JPS622009B2 - - Google Patents
Info
- Publication number
- JPS622009B2 JPS622009B2 JP58130750A JP13075083A JPS622009B2 JP S622009 B2 JPS622009 B2 JP S622009B2 JP 58130750 A JP58130750 A JP 58130750A JP 13075083 A JP13075083 A JP 13075083A JP S622009 B2 JPS622009 B2 JP S622009B2
- Authority
- JP
- Japan
- Prior art keywords
- resistance
- strength
- less
- temperature
- strain
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C21—METALLURGY OF IRON
- C21D—MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING
- C21D8/00—Modifying the physical properties by deformation combined with, or followed by, heat treatment
- C21D8/10—Modifying the physical properties by deformation combined with, or followed by, heat treatment during manufacturing of tubular bodies
Landscapes
- Engineering & Computer Science (AREA)
- Chemical & Material Sciences (AREA)
- Manufacturing & Machinery (AREA)
- Physics & Mathematics (AREA)
- Thermal Sciences (AREA)
- Crystallography & Structural Chemistry (AREA)
- Mechanical Engineering (AREA)
- Materials Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Heat Treatment Of Steel (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP13075083A JPS6024321A (ja) | 1983-07-20 | 1983-07-20 | 耐サワ−性と耐圧潰性にすぐれた高強度電縫油井管の製造方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP13075083A JPS6024321A (ja) | 1983-07-20 | 1983-07-20 | 耐サワ−性と耐圧潰性にすぐれた高強度電縫油井管の製造方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS6024321A JPS6024321A (ja) | 1985-02-07 |
JPS622009B2 true JPS622009B2 (enrdf_load_stackoverflow) | 1987-01-17 |
Family
ID=15041741
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP13075083A Granted JPS6024321A (ja) | 1983-07-20 | 1983-07-20 | 耐サワ−性と耐圧潰性にすぐれた高強度電縫油井管の製造方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS6024321A (enrdf_load_stackoverflow) |
Families Citing this family (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS60187664A (ja) * | 1984-03-01 | 1985-09-25 | Nippon Steel Corp | 低硬度で降伏強度の高い電縫油井管及びその製造方法 |
JPS60187663A (ja) * | 1984-03-01 | 1985-09-25 | Nippon Steel Corp | 低硬度で降伏強度の高い電縫油井管及びその製造方法 |
Family Cites Families (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS607007B2 (ja) * | 1980-07-04 | 1985-02-21 | 新日本製鐵株式会社 | 低降伏比高張力電縫鋼管の製造方法 |
JPS57131319A (en) * | 1981-02-06 | 1982-08-14 | Nippon Steel Corp | Manufacture of high strength seam welded steel pipe for oil well |
-
1983
- 1983-07-20 JP JP13075083A patent/JPS6024321A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS6024321A (ja) | 1985-02-07 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US4946516A (en) | Process for producing high toughness, high strength steel having excellent resistance to stress corrosion cracking | |
JPH0741856A (ja) | 耐硫化物応力腐食割れ性に優れた高強度鋼管の製造法 | |
JP3620326B2 (ja) | 細粒組織で強度バラツキの小さい継目無鋼管 | |
JPH08104922A (ja) | 低温靱性の優れた高強度鋼管の製造方法 | |
JPH0250916A (ja) | 細粒化組織の低合金高張力シームレス鋼管の製造法 | |
KR950007785B1 (ko) | 고강도 대경선재의 제조방법 | |
JP3009558B2 (ja) | 耐サワー性の優れた薄手高強度鋼板の製造方法 | |
JPS622009B2 (enrdf_load_stackoverflow) | ||
JP3491149B2 (ja) | 強度−靱性バランスに優れた油井用高強度マルテンサイト系ステンレス鋼管およびその製造方法 | |
JPH0224904B2 (enrdf_load_stackoverflow) | ||
JPH05171361A (ja) | マルテンサイト系ステンレス鋼と製造方法 | |
JPH06293914A (ja) | 耐co2 腐食性、haz靱性に優れた低合金ラインパイプ用鋼板の製造方法 | |
JPH11310822A (ja) | 低温靭性に優れた高強度マルテンサイト系ステンレス鋼管の製造法 | |
JPH0741855A (ja) | 細粒フェライト主体の金属組織を呈した低降伏比高靭性継目無鋼管の製造法 | |
US5827379A (en) | Process for producing extra high tensile steel having excellent stress corrosion cracking resistance | |
JPS6137333B2 (enrdf_load_stackoverflow) | ||
JPH09324217A (ja) | 耐hic性に優れた高強度ラインパイプ用鋼の製造方法 | |
JPH07292414A (ja) | 優れた低温靱性を有する耐サワー薄手高強度鋼板の製造方法 | |
JPS5920423A (ja) | 低温靭性の優れた80kgf/mm2級継目無鋼管の製造方法 | |
JPS62971B2 (enrdf_load_stackoverflow) | ||
JPH08337817A (ja) | 耐水素遅れ割れ特性に優れた超高張力電縫鋼管の製造方法 | |
KR100345704B1 (ko) | 내수소유기응력부식균열성이우수한고강도열연강판의제조방법 | |
JPH0250912A (ja) | 細粒化組織の低合金高張力シームレス鋼管の製造法 | |
JPH0250915A (ja) | 細粒化組織の低合金高張力シームレス鋼管の製造法 | |
JPH11310823A (ja) | 低温靭性に優れたマルテンサイト系ステンレス鋼管の製造方法 |