JPH031364B2 - - Google Patents

Info

Publication number
JPH031364B2
JPH031364B2 JP60041251A JP4125185A JPH031364B2 JP H031364 B2 JPH031364 B2 JP H031364B2 JP 60041251 A JP60041251 A JP 60041251A JP 4125185 A JP4125185 A JP 4125185A JP H031364 B2 JPH031364 B2 JP H031364B2
Authority
JP
Japan
Prior art keywords
acid
cooling
water
amino acids
rolled steel
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
JP60041251A
Other languages
English (en)
Japanese (ja)
Other versions
JPS61201736A (ja
Inventor
Keiichi Tanigawa
Minoru Kamata
Hideo Sugano
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nippon Steel Corp
Original Assignee
Nippon Steel Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nippon Steel Corp filed Critical Nippon Steel Corp
Priority to JP4125185A priority Critical patent/JPS61201736A/ja
Publication of JPS61201736A publication Critical patent/JPS61201736A/ja
Publication of JPH031364B2 publication Critical patent/JPH031364B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Heat Treatment Of Strip Materials And Filament Materials (AREA)
  • Preventing Corrosion Or Incrustation Of Metals (AREA)
JP4125185A 1985-03-04 1985-03-04 表面特性の良好な冷延鋼帯の製造方法 Granted JPS61201736A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP4125185A JPS61201736A (ja) 1985-03-04 1985-03-04 表面特性の良好な冷延鋼帯の製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP4125185A JPS61201736A (ja) 1985-03-04 1985-03-04 表面特性の良好な冷延鋼帯の製造方法

Publications (2)

Publication Number Publication Date
JPS61201736A JPS61201736A (ja) 1986-09-06
JPH031364B2 true JPH031364B2 (enExample) 1991-01-10

Family

ID=12603217

Family Applications (1)

Application Number Title Priority Date Filing Date
JP4125185A Granted JPS61201736A (ja) 1985-03-04 1985-03-04 表面特性の良好な冷延鋼帯の製造方法

Country Status (1)

Country Link
JP (1) JPS61201736A (enExample)

Families Citing this family (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
KR100349809B1 (ko) * 2000-03-15 2002-08-23 (주)현광금속개발 금속재의 열처리방법

Family Cites Families (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS6052531A (ja) * 1983-09-02 1985-03-25 Nippon Steel Corp 冷延鋼帯の冷却用水溶液
JPS61149440A (ja) * 1984-12-25 1986-07-08 Nippon Steel Corp 連続焼鈍による冷延鋼板の製造方法

Also Published As

Publication number Publication date
JPS61201736A (ja) 1986-09-06

Similar Documents

Publication Publication Date Title
JPS634610B2 (enExample)
JP5282459B2 (ja) Si含有鋼板の製造方法
JP2009256701A (ja) アルミニウム材表面処理方法
JP4335737B2 (ja) Si含有鋼板の製造方法
CN111560576A (zh) 一种镀锌钢卷的生产工艺
JPS61201736A (ja) 表面特性の良好な冷延鋼帯の製造方法
JPH0323611B2 (enExample)
JPH031365B2 (enExample)
JPH044397B2 (enExample)
JPH0371487B2 (enExample)
JPH07835B2 (ja) 鋼板の変色防止方法
JPH0563528B2 (enExample)
JPH02170925A (ja) 連続焼鈍冷間圧延鋼板の製造方法
JPS62205290A (ja) 表面特性の良好な冷延鋼帯の製造方法
JPS61167000A (ja) 連続焼鈍鋼帯の酸化膜除去方法
JP4162404B2 (ja) アルミニウム及びアルミニウム合金の表面処理方法と表面処理剤
JPH01156429A (ja) 連続焼鈍冷延鋼板の冷却処理方法
JP4028014B2 (ja) 酸洗促進剤、酸洗促進剤を含んだ酸洗液組成物およびこれらを用いる金属の酸洗方法
JPH07316842A (ja) 溶融亜鉛めっき用鋼板
SU1624053A1 (ru) Способ химико-термической обработки стальных изделий
JP4894208B2 (ja) 鋼帯の製造方法
JPH04232297A (ja) 光沢、白色度および耐食性に優れたステンレス冷延鋼帯の製造方法
JP2025524414A (ja) 鋼板及びその製造方法
JPH05140718A (ja) 溶融亜鉛系合金化めつき鋼板の製造方法
JPS63192820A (ja) 鋼材の冷却方法