WO2005084433A1 - 撒き餌、それに用いる水溶性容器の製造方法及び該製造方法に使用する金型 - Google Patents

撒き餌、それに用いる水溶性容器の製造方法及び該製造方法に使用する金型 Download PDF

Info

Publication number
WO2005084433A1
WO2005084433A1 PCT/JP2005/003876 JP2005003876W WO2005084433A1 WO 2005084433 A1 WO2005084433 A1 WO 2005084433A1 JP 2005003876 W JP2005003876 W JP 2005003876W WO 2005084433 A1 WO2005084433 A1 WO 2005084433A1
Authority
WO
WIPO (PCT)
Prior art keywords
water
mold
soluble container
container
soluble
Prior art date
Application number
PCT/JP2005/003876
Other languages
English (en)
French (fr)
Inventor
Masateru Mizuno
Noriyoshi Kumooka
Koso Kato
Takanao Sogawa
Original Assignee
Foster Co., Ltd
Kabushiki Kaisha Hayashibara Seibutsu Kagaku Kenkyujo
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Foster Co., Ltd, Kabushiki Kaisha Hayashibara Seibutsu Kagaku Kenkyujo filed Critical Foster Co., Ltd
Priority to JP2006510767A priority Critical patent/JPWO2005084433A1/ja
Publication of WO2005084433A1 publication Critical patent/WO2005084433A1/ja

Abstract

 撒き餌の取扱が良好であると共に、仕掛けと確実に同調することを可能とし、環境にも優しい水溶性容器に内蔵される撒き餌を提供することを目的とする。  水溶性容器に内蔵される撒き餌において、該容器が水溶性多糖および/またはその誘導体を主成分とする材料で構成されていることを特徴とする。好ましくは、水溶性多糖および/またはその誘導体がプルランであり、また水溶性容器内にはリモナイト65,67を収容することを特徴とする。さらに、水溶性容器が半俵状の形状を有する胴部60と蓋部61とからなり、胴部の開口部分に蓋部の凸状部分を挿入するかまたは当該開口部分を蓋部の凹状部分で覆うことにより、容器を形成することを特徴する。

Description

撒き餌、それに用いる水溶性容器の製造方法及び該製造方法に使用す る金型
技術分野
[0001] 本発明は、魚介類を捕獲するための釣りに用いる撒き餌に関し、特に、温水、冷水
、海水などに素早く溶解すると共に、環境に優しい水溶性容器に内蔵された撒き餌 に関するものである。さらに、本発明は、前記撒き餌に用いる水溶性容器を効率的に 製造するための製造方法や、その製造方法で使用する金型に関する。
背景技術
[0002] 釣り用の撒き餌としては、魚介類嫌めさせるために、海面より撒くものや、海底に 沈め自然に崩壊させるもの、また、釣糸に固定した籠を用いて海水中で自然又はし やくりにより放出させる方法などがある。
撒き餌の材料としては、ォキアミ、アミェビなどが集魚力が高いと考えられており、一 般的に多く用いられている。また、魚種によってはサナギなどが集魚力を発揮するこ とがある。実際に撒き餌を使用する際には、パン粉やオカラなどと集魚剤を混ぜること により、狙う魚種の生息する棚に効果的に撒き餌することが可能であると考えられて いる。
[0003] これらの撒き餌の材料、特に集魚剤は、臭いが悪ぐ準備作業中に攪拌する際〖こ は、異臭が手に付くなどの問題がある。使用に関しても、仕掛けと撒き餌を同調しな ければ効果がないため、必要以上に大量の撒き餌を行うこともある。
また、残った撒き餌は海水中に廃棄されることが多ぐ撒き餌の材料や量によって 環境汚染に繋がる場合がある。
この撒き餌による環境汚染により、魚影が薄くなり釣果が得られなくなると、釣り人は さらに多くの撒き餌を用いて釣りを行うこととなる。このため、その撒き餌によりさらに環 境汚染が進むといった悪循環が発生することが危惧される。
撒き餌には、上述の問題を改善するべく以下のような事項が求められている。
( 1)臭 、や見た目などの取扱性が良好であること。 (2)使用量を抑えるために仕掛けと確実に同調させること。
(3)未使用の撒き餌を廃棄せずに、次回の釣りに持ち越しできること。
(4)環境汚染に繋がらな 、材料で構成されて!、ること。
[0004] これらの問題を解決すベぐ以下の特許文献 1又は 2においては、撒き餌の材料を 水溶性容器に内蔵する方法が開示されている。
これらの特許文献においては、撒き餌を所定の分量だけ小分けにし、各々を水溶 性容器に内蔵することが開示されており、これにより、異臭の発生を抑制することがで き、取扱性を良好にすることが可能となる。
また、所定時間で水溶性容器が溶解し、該容器内の撒き餌を海水中に放出させる ことが可能となる。
特に、水溶性容器の材料として、特許文献 1においてはポリビニルアルコール系ポ リマーが、特許文献 2においては、バオゲンなどの水溶性榭脂を用いた複合紙が提 示されている。
特許文献 1:実用新案登録第 2508558号公報
特許文献 2:特開平 11 341940号公報
[0005] また、一般に押し固められた撒き餌は水中で分散することが困難になってしまうた め、以下の特許文献 3— 5においては、撒き餌の材料の中に発泡剤を混合し、海水 中での分散を補助する方法が提案されて ヽる。
特許文献 3:特開平 2 - 163027号公報
特許文献 4:特開平 5— 192063号公報
特許文献 5 :特開 2001-86912号公報
[0006] 以上のような文献があるにも関わらず、現状では、水溶性容器を利用する撒き餌は
、市販されていない。これは、水溶性材料の多くが、体温程度の温度や、攪拌などの 条件が必要である上に、海水中の塩類によって溶解が阻害されるためと考えられる。 また、ポリビニルアルコールにおいては、溶解速度が低いため、比較的長い時間か けて溶解した方が好ましい場合に用いられる。バオゲンにおいては、溶解速度は高 いが、融点が 55°C程度と低いために、取扱に注意する必要がある。また、両者は食 品添加物としては未認可であり、環境への負荷も懸念される。 さらに、撒き餌を押し固めた場合においては、発泡剤を用いても十分に拡散させる ことが困難となるなどの問題を生じている。
発明の開示
発明が解決しょうとする課題
[0007] 本発明が解決しょうとする課題は、上述した問題を解決し、撒き餌の取扱が良好で あると共に、仕掛けと確実に同調することを可能とし、環境にも優しい水溶性容器に 内蔵される撒き餌を提供することである。
さらに、本発明は、前記撒き餌に用いる水溶性容器を効率的に製造するための製 造方法や、その製造方法で使用する金型を提供することを目的とする。
課題を解決するための手段
[0008] 上記課題を解決するための手段としては、請求項 1に係る発明は、水溶性容器に 内蔵される撒き餌にぉ ヽて、水溶性容器が水溶性多糖を主成分とする材料で構成さ れることを特徴とする。
本発明にお 、て「水溶性多糖」とは、水中での溶解速度が調整可能な材料であり、 容器を形成した際に撒き餌材料の充填作業並びに撒き餌使用時の取扱いに耐える 十分な機械的強度を有し、溶解した際に自然環境への負荷が極めて少ない多糖お よび Zまたはその誘導体を意味する。
[0009] 請求項 2に係る発明は、請求項 1に記載の撒き餌において、水溶性容器が半俵状 の形状を有する胴部と蓋部とからなり、胴部の開口部分に蓋部の凸状部分を挿入す る力または当該開口部分を蓋部の凹状部分で覆うことにより、容器を形成することを 特徴する。
[0010] 請求項 3に係る発明は、請求項 1又は 2に記載の撒き餌において、該水溶性多糖 および Zまたはその誘導体がプルランを主成分とする材料で構成されることを特徴と する。
[0011] 請求項 4に係る発明は、請求項 1乃至 3のいずれかに記載の撒き餌において、該水 溶性容器内には無機性水質浄ィ匕材を収容することを特徴とする。
本発明において「無機性水質浄ィ匕材」とは、例えば、黒ボタ、リン酸アパタイト、赤鉄 鉱、リモナイトなどの水質浄ィ匕材を意味し、請求項 5に係る発明のように、とりわけリモ ナイトが好ましぐまた、該リモナイトなどの無機性水質浄ィ匕材は粒状部分又は打状 部分を有することが好まし 、。
[0012] 請求項 6に係る発明は、請求項 1乃至 5のいずれかに記載の撒き餌において、水溶 性容器が嵌合して容器を形成する 2つの構造体カゝらなり、 2つの構造体の嵌合部は、 水溶性多糖および Zまたはその誘導体の水溶液で接着されていることを特徴とする また、好ましくは、該水溶性多糖および Zまたはその誘導体の水溶液はプルラン水 溶液であることを特徴とする。さらに好ましくは、該プルラン水溶液には、発酵乳酸ナ トリウムが添加されて 、ることを特徴とする。
[0013] 請求項 7に係る発明は、請求項 1乃至 6のいずれかに記載の撒き餌において、水溶 性容器が溶解時間の異なる少なくとも 2種の水溶性容器壁を有することを特徴とする
[0014] 請求項 8に係る発明は、請求項 1乃至 7のいずれかに記載の撒き餌において、水溶 性容器が水溶性材料又は生分解性材料による取付具、あるいは、金属製又は榭脂 製の取付具を有することを特徴とする。
[0015] 請求項 9に係る発明は、請求項 1乃至 8のいずれかに記載の撒き餌に用いる水溶 性容器の製造方法にお!ヽて、水溶性容器を構成する材料を含む水溶液中に金型を 浸漬する浸漬工程と、該金型を該水溶液力 引き上げる引き上げ工程と、該金型に 付着した水溶液を乾燥させる乾燥工程と、該金型から水溶性容器を離型する離型ェ 程とを含む水溶性容器の製造方法であり、該金型は、少なくとも該乾燥工程におい ては所定温度に維持され、該離型工程においては該所定温度より低い他の温度に 保持されると共に、該所定温度と該他の温度との間で体積変化率が 0. 1%以上を有 する材質で、少なくとも該金型の水溶性容器を形成する部分が構成されて!ヽることを 特徴とする。
[0016] 本発明において、「少なくとも乾燥工程においては」という意味は、浸漬工程、引き 上げ工程、及び乾燥工程のうち、乾燥工程のみ又は乾燥工程と他の工程との組み 合わせの!/、ずれの場合も含むと!、う意味である。
また、金型の「所定温度」とは、上記乾燥工程を含む各工程において、厳密に同一 温度であることを意味するものではなぐ金型に付着した水溶液を乾燥 ·硬化して水 溶性容器を形成するまでの間に、金型が温度変化により変形しても、所望の水溶性 容器が形成される温度範囲を含むものである。
さらに、本発明の「金型」とは、榭脂、金属などの多様な材料を利用することが可能 であり、上記体積変化率の条件を満足するものであれば、特に限定されるものではな い。
[0017] 請求項 9に係る発明においては、好ましくは、該浸漬工程、該引き上げ工程、該乾 燥工程を複数回繰り返すことを特徴とする。
また、請求項 9に係る発明において、好ましくは、該乾燥工程において、金型を斜 めに傾けて水溶液を乾燥させることを特徴とする。
また、請求項 9に係る発明において、好ましくは、該離型工程は、空気を水溶性容 器内部又は外部に送り込むことにより、あるいは水溶性容器を外側から吸着すること により、金型と水溶性容器を離型することを特徴とする。
[0018] 請求項 10に係る発明は、請求項 9のいずれかに記載の撒き餌に用いる水溶性容 器の製造方法において、該浸漬工程に利用する水溶液には、脱泡処理を施すことを 特徴とする。
[0019] 請求項 11に係る発明は、請求項 9又は 10のいずれかに記載の水溶性容器の製造 方法に使用する金型において、少なくとも該金型の水溶性容器を形成する部分が、 該所定温度と該他の温度との間で体積変化率が 0. 1%以上を有する材質で構成さ れていることを特徴とする。
[0020] 請求項 12に係る発明は、請求項 11に記載の水溶性容器の製造方法に使用する 金型において、該金型は、少なくとも該水溶液に接触する部分の吸水率が 0. 1-1 %の材質で形成されて!、ることを特徴とする。
[0021] 請求項 13に係る発明は、請求項 11又は 12に記載の水溶性容器の製造方法に使 用する金型において、該金型の表面には、金型の水溶性容器を形成する部分の領 域近傍に、水溶液の液溜りを形成する窪みを有していることを特徴とする。
[0022] 請求項 14に係る発明は、請求項 11乃至 13のいずれかに記載の水溶性容器の製 造方法に使用する金型において、該金型の内部には、金型の水溶性容器を形成す る部分に繋がる空気穴を有して 、ることを特徴とする。
発明の効果
[0023] 請求項 1に係る発明により、水溶性容器に内蔵される撒き餌において、水溶性容器 が水溶性多糖および Zまたはその誘導体を主成分とする材料で構成されるため、水 中で適切に撒き餌が撒布され、撒き餌の製造や取扱いが容易となり、さらに環境に 対しても優し!/ヽ撒き餌を提供することが可能となる。
[0024] 請求項 2に係る発明により、水溶性容器が半俵状の形状を有する胴部と蓋部とから なり、胴部の開口部分に蓋部の凸状部分を挿入する力または当該開口部分を蓋部 の凹状部分で覆うことにより、容器を形成するため、容器内に撒き餌材料を効率よく 充填できる上、容器に加わる機械的圧力による容器の破損防止することも可能となる
[0025] 請求項 3に係る発明により、水溶性多糖および Zまたはその誘導体がプルランを主 成分とする材料で構成されるため、温水、冷水、海水を問わず素早く溶解することが 可能となる。
また、プルランは溶解時にゲルィ匕することがなぐ該容器内の撒き餌の放出を阻害 することが少ない。し力もプルランは、食品添加物として多用されており、人体を含む 自然環境にも優 、素材である。
このような、プルランを原料とする水溶性容器に、撒き餌を内臓することによって、撒 き餌自体の異臭の発生を抑制することが可能となり、取扱性が良好であると共に、未 使用の撒き餌を廃棄せずに、次回の釣りに持ち越しできるなど、多くの利点を有する
[0026] 請求項 4に係る発明により、水溶性容器内には無機性水質浄化材を収容するため 、無機性水質浄化材が水中に拡散し、濁水性を向上させるだけでなぐ無機性水質 浄ィ匕材の水質浄ィ匕作用により、極めて環境に優しい撒き餌を提供することが可能と なる。
特に、請求項 5に係る発明のように、無機性水質浄ィ匕材としてリモナイトを用いること により、優れた濁水性や水質浄ィ匕作用を実現することが可能となる。
また、該リモナイトなどの無機性水質浄ィ匕材は粒状部分又は打状部分を有すること により、無機性水質浄ィ匕材の単位重量当りの表面積が低下し、リモナイトなどの無機 性水質浄化材の脱臭作用が低下することから、水溶性容器内に収容された魚粉など の撒き餌材料の臭いをリモナイトなどが吸収することを抑え、集魚性の低下が抑制さ れる。
また、打状部分は、水溶性容器内の仕切り部材としても使用でき、異なる種類の撒 き餌材料の分離や、撒き餌材料と他の添加剤との分離、さらには、粉体のリモナイトと 臭い成分有する撒き餌材料との分離などに効果的に使用できる。
[0027] 請求項 6に係る発明により、水溶性容器が嵌合して容器を形成する 2つの構造体か らなり、 2つの構造体の嵌合部は、水溶性多糖および Zまたはその誘導体の水溶液 で接着されているため、接着材料の水溶性容器との接着性が良好であり、接着後は 容器壁面と一体化する。また、接着材料も容器と同様に、水中で分解し、環境に与え る影響も少ない。
また、該水溶性多糖および Zまたはその誘導体の水溶液をプルラン水溶液とする ことにより、プルランの優れた特性を備えた接着材料となる。し力も、このようなプルラ ン水溶液に、発酵乳酸ナトリウムを添加することにより、プルラン水溶液が塗布された 箇所の容器が硬化せず、柔軟性を維持することが可能となる。その上、プルラン水溶 液の塗布作業中に液ダレを起こすことも防止できる。
[0028] 請求項 7に係る発明により、水溶性容器が溶解時間の異なる少なくとも 2種の水溶 性容器壁を有するため、水溶性容器の溶解時間を、該容器の部位で異なるように構 成することが可能であり、より早く溶解する部位力 内蔵する撒き餌を放出するために 、撒き餌の量や拡散に要する時間を調整することが可能となる。
[0029] 請求項 8に係る発明では、水溶性容器が水溶性材料又は生分解性材料による取 付具、あるいは、金属製又は榭脂製の取付具を有している。水溶性もしくは生分解性 の取付具の場合には、所定の場所で水溶性容器に内蔵される撒き餌を固定すること が可能となり、仕掛けと撒き餌の同調を容易に実現することが可能となる。結果的に、 使用する撒き餌の量自体も抑制することが可能となる。また、取付具も容器と同様に 水中で溶解又は分解するため、極めて環境に優しい撒き餌を提供することが可能と なる。 [0030] また、金属製又は榭脂製の取付具の場合には、取付具を再利用でき、使用時には 取付具の先端部を水溶性容器に貫通させるだけで容易に取付具と水溶性容器と一 体化することが可能となる。
しかも、取付具の先端部を、水溶性容器を構成する 2つの構造体が接着されている 部分など、水溶性容器の中でも最後に溶解する部分あるいは機械的強度の高い部 分に固定することにより、水溶性容器を最後まで釣り糸に保持することなどが可能と なる。
[0031] 請求項 9に係る発明により、浸漬形成法に用いる金型は、少なくとも乾燥工程にお ける形状と、離型工程における形状とでは、体積変化率が 0. 1%以上も変化してい るため、離型工程時においては、金型と水溶性容器との間に隙間が形成され、水溶 性容器の金型力もの離型性を改善することが可能となる。
これにより、プルランを主成分とする水溶性容器のように離型性が劣る場合であつ ても、容易に製造することが可能となる。
[0032] また、浸漬工程、引き上げ工程、乾燥工程を複数回繰り返すことにより、所要の膜 厚を有する水溶性容器を製造することができ、水溶性容器の溶解時間を任意に調整 可能となる。
また、乾燥工程において、金型を斜めに傾けて水溶液を乾燥させることにより、水 溶液の液ダレを防ぎ、均一な厚みの容器を形成できると共に、容器の金型から離型 性を向上し、容器を離型した後に残る不要な水溶液の乾燥部分の発生も抑制するこ とが可能となる。
より好ましくは、乾燥時に金型を回転させることにより、均一な容器の形成など上記 効果をより高めることが可能となる。
さらに、離型工程は、空気を水溶性容器内部又は外部に送り込むことにより、あるい は水溶性容器を外側から吸着することにより、容易に金型と水溶性容器を離型するこ とが可能となる。
[0033] 請求項 10に係る発明により、浸漬工程に利用する水溶液には、超音波又は真空 状態を利用する脱泡処理が施されて!、るため、弓 Iき上げ工程時に金型に付着した水 溶液中に気泡が入り込むことが無ぐ水溶性容器へ気泡の混入を防止することが可 能となる。
[0034] 請求項 11に係る発明により、請求項 9に係る発明と同様に、金型の少なくとも水溶 性容器を形成する部分が、少なくとも乾燥工程における形状と、離型工程における形 状とでは、体積変化率が 0. 1%以上も変化しているため、離型工程時においては、 金型と水溶性容器との間に隙間が形成され、水溶性容器の金型からの離型性を改 善することが可能となる。
[0035] 請求項 12に係る発明により、金型は、少なくとも該水溶液に接触する部分の吸水 率が 0. 1— 1%の材質で形成されているため、水溶液が金型に付着し残留し易ぐし 力も乾燥した水溶性容器が金型力も離型され易い条件を満足することが可能となる。
[0036] 請求項 13に係る発明により、金型の表面には、金型の水溶性容器を形成する部分 の領域近傍に、水溶液の液溜りを形成する窪みが設けられているため、金型を下向 きに乾燥させた場合においては、溶液が金型力 完全に落下するのを防止し、金型 に溶液を残留させることを補助する効果を有する。また、金型を上向きに乾燥させる 場合には、金型の下部に液ダレが発生するのを防止する効果が期待できる。
[0037] 請求項 14に係る発明により、離型工程は、金型に設けられた空気穴により、空気を 水溶性容器内に送り込むことにより、金型と水溶性容器とを容易に離型することが可 能となる。
図面の簡単な説明
[0038] [図 1]本発明の水溶性容器に内蔵される撒き餌を釣具に用いた概略を示した図であ る。
[図 2]本発明の水溶性容器に内蔵される撒き餌を示した説明図である。
[図 3]本発明の撒き餌の使用経過を示す図である。
[図 4]本発明に係る金型部材の概略図である。
[図 5]本発明に係る金型の一部の拡大図である。
[図 6]本発明の撒き餌に用いる水溶性容器の製造方法を示す図である。
[図 7]本発明に係る撒き餌の組立の様子を示す図である。
[図 8]本発明の撒き餌に用いる取付具を示す図である。
[図 9]本発明の撒き餌に使用する無機性水質浄化材の収容状態を示す図である。 符号の説明
[0039] 1 釣竿
2 リール
3 釣糸
4 釣針
5 ゥキ
6 サノレカン
7 水溶性容器 (撒き餌内蔵)
8 誘導式サルカン
9, 63, 72 取付部
10, 61, 71 蓋部
11, 60, 70 月同部
12 付け餌
13 撒き餌
21 金型
22 支持体
23 窪み
24 空気穴
31 水溶液
40 恒温室
65, 67, 68 無機性水質浄化材
発明を実施するための最良の形態
[0040] 本発明に係る撒き餌及び該撒き餌に用いる水溶性容器の製造方法、並びに該製 造方法に使用する金型について、以下に詳細に説明する。
図 1は、水溶性容器に内蔵される撒き餌 7を誘導式サルカン 8を用いてに取り付け た状態を示す概略図であり、 1は釣竿、 2はリール、 3は釣糸、 4は釣針、 5はゥキ、 6 はサルカンを示す。
[0041] 図 2は、水溶性容器に内蔵される撒き餌 7の拡大図である。 水溶性容器に内蔵される撒き餌 7の水溶性容器は、俵型の形状を構成する、蓋部 10と胴部 11により形成されて 、る。水溶性容器の蓋部 10には取付部 9が設けられて いる。
[0042] 図 3は、水溶性容器に内蔵される撒き餌 7の使用経過図である。
海面から撒き餌をする場合の使用経過を示しており、図 3 (a)のように仕掛けを準備 しキャスティングを行う。海面上では、図 3 (b)のように容器が溶け、中の撒き餌 13を 放出し始める。その後、図 3 (c)のように付け餌 12と撒き餌 13が同調し始める。最後 は、図 3 (d)のように撒き餌を放出し終わる時期には、容器は海水中に溶解することと なる。
[0043] 水溶性容器は、プルランを主成分として構成されており、海水中で素早く溶解する ように材料が選定されており、該容器には撒き餌の材料と好ましくは放出補助剤が内 蔵されている。
[0044] 撒き餌の材料に必要な機能として、集魚性、拡散性、濁水性、沈殿性などが求めら れる。一般的にォキアミ、アミェビ、サナギ、ニンニク、コーポなどの集魚を目的とした ものの他に、パン粉、オカラ、ムギ、コーン、カキガラ、海砂などを狙う魚種によって適 宜混合して用いられて!/ヽる。これらの撒き餌の材料を乾燥状態で水溶性容器に内臓 することができる。
また、集魚剤から抽出したエキスを、浸透性の高い材料と混合して水溶性容器に内 蔵することも可能である。
[0045] さらに、水溶性容器内に収容する材料には、黒ボタ、リン酸アパタイト、赤鉄鋼、リモ ナイトなどの無機性水質浄ィ匕材を用いるのが好適であり、とりわけ、リモナイトが含ま れることが好ましい。
リモナイトは、褐鉄鉱とも呼ばれ、酸ィ匕鉄をはじめ多くのミネラル分を含むものであり 、水中では、水中の過剰なリンを吸着除去し、有用なミネラルの水への付加を行う作 用を持つ。このため、水質浄化 (藻の分解除去や透明度の向上など)に必要なバクテ リアの活動を活発にし、水質の浄ィ匕を促進する機能を有するものである。し力も、水 中で容易に拡散するため、釣りに好適な濁水性も有して 、る。
[0046] 図 3では、海面上に撒き餌 7が浮遊する状態にて撒き餌の散布を行う方法を示した 力 これに限らず、狙う魚種の生息する棚によって比重を変え、海面から撒き餌をす る方法や、海水の中層から撒き餌をする方法や、海底に沈めて撒き餌をする方法を とることが可能である。本発明の撒き餌においては、水溶性容器内に撒き餌材料を収 容した状態において、比重が 0. 8より小さいと、水面上で撒き餌が浮き過ぎ、水面と 撒き餌との接触面積が減少し、水溶性容器の溶解状態も不均一となるため、撒き餌 材料の撒布に支障を来たすこととなる。また、比重が 1. 5より大きいと、撒き餌の水中 での下降速度が速すぎ、撒き餌が下降途中で撒布され難ぐ集魚性が低下するとい う問題がある。比重に関して、より好ましくは、上物の魚を狙う場合は比重 0. 9前後、 底物の魚を狙うには 1. 05前後が望ましい。
なお、上記比重は、水溶性容器の寸法から体積を計算し、水溶性容器の重量を該 体積で除した数値を参考として 、る。
[0047] 上述した放出補助剤とは、撒き餌を放出する際に、溶解の始まった水溶性容器の 粘性により放出が阻害されることを避けるためのものである。また、撒き餌自体が固ま つてる場合も放出が困難になるが、その場合でも放出を補助することが必要である。
[0048] しかし、放出補助剤の割合を高くすることによって、撒き餌の材料自体の量が減ると 、集魚効果自体の低下に繋がってしまう。また、放出補助剤として発泡剤を用いた場 合、例えば炭酸水素ナトリウムとクェン酸を混合したものにより発生した二酸ィ匕炭素に よって、容器自体が浮力を持ってしまう可能性があり、海底付近に該容器を沈めて用 いることが困難になる。以上のことより、撒き餌の材料に対して放出補助剤は一割以 下となるように調整することが好ま 、。
[0049] 本発明に係る水溶性容器の材料としては、水中での溶解速度が調整可能な材料 であり、容器を形成した際に撒き餌材料の充填作業並びに撒き餌使用時の取扱いに 耐える十分な機械的強度を有し、溶解した際に自然環境への負荷が極めて少ない 水溶性多糖および Zまたはその誘導体が適して 、る。このような条件を満たす材料 に、プルランが該当する。
プルランは、デンプンを原料とし、黒酵母の一種である Aureobasidium pullulansを培 養して得られた、マルトトリオースが規則正しく α— 1, 6結合した天然多糖類である。 プルランは、急性毒性、亜急性毒性、慢性毒性、変異原性の各試験において安全 性が確認されており、我が国で使用制限のな 、添加物として扱われて ヽる。
プルランは、冷水、温水のいずれにも速やかに溶解し、ジメチルホルムアミドゃジメ チルスロホキシド以外の一般の有機溶媒には不溶である。しかも、プルラン水溶液は 他の多糖類に比べ、比較的低粘性で、ゲルィ匕することがなぐ粘着性の強い溶液に なる性質を有する。また、 pHや各種塩類の影響を受けにくぐ特に食塩に対しても安 定した粘度を維持する。ホウ素やチタンの混在により粘度が急激に増大するが、この 場合でもゲルイ匕することはな 、と 、う性質をもって 、る。
[0050] 本発明に係る水溶性容器の材料としては、上記のプルランに限定されるものではな ぐ上述した条件を満足する材料であれば、本発明に好適に使用可能である。 プルラン以外の水溶性材料を列挙すると、水溶性多糖としては、例えば、澱粉、 OC ィ匕澱粉、酸化澱粉、デキストリン、ジアルデヒド澱粉、リン酸化澱粉、ェチル化澱粉、 プロピル化澱粉、カルボキシメチルスターチ、カルボキシメチルセルロース、メチルセ ノレロース、ヒドロキシェチノレセノレロース、ヒドロキシプロピノレメチノレセノレロース、セノレ口 ースフタレートアセテート、アルギン酸、アルギン酸塩、マンナン、寒天、ぺクチン、キ サンタンガム、キトサン、ゲランガム、カラギーナンなどがある。
[0051] 本発明の水溶性容器に使用する際には、上記の各種材料を単体もしくは適宜組合 せ、また、必要に応じて種々の添加剤を添加することにより、上述した条件を満足す るよう調整することが、好ましい。以下では、プルランを中心に説明するが、これに限 定されるものではないことは、言うまでもない。
[0052] 水溶性多糖、特にプルランを主成分とした場合、水溶液を加熱乾燥することで成型 品を得ることができる。そのために用いることができる成型法は、浸漬成形である。浸 漬成形では、型をプルラン水溶液に浸漬することで附着させる。浸漬により得た薄膜 を加熱乾燥した後に離型させ、水溶性容器を得ることができる。浸漬成形においては 、附着、硬化 (乾燥)、離型が成型品を得るための条件となる。
水溶性容器の製造方法及び該製造方法で使用する金型につ!、ては、後で詳述す る。
[0053] 本発明においては、自然環境への負荷を軽減するため、可能な範囲でプルランを 多く含む水溶性容器を形成することが好ま Uヽ。プルランのみで水溶性容器を成形 することは可能であるが、必要に応じて硬化促進剤としてゲル化剤もしくは無機剤な どを添加することもできる。また、ゲル化剤等によって柔軟性や強度を持たせるなど、 多様な機能を付加することも可能である。ゲル化剤としては、例えば、カラギナン、キ サンタンガム、グァガム、ローカストビーンガム、ジエランガム、アラビアガム、サイリウ ムシードガム、カードラン、ぺクチン、タラガム、タマリンドシードガム、アルギン酸塩、 コンニヤクマンナン、ガラタトマンナン、澱粉、ゼラチン、カゼインなど多種の候補が挙 げられる。無機剤としては、酸化チタン、ケイソゥ土、活性白土などが挙げられる。 なお、ゲル化剤及び無機物についても、食品添加物として扱われており、安全性に ついては確認されている。
[0054] ゲル化剤の多くは海水中の塩類と反応しゲルを形成するために、ゲル化剤の添カロ が少量で済むように数種のゲル化剤を組み合わせたり、ゲルィ匕補助剤を用いるのが 好ましい。ここで言うゲルィ匕補助剤とは、ゲル化剤と反応し硬化を促進させる材料の ことである。ゲルィ匕補助剤としては、カルシウム塩、カリウム塩、ナトリウム塩などの塩 類ゃキレート物質がある。
なお、撒き餌を内蔵する水溶性容器としての目的を達成するためには、ゲル化剤の 量や種類を十分に選別する必要がある。
[0055] また、撒き餌の放出を調整するために水溶性容器の溶解速度を調整する必要があ る。
溶解速度の調整手段として、容器の厚みを調整する方法が好ましいが、強度や成 形性の点カゝら容器の厚みの調整だけでは、目的とする溶解時間が得られない場合も あり、このような場合には、二糖類などを添加し水溶性容器の溶解を速める方法など も併用することも可能である。
[0056] 本発明に係る撒き餌を組み立てる際には、図 2に示すような蓋部 10と胴部 11とを接 合し、水溶性容器を形成する方法だけでなぐ図 7に示すような容器も使用可能であ る。図 7の水溶性容器は、図 2と同様に水溶性容器を 2つの構造体である、半俵状の 形状を有する胴部 60と蓋部 61とから構成される。組立の際には、胴部 60に撒き餌材 料 (リモナイトなど必要な材料を含む)を入れ、胴部 60の開口部分に蓋部 61の凸状 部分を挿入して、図 7 (b)に示す矢印の箇所 (胴部と蓋部との接触部。特に胴部と蓋 部とが露出している境界線部分)を後述する接着材料で接合する。図 7に示すような 容器の構造は、胴部 60に撒き餌材料を挿入した後、蓋部 61を介して作業者の指や 必要な冶具により容器内の撒き餌材料を押圧し充填率を高めることができる。し力も 、図 2のような俵型と比較し、蓋部と胴部とを押圧する際に、容器の一部が変形又は 破損するなどの不具合も除去できる。
[0057] 水溶性容器内にリモナイトなどの無機性水質浄ィ匕材 (以下、リモナイトを中心に説 明する)を収容する際には、図 9 (a)に示すように、魚粉などの臭い成分を有する撒き 餌材料 66の中にリモナイト 65を分散させため、リモナイトを粒状に形成して混入する ことが好ましい。これは、リモナイトの単位重量当りの表面積が低下し、リモナイトの脱 臭作用が低下することから、水溶性容器内に収容された魚粉などの撒き餌材料の臭 ぃをリモナイトが吸収することを抑え、集魚性の低下を抑制するためである。
また、図 9 (b)に示すように、リモナイト 67を打状に形成し、上述した効果に加え、水 溶性容器内の仕切り部材として使用することも可能である。この仕切り部材は、異なる 種類の撒き餌材料の分離や、撒き餌材料と他の添加剤との分離、さら〖こは、単位重 量当りの表面積が多!、粉体のリモナイト 68と臭 、成分有する撒き餌材料 66との分離 などに効果的に使用できる。なお、粉体のリモナイトは水中で速やかに拡散するため 、本発明の撒き餌として好適に使用できる。
さらに、リモナイト以外の撒き餌材料の多くは、比重が水より軽い傾向があることから 、リモナイトを粒状又は打状とすることにより、上述した撒き餌の比重の調整が、極め て容易に行うことが可能となる。
[0058] 次に、撒き餌の釣り糸への取付具について説明する。
水溶性容器に内蔵される撒き餌を用いて釣りを行う際に、仕掛けと撒き餌を同調さ せるために、該容器を仕掛け付近に固定し、撒き餌を放出し終えるまでは固定し続 けなければならない。また、少なくとも撒き餌を放出し終えるまで溶解しないような取 付部が必要となる。ただし、取付部だけが残る場合には、新しい撒き餌を取り付ける 際に、まず残った取付部を外す必要があり、外した取付部をゴミとして処分するなど、 使用者としては使 、勝手が悪 、ものとなる。
[0059] また、取付部を極端に溶解を遅くしたとしても、海水中で水溶性容器の取付部付近 が溶解すれば、水溶性容器と取付部が外れ、結果として撒き餌が仕掛けカゝら離れた 場所で放出されることになる。
[0060] そこで、取付部付近には比較的溶解が遅 ヽ水溶性容器壁を有する構造にすること で撒き餌を放出し終えるまで固定することが可能となり、確実に仕掛けと撒き餌を同 調させることが可會 となる。
例えば、水溶性容器の蓋部 10を、胴部 11により溶解時間が長い構成とすることに より、放出時間中には、取付部 9と蓋部 10とが外れないよう設定されている。
[0061] また、取付部についてはキャスティングにも耐えうる強度が必要となる。それに加え て、取付部が水溶性容器本体力も外れないように、接合強度が高くなるような構造に もしなければならない。
[0062] 上記の観点を考慮し、図 8 (a)に示すように、金属製又は榭脂製の取付具 63を使 用することが好ましい。取付具 63は、針金などの線状材料を図 8 (a)のように折り曲げ て形成することができる。取付具には釣り糸に取付けられたサルカンなどと係合する ループ 64が形成されている。また、取付具の先端部は、水溶性容器に貫通され、水 溶性容器を保持する構成となって ヽる。取付具の先端部を水溶性容器に貫通させる 箇所は、水溶性容器を構成する胴部 60と蓋部 61とが接着されている部分など、水溶 性容器の中でも最後に溶解する部分ある ヽは機械的強度の高 ヽ部分に固定するこ とにより、水溶性容器を最後まで釣り糸に保持することなどが可能となる。
なお、取付具の形成方法は、上述した方法に限らず、射出成形などにより構成する ことも可能である。
[0063] また、図 8 (b)に示すように、胴部 70と蓋部 71とを接合し、プルランなどを使用した 取付具 72を水溶性容器に付着させることも可能である。取付具の付着部分 73は、胴 部 70と蓋部 71との接合箇所や、機械的強度が高い場合には図 2のように蓋部等に 接着すること可能である。
取付部の材料としては、環境への影響も考慮して、水溶性材料や生分解性材料を 利用することが好ましい。プルランは、フィルム状では、ポリビニールアルコールと比 較して、抗張力は約 3倍、弾性率は約 100倍であり、腰が強ぐ優れた引張り強度を 有して 、ることなどから、取付部の材料としてプルランを利用することも可能である。 また、プルランを利用することにより、取付部と水溶性容器とを同じ材料を多く含む 構成すとすることで、両者の接合強度を高くすることが可能である。
[0064] 水溶性容器に撒き餌を内蔵させた後には、胴部 11と蓋部 10とを接合することが好 ましい。胴部と蓋部とを嵌合させるのみでは、使用に耐えうる強度を得ることが困難で ある上、異臭の問題を十分に解決することができない。
接合方法としては、容器がプルランを主な成分とするため、水分もしくは蒸気によつ て接合する方法を採用することが可能である。あるいは、プルランを利用した糊料や テープ状シートを用いて接合することも可能である。
特に、胴部及び蓋部の 2つの構造体の嵌合部の接着剤には、水溶性多糖および Zまたはその誘導体の水溶液、特にプルラン水溶液を用いることが好ましぐさらに はプルラン水溶液に発酵乳酸ナトリウムを添加した材料を用いることが好ま 、。この ような接着剤は、プルラン水溶液が塗布された箇所の容器が硬化せず、柔軟性を維 持することが可能となる。しかも、接着剤が粘性を持っため、プルラン水溶液の塗布 作業中に液ダレを起こすことも防止できる。
[0065] 次に、本発明に係る撒き餌に用いる水溶性容器の製造方法及び該製造方法に使 用する金型について、以下に詳細に説明する。
図 4は、本発明に利用される金型部材の概略図である。
金型 21は、ヒータを内蔵した支持体 22に固定されている。ヒータは、支持体に設け るものに限らず、金型内に内蔵するよう構成することも可能である。また、このような内 蔵型のヒータを用いる代わりに、金型を湯水などの高温の液体に浸漬する方法や、 あるいは外部の熱源や誘導加熱手段などにより金型を加熱することも可能である。
[0066] 金型 21には、図 5に示すように、溝などの窪み 23が形成されている。金型は、図 5 の矢印 25の位置まで水溶液中に浸漬され、乾燥時には、図 4ように上向き、あるいは 下向きで静置される。該窪み 23により、金型を下向きに乾燥させた場合においては、 溶液が金型力 完全に落下するのを防止し、金型に溶液を残留させることを補助す る効果を生じ、また、金型を上向きに乾燥させる場合には、金型の下部に液ダレが発 生するのを防止する効果が生じる。
[0067] また、金型 21の内部には、図 5に示すように、空気穴 24が形成されている。該空気 穴 24は、離型工程時に、金型に設けられた空気穴から、外側に空気を送出すること により、水溶性容器内に空気を送り込み、金型と水溶性容器とを容易に離型すること を可能とする。
該空気穴 24の開口部の大きさは、金型を上向きで乾燥させる場合には、水溶液が 空気穴に侵入することがない範囲で任意に選択することが可能である。また、空気穴 の数も、 1つ以上設けることも可能である。
[0068] 金型の材質としては、水溶性容器の形状を決定する乾燥工程における金型の形状 と、離型工程における金型の形状とでは、体積変化率が 0. 1%以上の変化を生ずる 材質が好ましい。
プルランを多く含む水溶性容器のように離型性が劣る容器を形成する場合、容器 の内側の体積 (乾燥時の金型の体積)と、該容器に取り囲まれた金型の体積 (離型時 の金型の体積)とが、体積変化率で 0. 1%以上の差がある場合には、金型と水溶性 容器との間に隙間が形成され、容器を容易に金型から離型することが可能となる。 このような体積変化は、金型の温度を変更することにより容易に達成することが可能 であり、乾燥工程時の温度と離型工程時の温度との差が大きい場合には、熱膨張係 数が小さい材質も、本発明の金型として利用することが可能である。
[0069] また、金型に関しては、水溶性容器を形成する水溶液が金型に付着することが必 要であると共に、該水溶液が乾燥した後は容易に金型力 剥がれることが必要である ことから、金型の材質として、少なくとも該水溶液に接触する部分の吸水率が 0. 1— 1%であることが好ましい。
金型への水溶液の付着特性は、金型の吸水率のみに依存するものではなぐ水溶 液の粘性にも依存する。し力しながら、粘性が高い水溶液を用いる場合には、水溶 性容器の厚みが増すと共に、容器内の部位 (上部、胴部、開口部など)により膜の厚 みが異なる傾向となる。特に、数十一数百 mの範囲内で、均質な膜厚を形成する 場合には、吸水率が 0. 1— 1%の範囲内に抑制することが好ましい。
吸水率とは、常温で 24時間、乾燥した試料を水に浸漬させた場合、試料が吸収す る水の重量を、試料の乾燥重量で除した割合である。
[0070] 上記体積変化率や吸水率を満足する金型の材料としては、金属、榭脂など多種の ものがあるが、中でもポリアセタールなどの榭脂系材料に好適なものが多く見られる。 また、本発明においては、温度変化を利用して体積変化を発生させているため、金 型の水溶性容器に取り囲まれた部分を均等に変化させるためには、金型の材料とし ては熱伝導性が高 、ものの方が好ま U、。
[0071] 次に、水溶性容器の製造方法について説明する。
図 6に示すように、水溶性容器の製造方法は、浸漬工程 (図 6 (a) )、引き上げ工程 、乾燥工程 (図 6 (b) )、離型工程 (図 6 (c) )により構成され、必要な膜厚を得るために 、乾燥工程後に、再度、浸漬工程、引き上げ工程、乾燥工程を複数回繰り返すことも 可能である。
[0072] 浸漬工程においては、図 6 (a)に示すように、容器 10内に蓄えられた水溶液 11に、 金型 1の先端を浸漬させる。金型は図 5に示す矢印 25の位置まで、浸漬させられる。 水溶液は、水溶性容器を構成する材料を水に溶解させたものである。浸漬工程時 の水溶液の温度は、常温あるいは昇温など、適宜設定することができる。ただし、 10 0°C以上に加温すると、溶媒の水が気化し、気泡が発生する原因ともなり好ましくない また、水溶液は粘性を有しており、溶液中に気泡が混入する場合がある。このような 気泡は、浸漬形成法では、成形体に空洞を形成する原因ともなることから、水溶液に 超音波を印加する方法、あるいは、水溶液を真空中に静置させる方法などにより脱 泡処理することが好ましい。
[0073] 金型の浸漬時間は、期待する水溶性容器の膜厚などにより適宜設定することが可 能である。
浸漬工程後は、金型を水溶液中から引き上げる、図示していない引き上げ工程に 移る。引き上げ工程は、金型に付着した余分な水溶液を落とし、膜厚を均質化するた めに行われる。
[0074] 乾燥工程においては、水溶液 31が付着した金型を図 6 (b)のように上向きに静置、 あるいは下向きに静置させ、恒温室 40内に収容し、水溶液 31中の水分を蒸発させ る。
乾燥時間は、水溶液の組成や加熱炉の温度、さらには複数回浸漬させる場合の途 中の段階か最終段階かにより異なるが、離型工程に移る前には、金型と水溶性容器 との離型が行える程度に、充分乾燥し硬化させることが必要である。
[0075] 乾燥工程においては、金型を、支持体等に内蔵したヒータにより加熱し、必要な水 溶性容器の形状に保持することが必要である。なお、金型の加熱は、乾燥工程時の みならず、浸漬工程、引き上げ工程などにおいても行うことが可能である。ただし、加 熱温度は、上述した水溶液の加熱と同様に、 100°C以下とすることが好ましい。 また、この金型の加熱は、金型に付着した水溶液の乾燥を補助する役割も期待で きる。
[0076] さらに、乾燥工程においては、金型を鉛直方向に対して斜めに傾けて水溶液を乾 燥させることが好ましい。この構成により、水溶液の液ダレを防ぎ、均一な厚みの容器 を形成できると共に、容器の金型から離型性を向上し、容器を離型した後に残る不要 な水溶液の乾燥部分の発生も抑制することが可能となる。
し力も、乾燥時に金型を回転させることにより、均一な容器の形成など上記効果をよ り一層高めることが可能となる。
[0077] 離型工程にぉ 、ては、金型を冷却し、図 6 (c)のように、金型に設けた空気穴より空 気 50を送出し、金型から水溶性容器 42を離型する。
冷却温度は、恒温室 40における金型の体積と比較し、体積変化率が 0. 1%以上と なる温度を設定する。
水溶性容器に対する空気の送出は、図 6 (c)のように金型の内部に設けた空気穴 力 行うだけでなぐ金型の周囲に圧縮空気の送出手段を一つ以上配置し、水溶性 容器の開口部付近から、該水溶性容器を取り出す方向に向けて、空気を送出するよ う構成することにより、より効果的に水溶性容器の離型を行うことが可能となる。
また、空気の送出に限らず、吸着手段を利用して、水溶性容器の外側から該水溶 性容器を吸着した状態で、該吸着手段を金型力も離間させることにより、水溶性容器 を金型力ゝら離型することも可能である。
[0078] 金型が図 5に示すように窪み 23を有する場合には、該窪み部分が離型を阻害する 場合がある。このような場合には、窪み 23の上側の位置で乾燥した水溶性容器に切 り込みを入れ、該切り込みの下側に付着する水溶液の乾燥又は半乾燥状態の部分 を除去する。そして、その後、上述した離型工程を行うことが好ましい。 乾燥又は半乾燥状態の切除部は、水に溶解させて水溶性容器の原料として、再利 用することが可能である。
実施例
[0079] 以下、本発明に係る具体的な実施例について説明する。
(水溶液の製造)
プルラン (商品名 PF— 20,株式会社林原製)を 50gを水 200gに入れ、攪拌してプ ルランを溶解した。プルラン水溶液を一晩放置することにより脱泡処理を行い、水溶 液 1を得た。
[0080] (金型)
ポリアセタール (製品名ポリペンコアセタール, 日本ポリペンコネ土製,吸水率 0. 2% )を用いて切削加工を施し、直径 35mmの円柱状で先端部に同径の半球状の曲部を 有する金型 1を得た。
次に、ナイロン 66 (製品名ポリペンコ N, 日本ポリペンコ社製,吸水率 8. 4%)、を用 いて、金型 1と同様にカ卩ェし、金型 2を得た。
アルミニウム (製品名 A5052,住友軽金属社製,吸水率 0%)、真鍮 (製品名 C360 4,三宝伸銅工業社製,吸水率 0%)、鉄 (製品名 SS400,新日本製鉄社製,吸水率 0%)を用いて、金型 1と同様に加工し、金型 3, 4, 5を得た。
[0081] (水溶性容器の製造)
30°Cの水溶液 1に、 90°Cに加熱した金型 1を 15秒浸漬し (浸漬工程)、その後、金 型 1を水溶液から引き上げ、水溶液上で 30秒間静止して余分な水溶液を落下させた (引き上げ工程)。
水溶液の付着した金型 1を、水溶性容器側を上向きにして、 90°Cの恒温室内にて 10分間加熱し、水溶液を乾燥させた (乾燥工程)。金型 1を恒温室から取り出し、 50 °Cまで冷却した後、成形された水溶性容器を金型 1から取り出し (離型工程)、実施 例 1の水溶性容器を得た。
以下、表 1に示すように、水溶液 1, 2と金型 1一 4、並びに冷却温度とを組合わせて 、実施例 1と同様に成形し、実施例 2— 8の水溶性容器を得た。 体積変化率は、各金型が 90°Cと冷却温度にお!ヽて示す金型の直径をノギスで測 £し、算出し 7こ。
[0082] (離型性の評価)
成形した各水溶性容器に関し、金型上に形成された水溶性容器の開口部付近か ら、該水溶性容器を取り出す方向に向けて、圧縮空気を供給し、該容器の金型から の剥がれ易さを、金型力 容易に離型可能なものを〇、容器の一部は剥離するが完 全に離型するのが困難であるもの△、離型が全く困難であったものを Xとして、離型 性を評価した。
[0083] (水溶液の付着性の評価)
成形した各水溶性容器に関し、引き上げ工程において、水溶液の金型への付着状 態を目視により観察し、付着状態が良好なものを〇、付着しない部分が見られるもの を Xとして、付着性を評価した。
[0084] [表 1]
Figure imgf000024_0001
[0085] 表 1の結果より、体積変化率力 以上の場合には、離型性が改善するものの、 実施例 2のように、吸水率が 8. 4%と高い場合には、体積変化率が高くても、離型性 が低下することが理解される。
また、吸水率が 0%となる金型 3— 5を用いる場合には、水溶液の付着性が劣り、水 溶液 1よりプルランを多く含む粘性の高い水溶液を用いる必要がある。ただし、粘性 が高い場合には、一般的に均一な厚みの膜や薄い膜を形成することが困難となる傾 向にあり、金型に応じた最適な粘性を確保することが必要である。
本出願人が詳細に検証したところ、体積変化率が 0. 1%以上の場合には、良好な 離型性が確保でき、吸水性に関しては、 0. 1一 1%の範囲であるなら、離型性を阻害 せず、良好な付着性を確保することが可能であることが判明した。
[0086] 金型の特徴として、金型の材料に金属を用いた場合には、材料の熱伝導率が高い ため、加熱や乾燥の際に必要とする時間が短い傾向にあるが、水溶液の付着性や 離型性に関しては劣る傾向にある。また、金型の材料に榭脂を用いた場合には、熱 伝導率が低いために、加熱や乾燥に必要な時間が長い傾向にあるが、離型性に関 してはポリアセタールが良好な結果が得られた。この原因として、ポリアセタールの膨 張率、吸水率が金型として好ましい状況にあるという理由だけでなぐポリアセタール 自体の潤滑性も寄与して 、ると想定される。
[0087] (複数回の浸漬による膜厚調整)
30°Cの水溶液 1に、 90°Cに加熱した金型 1を 15秒浸漬し (浸漬工程)、その後、金 型 1を水溶液から引き上げ、水溶液上で 30秒間静止して余分な水溶液を落下させた (引き上げ工程)。水溶液の付着した金型 4を、水溶性容器側を上向きにして、 90°C の恒温室内にて 5分間加熱し、水溶液を乾燥させた (乾燥工程)。
再度、 30°Cの水溶液 1に、 90°Cに加熱した上記金型 1を 15秒浸漬し (浸漬工程)、 その後、金型 4を水溶液から引き上げ、水溶液上で 30秒間静止して余分な水溶液を 落下させた (引き上げ工程)。水溶液の付着した金型 1を、水溶性容器側を上向きに して、 90°Cの恒温室内にて 15分間加熱し、水溶液を乾燥させた(乾燥工程)。
金型 1を恒温室から取り出し、 50°Cまで冷却した後、成形された水溶性容器を金型 1から取り出し (離型工程)、実施例 6の水溶性容器を得た。
[0088] 実施例 6について、水溶性容器の膜厚を、容器の先端を除く上部側面と、容器開 口部を除く下部側面とで測定したところ、上部側面では 80 m、下部側面では 70 mが得られた。なお、実施例 1の水溶性容器の膜厚は、上部側面では 40 /z m 下部 側面では 35 μ mであった。
このことから、本発明による浸漬形成法を用いることにより、適切な膜厚に調整可能 なことが理解される。
[0089] (金型の空気穴による離型)
金型 1の長軸に沿って、金型中央に直径 0.5mmの空気穴を開けた金型を利用して 、上記実施例 1と同様に水溶性容器を成形した。 離型工程時に、該空気穴より、圧縮空気を送出したところ、水溶性容器が容易に金 型から離型された。
[0090] (金型の窪みによる効果)
金型 4の先端から 5cmの位置に、幅 8mm、深さ lmmの半球形状の溝を掘り、上記 実施例 4と同様に水溶性容器を成形した。
引き上げ工程時の様子を観察すると、水溶液の金型への付着が不十分な部分も存 在するものの、実施例 4と比較して、未付着部分の範囲が大幅に縮小していることが 理解された。
また、金型 1に、金型 4と同様の処理を施し、上記実施例 1と同様に水溶性容器を 形成したところ、乾燥工程時に上向きに静置した金型力ゝらの液ダレが、該溝から下へ の液ダレが、実施例 1のものより、減少していることが確認された。
[0091] (水溶液のプルラン濃度について)
水 200gに対して、プルラン (株式会社林原製、商品名 PF— 20)を 40g、 50g、 60g 、 70g、 80gと変化させた水溶液を作成し、上記実施例 1と同様に水溶性容器を成形 した。
[0092] その結果、プルランの添加量が多いほど粘性が高くなるため、プルランを 70g以上 カロえた場合には、一晩放置しても十分な脱泡はできず、容器を成形する際にも気泡 が容器壁に残存するなどの不具合が生じた。
また、 70g以上加えた粘度の高い溶液では、容器の壁面の厚みムラが大きぐ例え ば、厚い部分に合わせて乾燥時間を長した場合に、薄い部分の水分含有量が極端 に低くなり、容器の壁がひび割れや欠けなどの問題を生じる。さらに、容器の壁の厚 みが異なる場合には、水中での溶解時間にもバラツキが生じることとなる。
[0093] プルランを 40gカ卩えた粘度の低い水溶液では、金型への付着が悪ぐ乾燥途中で 剥がれが発生する。
ムラのなく付着性のよい水溶液としては、水 200gに対するプルランの添カ卩量は、 4 Ogより多く、 70gより少ない範囲が好ましぐより最適には、プルランを 50g— 60g添カロ した時に取扱の良好なプルラン水溶液を得ることができる。
[0094] (ゲル化剤等の添加剤による成形性の変化) 水 200gに対し、プルランを 40g添カ卩した水溶液 2、該水溶液 2に酸ィ匕チタン 4gを添 加した水溶液 3、該水溶液 2にカッパカラギナン 2gと塩ィ匕カリウム 2gを添カ卩した水溶 液 4、及び該水溶液 2にカッパカラギナン lgとキサンタンガム lgを添カ卩した水溶液 5と を、水溶液 1と同様に調整した。
次に、実施例 1と同様に金型 1を用いて水溶性容器を成形し、実施例 7— 10を得た
[0095] 実施例 7— 10に関し、付着性、乾燥性及び離型性を評価した。
付着性については、実施例 7を基準に、付着性が良くなるものを〇、若干良くなるも のを△、悪くなるものを Xとして評価する。
乾燥性については、実施例 7を基準に、乾燥が速いものを〇、乾燥が若干遅いもの を△、乾燥がより遅いものを Xとして評価する。
離型性については、実施例 7を基準に、離型し易くなるものを〇、離型性に差異が ないものを△、離型し難《なるものを Xとして評価する。
これらの評価結果を表 2に示す。
[0096] [表 2]
Figure imgf000027_0001
[0097] 表 2の結果より、酸ィ匕チタンを添加する場合には、実施例 8のように、付着性の低下 は見られるものの、乾燥性や離型性は向上することが理解される。
また、ゲル化剤であるカッパカラギナンとゲルィ匕補助剤である塩ィ匕カリウムを添加す る場合には、実施例 9のように、付着性、乾燥性、及び離型性のいずれも性能が向上 することが理解される。
ゲル化剤であるカッパカラギナンとキサンタンガムとを添加する場合には、付着性及 び離型性は向上するものの、乾燥性が劣る上、容器の膜厚ムラが大きくなる。
[0098] ゲル化剤を添加することにより、一般的に付着性や離型性が向上するが、他方、乾 燥性や膜厚の均一性が低下する傾向にあるため、ゲル化剤の種類及び添加量は、 適切に選択することが必要である。
[0099] (溶解時間の変化)
上記実施例 7— 10の各容器を利用して撒き餌用の水溶性容器を構成し、該水溶 性容器内に撒き餌 10gを収容した撒き餌カプセルを作成した。
該撒き餌カプセルを、 18°Cの流れのない海水に投下し、水溶性容器内の撒き餌の 放出開始時間を計測したところ、実施例 7のカプセルは約 2分半、実施例 8のカプセ ル及び実施例 9のカプセルは約 3分、そして、実施例 10のカプセルは約 4分であった 水溶性容器の溶解時間は、容器の厚みが厚くなるに従い、長くなる傾向にあり、ま た、ゲル化剤を添加することにより、溶解時間が遅延する傾向にあることが理解される 産業上の利用可能性
[0100] 本発明によれば、撒き餌の取扱が良好であると共に、仕掛けと確実に同調すること を可能とし、環境にも優しい水溶性容器に内蔵される撒き餌を提供することが可能と なる。
し力も、本発明は、前記撒き餌に用いる水溶性容器を効率的に製造するための製 造方法や、その製造方法で使用する金型を提供することができるなど、多くの利点を 有するものである。

Claims

請求の範囲
[1] 水溶性容器に内蔵される撒き餌において、水溶性容器が水溶性多糖および Zまた はその誘導体を主成分とする材料で構成されることを特徴とする撒き餌。
[2] 請求項 1に記載の撒き餌にぉ 、て、水溶性容器が半俵状の形状を有する胴部と蓋 部とからなり、胴部の開口部分に蓋部の凸状部分を挿入する力または当該開口部分 を蓋部の凹状部分で覆うことにより、容器を形成することを特徴する撒き餌。
[3] 請求項 1又は 2に記載の撒き餌において、該水溶性多糖および Zまたはその誘導 体がプルランを主成分とする材料で構成されることを特徴とする撒き餌。
[4] 請求項 1乃至 3のいずれかに記載の撒き餌において、該水溶性容器内には無機性 水質浄化材を収容することを特徴とする撒き餌。
[5] 請求項 4に記載の撒き餌において、該水溶性容器内に収容される無機性水質浄化 材がリモナイトであることを特徴とする撒き餌。
[6] 請求項 1乃至 5のいずれかに記載の撒き餌において、水溶性容器が嵌合して容器 を形成する 2つの構造体からなり、 2つの構造体の嵌合部は、水溶性多糖および Zま たはその誘導体の水溶液で接着されていることを特徴とする撒き餌。
[7] 請求項 1乃至 6のいずれかに記載の撒き餌において、水溶性容器が溶解時間の異 なる少なくとも 2種の水溶性容器壁を有することを特徴とする撒き餌。
[8] 請求項 1乃至 7のいずれかに記載の撒き餌において、水溶性容器が水溶性材料又 は生分解性材料による取付具、あるいは、金属製又は榭脂製の取付具を有すること を特徴とする撒き餌。
[9] 請求項 1乃至 8のいずれかに記載の撒き餌に用いる水溶性容器の製造方法にお いて、
水溶性容器を構成する材料を含む水溶液中に金型を浸漬する浸漬工程と、該金 型を該水溶液カゝら引き上げる引き上げ工程と、該金型に付着した水溶液を乾燥させ る乾燥工程と、該金型から水溶性容器を離型する離型工程とを含む水溶性容器の 製造方法であり、
該金型は、少なくとも該乾燥工程においては所定温度に維持され、該離型工程に おいては該所定温度より低い他の温度に保持されると共に、該所定温度と該他の温 度との間で体積変化率が 0. 1%以上を有する材質で、少なくとも該金型の水溶性容 器を形成する部分が構成されていることを特徴とする撒き餌に用いる水溶性容器の 製造方法。
[10] 請求項 9のいずれかに記載の撒き餌に用いる水溶性容器の製造方法において、該 浸漬工程に利用する水溶液には、脱泡処理を施すことを特徴とする撒き餌に用いる 水溶性容器の製造方法。
[11] 請求項 9又は 10のいずれかに記載の水溶性容器の製造方法に使用する金型にお いて、少なくとも該金型の水溶性容器を形成する部分が、該所定温度と該他の温度 との間で体積変化率が 0. 1%以上を有する材質で構成されていることを特徴とする 水溶性容器の製造方法に使用する金型。
[12] 請求項 11に記載の水溶性容器の製造方法に使用する金型において、該金型は、 少なくとも該水溶液に接触する部分の吸水率が 0. 1— 1%の材質で形成されている ことを特徴とする水溶性容器の製造方法に使用する金型。
[13] 請求項 11又は 12に記載の水溶性容器の製造方法に使用する金型において、該 金型の表面には、金型の水溶性容器を形成する部分の領域近傍に、水溶液の液溜 りを形成する窪みを有していることを特徴とする水溶性容器の製造方法に使用する 金型。
[14] 請求項 11乃至 13のいずれかに記載の水溶性容器の製造方法に使用する金型に おいて、該金型の内部には、金型の水溶性容器を形成する部分に繋がる空気穴を 有していることを特徴とする水溶性容器の製造方法に使用する金型。
PCT/JP2005/003876 2004-03-09 2005-03-07 撒き餌、それに用いる水溶性容器の製造方法及び該製造方法に使用する金型 WO2005084433A1 (ja)