JPS6219276B2 - - Google Patents
Info
- Publication number
- JPS6219276B2 JPS6219276B2 JP11201482A JP11201482A JPS6219276B2 JP S6219276 B2 JPS6219276 B2 JP S6219276B2 JP 11201482 A JP11201482 A JP 11201482A JP 11201482 A JP11201482 A JP 11201482A JP S6219276 B2 JPS6219276 B2 JP S6219276B2
- Authority
- JP
- Japan
- Prior art keywords
- pipe
- tube
- stress
- welded part
- residual stress
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K31/00—Processes relevant to this subclass, specially adapted for particular articles or purposes, but not covered by any single one of main groups B23K1/00 - B23K28/00
Landscapes
- Engineering & Computer Science (AREA)
- Mechanical Engineering (AREA)
- Heat Treatment Of Articles (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP11201482A JPS594989A (ja) | 1982-06-29 | 1982-06-29 | 配管溶接部の残留応力改善方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP11201482A JPS594989A (ja) | 1982-06-29 | 1982-06-29 | 配管溶接部の残留応力改善方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS594989A JPS594989A (ja) | 1984-01-11 |
| JPS6219276B2 true JPS6219276B2 (Direct) | 1987-04-27 |
Family
ID=14575807
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP11201482A Granted JPS594989A (ja) | 1982-06-29 | 1982-06-29 | 配管溶接部の残留応力改善方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS594989A (Direct) |
-
1982
- 1982-06-29 JP JP11201482A patent/JPS594989A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS594989A (ja) | 1984-01-11 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US7866166B2 (en) | Method for improving residual stress in pipe and apparatus | |
| EP1927668B1 (en) | Restoration method for deteriorated part and restoration apparatus for deteriorated part | |
| JPS5950730B2 (ja) | オ−ステナイト系ステンレス鋼管などの残留応力の改善方法 | |
| JPH0724577A (ja) | クラッド管の突合せ溶接方法 | |
| JPS6219276B2 (Direct) | ||
| WO2009096004A1 (ja) | 劣化部の再生方法、劣化部の再生装置 | |
| US4772336A (en) | Method of improving residual stress in circumferential weld zone | |
| US4588869A (en) | Method for relieving residual stresses by controlling weld heat input | |
| JP4857375B2 (ja) | 配管の残留応力改善装置 | |
| JPS5952689B2 (ja) | 鋼管内外面の残留応力改善方法 | |
| JPH0734992B2 (ja) | 金属管の溶接方法 | |
| JPS6018293A (ja) | オ−ステナイト系ステンレス鋼の多層盛溶接方法 | |
| JPH0246654B2 (ja) | Chukutainozanryuoryokukaizenhoho | |
| JPH0230716A (ja) | 円周溶接部の残留応力改善方法 | |
| JPS61170516A (ja) | 金属管の残留応力改善方法 | |
| JP2500165B2 (ja) | 燃料被覆管の製造方法 | |
| JPS5852428A (ja) | 軸の応力改善熱処理法 | |
| JPH06182578A (ja) | 配管の溶接方法及び装置 | |
| JPH05169255A (ja) | 管と管の溶接法 | |
| JPH0699755B2 (ja) | 金属管の熱処理方法 | |
| JPS6328825A (ja) | 金属管の残留応力改善方法 | |
| JPH03285021A (ja) | 管溶接継手の応力改善方法 | |
| JPH03146620A (ja) | 金属管の残留応力改善方法 | |
| JPH04127993A (ja) | 容器貫通管取り付け溶接部の応力改善方法 | |
| JPH02137670A (ja) | 配管の補強溶接方法 |