JPS62207830A - 表面特性の良好な冷延鋼帯の製造方法 - Google Patents

表面特性の良好な冷延鋼帯の製造方法

Info

Publication number
JPS62207830A
JPS62207830A JP4841586A JP4841586A JPS62207830A JP S62207830 A JPS62207830 A JP S62207830A JP 4841586 A JP4841586 A JP 4841586A JP 4841586 A JP4841586 A JP 4841586A JP S62207830 A JPS62207830 A JP S62207830A
Authority
JP
Japan
Prior art keywords
water
cooling
rolled steel
steel strip
cold
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP4841586A
Other languages
English (en)
Japanese (ja)
Other versions
JPH031365B2 (enExample
Inventor
Keiichi Tanigawa
谷川 啓一
Hideo Sugano
秀雄 菅野
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nippon Steel Corp
Original Assignee
Nippon Steel Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nippon Steel Corp filed Critical Nippon Steel Corp
Priority to JP4841586A priority Critical patent/JPS62207830A/ja
Publication of JPS62207830A publication Critical patent/JPS62207830A/ja
Publication of JPH031365B2 publication Critical patent/JPH031365B2/ja
Granted legal-status Critical Current

Links

Classifications

    • CCHEMISTRY; METALLURGY
    • C23COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
    • C23FNON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
    • C23F11/00Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent
    • C23F11/08Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent in other liquids

Landscapes

  • Chemical & Material Sciences (AREA)
  • Engineering & Computer Science (AREA)
  • Materials Engineering (AREA)
  • Mechanical Engineering (AREA)
  • Metallurgy (AREA)
  • Organic Chemistry (AREA)
  • Chemical Treatment Of Metals (AREA)
  • Heat Treatment Of Strip Materials And Filament Materials (AREA)
  • Preventing Corrosion Or Incrustation Of Metals (AREA)
JP4841586A 1986-03-07 1986-03-07 表面特性の良好な冷延鋼帯の製造方法 Granted JPS62207830A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP4841586A JPS62207830A (ja) 1986-03-07 1986-03-07 表面特性の良好な冷延鋼帯の製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP4841586A JPS62207830A (ja) 1986-03-07 1986-03-07 表面特性の良好な冷延鋼帯の製造方法

Publications (2)

Publication Number Publication Date
JPS62207830A true JPS62207830A (ja) 1987-09-12
JPH031365B2 JPH031365B2 (enExample) 1991-01-10

Family

ID=12802675

Family Applications (1)

Application Number Title Priority Date Filing Date
JP4841586A Granted JPS62207830A (ja) 1986-03-07 1986-03-07 表面特性の良好な冷延鋼帯の製造方法

Country Status (1)

Country Link
JP (1) JPS62207830A (enExample)

Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS57101618A (en) * 1980-12-16 1982-06-24 Nippon Steel Corp Continuous annealing of cold-rolled steel plate
JPS57149429A (en) * 1981-03-11 1982-09-16 Nippon Kokan Kk <Nkk> Preparation of cold rolled steel plate having excellent corrosion resistance and formation-treatment property
JPS6052531A (ja) * 1983-09-02 1985-03-25 Nippon Steel Corp 冷延鋼帯の冷却用水溶液
JPS60128216A (ja) * 1983-12-13 1985-07-09 Nippon Steel Corp 冷延鋼板の連続焼鈍における冷却法

Patent Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS57101618A (en) * 1980-12-16 1982-06-24 Nippon Steel Corp Continuous annealing of cold-rolled steel plate
JPS57149429A (en) * 1981-03-11 1982-09-16 Nippon Kokan Kk <Nkk> Preparation of cold rolled steel plate having excellent corrosion resistance and formation-treatment property
JPS6052531A (ja) * 1983-09-02 1985-03-25 Nippon Steel Corp 冷延鋼帯の冷却用水溶液
JPS60128216A (ja) * 1983-12-13 1985-07-09 Nippon Steel Corp 冷延鋼板の連続焼鈍における冷却法

Also Published As

Publication number Publication date
JPH031365B2 (enExample) 1991-01-10

Similar Documents

Publication Publication Date Title
KR101578848B1 (ko) 6 내지 30 중량%의 Mn을 함유하는 열간 압연 또는 냉간 압연 평탄형 강 제품을 금속 보호층으로 도금하는 방법
WO2020113844A1 (zh) 一种耐腐蚀热冲压零件的制备方法及装置
EP0140027B1 (en) Aqueous solution for cooling cold-rolled steel strip in a continuous annealing process
JPS61201737A (ja) 表面特性の良好な冷延鋼帯の製造方法
JPH0371487B2 (enExample)
JPS58181855A (ja) アルミニウムベ−ス複合溶融めつき鋼板の製造方法
JP4834922B2 (ja) 溶融亜鉛めっき鋼板の製造方法
JPS62205290A (ja) 表面特性の良好な冷延鋼帯の製造方法
JPS6028909B2 (ja) 化成処理性に優れた鋼板
JPH031365B2 (enExample)
JP3400289B2 (ja) めっき密着性に優れた合金化溶融亜鉛めっき鋼板の製造方法
JPH02170925A (ja) 連続焼鈍冷間圧延鋼板の製造方法
JP2978074B2 (ja) 均一表面外観に優れた電気Znめっき鋼板の製造方法
CN120682679B (zh) 一种具有高加热效率和油漆附着力的铝系镀层热成形钢板及制造方法和应用
CN120843992B (zh) 铝硅镀层热成形钢板、具有牺牲阳极保护和优异涂装性能的铝硅镀层热成形钢制零部件及其制备方法
EP4541949A1 (en) Steel sheet and manufacturing method therefor
JPH031364B2 (enExample)
EP4282994A1 (en) Method for producing annealed and pickled steel sheet
JPH04232297A (ja) 光沢、白色度および耐食性に優れたステンレス冷延鋼帯の製造方法
JPS5933172B2 (ja) 冷延鋼板の連続焼鈍処理方法
KR850000579B1 (ko) 냉간 압연강 스트립(strip)의 연속 어니일링 방법
JPS58144477A (ja) 金属表面のリン酸塩処理法
JPH07243012A (ja) 表面外観に優れた合金化溶融Znめっき鋼板の製造方法
JPH01139728A (ja) 化成処理性に優れた連続焼鈍冷延鋼板の冷却処理方法
JPH0474900A (ja) ステンレス鋼表面の酸化物による被覆方法