:水洗温度为40-50℃,水洗布速为9-10米/分钟;
C、定型:水洗结束后直接定型,定型温度控制在110-120℃,定型布速根据坯布的克重而定;
D、整理:定型后整理成品。
CN200810019891A 2008-03-21 2008-03-21 腈棉混纺毛毯的生产工艺 Pending CN101538790A (zh)