JPS6312311Y2 - - Google Patents
Info
- Publication number
- JPS6312311Y2 JPS6312311Y2 JP1982103659U JP10365982U JPS6312311Y2 JP S6312311 Y2 JPS6312311 Y2 JP S6312311Y2 JP 1982103659 U JP1982103659 U JP 1982103659U JP 10365982 U JP10365982 U JP 10365982U JP S6312311 Y2 JPS6312311 Y2 JP S6312311Y2
- Authority
- JP
- Japan
- Prior art keywords
- heat
- adhesive layer
- shrinkable
- weld bead
- base material
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Protection Of Pipes Against Damage, Friction, And Corrosion (AREA)
- Rigid Pipes And Flexible Pipes (AREA)
- Lining Or Joining Of Plastics Or The Like (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP10365982U JPS597990U (ja) | 1982-07-08 | 1982-07-08 | 管体溶接ビート部被覆用熱収縮性部材 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP10365982U JPS597990U (ja) | 1982-07-08 | 1982-07-08 | 管体溶接ビート部被覆用熱収縮性部材 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS597990U JPS597990U (ja) | 1984-01-19 |
| JPS6312311Y2 true JPS6312311Y2 (en:Method) | 1988-04-08 |
Family
ID=30243738
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP10365982U Granted JPS597990U (ja) | 1982-07-08 | 1982-07-08 | 管体溶接ビート部被覆用熱収縮性部材 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS597990U (en:Method) |
Family Cites Families (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5913781Y2 (ja) * | 1975-11-20 | 1984-04-23 | ヤンマー農機株式会社 | コンバインにおける穀稈縦搬送装置 |
-
1982
- 1982-07-08 JP JP10365982U patent/JPS597990U/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS597990U (ja) | 1984-01-19 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPS5852969Y2 (ja) | 熱収縮性シ−ト | |
| US3226807A (en) | Method of constructing a continuous pipeline | |
| GB2136524A (en) | Reinsulation of pipe joints | |
| JPS6312311Y2 (en:Method) | ||
| JPS5887015A (ja) | 被覆鋼管の接続部の被覆保護層形成方法 | |
| JP3155696B2 (ja) | 管溶接継手部被覆方法 | |
| JPH06182872A (ja) | 鋼管の部分防食方法 | |
| JPH0148860B2 (en:Method) | ||
| KR20010072879A (ko) | 그 안의 개구를 차폐시키는 설비를 갖춘 케이스 | |
| JPS5925622Y2 (ja) | 熱収縮性チユ−ブ | |
| JPS6319677Y2 (en:Method) | ||
| JPS58132513A (ja) | 鋼管の防蝕方法 | |
| JPH0332458B2 (en:Method) | ||
| JP3655291B2 (ja) | 大容量変圧器本体とコンサベ−タを結合するフランジ接続部の油漏れ処理方法 | |
| JP2522104Y2 (ja) | 分岐管防食用熱収縮性成形体 | |
| JP3155175B2 (ja) | ガス配管の活管分岐部の防食部材 | |
| JPS6310277Y2 (en:Method) | ||
| JPS5814957B2 (ja) | 防蝕鋼管の接続部分の防蝕方法 | |
| JPS604752Y2 (ja) | 突起つき熱収縮性シ−ト | |
| JPH039360B2 (en:Method) | ||
| JPS6120843Y2 (en:Method) | ||
| JPS608980Y2 (ja) | 熱収縮性物品 | |
| JP3299675B2 (ja) | 防食被覆鋼管の継手部の防食被覆方法 | |
| JPS5973696A (ja) | エルボ管の防食方法 | |
| JP2575504B2 (ja) | 管交叉部の表面防食用シート |