CN100428541C - 碱蓄电池用贮氢合金及其制造方法及碱蓄电池 - Google Patents
碱蓄电池用贮氢合金及其制造方法及碱蓄电池 Download PDFInfo
- Publication number
- CN100428541C CN100428541C CNB2005100036714A CN200510003671A CN100428541C CN 100428541 C CN100428541 C CN 100428541C CN B2005100036714 A CNB2005100036714 A CN B2005100036714A CN 200510003671 A CN200510003671 A CN 200510003671A CN 100428541 C CN100428541 C CN 100428541C
- Authority
- CN
- China
- Prior art keywords
- hydrogen storage
- sub
- storage alloy
- alkaline
- storage battery
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Images
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/36—Selection of substances as active materials, active masses, active liquids
- H01M4/38—Selection of substances as active materials, active masses, active liquids of elements or alloys
- H01M4/383—Hydrogen absorbing alloys
-
- C—CHEMISTRY; METALLURGY
- C01—INORGANIC CHEMISTRY
- C01B—NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C
- C01B3/00—Hydrogen; Gaseous mixtures containing hydrogen; Separation of hydrogen from mixtures containing it; Purification of hydrogen
- C01B3/0005—Reversible uptake of hydrogen by an appropriate medium, i.e. based on physical or chemical sorption phenomena or on reversible chemical reactions, e.g. for hydrogen storage purposes ; Reversible gettering of hydrogen; Reversible uptake of hydrogen by electrodes
- C01B3/001—Reversible uptake of hydrogen by an appropriate medium, i.e. based on physical or chemical sorption phenomena or on reversible chemical reactions, e.g. for hydrogen storage purposes ; Reversible gettering of hydrogen; Reversible uptake of hydrogen by electrodes characterised by the uptaking medium; Treatment thereof
- C01B3/0031—Intermetallic compounds; Metal alloys; Treatment thereof
- C01B3/0047—Intermetallic compounds; Metal alloys; Treatment thereof containing a rare earth metal; Treatment thereof
- C01B3/0057—Intermetallic compounds; Metal alloys; Treatment thereof containing a rare earth metal; Treatment thereof also containing nickel
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M10/00—Secondary cells; Manufacture thereof
- H01M10/34—Gastight accumulators
- H01M10/345—Gastight metal hydride accumulators
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M2004/021—Physical characteristics, e.g. porosity, surface area
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/04—Processes of manufacture in general
- H01M4/0402—Methods of deposition of the material
- H01M4/0404—Methods of deposition of the material by coating on electrode collectors
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/30—Hydrogen technology
- Y02E60/32—Hydrogen storage
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02P—CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02P70/00—Climate change mitigation technologies in the production process for final industrial or consumer products
- Y02P70/50—Manufacturing or production processes characterised by the final manufactured product
Landscapes
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Engineering & Computer Science (AREA)
- Organic Chemistry (AREA)
- Electrochemistry (AREA)
- General Chemical & Material Sciences (AREA)
- Life Sciences & Earth Sciences (AREA)
- Environmental & Geological Engineering (AREA)
- General Life Sciences & Earth Sciences (AREA)
- Geology (AREA)
- Combustion & Propulsion (AREA)
- Inorganic Chemistry (AREA)
- Manufacturing & Machinery (AREA)
- Battery Electrode And Active Subsutance (AREA)
Applications Claiming Priority (3)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2004016553A JP4290023B2 (ja) | 2004-01-26 | 2004-01-26 | アルカリ蓄電池用水素吸蔵合金及びその製造方法並びにアルカリ蓄電池 |
| JP2004016553 | 2004-01-26 | ||
| JP2004-016553 | 2004-01-26 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| CN1649191A CN1649191A (zh) | 2005-08-03 |
| CN100428541C true CN100428541C (zh) | 2008-10-22 |
Family
ID=34792482
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| CNB2005100036714A Expired - Lifetime CN100428541C (zh) | 2004-01-26 | 2005-01-10 | 碱蓄电池用贮氢合金及其制造方法及碱蓄电池 |
Country Status (3)
| Country | Link |
|---|---|
| US (1) | US7514178B2 (enExample) |
| JP (1) | JP4290023B2 (enExample) |
| CN (1) | CN100428541C (enExample) |
Families Citing this family (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2007092115A (ja) * | 2005-09-28 | 2007-04-12 | Sanyo Electric Co Ltd | 水素吸蔵合金及び該合金を用いたニッケル水素蓄電池 |
| JP4873947B2 (ja) * | 2005-12-22 | 2012-02-08 | 三洋電機株式会社 | 水素吸蔵合金及び該水素吸蔵合金を用いたアルカリ二次電池 |
| FR2897875B1 (fr) * | 2006-02-28 | 2008-12-05 | Accumulateurs Fixes | Alliage hydrurable pour accumulateur alcalin |
| CN102403489A (zh) * | 2010-09-17 | 2012-04-04 | 北京有色金属研究总院 | 一种长寿命低自放电型动力电池用负极储氢合金 |
| FR2968015B1 (fr) | 2010-11-29 | 2013-01-04 | Saft Groupe Sa | Matiere active pour electrode negative d'accumulateur alcalin de type nickel hydrure metallique. |
| JP7261059B2 (ja) | 2019-03-29 | 2023-04-19 | Fdk株式会社 | ニッケル水素二次電池用の負極、この負極の製造方法、この負極を用いたニッケル水素二次電池及び水素吸蔵合金粉末 |
Citations (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN1219001A (zh) * | 1997-11-28 | 1999-06-09 | 株式会社东芝 | 镍氢二次电池 |
| CN1312594A (zh) * | 2001-04-13 | 2001-09-12 | 西安交通大学 | 一种大容量混合稀土镍氢电极合金 |
| JP2001316744A (ja) * | 2000-05-10 | 2001-11-16 | Toshiba Battery Co Ltd | 水素吸蔵合金およびアルカリ二次電池 |
| JP2002083593A (ja) * | 2000-09-06 | 2002-03-22 | Toshiba Corp | ニッケル水素二次電池、ハイブリッドカー及び電気自動車 |
| JP2002105563A (ja) * | 2000-09-29 | 2002-04-10 | Toshiba Corp | 水素吸蔵合金およびそれを用いたニッケル−水素二次電池 |
| US20030096164A1 (en) * | 1999-12-27 | 2003-05-22 | Isao Sakai | Hydrogen absorbing alloy and secondary battery |
| CN1443861A (zh) * | 2003-04-16 | 2003-09-24 | 华南理工大学 | 一种纳米晶多相混合稀土-镁系贮氢合金及其制备方法 |
Family Cites Families (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH11323469A (ja) | 1997-06-17 | 1999-11-26 | Toshiba Corp | 水素吸蔵合金及び二次電池 |
| KR100276018B1 (ko) * | 1997-11-28 | 2000-12-15 | 니시무로 타이죠 | 니켈수소 이차전지 |
-
2004
- 2004-01-26 JP JP2004016553A patent/JP4290023B2/ja not_active Expired - Lifetime
-
2005
- 2005-01-10 CN CNB2005100036714A patent/CN100428541C/zh not_active Expired - Lifetime
- 2005-01-25 US US11/041,678 patent/US7514178B2/en not_active Expired - Fee Related
Patent Citations (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN1219001A (zh) * | 1997-11-28 | 1999-06-09 | 株式会社东芝 | 镍氢二次电池 |
| US20030096164A1 (en) * | 1999-12-27 | 2003-05-22 | Isao Sakai | Hydrogen absorbing alloy and secondary battery |
| JP2001316744A (ja) * | 2000-05-10 | 2001-11-16 | Toshiba Battery Co Ltd | 水素吸蔵合金およびアルカリ二次電池 |
| JP2002083593A (ja) * | 2000-09-06 | 2002-03-22 | Toshiba Corp | ニッケル水素二次電池、ハイブリッドカー及び電気自動車 |
| JP2002105563A (ja) * | 2000-09-29 | 2002-04-10 | Toshiba Corp | 水素吸蔵合金およびそれを用いたニッケル−水素二次電池 |
| CN1312594A (zh) * | 2001-04-13 | 2001-09-12 | 西安交通大学 | 一种大容量混合稀土镍氢电极合金 |
| CN1443861A (zh) * | 2003-04-16 | 2003-09-24 | 华南理工大学 | 一种纳米晶多相混合稀土-镁系贮氢合金及其制备方法 |
Non-Patent Citations (1)
| Title |
|---|
| A study on the structure andelectrochemicalpropertiesofLa2Mg(Ni0.95M0.05)9 (M = Co,Mn, Fe, Al, Cu,Sn)hydrogenstorage electrode alloys. B.Liao et.al.Journal of Alloys and compounds,Vol.376 . 2004 * |
Also Published As
| Publication number | Publication date |
|---|---|
| JP4290023B2 (ja) | 2009-07-01 |
| CN1649191A (zh) | 2005-08-03 |
| US7514178B2 (en) | 2009-04-07 |
| US20050164083A1 (en) | 2005-07-28 |
| JP2005206908A (ja) | 2005-08-04 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN101378123B (zh) | 储氢合金电极及使用该储氢合金电极的碱蓄电池 | |
| CN102104145A (zh) | 贮氢合金、贮氢合金的制造方法和碱性蓄电池 | |
| CN101017894B (zh) | 碱性蓄电池用贮氢合金及碱性蓄电池 | |
| CN100428541C (zh) | 碱蓄电池用贮氢合金及其制造方法及碱蓄电池 | |
| JP4849854B2 (ja) | 水素吸蔵合金電極、アルカリ蓄電池及びアルカリ蓄電池の製造方法 | |
| CN100418253C (zh) | 碱蓄电池用贮氢合金、碱蓄电池及碱蓄电池的制造方法 | |
| JP2008210554A (ja) | アルカリ蓄電池用負極及びアルカリ蓄電池 | |
| JP4420767B2 (ja) | ニッケル・水素蓄電池 | |
| JP4958411B2 (ja) | 水素吸蔵合金電極及びアルカリ蓄電池 | |
| CN100433419C (zh) | 碱性蓄电池用贮氢合金及其制造方法和碱性蓄电池 | |
| JP5219338B2 (ja) | アルカリ蓄電池の製造方法 | |
| CN104584313B (zh) | 蓄电池系统 | |
| JP2004273261A (ja) | アルカリ蓄電池 | |
| JP4663451B2 (ja) | アルカリ蓄電池用水素吸蔵合金、アルカリ蓄電池用水素吸蔵合金の製造方法及びアルカリ蓄電池 | |
| CN111118346B (zh) | 含锆或钛a2b7型储氢合金、负极、电池及制备方法 | |
| CN1336014A (zh) | 贮氢合金电极、电极制造方法及碱性蓄电池 | |
| JP2008059818A (ja) | アルカリ蓄電池 | |
| JP5482024B2 (ja) | アルカリ蓄電池用水素吸蔵合金電極 | |
| CN115466880A (zh) | 低温型储氢合金、制备方法、镍氢合金电极及镍氢电池 | |
| JP2007066675A (ja) | アルカリ蓄電池用水素吸蔵合金の製造方法、アルカリ蓄電池用水素吸蔵合金及びアルカリ蓄電池 | |
| JPH0850919A (ja) | ニッケル・金属水素化物電池の製造方法 | |
| JP2006127817A (ja) | 水素吸蔵合金電極及びアルカリ蓄電池 | |
| JP2006107966A (ja) | ニッケル・水素蓄電池 | |
| JP2006278189A (ja) | アルカリ蓄電池用水素吸蔵合金及びニッケル・水素蓄電池 | |
| JP2004265720A (ja) | ニッケル−水素蓄電池 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| C06 | Publication | ||
| PB01 | Publication | ||
| C10 | Entry into substantive examination | ||
| SE01 | Entry into force of request for substantive examination | ||
| C14 | Grant of patent or utility model | ||
| GR01 | Patent grant | ||
| ASS | Succession or assignment of patent right |
Owner name: FDK CORPORATION Free format text: FORMER OWNER: SANYO ELECTRIC CO., LTD. Effective date: 20100409 |
|
| C41 | Transfer of patent application or patent right or utility model | ||
| COR | Change of bibliographic data |
Free format text: CORRECT: ADDRESS; FROM: OSAKA, JAPAN TO: TOKYO, JAPAN |
|
| TR01 | Transfer of patent right |
Effective date of registration: 20100409 Address after: Tokyo, Japan Patentee after: FDK Corp. Address before: Japan Osaka Patentee before: Sanyo Electric Co.,Ltd. |
|
| CX01 | Expiry of patent term | ||
| CX01 | Expiry of patent term |
Granted publication date: 20081022 |