JPS6219798B2 - - Google Patents
Info
- Publication number
- JPS6219798B2 JPS6219798B2 JP56061023A JP6102381A JPS6219798B2 JP S6219798 B2 JPS6219798 B2 JP S6219798B2 JP 56061023 A JP56061023 A JP 56061023A JP 6102381 A JP6102381 A JP 6102381A JP S6219798 B2 JPS6219798 B2 JP S6219798B2
- Authority
- JP
- Japan
- Prior art keywords
- additive
- strength
- soft soil
- soil
- mixing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- E—FIXED CONSTRUCTIONS
- E02—HYDRAULIC ENGINEERING; FOUNDATIONS; SOIL SHIFTING
- E02D—FOUNDATIONS; EXCAVATIONS; EMBANKMENTS; UNDERGROUND OR UNDERWATER STRUCTURES
- E02D3/00—Improving or preserving soil or rock, e.g. preserving permafrost soil
- E02D3/12—Consolidating by placing solidifying or pore-filling substances in the soil
Landscapes
- Engineering & Computer Science (AREA)
- Structural Engineering (AREA)
- Life Sciences & Earth Sciences (AREA)
- General Life Sciences & Earth Sciences (AREA)
- Soil Sciences (AREA)
- Environmental & Geological Engineering (AREA)
- Agronomy & Crop Science (AREA)
- Mining & Mineral Resources (AREA)
- Paleontology (AREA)
- Civil Engineering (AREA)
- General Engineering & Computer Science (AREA)
- Consolidation Of Soil By Introduction Of Solidifying Substances Into Soil (AREA)
- Soil Conditioners And Soil-Stabilizing Materials (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6102381A JPS57174523A (en) | 1981-04-22 | 1981-04-22 | Increase of strength of wet soft soil |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6102381A JPS57174523A (en) | 1981-04-22 | 1981-04-22 | Increase of strength of wet soft soil |
Related Child Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP16482083A Division JPS5980486A (ja) | 1983-09-07 | 1983-09-07 | 悪臭を持つ含水軟弱土の脱臭を伴う強度増加方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS57174523A JPS57174523A (en) | 1982-10-27 |
JPS6219798B2 true JPS6219798B2 (enrdf_load_stackoverflow) | 1987-05-01 |
Family
ID=13159290
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP6102381A Granted JPS57174523A (en) | 1981-04-22 | 1981-04-22 | Increase of strength of wet soft soil |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS57174523A (enrdf_load_stackoverflow) |
Families Citing this family (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6451198A (en) * | 1987-08-21 | 1989-02-27 | Telnite Ltd | Modifying method for drilling soil |
JPS6372783A (ja) * | 1987-09-12 | 1988-04-02 | Chiyoda Chem Eng & Constr Co Ltd | 悪臭を持つ含水軟弱土の脱臭を伴う強度増加方法 |
JPH01139198A (ja) * | 1987-11-26 | 1989-05-31 | Terunaito:Kk | 汚泥の改質方法 |
JP5407112B2 (ja) * | 2007-03-23 | 2014-02-05 | 宇部興産株式会社 | 高圧噴射工法用セメント系固化材および高圧噴射工法 |
JP2012072301A (ja) * | 2010-09-29 | 2012-04-12 | Tachibana Material Co Ltd | 土質改良固化材 |
Family Cites Families (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5320610A (en) * | 1976-08-10 | 1978-02-25 | Nippon Hodo | Subsoil stabilizing method |
JPS54113911A (en) * | 1978-02-24 | 1979-09-05 | Onoda Cement Co Ltd | Improving material of organic matter soft ground |
JPS56100920A (en) * | 1980-01-18 | 1981-08-13 | Chiyoda Chem Eng & Constr Co Ltd | Improvement of water content poorsoil |
-
1981
- 1981-04-22 JP JP6102381A patent/JPS57174523A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS57174523A (en) | 1982-10-27 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS6314028B2 (enrdf_load_stackoverflow) | ||
US4465518A (en) | Process for strengthening soft soil | |
Tashima et al. | Compressive strength and microstructure of alkali-activated blast furnace slag/sewage sludge ash (GGBS/SSA) blends cured at room temperature | |
JP5800387B2 (ja) | 土質改良材 | |
JP2003306359A (ja) | セメント組成物及び水和硬化体 | |
CN115594455B (zh) | 一种磷石膏路面基层水稳材料的制备方法 | |
CN110467368B (zh) | 一种用于无机固体废弃物建材化的活性激发剂及其制备方法 | |
JP2004518605A (ja) | セメント材料 | |
KR100771490B1 (ko) | 유·무기성 폐자원용 고화제의 제조방법 | |
JP6662046B2 (ja) | 泥土含有固化体の製造方法 | |
EP4253340A1 (en) | Supplementary cementitious materials from recycled cement paste | |
CN109095877A (zh) | 一种土体固化剂及其制备方法、固化土壤的方法 | |
JPS6219798B2 (enrdf_load_stackoverflow) | ||
KR100375407B1 (ko) | 폐기물의 중금속 용출방지를 위한 고형체 제조방법 및이에 의해 제조된 고형체 | |
CN118026605A (zh) | 一种硅铝基胶凝材料协同固化垃圾焚烧飞灰处理方法 | |
CN111892312A (zh) | 一种多固废大掺量利用方法 | |
JP2017019714A (ja) | 脱硫スラグを用いた水和固化体 | |
KR20040020494A (ko) | 폐콘크리트를 이용한 유해 폐기물 고화용 시멘트 제조방법및 이로부터 제조된 시멘트 | |
JPH0826794A (ja) | セメントの製造方法 | |
JPS6217637B2 (enrdf_load_stackoverflow) | ||
KR20030075045A (ko) | 해양수산폐기물과 산업폐기물을 이용한 함수연약토의지반개량형 고화재의 조성물 및 그 제조방법 | |
JPS6365717B2 (enrdf_load_stackoverflow) | ||
JPS6158239B2 (enrdf_load_stackoverflow) | ||
JPH0138431B2 (enrdf_load_stackoverflow) | ||
JP7615205B2 (ja) | セメント組成物及びその製造方法 |