US20030002210A1 - Thin-film coil, magnetic head, method of manufacturing the thin-film coil, and method of manufacturing the magnetic head - Google Patents

Thin-film coil, magnetic head, method of manufacturing the thin-film coil, and method of manufacturing the magnetic head Download PDF

Info

Publication number
US20030002210A1
US20030002210A1 US10/145,507 US14550702A US2003002210A1 US 20030002210 A1 US20030002210 A1 US 20030002210A1 US 14550702 A US14550702 A US 14550702A US 2003002210 A1 US2003002210 A1 US 2003002210A1
Authority
US
United States
Prior art keywords
coil
film
thin
winding
manufacturing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Abandoned
Application number
US10/145,507
Other languages
English (en)
Inventor
Teruo Inaguma
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Sony Corp
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Assigned to SONY CORPORATION reassignment SONY CORPORATION ASSIGNMENT OF ASSIGNORS INTEREST (SEE DOCUMENT FOR DETAILS). Assignors: INAGUMA, TERUO
Publication of US20030002210A1 publication Critical patent/US20030002210A1/en
Priority to US10/737,566 priority Critical patent/US7428776B2/en
Abandoned legal-status Critical Current

Links

Images

Classifications

    • H—ELECTRICITY
    • H01—ELECTRIC ELEMENTS
    • H01F—MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
    • H01F5/00—Coils
    • H01F5/003—Printed circuit coils
    • G—PHYSICS
    • G11—INFORMATION STORAGE
    • G11B—INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORD CARRIER AND TRANSDUCER
    • G11B5/00—Recording by magnetisation or demagnetisation of a record carrier; Reproducing by magnetic means; Record carriers therefor
    • G11B5/127—Structure or manufacture of heads, e.g. inductive
    • G—PHYSICS
    • G11—INFORMATION STORAGE
    • G11B—INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORD CARRIER AND TRANSDUCER
    • G11B5/00—Recording by magnetisation or demagnetisation of a record carrier; Reproducing by magnetic means; Record carriers therefor
    • G11B5/127—Structure or manufacture of heads, e.g. inductive
    • G11B5/17—Construction or disposition of windings
    • G—PHYSICS
    • G11—INFORMATION STORAGE
    • G11B—INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORD CARRIER AND TRANSDUCER
    • G11B5/00—Recording by magnetisation or demagnetisation of a record carrier; Reproducing by magnetic means; Record carriers therefor
    • G11B5/127—Structure or manufacture of heads, e.g. inductive
    • G11B5/31—Structure or manufacture of heads, e.g. inductive using thin films
    • G11B5/3103—Structure or manufacture of integrated heads or heads mechanically assembled and electrically connected to a support or housing
    • G—PHYSICS
    • G11—INFORMATION STORAGE
    • G11B—INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORD CARRIER AND TRANSDUCER
    • G11B5/00—Recording by magnetisation or demagnetisation of a record carrier; Reproducing by magnetic means; Record carriers therefor
    • G11B5/127—Structure or manufacture of heads, e.g. inductive
    • G11B5/31—Structure or manufacture of heads, e.g. inductive using thin films
    • G11B5/3109—Details
    • G11B5/313—Disposition of layers
    • H—ELECTRICITY
    • H01—ELECTRIC ELEMENTS
    • H01F—MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
    • H01F41/00—Apparatus or processes specially adapted for manufacturing or assembling magnets, inductances or transformers; Apparatus or processes specially adapted for manufacturing materials characterised by their magnetic properties
    • H01F41/02—Apparatus or processes specially adapted for manufacturing or assembling magnets, inductances or transformers; Apparatus or processes specially adapted for manufacturing materials characterised by their magnetic properties for manufacturing cores, coils, or magnets
    • H01F41/04—Apparatus or processes specially adapted for manufacturing or assembling magnets, inductances or transformers; Apparatus or processes specially adapted for manufacturing materials characterised by their magnetic properties for manufacturing cores, coils, or magnets for manufacturing coils
    • H01F41/041—Printed circuit coils
    • H01F41/042—Printed circuit coils by thin film techniques
    • H—ELECTRICITY
    • H01—ELECTRIC ELEMENTS
    • H01F—MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
    • H01F17/00—Fixed inductances of the signal type
    • H01F17/0006—Printed inductances
    • Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y10—TECHNICAL SUBJECTS COVERED BY FORMER USPC
    • Y10T—TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION
    • Y10T29/00—Metal working
    • Y10T29/49—Method of mechanical manufacture
    • Y10T29/49002—Electrical device making
    • Y10T29/4902—Electromagnet, transformer or inductor
    • Y10T29/49021—Magnetic recording reproducing transducer [e.g., tape head, core, etc.]
    • Y10T29/49032—Fabricating head structure or component thereof
    • Y10T29/49036—Fabricating head structure or component thereof including measuring or testing
    • Y10T29/49041—Fabricating head structure or component thereof including measuring or testing with significant slider/housing shaping or treating
    • Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y10—TECHNICAL SUBJECTS COVERED BY FORMER USPC
    • Y10T—TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION
    • Y10T29/00—Metal working
    • Y10T29/49—Method of mechanical manufacture
    • Y10T29/49002—Electrical device making
    • Y10T29/4902—Electromagnet, transformer or inductor
    • Y10T29/49021—Magnetic recording reproducing transducer [e.g., tape head, core, etc.]
    • Y10T29/49032—Fabricating head structure or component thereof
    • Y10T29/4906—Providing winding
    • Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y10—TECHNICAL SUBJECTS COVERED BY FORMER USPC
    • Y10T—TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION
    • Y10T29/00—Metal working
    • Y10T29/49—Method of mechanical manufacture
    • Y10T29/49002—Electrical device making
    • Y10T29/4902—Electromagnet, transformer or inductor
    • Y10T29/49021—Magnetic recording reproducing transducer [e.g., tape head, core, etc.]
    • Y10T29/49032—Fabricating head structure or component thereof
    • Y10T29/4906—Providing winding
    • Y10T29/49062—Multilayered winding
    • Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y10—TECHNICAL SUBJECTS COVERED BY FORMER USPC
    • Y10T—TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION
    • Y10T29/00—Metal working
    • Y10T29/49—Method of mechanical manufacture
    • Y10T29/49002—Electrical device making
    • Y10T29/4902—Electromagnet, transformer or inductor
    • Y10T29/49073—Electromagnet, transformer or inductor by assembling coil and core
    • Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y10—TECHNICAL SUBJECTS COVERED BY FORMER USPC
    • Y10T—TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION
    • Y10T29/00—Metal working
    • Y10T29/49—Method of mechanical manufacture
    • Y10T29/49002—Electrical device making
    • Y10T29/49117—Conductor or circuit manufacturing
    • Y10T29/49124—On flat or curved insulated base, e.g., printed circuit, etc.
    • Y10T29/49155—Manufacturing circuit on or in base
    • Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y10—TECHNICAL SUBJECTS COVERED BY FORMER USPC
    • Y10T—TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION
    • Y10T29/00—Metal working
    • Y10T29/49—Method of mechanical manufacture
    • Y10T29/49002—Electrical device making
    • Y10T29/49117—Conductor or circuit manufacturing
    • Y10T29/49124—On flat or curved insulated base, e.g., printed circuit, etc.
    • Y10T29/49155—Manufacturing circuit on or in base
    • Y10T29/49156—Manufacturing circuit on or in base with selective destruction of conductive paths

Definitions

  • This invention relates to a thin-film coil having a first coil and a second coil which are combined with each other, a magnetic head using the thin-film coil, a method of manufacturing the thin-film coil, and a method of manufacturing the magnetic head.
  • a composite thin-film magnetic head which includes a recording head having an inductive type magnetic transducer for writing and a reproducing head having a magneto-resistive effect element for reading.
  • a coil is formed so as to generate a magneto-motive force.
  • the coil is formed by means of a photolithographic process used for fabrication of semiconductor devices.
  • a coil formed by the process is generally referred to hereinafter as a thin-film coil.
  • a resist-film pattern P is formed in the shape of a coil as shown in FIG. 42A, a conductive film is then formed by plating and sputtering so as to obtain a thin-film coil L′ of a conductive film, as shown in FIG. 42B.
  • a shape and a space between winding portions are defined by patterning accuracy of the resist-film.
  • the patterning accuracy of the resist-film depends on conditions such as resist-film materials and performance of fabricating apparatuses including applicators, exposing devices, and developing devices, for example. Some apparatuses used in semiconductor fabrication may provide a line-space less than or equal to 1 ⁇ m.
  • a thickness of a thin-film coil of a magnetic head and a thickness of a coil used in a thin-film inductor for a variety of converters are in a range of a few ⁇ m to 10's ⁇ m. It is very difficult to form a line-space less than or equal to 1 ⁇ m by using a resist film which is applicable to such a thick conductive film.
  • two coils are stacked or two-layered so that terminals thereof may be electrically connected to form a thin-film coil. Its thickness, however, increases and the thin-film coil may not meet miniaturization requirements.
  • the thin-film coil formed to have a width within the value is also required to be no more than a predetermined resistance. Accordingly, the thin-film coil should be formed so as to be of very high density, that is, better space factor.
  • Japanese Patent Application Publication Laid Open Hei 11-345404 discloses a magnetic head and a manufacturing method.
  • the publication discloses a process for forming a thin-film coil of high space factor. In the process, a first coil and a second coil are formed on substantially the same plane.
  • an underlying film used to form the second coil remains between the first and second coils so that a short circuit is likely to happen between the remaining underlying film, electrically connected with the second coil, and the first coil.
  • the insulating film may become too thin or broken by polishing, or some polishing refuse may cause a short circuit between winding portions. Further, undesirable capacity may be generated between the first coil and the underlying film and it may raise a serious problem in coil characteristics.
  • the present invention seeks to solve such problems.
  • the present invention provides a thin-film coil comprising a first coil and a second coil each having a desired number of winding, the first coil and the second coil being electrically connected in series, also provides a magnetic head using the thin-film coil.
  • the second coil is formed between winding portions of the first coil so as to be substantially on the same plane, and only an insulating film is interposed between the first and the second coils.
  • the present invention also provides a method of manufacturing a thin-film coil and a magnetic head comprising the steps of: forming a first coil having a predetermined number of winding via a first insulating film; forming a second insulating film on a surface of the first coil and between its winding portions; forming an underlying conductive film on the second insulating film, and treating the underlying conductive film so as to leave only its bottom portions between the winding portions of the first coil; and growing deposition originating from a remaining portion of the underlying conductive film on the bottom portions between the winding portions of the first coil so as to form a second coil.
  • the present invention provides the following advantages: complete insulation between winding portions of the first and second coils is achieved because only an insulating film is interposed between the first coil and the second coil; reliability and performance of coil are provided because undesired capacity is not caused between the winding portions; a space between thin-film coils may be small so as to allow miniaturization; a thin-film coil of high space factor may be manufactured with a reduced accuracy in patterning so as to simplify manufacturing processes and to improve its yield and productivity; the first coil and the second coil compensate for resistance because of thickness, that is, width of the coils so that a total resistance of the coils is substantially constant regardless of pattern accuracy; and coils of substantially the same turns are formed on one plane and a thickness in height direction is no more than half of conventional one so that a finished surface may be smooth or even.
  • a magnetic circuit length may be shortened and recording efficiencies may be improved; productivity of magnetic heads may be increased; a high yield and low cost may be achieved; because of the constant resistance, it may be easy to design a variety of circuits for driving a magnetic head; and a magnetic core is formed on an even surface so that generation of magnetic domain walls may be suppressed, strain may be relieved, and magnetic characteristics may be improved as well.
  • FIGS. 1A and 1B are schematic views for explaining a thin-film coil according to an embodiment of the present invention, in which FIG. 1A is a plan view and FIG. 1B is a cross-sectional view;
  • FIGS. 2A and 2B are schematic views for explaining winding directions of each coil, in which FIG. 2A shows a first coil and a second coil separately and FIG. 2B shows a state of the second coil interposed between the first coil;
  • FIG. 3 is a schematic perspective view showing an example of a thin-film magnetic head
  • FIGS. 4A and 4B are schematic views (No. 1) for explaining a manufacturing process, in which FIG. 4A is a plan view and FIG. 4B is a cross-sectional view cut along line IV-IV of FIG. 4A;
  • FIGS. 5A and 5B are schematic views (No. 2) for explaining a manufacturing process, in which FIG. 5A is a plan view and FIG. 5B is a cross-sectional view cut along line V-V of FIG. 5A;
  • FIGS. 6A and 6B are schematic views (No. 3) for explaining a manufacturing process, in which FIG. 6A is a plan view and FIG. 6B is a cross-sectional view cut along line VI-VI of FIG. 6A;
  • FIGS. 7A and 7B are schematic views (No. 4) for explaining a manufacturing process, in which FIG. 7A is a plan view and FIG. 7B is a cross-sectional view cut along line VII-VII of FIG. 7A;
  • FIGS. 8A and 8B are schematic views (No. 5) for explaining a manufacturing process, in which FIG. 8A is a plan view and FIG. 8B is a cross-sectional view cut along line VIII-VIII of FIG. 8A;
  • FIGS. 9A and 9B are schematic views (No. 6) for explaining a manufacturing process, in which FIG. 9A is a plan view and FIG. 9B is a cross-sectional view cut along line IX-IX of FIG. 9A;
  • FIGS. 10A and 10B are schematic views (No. 7) for explaining a manufacturing process, in which FIG. 10A is a plan view and FIG. 10B is a cross-sectional view cut along line X-X of FIG. 10A;
  • FIGS. 11A and 11B are schematic views (No. 8) for explaining a manufacturing process, in which FIG. 11A is a plan view and FIG. 11B is a cross-sectional view cut along line XI-XI of FIG. 11A;
  • FIGS. 12A and 12B are schematic views (No. 9) for explaining a manufacturing process, in which FIG. 12A is a plan view and FIG. 12B is a cross-sectional view cut along line XII-XII of FIG. 12A;
  • FIGS. 13A and 13B are schematic representation (No. 10) for explaining a manufacturing process, in which FIG. 13A is a plan view and FIG. 13B is a cross-sectional view cut along line XIII-XIII of FIG. 13A;
  • FIGS. 14A and 14B are schematic representation (No. 11) for explaining a manufacturing process, in which FIG. 14A is a plan view and FIG. 14B is a cross-sectional view cut along line XIV-XIV of FIG. 14A;
  • FIGS. 15A and 15B are schematic representation (No. 12) for explaining a manufacturing process, in which FIG. 15A is a plan view and FIG. 15B is a cross-sectional view cut along line XV-XV of FIG. 15A;
  • FIG. 16 is a schematic view (No. 13) for explaining a manufacturing process
  • FIG. 17 is a schematic view (No. 14) for explaining a manufacturing process
  • FIG. 18 is a schematic view (No. 15) for explaining a manufacturing process
  • FIG. 19 is a schematic view (No. 16) for explaining a manufacturing process
  • FIG. 20 is a schematic view showing a state of an underlying conductive film for plating
  • FIG. 21 is a schematic view showing a state of a remaining portion of the underlying conductive film for plating after removal
  • FIGS. 22A and 22B are schematic views (No. 17) for explaining a manufacturing process, in which FIG. 22A is a plan view and FIG. 22B is a cross-sectional view cut along line XXII-XXII of FIG. 22A;
  • FIGS. 23A and 23B are schematic views (No. 18) for explaining a manufacturing process, in which FIG. 23A is a plan view and FIG. 23B is a cross-sectional view cut along line XXIII-XXIII of FIG. 23A;
  • FIGS. 24A and 24B are schematic views (No. 19) for explaining a manufacturing process, in which FIG. 24A is a plan view and FIG. 24B is a cross-sectional view cut along line XXIV-XXIV of FIG. 24A;
  • FIGS. 25A and 25B are schematic views (No. 20) for explaining a manufacturing process, in which FIG. 25A is a plan view and FIG. 25B is a cross-sectional view cut along line XXV-XXV of FIG. 25A;
  • FIGS. 26A and 26B are schematic views (No. 21) for explaining a manufacturing process, in which FIG. 26A is a plan view and FIG. 26B is a cross-sectional view cut along line XXVI-XXVI of FIG. 26A;
  • FIGS. 27A and 27B are schematic views (No. 22) for explaining a manufacturing process, in which FIG. 27A is a plan view and FIG. 27B is a cross-sectional view cut along line XXVII-XXVII of FIG. 27A;
  • FIGS. 28A and 28B are schematic views (No. 23) for explaining a manufacturing process, in which FIG. 28A is a plan view and FIG. 28B is a cross-sectional view cut along line XXVIII-XXVIII of FIG. 28A;
  • FIGS. 29A and 29B are schematic views (No. 24) for explaining a manufacturing process, in which FIG. 29A is a plan view and FIG. 29B is a cross-sectional view cut along line XXIX-XXIX of FIG. 29A;
  • FIGS. 30A and 30B are schematic views (No. 25) for explaining a manufacturing process, in which FIG. 30A is a plan view and FIG. 30B is a cross-sectional view cut along line XXX-XXX of FIG. 30A;
  • FIGS. 31A and 31B are schematic views (No. 26) for explaining a manufacturing process, in which FIG. 31A is a plan view and FIG. 31B is a cross-sectional view cut along line XXXI-XXXI of FIG. 31A;
  • FIGS. 32A and 32B are schematic views (No. 27) for explaining a manufacturing process, in which FIG. 32A is a plan view and FIG. 32B is a cross-sectional view cut along line XXXII-XXXII of FIG. 32A;
  • FIG. 33 is a schematic view (No. 28) for explaining a manufacturing process
  • FIG. 34 is a schematic view (No. 29) for explaining a manufacturing process
  • FIG. 35 is a schematic view (No. 30) for explaining a manufacturing process
  • FIG. 36 is a schematic view (No. 31) for explaining a manufacturing process
  • FIG. 37 is a schematic cross-sectional view showing a magnetic head
  • FIG. 38 is a graph showing a coil width to a number of winding in a case where a thin-film is formed by means of a conventional forming process
  • FIG. 39 is a graph showing a coil thickness to a number of winding where resistance is set to 3 ⁇ in a case where a thin-film is formed by means of a conventional forming process;
  • FIG. 40 is a graph showing a coil width to a number of winding in a case where a thin-film coil is formed by a process in accordance with the present embodiment
  • FIG. 41 is a graph showing a coil thickness to a number of winding in a case where resistance is set to 3 ⁇ in accordance with the present embodiment
  • FIGS. 42A and 42B are schematic views for explaining a conventional manufacturing process
  • FIGS. 43A and 43B are schematic views for explaining a case where two coils are stacked, in which FIG. 43A shows a state before stacking and FIG. 43B shows a state after the coils are stacked;
  • FIG. 44 is a schematic view for explaining patterning of a resist film in a conventional process (No. 1);
  • FIGS. 45A, 45B and 45 C are schematic views for explaining patterning of a resist film in a conventional process (No. 2);
  • FIG. 46 is a schematic view for explaining plating carried out when pattern mismatching occurs.
  • FIGS. 1A and 1B are schematic views of a thin-film coil according to an embodiment of the present invention
  • FIG. 1A is a plan view
  • FIG. 1B is a cross-sectional view.
  • a thin-film coil L is provided in such a way that a first coil L 1 having a desired number of winding and a second coil L 2 having a desired number of winding are electrically connected in series and mounted in the thin-film coil L.
  • the second coil L 2 is formed between winding portions of the first coil L 1 to be substantially on the same plane, and only an insulating film 12 is interposed between the second coil L 2 and the first coil L 1 .
  • the first coil L 1 and the second coil L 2 are electrically connected at their terminals so as to constitute the thin-film coil L.
  • FIGS. 2A and 2B are schematic views to explain winding directions of each coil.
  • the first coil L 1 is, for example, is wound from outside to inside along current directions (as shown by arrows in FIG. 2A).
  • the second coil L 2 is also wound from outside to inside along current directions.
  • the second coil L 2 is formed between winding portions of the first coil L 1 and an inner terminal of the first coil L 1 and an outer terminal of the second coil L 2 are electrically and mechanically connected as shown in FIG. 2B.
  • the first coil L 1 and the second coil L 2 each have substantially rectangular cross sections, however, the cross sections may be trapezoids where a longer side (base edge) of one trapezoid is adjacent to a shorter side (top edge) of the other trapezoid.
  • the cross section of the first coil L 1 as in FIG. 1B is a trapezoid in which the base edge is longer, the insulating film 12 covering the first coil L 1 is provided with a good throwing power, whereby the insulating film 12 may be thinner.
  • Such a thin-film coil L is applicable to a thin-film inductor, a thin-film magnetic head as shown in FIG. 3, and the like.
  • a film 3 of magneto-resistive effect element and a thin-film coil L are formed on a hard non-magnetic substrate 1 which is, with a bonding substrate 25 on it, polished at sliding surfaces 1 a and 25 a so as to be in a substantial arc-shape and is cut so as to have an azimuth angle ⁇ .
  • This embodiment is characterized in a thin-film coil employed in a thin-film magnetic head, for example, and in a method of manufacturing the thin-film coil.
  • the method of manufacturing the thin-film coil and a method of manufacturing the magnetic head will be described hereinafter in order.
  • a substrate 1 is prepared as shown in FIGS. 4A and 4B.
  • Materials for the substrate 1 are not limited to this embodiment and any materials may be selected according to its use.
  • Al 2 O 3 —TiC (AlTiC), ⁇ -Fe 2 O 3 (hematite) which is one of iron oxides and the like are suitable.
  • a substrate of 4 inches in diameter and 2 mm in thickness is prepared.
  • a lower-layer core material 5 is formed to be a lower-layer core of a magnetic recording head. Any material may be selected for the lower-layer core material 5 as long as it is allowable in terms of magnetic characteristics. To increase recording efficiencies, it is preferable to use a soft magnetic film of higher magnetic permeability and of higher saturation magnetic-flux density as long as possible. In this embodiment, FeAlSi (sendust) film of 2.5 ⁇ m is formed by means of sputtering. Any method of forming the lower-layer core material 5 may be selected. The thickness of the lower-layer core material 5 is preferably more than or equal to 2 ⁇ m.
  • the lower-layer core material is patterned and etched then cut into portions for respective magnetic heads to form lower-layer cores 6 .
  • the lower-layer cores 6 are formed in such a manner that patterning of a resist film is carried out by means of a photolithographic process and undesirable portions are removed by means of an ion etching process, however, other processes may be applicable.
  • the rugged lower-layer cores 6 are embedded within a non-magnetic material.
  • an Al 2 O 3 film 7 having the same thickness as the lower-layer cores 6 is coated by sputtering, then an uneven surface is planarized by means of CMP (chemical mechanical polishing) or buffing.
  • CMP chemical mechanical polishing
  • buffing The method and materials for planarization are not limited to this embodiment and any method or material may be selected.
  • a gap film 8 is provided to form a front gap of a recording head where a SiO 2 film of 0.2 ⁇ m thick is formed by sputtering.
  • Materials for the gap film 8 need only be non-magnetic and non-conductive, and Al 2 O 3 may be used other than SiO 2 .
  • a thickness of the gap film 8 is determined in accordance with overwriting characteristics and a magneto-motive force which are required by systems.
  • a process of forming a thin-film coil a major process of this embodiment, will be described hereafter.
  • a film comprising Ti/Cu layers to be an underlying conductive film 9 for plating is formed by sputtering on a surface of the gap film 8 .
  • the underlying conductive film 9 functions as a conductive portion to distribute plating current to the whole surface of the substrate (wafer) during plating.
  • the underlying conductive film 9 for plating As to the Ti/Cu layer, the underlying conductive film 9 for plating, the Ti layer is set to a thickness of 30 nm and the Cu layer is set to a thickness of 100 nm. The Ti layer is coated to increase adhesion between the gap film 8 and the Cu layer, any thickness may be selected for the Ti layer.
  • the material Cu is selected considering the subsequent Cu-plating process to form a thin-film coil so as to be the same material. Some portions of the underlying conductive film 9 for plating become a part of the thin-film coil to be formed later. Since other portions of the underlying conductive film 9 are to be removed, a thickness of the underlying conductive film 9 for plating is not so large and is preferably less than or equal to 0.3 ⁇ m, for example.
  • a pattern 10 having an opening corresponding to a shape of the first coil, as shown in FIG. 10A, is formed by means of a photolithographic process.
  • a resist film used in this process has a thickness of about 8 ⁇ m.
  • the film is coated at 2000 rpm, for example. Any material for the resist film may be selected as far as its profile is sufficient. Since the first coil is set to a thickness of about 6 ⁇ m, a thickness t10 of the pattern 10 of the resist film needs to be at least greater than that of the first coil.
  • copper (Cu) is deposited to form a first coil deposition 11 at opening potions of the resist pattern 10 .
  • the deposition may be carried out by means of electroplating using a copper sulfate solution or a copper pyrophosphate solution.
  • Plating solutions are not limited to such a copper sulfate solution or a copper pyrophosphate solution, and any solution may be used.
  • Metals dissolved in such a plating solution is not limited to copper and other metals such as gold may be used, in which case it is preferable to match materials for the underlying conductive film 9 with the materials to be deposited.
  • the thickness t11 of the deposition is selected to be 6 ⁇ m.
  • the patterned resist film is dissolved in an organic solvent and removed, then the underlying conductive film 9 for plating, except for that at the coil, is removed by treating the whole surface of the substrate by means of ion etching, in which an incident angle to the substrate is preferably set to be as perpendicular as possible so as to remove the underlying conductive film between winding portions of the coil completely.
  • the incident angle is set to 0 degree (perpendicular incidence).
  • the angle of incidence may be optimized such that an etching apparatus can remove the whole underlying conductive film 9 between coils or winding portions completely.
  • an insulating film 12 is formed between the first coil L 1 and the second coil (not shown) to insulate the first coil L 1 from the second coil.
  • the second coil is formed, as will be described, threading between and along winding portions of the first coil L 1 so that a space between the first coil L 1 and the second coil is very narrow.
  • An electrically non-conductive film (the insulating film 12 ) is provided to electrically insulate one coil from the other coil.
  • an Al 2 O 3 film with a thickness of 0.5 ⁇ m is formed by a sputtering process.
  • any material for the insulating film 12 may be selected as far as it is electrically non-conductive and non-magnetic.
  • the thickness of the insulating film 12 is selected to be 0.5 ⁇ m so as to obtain sufficient insulation with minimum quantity of the material and to coat sidewalls of the first coil L 1 and bottom portions between winding portions completely, thus the sputtering process is preferably chosen. Any other method, such as vapor deposition, may be employed. Covering effect or status of the first coil L 1 may vary depending on forming processes and apparatuses. Thus, any forming process and apparatus may be selected as long as the first coil is completely covered.
  • an underlying conductive film 13 (such as a film of Ti/Cu) for plating to be used for the second coil is formed by a sputtering process.
  • the underlying conductive film 13 underlies during depositing the second coil.
  • a thickness of the underlying conductive film 13 is preferably somewhat greater than that of the underlying conductive film 9 of the first coil L 1 .
  • the Ti layer is set to a thickness of 30 nm and the Cu layer is set to a thickness of 200 nm.
  • a step for removing the underlying conductive film 13 for plating the step being a major feature of this embodiment, will be described in detail.
  • a plating step for the second coil does not immediately follow the plating, but follows the step for removing the underlying conductive film 13 partially. Reasons why will be described later. It is noted that the method and the material used for forming the second coil are the same as those used for forming the first coil.
  • a protective resist film 14 is patterned by a photolithographic process so as to cover desired parts of the underlying conductive film 13 such that the desired parts are not removed.
  • the desired parts to be left are peripheral portions of the second coil and an entrance portion of the second coil to supply the second coil with plating current.
  • An area to be the second coil that is formed by growing plating is between the winding portions of the first coil L 1 .
  • the underlying conductive film 13 for plating at the area needs to be left during the plating process.
  • the pattern of the resist film 14 has an opening between the winding portions of the first coil L 1 except the entrance portion.
  • the underlying conductive film 13 at the bottom portions between the winding portions of the first coil L 1 is not removed.
  • the underlying conductive film 13 at the bottoms functions as an underlying conductive film during plating of the second coil.
  • an ion etching process is applied to the whole surface of the substrate where the ion etching process is carried out with an angle.
  • the reason is that the underlying conductive film 13 for plating the second coil covers the first coil L 1 , and the underlying conductive film 13 on tops and sidewalls of the first coil L 1 is removed so as to leave only the underlying conductive film 13 at the bottom portions between the winding portions of the first coil L 1 (see FIG. 17).
  • the substrate 1 is tilted during the ion etching process so as to obtain such a shape.
  • the tilted angle is theoretically expressed by the followings:
  • the underlying conductive film 13 is not left on the sidewalls of the first coil L 1 as shown in FIG. 20. Several parts of the underlying conductive film 13 are to be removed as shown in FIG. 17 or FIG. 21. Whichever, it is important to remove the underlying conductive film 13 located on the tops and the sidewalls of the first coil L 1 .
  • the protective resist film 14 is dissolved and removed by an organic solution, then, as shown in FIGS. 22A and 22B, a resist film 15 having an opening for the second coil is patterned by means of a photolithographic process.
  • the resist film 15 does not have the shape of a coil pattern as formed for the first coil L 1 but has an opening which correspond to the whole of the first coil L 1 . As to the winding portions, the resist film 15 only covers circumferences of the first coil L 1 .
  • the resist film 15 needs to be formed so as to cover the first coil L 1 completely.
  • the first coil L 1 Since the first coil L 1 is built up as high as 6 ⁇ m, it is very difficult to cover the whole of the first coil L 1 completely with a thin film. This is because there may be problems with pattern mismatching as shown in FIG. 45A, sharpened pattern as shown in FIG. 45B, or remaining resist as shown in FIG. 45C.
  • the resist film 15 to cover becomes uneven, whereby several parts of the tops and the sidewalls of the first coil L 1 may often be exposed.
  • the resist film on edges of the tops of the first coil L 1 tends to be thin, which results in that the edges are mostly exposed in fact.
  • deposition is carried out, and a result is as shown in FIG. 46.
  • deposition M grows fast out of tops of the sidewalls closest to opposite poles, whereas deposition in the trenches grows slowly because a plating solution remains in the trenches.
  • holes may be formed within the trenches.
  • FIGS. 23A and 23B show an intermediate product where deposition according to the plating is grown in such a way described above, in which both ends of the second coil L 2 have larger areas so as to allow external connection. Any size may be selected for the ends.
  • the resist film 15 coated for plating the second coil L 2 is dissolved and removed by an organic solution, thereby providing a thin-film coil L where the second coil L 2 is interposed between winding portions of the first coil L 1 and the first and second coils are on substantially the same plane.
  • the underlying conductive film 13 remaining at a periphery of the thin-film coil L is removed by means of an ion etching process.
  • the ion etching process does not have to be set to a particular angle or so because no underlying conductive film exists at small portions or hidden portions.
  • a resist film 17 having openings corresponding to both the ends and the front gap portion is patterned by means of a photolithographic process.
  • the resist film 17 is patterned to obtain an opening at a portion corresponding to a distal end of a magnetic core. Any shape may be selected for both ends of the first coil L 1 as long as they are large enough to be connected.
  • an opening at the center portion is a circle with a radius of 5 ⁇ m and an opposite-side terminal portion is a rectangle with edges of about 20 ⁇ m.
  • the exposed insulating film 12 is removed by an ion etching process or a wet etching process.
  • the exposed insulating film 12 is removed by means of the wet etching process then by means of the ion etching as well in order to clean its surface. Any removing process may apply to the removal of the film.
  • the patterned resist film 17 is dissolved and removed by an organic solvent, resulting in a status as shown in FIGS. 27A and 27B. Both the ends of the first coil L 1 are exposed by the process.
  • a resist film 18 having an opening of a back gap portion is formed by a photolithographic process.
  • the front gap portion is connected to an upper-layer core (not shown) via a gap material, and the back gap portion is directly connected to the upper-layer core.
  • the gap film 8 and the insulating film 12 at the back gap portion Accordingly, these non-magnetic films must be removed before forming the upper-layer core.
  • the gap film 8 and the insulating film 12 located at the opening of the resist film 18 is removed by means of an ion etching process or a wet etching process.
  • any removing process may be used. Any shape may be applied to the back gap portion, however, it is preferable to bring the back gap portion as close as possible to the front gap portion and to make it as large as possible in order to have higher recording efficiency.
  • the back gap portion is in the shape of an ellipse with a transverse axis of 25 ⁇ m and a conjugate axis of 10 ⁇ m, whereby the back gap portion of the lower-layer core 6 is exposed.
  • a resist film 19 for planarization is patterned by means of a photolithographic process so as to cover the whole of the thin-film coil L.
  • the resist film 19 has a pattern in which any resist film remains at neither the back gap portion nor any end of the first coil L 1 and the second coil L 2 .
  • Any type of the resist film 19 for planarization or any method for manufacturing the same may be applicable.
  • the substrate, as it is, is heated at about 300° C. for about 1 hour, whereby the resist film 19 is hardened and becomes insoluble even in an organic solvent.
  • the upper-layer core 20 is formed. Any process may be applied to forming the upper-layer core 20 .
  • a layer of Ni, Fe or the like to be the upper-layer core 20 may be formed by means of sputtering or plating, and coated with a resist film of a desired pattern, and undesirable portions may be removed by means of an etching process; or the layer may be patterned with a resist film having openings of desired shape then a plating process may be carried out, whereby an upper-layer core of a desired shape may be obtained.
  • any material of sufficient soft-magnetic characteristic may be used. Considering recording efficiency, it is preferable to use a material having higher magnetic permeability and higher saturation magnetic-flux density as long as possible. In this embodiment, a plating film of Ni/Fe is used. Any shape is applicable to the upper-layer core 20 .
  • a transverse width of a magnetization pattern, that is a track width, is determined by a transverse width of the front gap which is a width of the lower-layer core 6 or that of the upper-layer core 20 , whichever is narrower.
  • the back gap portion is also covered with the upper-layer core 20 .
  • a thickness of the upper-layer core 20 is selected to 2.5 ⁇ m, because the upper-layer core 20 needs to have sufficient volume not to saturate recording magnetization intensity.
  • the first coil L 1 and the second coil L 2 are connected with each other and terminals are formed to allow external connection.
  • An end of the first coil L 1 and an end of the second coil L 2 are connected by a coil connecting lead 22 as shown in FIG. 32A so that the thin-film coil becomes electrically conductive.
  • An external connecting terminal 21 is formed at each end of the first and second coils in order to have an electrical connection with an external device.
  • each coil connecting lead 22 may have any size or any shape, it is preferable to allow the terminal to have as large a surface area as possible in order to decrease its resistance.
  • any process is applicable to the forming of the coil connecting lead 22 .
  • a resist film having openings in a desired shape is patterned by means of a photolithographic process beforehand, then an electroplating process is carried out in a copper sulfate solution for plating so as to grow Cu plating at desired portions.
  • the plating solution is not limited to the copper sulfate solution. Any material to be plated may be used as far as the material is electrically conductive.
  • Rugged portions formed on the substrate (wafer) due to various patterns used in previous processes are smoothed or planarized.
  • an Al 2 O 3 film with a thickness of about 20 ⁇ m is sputtered on the whole surface of the wafer, the surface is ground by means of a mechanical polishing process in order to smooth the surface.
  • the Al 2 O 3 film functions as an embedding layer 23 for planarization and the thin-film coil L and a magnetic core element are embedded in the embedding layer 23 as shown in FIG. 32B.
  • magnetic head elements where the thin-film coil L are formed are cut out of the substrate (wafer) into blocks of a few elements in a unit. Although a cut block 24 is obtained every five elements, as shown in FIG. 33, any number of elements per block may be selected.
  • a bonding substrate 25 to protect the magnetic head elements is bonded to the cut block 24 .
  • a material for the bonding substrate 25 is the same as that of the substrate 1 , however, any material may be used.
  • the bonding substrate 25 needs to be smaller in size than the cut block 24 in order that the external connecting terminals of the magnetic head elements that are formed on the substrate 1 may be exposed.
  • the bonding may be performed by using resin adhesives.
  • a surface to be the upper surfaces 1 a and 25 a (which slide on magnetic tape) of the bonded block are finished in the shape of an arc so as to conveniently fit on magnetic tape. Shapes of such surfaces depend on systems to be used, and so will not be described in any further detail.
  • cutting may be carried out with a desired azimuth angle ⁇ .
  • the magnetic head (see FIG. 3) using the thin-film coil in accordance with the present embodiment is completed.
  • FIG. 37 is a schematic cross-sectional view showing an exemplary magnetic head.
  • a width of the magnetic head body that is a width in slide-contact with a magnetic tape, is referred hereafter to as “contact width”.
  • the contact width is defined by a system. The width may be no more than about 100 ⁇ m, for example.
  • a conventional MIG (Metal In Gap) head has a winding portion using copper wire in which its total resistance is about 3 ⁇ .
  • a required total resistance for the thin-film coil is preferably no more than about 3 ⁇ .
  • a specification for a magnetic head in accordance with the present embodiment should at least request that a number of winding be no less than 10 turns, a total resistance be no more than 3 ⁇ . and a contact width be no more than 100 ⁇ m.
  • a conventional stepper exposure system using g-ray and i-ray unless it is of a high accuracy, provides at most an aspect ratio of 6 ⁇ m for a width of 2 ⁇ m of a resist film pattern.
  • the winding should be provided within 32 ⁇ m.
  • FIG. 38 is a graph showing a coil width to a number of winding in case a thin-film is formed by means of a resist film in accordance with a conventional forming process
  • FIG. 39 is a graph showing a coil thickness to a number of winding where resistance is set to 3 ⁇ .
  • Each width of resist film patterns is set to 2 ⁇ m which is generally a minimum width.
  • a width of one turn of the coil may be about 1.5 ⁇ m. If copper plating has a specific resistance of 2.2 ⁇ cm, the width of one turn exceeds 12 ⁇ m in order to have a total resistance of 3 ⁇ for the thin film coil and no coils can be formed.
  • FIG. 40 is a graph showing a coil width to a number of winding where a thin-film coil is formed by a process in accordance with the present embodiment
  • FIG. 41 is a graph showing a coil thickness to a number of winding where resistance is set to 3 ⁇ in accordance with the present embodiment.
  • a thickness of the insulating film between thin-film coils is defined by sputtering, resulting in an accurate thickness as close as to its target.
  • the space between the thin film coils is no more than 1 ⁇ m so that very high space factor is provided.
  • a thickness of a thin-film coil is about 6 ⁇ m for ten turns in order to allow a total resistance of 3 ⁇ for the thin-film coil.
  • a second coil is formed between winding portions of a first coil. Since a pattern of a resist film has pattern portions which are located at every other winding portion, the pattern portions may have a width of 4.3 ⁇ m and a height (thickness) of 7 ⁇ m when forming the first coil. Such patterning is easily accomplished in accordance with the embodiment.
  • a magnetic head which meets the specification described above may be produced with a good degree of accuracy without using an accurate exposure system.

Landscapes

  • Engineering & Computer Science (AREA)
  • Manufacturing & Machinery (AREA)
  • Power Engineering (AREA)
  • Magnetic Heads (AREA)
  • Insulating Of Coils (AREA)
  • Manufacturing Cores, Coils, And Magnets (AREA)
  • Coils Or Transformers For Communication (AREA)
US10/145,507 2001-05-21 2002-05-14 Thin-film coil, magnetic head, method of manufacturing the thin-film coil, and method of manufacturing the magnetic head Abandoned US20030002210A1 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
US10/737,566 US7428776B2 (en) 2001-05-21 2003-12-16 Method of manufacturing a magnetic head

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
JP2001150249A JP2002343639A (ja) 2001-05-21 2001-05-21 薄膜コイルおよび磁気ヘッドならびに薄膜コイルの製造方法および磁気ヘッドの製造方法
JPP2001-150249 2001-05-21

Related Child Applications (1)

Application Number Title Priority Date Filing Date
US10/737,566 Division US7428776B2 (en) 2001-05-21 2003-12-16 Method of manufacturing a magnetic head

Publications (1)

Publication Number Publication Date
US20030002210A1 true US20030002210A1 (en) 2003-01-02

Family

ID=18995290

Family Applications (2)

Application Number Title Priority Date Filing Date
US10/145,507 Abandoned US20030002210A1 (en) 2001-05-21 2002-05-14 Thin-film coil, magnetic head, method of manufacturing the thin-film coil, and method of manufacturing the magnetic head
US10/737,566 Expired - Fee Related US7428776B2 (en) 2001-05-21 2003-12-16 Method of manufacturing a magnetic head

Family Applications After (1)

Application Number Title Priority Date Filing Date
US10/737,566 Expired - Fee Related US7428776B2 (en) 2001-05-21 2003-12-16 Method of manufacturing a magnetic head

Country Status (2)

Country Link
US (2) US20030002210A1 (enExample)
JP (1) JP2002343639A (enExample)

Cited By (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US20040240106A1 (en) * 2003-05-29 2004-12-02 Tdk Corporation Thin film coil and method of forming the same, and thin film magnetic head and method of manufacturing the same
US20140110822A1 (en) * 2012-10-19 2014-04-24 Infineon Technologies Austria Ag Semiconductor Device Including Magnetically Coupled Monolithic Integrated Coils
CN108303596A (zh) * 2018-01-16 2018-07-20 宁波市计量测试研究院(宁波市衡器管理所、宁波新材料检验检测中心) 一种利用薄膜沉积技术制作超薄线圈的方法及超薄线圈
CN109698062A (zh) * 2017-10-24 2019-04-30 三星电机株式会社 线圈组件和用于制造该线圈组件的方法
CN110504239A (zh) * 2018-05-17 2019-11-26 日月光半导体制造股份有限公司 半导体装置封装及其制造方法
US11145452B2 (en) 2017-01-06 2021-10-12 Samsung Electro-Mechanics Co., Ltd. Inductor and method for manufacturing the same

Families Citing this family (10)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2007278734A (ja) * 2006-04-03 2007-10-25 Asahi Kasei Electronics Co Ltd 磁気センサ及びその製造方法
JP2007278733A (ja) * 2006-04-03 2007-10-25 Asahi Kasei Electronics Co Ltd 磁気センサ及びその製造方法
WO2007119569A1 (ja) 2006-04-13 2007-10-25 Asahi Kasei Emd Corporation 磁気センサ及びその製造方法
JP4842052B2 (ja) * 2006-08-28 2011-12-21 富士通株式会社 インダクタ素子および集積型電子部品
US7468899B1 (en) * 2007-01-09 2008-12-23 National Semiconductor Corporation Apparatus and method for wafer level fabrication of high value inductors on semiconductor integrated circuits
KR101408505B1 (ko) * 2012-11-07 2014-06-17 삼성전기주식회사 커먼 모드 필터 및 그 제조방법
US9748324B2 (en) 2013-05-21 2017-08-29 Taiwan Semiconductor Manufacturing Co., Ltd. Method of fabricating magnetic core inductors for an integrated voltage regulator
US9047890B1 (en) * 2013-12-30 2015-06-02 International Business Machines Corporation Inductor with non-uniform lamination thicknesses
CN107039395B (zh) * 2017-05-03 2019-06-21 电子科技大学 一种集成螺线管型双层磁膜电感及其制备方法
CN109412354B (zh) * 2018-11-27 2024-01-12 厦门新鸿洲精密科技有限公司 一种可感测运动轨迹的音圈马达

Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US4703383A (en) * 1984-10-05 1987-10-27 Fuji Photo Film Co., Ltd. Coil conductor structure in thin-film magnetic head
US4804816A (en) * 1981-12-21 1989-02-14 Kabushiki Kaisha Kenwood Method of making a thin-film magnetic head having a multi-layered coil structure
US5045961A (en) * 1984-07-25 1991-09-03 Hitachi, Ltd. Thin film magnetic head
US6191918B1 (en) * 1998-10-23 2001-02-20 International Business Machines Corporation Embedded dual coil planar structure

Family Cites Families (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
DE2857725C2 (de) * 1977-12-13 1984-10-11 Fujitsu Ltd., Kawasaki, Kanagawa Verfahren zum Herstellen einer Dünnschichtspule
JPH0573843A (ja) * 1991-09-13 1993-03-26 Sony Corp 薄膜磁気ヘツド及びその製造方法
JPH11283215A (ja) * 1998-03-30 1999-10-15 Tdk Corp 薄膜磁気ヘッドおよびその製造方法

Patent Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US4804816A (en) * 1981-12-21 1989-02-14 Kabushiki Kaisha Kenwood Method of making a thin-film magnetic head having a multi-layered coil structure
US5045961A (en) * 1984-07-25 1991-09-03 Hitachi, Ltd. Thin film magnetic head
US4703383A (en) * 1984-10-05 1987-10-27 Fuji Photo Film Co., Ltd. Coil conductor structure in thin-film magnetic head
US6191918B1 (en) * 1998-10-23 2001-02-20 International Business Machines Corporation Embedded dual coil planar structure

Cited By (8)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US20040240106A1 (en) * 2003-05-29 2004-12-02 Tdk Corporation Thin film coil and method of forming the same, and thin film magnetic head and method of manufacturing the same
US7319572B2 (en) * 2003-05-29 2008-01-15 Tdk Corporation Thin film coil and method of forming the same, and thin film magnetic head and method of manufacturing the same
US20140110822A1 (en) * 2012-10-19 2014-04-24 Infineon Technologies Austria Ag Semiconductor Device Including Magnetically Coupled Monolithic Integrated Coils
US9640602B2 (en) * 2012-10-19 2017-05-02 Infineon Technologies Austria Ag Semiconductor device including magnetically coupled monolithic integrated coils
US11145452B2 (en) 2017-01-06 2021-10-12 Samsung Electro-Mechanics Co., Ltd. Inductor and method for manufacturing the same
CN109698062A (zh) * 2017-10-24 2019-04-30 三星电机株式会社 线圈组件和用于制造该线圈组件的方法
CN108303596A (zh) * 2018-01-16 2018-07-20 宁波市计量测试研究院(宁波市衡器管理所、宁波新材料检验检测中心) 一种利用薄膜沉积技术制作超薄线圈的方法及超薄线圈
CN110504239A (zh) * 2018-05-17 2019-11-26 日月光半导体制造股份有限公司 半导体装置封装及其制造方法

Also Published As

Publication number Publication date
US20040123449A1 (en) 2004-07-01
JP2002343639A (ja) 2002-11-29
US7428776B2 (en) 2008-09-30

Similar Documents

Publication Publication Date Title
US7428776B2 (en) Method of manufacturing a magnetic head
US6804879B2 (en) Method of fabricating a magnetic transducer with a write head having a multi-layer coil
US6922316B2 (en) Thin-film magnetic head and method of manufacturing same
JP3914173B2 (ja) 薄膜コイルおよびその形成方法ならびに薄膜磁気ヘッドおよびその製造方法
JP3617953B2 (ja) 薄膜磁気ヘッドの製造方法
JP2001118216A (ja) 分割コイル構造を有する磁気書き込みヘッド、薄膜磁気書き込みヘッド及びその製造方法
JPH11283215A (ja) 薄膜磁気ヘッドおよびその製造方法
JP4297410B2 (ja) 薄膜磁気ヘッドを製造する方法
US20020060879A1 (en) Thin film magnetic head having a plurality of coil layers
JP3499458B2 (ja) 薄膜磁気ヘッドおよびその製造方法、ならびに薄膜コイルの形成方法
JP2005025909A (ja) 薄膜構造体及びその製造方法
JP3579271B2 (ja) 薄膜磁気ヘッドの製造方法
US6525905B1 (en) Thin film magnetic head having a non-magnetic body and method of manufacturing the same
US20020191334A1 (en) Magnetic transducer with pedestal pole piece structure
US6678942B1 (en) Thin film magnetic head and method of manufacturing the same
US6643095B1 (en) Thin-film magnetic head having a thin-film coil and method of manufacturing same
JP3839164B2 (ja) 薄膜磁気ヘッドおよびその製造方法
JPH06267776A (ja) 薄膜磁気コイルの製造方法
JP2001195707A (ja) 薄膜磁気ヘッド及びその製造方法
US6937438B2 (en) Thin film magnetic head having conductive pad including insulating protective layers
US6519834B1 (en) Method of manufacturing thin-film magnetic head
JP2534082B2 (ja) 薄膜磁気ヘッド
JPS6247812A (ja) 薄膜磁気ヘツド
JP2001110006A (ja) 薄膜磁気ヘッドの製造方法
JP5289717B2 (ja) 薄膜構造体のコンタクト形成方法

Legal Events

Date Code Title Description
AS Assignment

Owner name: SONY CORPORATION, JAPAN

Free format text: ASSIGNMENT OF ASSIGNORS INTEREST;ASSIGNOR:INAGUMA, TERUO;REEL/FRAME:013239/0317

Effective date: 20020801

STCB Information on status: application discontinuation

Free format text: ABANDONED -- FAILURE TO RESPOND TO AN OFFICE ACTION