JPS6230262B2 - - Google Patents
Info
- Publication number
- JPS6230262B2 JPS6230262B2 JP22847183A JP22847183A JPS6230262B2 JP S6230262 B2 JPS6230262 B2 JP S6230262B2 JP 22847183 A JP22847183 A JP 22847183A JP 22847183 A JP22847183 A JP 22847183A JP S6230262 B2 JPS6230262 B2 JP S6230262B2
- Authority
- JP
- Japan
- Prior art keywords
- layer
- acid
- main component
- nitric acid
- blackening treatment
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C22/00—Chemical surface treatment of metallic material by reaction of the surface with a reactive liquid, leaving reaction products of surface material in the coating, e.g. conversion coatings, passivation of metals
- C23C22/05—Chemical surface treatment of metallic material by reaction of the surface with a reactive liquid, leaving reaction products of surface material in the coating, e.g. conversion coatings, passivation of metals using aqueous solutions
- C23C22/06—Chemical surface treatment of metallic material by reaction of the surface with a reactive liquid, leaving reaction products of surface material in the coating, e.g. conversion coatings, passivation of metals using aqueous solutions using aqueous acidic solutions with pH less than 6
- C23C22/48—Chemical surface treatment of metallic material by reaction of the surface with a reactive liquid, leaving reaction products of surface material in the coating, e.g. conversion coatings, passivation of metals using aqueous solutions using aqueous acidic solutions with pH less than 6 not containing phosphates, hexavalent chromium compounds, fluorides or complex fluorides, molybdates, tungstates, vanadates or oxalates
- C23C22/53—Treatment of zinc or alloys based thereon
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C22/00—Chemical surface treatment of metallic material by reaction of the surface with a reactive liquid, leaving reaction products of surface material in the coating, e.g. conversion coatings, passivation of metals
- C23C22/05—Chemical surface treatment of metallic material by reaction of the surface with a reactive liquid, leaving reaction products of surface material in the coating, e.g. conversion coatings, passivation of metals using aqueous solutions
- C23C22/06—Chemical surface treatment of metallic material by reaction of the surface with a reactive liquid, leaving reaction products of surface material in the coating, e.g. conversion coatings, passivation of metals using aqueous solutions using aqueous acidic solutions with pH less than 6
- C23C22/48—Chemical surface treatment of metallic material by reaction of the surface with a reactive liquid, leaving reaction products of surface material in the coating, e.g. conversion coatings, passivation of metals using aqueous solutions using aqueous acidic solutions with pH less than 6 not containing phosphates, hexavalent chromium compounds, fluorides or complex fluorides, molybdates, tungstates, vanadates or oxalates
- C23C22/58—Treatment of other metallic material
Landscapes
- Chemical & Material Sciences (AREA)
- General Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Mechanical Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Electroplating Methods And Accessories (AREA)
- Chemical Treatment Of Metals (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP22847183A JPS60121275A (ja) | 1983-12-05 | 1983-12-05 | 黒色化鋼板とその製法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP22847183A JPS60121275A (ja) | 1983-12-05 | 1983-12-05 | 黒色化鋼板とその製法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS60121275A JPS60121275A (ja) | 1985-06-28 |
| JPS6230262B2 true JPS6230262B2 (enEXAMPLES) | 1987-07-01 |
Family
ID=16876995
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP22847183A Granted JPS60121275A (ja) | 1983-12-05 | 1983-12-05 | 黒色化鋼板とその製法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS60121275A (enEXAMPLES) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| DE4310316A1 (de) * | 1992-03-31 | 1993-12-02 | Nippon Kokan Kk | Schweißbares schwarzes Stahlblech von glanzarmem Aussehen |
Families Citing this family (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS61238979A (ja) * | 1985-04-15 | 1986-10-24 | Kobe Steel Ltd | 着色亜鉛合金めつき鋼板の製造方法 |
| JPS6277482A (ja) * | 1985-09-30 | 1987-04-09 | Nippon Steel Corp | 耐食性黒色亜鉛合金メツキ鋼板の製造方法 |
| US4968391A (en) * | 1988-01-29 | 1990-11-06 | Nippon Steel Corporation | Process for the preparation of a black surface-treated steel sheet |
| JP2553963Y2 (ja) * | 1991-11-26 | 1997-11-12 | 株式会社テック | 照明器具 |
| EP1222319A1 (de) * | 1998-08-18 | 2002-07-17 | Walter Hillebrand GmbH & Co. | Passivierungsverfahren für zink-nickel-schichten |
| DE19905134A1 (de) * | 1999-02-09 | 2000-09-28 | Hillebrand Walter Gmbh & Co Kg | Passivierungsverfahren |
| JP5443790B2 (ja) * | 2009-03-10 | 2014-03-19 | Dowaメタルテック株式会社 | ニッケルめっき材の製造方法 |
-
1983
- 1983-12-05 JP JP22847183A patent/JPS60121275A/ja active Granted
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| DE4310316A1 (de) * | 1992-03-31 | 1993-12-02 | Nippon Kokan Kk | Schweißbares schwarzes Stahlblech von glanzarmem Aussehen |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS60121275A (ja) | 1985-06-28 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP2003171778A (ja) | 金属の保護皮膜形成方法及び金属の保護皮膜 | |
| JPS6230262B2 (enEXAMPLES) | ||
| JPH03138389A (ja) | めっき密着性および耐食性に優れたZn―Mg合金めっき鋼板およびその製造方法 | |
| JP2950481B2 (ja) | 金属表面処理方法 | |
| JP2816559B2 (ja) | 黒色亜鉛めっき鋼板の製造方法 | |
| JPH0564237B2 (enEXAMPLES) | ||
| JPS63130796A (ja) | 耐食性と塗料密着性に優れた複合化成処理鋼板およびその製造方法 | |
| JP2839971B2 (ja) | 透明フッ素樹脂被覆ステンレス鋼板の製造方法 | |
| JP3114642B2 (ja) | 黒色溶融Al−Zn合金めっき鋼板およびその製造方法 | |
| JPH0762554A (ja) | 亜鉛系めっき材料の黒色化処理方法 | |
| JP3116811B2 (ja) | 黒色化溶融Zn−Al合金めっき鋼板とその製造方法 | |
| JPS6230263B2 (enEXAMPLES) | ||
| JP2001279414A (ja) | 黒色化溶融Zn−Al基合金めっき鋼板 | |
| JP3296210B2 (ja) | 加工密着性、耐食性に優れた有機樹脂被覆鋼板用亜鉛めっき鋼板及びその製造方法 | |
| JPS596383A (ja) | アルミニウム部品に腐蝕保護層を電流を用いないで製出する方法 | |
| CN117165888A (zh) | 一种具有优异脱脂和磷化性能的锌系镀层钢板及其制造方法 | |
| JP2701145B2 (ja) | メツキ鋼板のクロメート化成処理方法 | |
| JP3279196B2 (ja) | 加工密着性、耐食性に優れた有機樹脂被覆鋼板用亜鉛めっき鋼板 | |
| KR100293233B1 (ko) | 크로메이트바탕피막제조용전처리용액및이를이용한표면외관및내식성이우수한도포형크로메이트피막제조방법 | |
| JPS6123769A (ja) | 化成処理されたアルミニウム含有亜鉛めつき合金鋼板 | |
| JPH042758A (ja) | プレス成形性及び塗装耐食性に優れた溶融系合金亜鉛めっき鋼板の製造方法 | |
| JP2005187838A (ja) | 金属表面処理液および金属表面処理方法 | |
| CN116987996A (zh) | 一种具有优良脱脂性能的锌镁铝镀层钢板及其制造方法 | |
| JPH09195062A (ja) | 耐食性、耐黒変性および耐疵つき性に優れた溶融亜鉛系めっき鋼板の製造方法 | |
| JPS624880A (ja) | 亜鉛めつきまたは合金化亜鉛めつき鋼板の表面処理方法 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| LAPS | Cancellation because of no payment of annual fees |