RU2537730C1 - Mixture for making enamel coating - Google Patents

Mixture for making enamel coating Download PDF

Info

Publication number
RU2537730C1
RU2537730C1 RU2013155351/03A RU2013155351A RU2537730C1 RU 2537730 C1 RU2537730 C1 RU 2537730C1 RU 2013155351/03 A RU2013155351/03 A RU 2013155351/03A RU 2013155351 A RU2013155351 A RU 2013155351A RU 2537730 C1 RU2537730 C1 RU 2537730C1
Authority
RU
Russia
Prior art keywords
enamel coating
mixture
frit
mullite
bone ash
Prior art date
Application number
RU2013155351/03A
Other languages
Russian (ru)
Inventor
Юлия Алексеевна Щепочкина
Original Assignee
Юлия Алексеевна Щепочкина
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Юлия Алексеевна Щепочкина filed Critical Юлия Алексеевна Щепочкина
Priority to RU2013155351/03A priority Critical patent/RU2537730C1/en
Application granted granted Critical
Publication of RU2537730C1 publication Critical patent/RU2537730C1/en

Abstract

FIELD: chemistry.
SUBSTANCE: mixture for making enamel coating contains, wt %: frit 72.0-74.0; mullite 7.0-9.0; bone ash 17.0-21.0. The coating has heat resistance of 25 thermal cycles. A suspension is deposited on the surface of articles and fixed by firing at 1200°C.
EFFECT: high heat resistance of the enamel coating.
1 tbl

Description

Изобретение относится к составам масс для получения эмалевого покрытия на керамических изделиях, в том числе хозяйственно-бытового назначения.The invention relates to compositions of the masses to obtain an enamel coating on ceramic products, including domestic purposes.

Известна масса для получения эмалевого покрытия, содержащая, мас.%: фритта 75,0-96,0; муллит 2,0-15,0 [1].Known mass to obtain an enamel coating, containing, wt.%: Frit 75.0-96.0; mullite 2.0-15.0 [1].

Задачей изобретения является повышение термостойкости эмалевого покрытия.The objective of the invention is to increase the heat resistance of the enamel coating.

Технический результат достигается тем, что масса для получения эмалевого покрытия, содержащая фритту и муллит, дополнительно содержит костяную золу при следующем соотношении компонентов, мас.%: фритта 72,0-74,0; муллит 7,0-9,0; костяная зола 17,0-21,0.The technical result is achieved in that the mass to obtain an enamel coating containing frit and mullite, additionally contains bone ash in the following ratio of components, wt.%: Frit 72.0-74.0; mullite 7.0-9.0; bone ash 17.0-21.0.

В таблице приведены составы массы для получения эмалевого покрытия.The table shows the composition of the mass to obtain an enamel coating.

СоставStructure Компоненты, мас.%Components, wt.% фриттаfrit муллитmullite костяная золаbone ash 1one 72,072.0 7,07.0 21,021.0 22 73,073.0 8,08.0 19,019.0 33 74,074.0 9,09.0 17,017.0

Используют типовой состав фритты В 1 с, используемой в производстве изделий санитарной керамики.Use a typical composition of frits B 1 s, used in the manufacture of sanitary ceramics.

Фритту В 1 с получают сплавлением следующих компонентов, мас.%: полевой пшат 15,6; песок кварцевый 15,5; мел 23,0; тальк 10,4; оксид цинка 2,0; барий углекислый 4,1; цирконовый концентрат 29,4 [2].Frit B 1 s is obtained by fusion of the following components, wt.%: Field wheat 15.6; quartz sand 15.5; chalk 23.0; talcum 10.4; zinc oxide 2.0; barium carbonate 4.1; zircon concentrate 29.4 [2].

Фритту, муллит, костяную золу дозируют в требуемых количествах, загружают в шаровую мельницу, добавляют воду и размалывают до полного прохождения через сетку 0056. Из полученной массы готовят суспензию с влажностью 45-60%. Суспензию наносят на поверхность керамических изделий и закрепляют обжигом при температуре ~ 1200°C. Термостойкость эмалевого покрытия составит ~ 25 теплосмен (нагрев до 450°C - охлаждение на воздухе) для любого состава, приведенного в таблице.Frit, mullite, bone ash are metered in the required quantities, loaded into a ball mill, water is added and ground until it passes through the 0056 mesh. A suspension with a moisture content of 45-60% is prepared from the resulting mass. The suspension is applied to the surface of ceramic products and fixed by firing at a temperature of ~ 1200 ° C. The heat resistance of the enamel coating will be ~ 25 heat exchange (heating to 450 ° C - cooling in air) for any composition shown in the table.

Источники информацииInformation sources

1. JP 9169543.1.JP 9169543.

2. Канаев В.К. Новая технология строительной керамики. - М.: Стройиздат, 1990. - С.63.2. Kanaev V.K. New technology for building ceramics. - M .: Stroyizdat, 1990. - P.63.

Claims (1)

Масса для получения эмалевого покрытия, содержащая фритту и муллит, отличающаяся тем, что дополнительно содержит костяную золу при следующем соотношении компонентов, мас.%: фритта 72,0-74,0; муллит 7,0-9,0; костяная зола 17,0-21,0. A mass for obtaining an enamel coating containing frit and mullite, characterized in that it further comprises bone ash in the following ratio of components, wt.%: Frit 72.0-74.0; mullite 7.0-9.0; bone ash 17.0-21.0.
RU2013155351/03A 2013-12-12 2013-12-12 Mixture for making enamel coating RU2537730C1 (en)