WO2009069685A1 - 自立膜型電解質・電極接合体 - Google Patents
自立膜型電解質・電極接合体 Download PDFInfo
- Publication number
- WO2009069685A1 WO2009069685A1 PCT/JP2008/071516 JP2008071516W WO2009069685A1 WO 2009069685 A1 WO2009069685 A1 WO 2009069685A1 JP 2008071516 W JP2008071516 W JP 2008071516W WO 2009069685 A1 WO2009069685 A1 WO 2009069685A1
- Authority
- WO
- WIPO (PCT)
- Prior art keywords
- electrolyte
- thickness
- free
- electrode assembly
- ions move
- Prior art date
Abstract
Priority Applications (5)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP2009543840A JP5021761B2 (ja) | 2007-11-27 | 2008-11-27 | 自立膜型電解質・電極接合体 |
DE602008005190T DE602008005190D1 (de) | 2007-11-27 | 2008-11-27 | Freistehende membranelektrolyt-elektrodenanordnung |
AT08854112T ATE499717T1 (de) | 2007-11-27 | 2008-11-27 | Freistehende membranelektrolyt- elektrodenanordnung |
US12/740,060 US8399146B2 (en) | 2007-11-27 | 2008-11-27 | Free-standing membrane electrolyte electrode assembly |
EP08854112A EP2224521B1 (en) | 2007-11-27 | 2008-11-27 | Free-standing membrane electrolyte electrode assembly |
Applications Claiming Priority (2)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP2007-306337 | 2007-11-27 | ||
JP2007306337 | 2007-11-27 |
Publications (2)
Publication Number | Publication Date |
---|---|
WO2009069685A1 true WO2009069685A1 (ja) | 2009-06-04 |
WO2009069685A9 WO2009069685A9 (ja) | 2009-08-13 |
Family
ID=40678577
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
PCT/JP2008/071516 WO2009069685A1 (ja) | 2007-11-27 | 2008-11-27 | 自立膜型電解質・電極接合体 |
Country Status (6)
Country | Link |
---|---|
US (1) | US8399146B2 (ja) |
EP (1) | EP2224521B1 (ja) |
JP (1) | JP5021761B2 (ja) |
AT (1) | ATE499717T1 (ja) |
DE (1) | DE602008005190D1 (ja) |
WO (1) | WO2009069685A1 (ja) |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2011171289A (ja) * | 2010-01-19 | 2011-09-01 | Honda Motor Co Ltd | 電解質・電極接合体及びその製造方法 |
JP2017504946A (ja) * | 2014-01-14 | 2017-02-09 | エルコゲン エーエス | Sofc陰極拡散バリア層を生成する方法およびsofc |
US10774012B2 (en) | 2015-07-30 | 2020-09-15 | Mitsui Mining & Smelting Co., Ltd. | Substrate/oriented apatite-type composite oxide film complex and method for producing same |
Families Citing this family (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
WO2019146493A1 (ja) * | 2018-01-29 | 2019-08-01 | 三井金属鉱業株式会社 | 酸素透過素子及びスパッタリングターゲット材 |
JP2023097844A (ja) * | 2021-12-28 | 2023-07-10 | 株式会社デンソー | 自立型薄膜及びその製造方法 |
Citations (7)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH09190825A (ja) | 1996-01-10 | 1997-07-22 | Toho Gas Co Ltd | 固体電解質型燃料電池及びそれに用いられる単電池 |
JPH1171169A (ja) * | 1997-08-27 | 1999-03-16 | Miyuki Kawaguchi | 酸化物イオン導電性セラミックス及びその製造方法 |
JPH11130595A (ja) | 1997-10-30 | 1999-05-18 | Daiichi Kigensokagaku Kogyo Co Ltd | 酸化物イオン導電性単結晶及びその製造方法 |
JP2003277024A (ja) * | 2002-03-22 | 2003-10-02 | Honda Motor Co Ltd | 酸化物イオン導電体およびその製造方法 |
JP2005149795A (ja) | 2003-11-12 | 2005-06-09 | Honda Motor Co Ltd | 電解質・電極接合体及びその製造方法 |
JP2005149797A (ja) * | 2003-11-12 | 2005-06-09 | Honda Motor Co Ltd | 電解質・電極接合体 |
JP2005158377A (ja) * | 2003-11-25 | 2005-06-16 | Nissan Motor Co Ltd | 固体電解質型燃料電池 |
Family Cites Families (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
AU2001274926A1 (en) * | 2000-05-22 | 2001-12-03 | Acumentrics Corporation | Electrode-supported solid state electrochemical cell |
US6770395B2 (en) * | 2000-10-23 | 2004-08-03 | Materials And Systems Research, Inc. | Internally manifolded, planar solid oxide fuel cell (SOFC) stack with an inexpensive interconnect |
EP1531511B1 (en) * | 2003-11-12 | 2012-10-24 | Honda Motor Co., Ltd. | Electrolyte-electrode assembly and method for producing the same |
KR20080020259A (ko) * | 2006-08-31 | 2008-03-05 | 삼성에스디아이 주식회사 | 연료 전지용 막-전극 어셈블리, 이의 제조방법 및 이를포함하는 연료 전지 시스템 |
-
2008
- 2008-11-27 US US12/740,060 patent/US8399146B2/en active Active
- 2008-11-27 JP JP2009543840A patent/JP5021761B2/ja active Active
- 2008-11-27 WO PCT/JP2008/071516 patent/WO2009069685A1/ja active Application Filing
- 2008-11-27 EP EP08854112A patent/EP2224521B1/en not_active Not-in-force
- 2008-11-27 DE DE602008005190T patent/DE602008005190D1/de active Active
- 2008-11-27 AT AT08854112T patent/ATE499717T1/de not_active IP Right Cessation
Patent Citations (7)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH09190825A (ja) | 1996-01-10 | 1997-07-22 | Toho Gas Co Ltd | 固体電解質型燃料電池及びそれに用いられる単電池 |
JPH1171169A (ja) * | 1997-08-27 | 1999-03-16 | Miyuki Kawaguchi | 酸化物イオン導電性セラミックス及びその製造方法 |
JPH11130595A (ja) | 1997-10-30 | 1999-05-18 | Daiichi Kigensokagaku Kogyo Co Ltd | 酸化物イオン導電性単結晶及びその製造方法 |
JP2003277024A (ja) * | 2002-03-22 | 2003-10-02 | Honda Motor Co Ltd | 酸化物イオン導電体およびその製造方法 |
JP2005149795A (ja) | 2003-11-12 | 2005-06-09 | Honda Motor Co Ltd | 電解質・電極接合体及びその製造方法 |
JP2005149797A (ja) * | 2003-11-12 | 2005-06-09 | Honda Motor Co Ltd | 電解質・電極接合体 |
JP2005158377A (ja) * | 2003-11-25 | 2005-06-16 | Nissan Motor Co Ltd | 固体電解質型燃料電池 |
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2011171289A (ja) * | 2010-01-19 | 2011-09-01 | Honda Motor Co Ltd | 電解質・電極接合体及びその製造方法 |
US9070946B2 (en) | 2010-01-19 | 2015-06-30 | Honda Motor Co., Ltd. | Electrolyte-electrode joined assembly and method for producing the same |
JP2017504946A (ja) * | 2014-01-14 | 2017-02-09 | エルコゲン エーエス | Sofc陰極拡散バリア層を生成する方法およびsofc |
US10774012B2 (en) | 2015-07-30 | 2020-09-15 | Mitsui Mining & Smelting Co., Ltd. | Substrate/oriented apatite-type composite oxide film complex and method for producing same |
Also Published As
Publication number | Publication date |
---|---|
JP5021761B2 (ja) | 2012-09-12 |
DE602008005190D1 (de) | 2011-04-07 |
ATE499717T1 (de) | 2011-03-15 |
EP2224521A4 (en) | 2010-09-01 |
JPWO2009069685A1 (ja) | 2011-04-14 |
EP2224521B1 (en) | 2011-02-23 |
US20100248073A1 (en) | 2010-09-30 |
EP2224521A1 (en) | 2010-09-01 |
WO2009069685A9 (ja) | 2009-08-13 |
US8399146B2 (en) | 2013-03-19 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
WO2008061174A3 (en) | Secondary electrochemical cell with high rate capability | |
WO2008066853A3 (en) | Activation of solid oxide fuel cell electrode surfaces | |
WO2009069685A1 (ja) | 自立膜型電解質・電極接合体 | |
WO2009155546A8 (en) | Electrolysis cell having electrodes with various-sized/shaped apertures | |
WO2009089018A3 (en) | Porous electrodes and associated methods | |
WO2008121972A3 (en) | Deposited microarchitectured battery and manufacturing method | |
WO2008139157A8 (en) | A silicon anode for a rechargeable battery | |
DK1877168T3 (da) | SOFC-katodemateriale med høj ydeevne i intervallet 450C - 650C | |
WO2008078755A1 (ja) | 電池、電極およびこれらに用いる集電体 | |
TW200725970A (en) | High rate capability design of lithium ion secondary battery | |
WO2005121413A3 (en) | Battery with molten salt electrolyte and phosphorus-containing cathode | |
GB0501590D0 (en) | Processing of enhanced performance LSCF fuel cell cathode microstructure and a fuel cell cathode | |
TWI365564B (en) | Cathode for fuel cell having two kinds of water-repellency and method of preparing the same and membrane electrode assembly and fuel cell comprising the same | |
WO2008118137A3 (en) | Solar cells which include the use of high modulus encapsulant sheets | |
WO2006013108A3 (en) | Long-life membrane electrode assemblies | |
WO2004093217A3 (en) | Cathode active material with increased alkali metal content and method of making the same | |
JP2007280665A5 (ja) | ||
WO2008023322A3 (en) | Electrochemical energy source, and method for manufacturing of such an electrochemical energy source | |
WO2007134091A3 (en) | Secondary electrochemical cell with increased current collecting efficiency | |
WO2008126358A1 (ja) | 高分子電解質形燃料電池及びそれを備える燃料電池スタック | |
WO2009011132A1 (ja) | リチウムイオン二次電池 | |
MX2013000695A (es) | Bateria bipolar. | |
WO2006104543A3 (en) | Durable hydrophilic coatings for fuel cell bipolar plates | |
WO2011064637A8 (en) | Fuel cell | |
EP2421080A3 (en) | Non-aqueous electrolyte battery |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
ENP | Entry into the national phase |
Ref document number: 2009543840 Country of ref document: JP Kind code of ref document: A |
|
121 | Ep: the epo has been informed by wipo that ep was designated in this application |
Ref document number: 08854112 Country of ref document: EP Kind code of ref document: A1 |
|
WWE | Wipo information: entry into national phase |
Ref document number: 2008854112 Country of ref document: EP |
|
WWE | Wipo information: entry into national phase |
Ref document number: 12740060 Country of ref document: US |
|
NENP | Non-entry into the national phase |
Ref country code: DE |