WO2023157663A1 - Accessoire de prothèse dentaire de type à aimant - Google Patents

Accessoire de prothèse dentaire de type à aimant Download PDF

Info

Publication number
WO2023157663A1
WO2023157663A1 PCT/JP2023/003398 JP2023003398W WO2023157663A1 WO 2023157663 A1 WO2023157663 A1 WO 2023157663A1 JP 2023003398 W JP2023003398 W JP 2023003398W WO 2023157663 A1 WO2023157663 A1 WO 2023157663A1
Authority
WO
WIPO (PCT)
Prior art keywords
magnetic
stainless steel
magnet
cap
shield plate
Prior art date
Application number
PCT/JP2023/003398
Other languages
English (en)
Japanese (ja)
Inventor
本蔵義信
菊池永喜
本蔵晋平
Original Assignee
マグネデザイン株式会社
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by マグネデザイン株式会社 filed Critical マグネデザイン株式会社
Publication of WO2023157663A1 publication Critical patent/WO2023157663A1/fr

Abstract

[Problème] Former une partie de soudure ayant une excellente résistance à la soudure, assurant une force d'attraction magnétique élevée et un blindage magnétique suffisant, tout en simplifiant également le traitement. [Solution] Un capuchon 1 loge un aimant permanent 2 et comprend un acier inoxydable magnétique Cr. Une plaque de blindage 3 qui est un couvercle pour une ouverture évidée du capuchon 1 comprend un bord externe 32 formé à partir d'une partie non magnétique comprenant un acier inoxydable 18Cr-8Ni non modifié magnétiquement et une partie 31 constituant le reste, c'est-à-dire autre que le bord externe, de la plaque de blindage 3 et comprenant un aimant en acier inoxydable 18Cr-8Ni. Une partie de soudure est formée par soudage au laser à la limite entre le capuchon 1 et le bord externe 32 (partie non magnétique) de la plaque de blindage 3. Un dispositif de maintien (102) comprend un acier inoxydable magnétique doux Cr, et une couche de diffusion Cr est formée sur une face d'aspiration associée.
PCT/JP2023/003398 2022-02-18 2023-02-02 Accessoire de prothèse dentaire de type à aimant WO2023157663A1 (fr)

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
JP2022-023463 2022-02-18
JP2022023463A JP7125684B1 (ja) 2022-02-18 2022-02-18 磁石式義歯アタッチメント

Publications (1)

Publication Number Publication Date
WO2023157663A1 true WO2023157663A1 (fr) 2023-08-24

Family

ID=83005035

Family Applications (1)

Application Number Title Priority Date Filing Date
PCT/JP2023/003398 WO2023157663A1 (fr) 2022-02-18 2023-02-02 Accessoire de prothèse dentaire de type à aimant

Country Status (2)

Country Link
JP (1) JP7125684B1 (fr)
WO (1) WO2023157663A1 (fr)

Families Citing this family (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP7182231B1 (ja) 2022-03-18 2022-12-02 マグネデザイン株式会社 複合磁性Cr-Ni系ステンレス鋼製プレートとその製作する方法および複合磁性Cr-Ni系ステンレス磁石の製造方法

Citations (8)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS63122449A (ja) * 1986-09-15 1988-05-26 アンドレ.ガレル 着脱可能の義歯用保磁装置
US5123843A (en) * 1989-03-15 1992-06-23 Elephant Edelmetaal B.V. Magnet element for a dental prosthesis
JPH10179611A (ja) * 1996-12-19 1998-07-07 Aichi Steel Works Ltd 義歯アタッチメント磁石構造体の製造方法
JPH11309592A (ja) * 1998-04-23 1999-11-09 Aichi Steel Works Ltd 軟磁性体接合部の非磁性溶接方法
JP2001112784A (ja) * 1999-10-20 2001-04-24 Aichi Steel Works Ltd 義歯アタッチメント
JP2001321393A (ja) * 2000-03-09 2001-11-20 Aichi Steel Works Ltd 義歯アタッチメント
WO2015151845A1 (fr) * 2014-04-04 2015-10-08 日立金属株式会社 Structure d'aimant pour une fixation magnétique dentaire
JP2021063242A (ja) * 2019-10-10 2021-04-22 マグネデザイン株式会社 ステンレス磁石

Patent Citations (8)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS63122449A (ja) * 1986-09-15 1988-05-26 アンドレ.ガレル 着脱可能の義歯用保磁装置
US5123843A (en) * 1989-03-15 1992-06-23 Elephant Edelmetaal B.V. Magnet element for a dental prosthesis
JPH10179611A (ja) * 1996-12-19 1998-07-07 Aichi Steel Works Ltd 義歯アタッチメント磁石構造体の製造方法
JPH11309592A (ja) * 1998-04-23 1999-11-09 Aichi Steel Works Ltd 軟磁性体接合部の非磁性溶接方法
JP2001112784A (ja) * 1999-10-20 2001-04-24 Aichi Steel Works Ltd 義歯アタッチメント
JP2001321393A (ja) * 2000-03-09 2001-11-20 Aichi Steel Works Ltd 義歯アタッチメント
WO2015151845A1 (fr) * 2014-04-04 2015-10-08 日立金属株式会社 Structure d'aimant pour une fixation magnétique dentaire
JP2021063242A (ja) * 2019-10-10 2021-04-22 マグネデザイン株式会社 ステンレス磁石

Also Published As

Publication number Publication date
JP2023120529A (ja) 2023-08-30
JP7125684B1 (ja) 2022-08-25

Similar Documents

Publication Publication Date Title
US6652278B2 (en) Dental bar attachment for implants
WO2023157663A1 (fr) Accessoire de prothèse dentaire de type à aimant
US6299450B1 (en) Dental magnetic attachment
JPH08317941A (ja) 義歯アタッチメント
US6659771B2 (en) Denture attachment
JP3196249B2 (ja) 義歯安定用永久磁石組立体
JP7125686B1 (ja) 磁石式義歯アタッチメント
KR100808357B1 (ko) 의치 어태치먼트 및 그의 제조 방법
JP2795755B2 (ja) 義歯安定用永久磁石組立体
JP7125685B1 (ja) スリーブ付き磁石式義歯アタッチメントとその製造方法
EP3127506B1 (fr) Structure d'aimant pour une fixation magnétique dentaire
KR100331590B1 (ko) 의치 어태치먼트
JP3287531B2 (ja) 義歯固定用磁性アタッチメントおよびその製造方法
EP1586282B1 (fr) Fixation pour prothèse dentaire
JP2001112784A (ja) 義歯アタッチメント
JP7182231B1 (ja) 複合磁性Cr-Ni系ステンレス鋼製プレートとその製作する方法および複合磁性Cr-Ni系ステンレス磁石の製造方法
JP3483184B2 (ja) 義歯アタッチメント磁石構造体の製造方法
JP4811583B2 (ja) 磁性アタッチメント
JP3416932B2 (ja) 軟磁性体接合部の非磁性溶接方法ならびに義歯アタッチメント
EP1095629B1 (fr) Fixation magnétique dentaire
JPH10277062A (ja) 歯科用磁性アタッチメント及びその製造方法
JP3023315B2 (ja) 永久磁石構造体の製造方法および義歯固定用磁性アタッチメント
JP2007054618A5 (fr)
JP2002125987A (ja) 義歯固定用磁性アタッチメント
JP3496852B2 (ja) 義歯アタッチメント

Legal Events

Date Code Title Description
121 Ep: the epo has been informed by wipo that ep was designated in this application

Ref document number: 23756190

Country of ref document: EP

Kind code of ref document: A1