JPS63210027A - 結晶質酸化チタン一酸化スズゾル及びその製造方法 - Google Patents
結晶質酸化チタン一酸化スズゾル及びその製造方法Info
- Publication number
- JPS63210027A JPS63210027A JP4161587A JP4161587A JPS63210027A JP S63210027 A JPS63210027 A JP S63210027A JP 4161587 A JP4161587 A JP 4161587A JP 4161587 A JP4161587 A JP 4161587A JP S63210027 A JPS63210027 A JP S63210027A
- Authority
- JP
- Japan
- Prior art keywords
- gel
- sol
- titanium oxide
- tin oxide
- tin
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Inorganic Compounds Of Heavy Metals (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP4161587A JPS63210027A (ja) | 1987-02-24 | 1987-02-24 | 結晶質酸化チタン一酸化スズゾル及びその製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP4161587A JPS63210027A (ja) | 1987-02-24 | 1987-02-24 | 結晶質酸化チタン一酸化スズゾル及びその製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS63210027A true JPS63210027A (ja) | 1988-08-31 |
| JPH0427168B2 JPH0427168B2 (enrdf_load_stackoverflow) | 1992-05-11 |
Family
ID=12613242
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP4161587A Granted JPS63210027A (ja) | 1987-02-24 | 1987-02-24 | 結晶質酸化チタン一酸化スズゾル及びその製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS63210027A (enrdf_load_stackoverflow) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| EP0606122A1 (en) * | 1993-01-08 | 1994-07-13 | Hoogovens Industrial Ceramics B.V. | Ceramic ultrafiltration membrane and method of producing it |
| WO1998013299A1 (de) * | 1996-09-27 | 1998-04-02 | Coty B.V. | Ti-Sn-O-NANOCLUSTER, VERFAHREN ZU IHRER HERSTELLUNG UND VERWENDUNG DERSELBEN |
| WO2013081136A1 (ja) * | 2011-12-02 | 2013-06-06 | 日産化学工業株式会社 | ルチル型酸化チタンゾルの製造方法 |
Families Citing this family (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP5209857B2 (ja) * | 2006-07-14 | 2013-06-12 | Hoya株式会社 | コーティング組成物の製造方法 |
| JP5228980B2 (ja) * | 2009-02-17 | 2013-07-03 | 住友大阪セメント株式会社 | ルチル型複合微粒子及びルチル型複合微粒子分散液並びにルチル型複合微粒子の製造方法 |
Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6177623A (ja) * | 1984-09-21 | 1986-04-21 | Hakusui Kagaku Kogyo Kk | 複合導電性粉末の製造法 |
-
1987
- 1987-02-24 JP JP4161587A patent/JPS63210027A/ja active Granted
Patent Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6177623A (ja) * | 1984-09-21 | 1986-04-21 | Hakusui Kagaku Kogyo Kk | 複合導電性粉末の製造法 |
Cited By (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| EP0606122A1 (en) * | 1993-01-08 | 1994-07-13 | Hoogovens Industrial Ceramics B.V. | Ceramic ultrafiltration membrane and method of producing it |
| WO1998013299A1 (de) * | 1996-09-27 | 1998-04-02 | Coty B.V. | Ti-Sn-O-NANOCLUSTER, VERFAHREN ZU IHRER HERSTELLUNG UND VERWENDUNG DERSELBEN |
| WO2013081136A1 (ja) * | 2011-12-02 | 2013-06-06 | 日産化学工業株式会社 | ルチル型酸化チタンゾルの製造方法 |
| JPWO2013081136A1 (ja) * | 2011-12-02 | 2015-04-27 | 日産化学工業株式会社 | ルチル型酸化チタンゾルの製造方法 |
| US9023147B2 (en) | 2011-12-02 | 2015-05-05 | Nissan Chemical Industries, Ltd. | Method for producing rutile type titanium oxide sol |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0427168B2 (enrdf_load_stackoverflow) | 1992-05-11 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPS6317221A (ja) | 結晶質酸化チタンゾル及びその製造方法 | |
| JP2709222B2 (ja) | チタン酸塩からなる球形微粉末の製造方法及びそれにより得られた球形微粉末 | |
| JPH01148710A (ja) | 結晶質酸化第二セリウムゾルの製造法 | |
| JPS627160B2 (enrdf_load_stackoverflow) | ||
| JPS63210027A (ja) | 結晶質酸化チタン一酸化スズゾル及びその製造方法 | |
| JP3205681B2 (ja) | ジルコニア粉末の製造方法 | |
| JPH0445453B2 (enrdf_load_stackoverflow) | ||
| KR100483169B1 (ko) | 다성분계 금속산화물 분말의 제조방법 | |
| JP2005008445A (ja) | チタン酸バリウム粉末の製造方法 | |
| JPS61251515A (ja) | 複合酸化物セラミツク粉末の製造方法 | |
| JPS60161338A (ja) | BaTiO▲下3▼とBaSn(OH)▲下6▼より成る混合微粒子の製造方法 | |
| JPS61251516A (ja) | ペロブスカイト型酸化物の製造法 | |
| JPH01294528A (ja) | Abo↓3型ペロブスカイト型酸化物の製法 | |
| JP2607519B2 (ja) | 光学セラミックスの製造方法 | |
| JPS61146712A (ja) | チタン酸バリウムの製造法 | |
| JPS63206316A (ja) | チタンジルコニウム酸鉛微粒子の製造方法 | |
| JPH0262496B2 (enrdf_load_stackoverflow) | ||
| KR960004388B1 (ko) | 지르콘-티탄산납계 압전분말의 제조방법 | |
| JPH06171944A (ja) | 酸化ジルコニウム粉末を製造する方法 | |
| JPH08151214A (ja) | 複合酸化物製造方法 | |
| JPS63288960A (ja) | (Pb,Bi)(Zr,Ti)0↓3の製造方法 | |
| CN1036190C (zh) | 高纯微细钛酸盐合成新工艺 | |
| JPH01122907A (ja) | ペロブスカイト酸化物紛末の製造方法 | |
| JPH09286617A (ja) | チタン酸鉛粉末の製造方法 | |
| JPH06166518A (ja) | Ba(SnxTi1−x )O3 固溶体微粒子の製造方法 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| R250 | Receipt of annual fees |
Free format text: JAPANESE INTERMEDIATE CODE: R250 |
|
| EXPY | Cancellation because of completion of term |