JPS61201743A - 溶融メツキ用高耐食性高加工性Zn合金の製造法 - Google Patents
溶融メツキ用高耐食性高加工性Zn合金の製造法Info
- Publication number
- JPS61201743A JPS61201743A JP4229585A JP4229585A JPS61201743A JP S61201743 A JPS61201743 A JP S61201743A JP 4229585 A JP4229585 A JP 4229585A JP 4229585 A JP4229585 A JP 4229585A JP S61201743 A JPS61201743 A JP S61201743A
- Authority
- JP
- Japan
- Prior art keywords
- alloy
- content
- hot
- corrosion resistance
- plating
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Coating With Molten Metal (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP4229585A JPS61201743A (ja) | 1985-03-04 | 1985-03-04 | 溶融メツキ用高耐食性高加工性Zn合金の製造法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP4229585A JPS61201743A (ja) | 1985-03-04 | 1985-03-04 | 溶融メツキ用高耐食性高加工性Zn合金の製造法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS61201743A true JPS61201743A (ja) | 1986-09-06 |
JPH0135057B2 JPH0135057B2 (zh) | 1989-07-24 |
Family
ID=12632046
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP4229585A Granted JPS61201743A (ja) | 1985-03-04 | 1985-03-04 | 溶融メツキ用高耐食性高加工性Zn合金の製造法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS61201743A (zh) |
Cited By (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
EP0795617A1 (en) * | 1996-03-14 | 1997-09-17 | Matsushita Electric Industrial Co., Ltd. | Method of manufacturing zinctitanium mother alloy and manganese dry battery |
KR100402126B1 (ko) * | 1997-07-21 | 2004-03-20 | 주식회사 포스코 | 착색용융아연도금강판제조용아연-티타늄모합금제조방법 |
CN101934296A (zh) * | 2010-08-30 | 2011-01-05 | 江门市三七电池实业有限公司 | 一种降低锌筒质量的锌筒生产方法 |
CN109536779A (zh) * | 2019-01-28 | 2019-03-29 | 东北大学 | 一种建筑用锌基合金板材及其制备方法 |
CN113528875A (zh) * | 2021-06-29 | 2021-10-22 | 海西华汇化工机械有限公司 | 一种钢铁热镀锌用合金元素添加方法 |
Citations (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5861264A (ja) * | 1981-10-09 | 1983-04-12 | Sumitomo Metal Mining Co Ltd | 硅素含有鋼用溶融亜鉛メツキ浴組成物 |
JPS5891143A (ja) * | 1981-11-24 | 1983-05-31 | Sadaji Nagabori | 溶融メツキ用高耐食性Zn合金 |
JPS5974252A (ja) * | 1982-10-19 | 1984-04-26 | Sadaji Nagabori | 溶融メツキ用高耐食性Zn合金 |
-
1985
- 1985-03-04 JP JP4229585A patent/JPS61201743A/ja active Granted
Patent Citations (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5861264A (ja) * | 1981-10-09 | 1983-04-12 | Sumitomo Metal Mining Co Ltd | 硅素含有鋼用溶融亜鉛メツキ浴組成物 |
JPS5891143A (ja) * | 1981-11-24 | 1983-05-31 | Sadaji Nagabori | 溶融メツキ用高耐食性Zn合金 |
JPS5974252A (ja) * | 1982-10-19 | 1984-04-26 | Sadaji Nagabori | 溶融メツキ用高耐食性Zn合金 |
Cited By (7)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
EP0795617A1 (en) * | 1996-03-14 | 1997-09-17 | Matsushita Electric Industrial Co., Ltd. | Method of manufacturing zinctitanium mother alloy and manganese dry battery |
US5853920A (en) * | 1996-03-14 | 1998-12-29 | Mitsui Mining & Smelting Co., Ltd. | Method of manufacturing zinc-titanium mother alloy and manganese dry battery |
CN1081677C (zh) * | 1996-03-14 | 2002-03-27 | 松下电器产业株式会社 | 制造锌-钛母合金的方法和锰干电池 |
KR100402126B1 (ko) * | 1997-07-21 | 2004-03-20 | 주식회사 포스코 | 착색용융아연도금강판제조용아연-티타늄모합금제조방법 |
CN101934296A (zh) * | 2010-08-30 | 2011-01-05 | 江门市三七电池实业有限公司 | 一种降低锌筒质量的锌筒生产方法 |
CN109536779A (zh) * | 2019-01-28 | 2019-03-29 | 东北大学 | 一种建筑用锌基合金板材及其制备方法 |
CN113528875A (zh) * | 2021-06-29 | 2021-10-22 | 海西华汇化工机械有限公司 | 一种钢铁热镀锌用合金元素添加方法 |
Also Published As
Publication number | Publication date |
---|---|
JPH0135057B2 (zh) | 1989-07-24 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JP4584179B2 (ja) | 耐食性および加工性に優れた溶融Zn−Al合金めっき鋼板の製造方法 | |
JP4542434B2 (ja) | 表面外観に優れた溶融Zn−Al−Mg−Siめっき鋼板及びその製造方法。 | |
TW201837207A (zh) | 鍍敷鋼板 | |
JP3715220B2 (ja) | 耐食性に優れたZn−Al−Mg系溶融めっき鋼材 | |
JP3566262B2 (ja) | 加工性に優れた溶融Al−Zn合金めっき鋼板及びその製造方法 | |
JPH09256132A (ja) | 溶融Al−Zn合金めっき鋼板およびその製造方法 | |
JP2825671B2 (ja) | 溶融Zn−Mg−Al−Snめっき鋼板 | |
CN105648273A (zh) | 一种添加稀土的锌铝镁镀层钢板 | |
KR101568508B1 (ko) | 산화칼슘 함유 용융 아연합금 도금 조성물, 용융 아연합금 도금강판 및 그 제조방법 | |
JPS61201743A (ja) | 溶融メツキ用高耐食性高加工性Zn合金の製造法 | |
CN114182188B (zh) | 一种热浸镀锌铝镁镀层钢板及其制备方法 | |
JPS6311420B2 (zh) | ||
JP2004131818A (ja) | 加工性と耐食性に優れた溶融Sn−Zn系めっき鋼板 | |
JP2002317233A (ja) | 溶融Sn−Zn系めっき鋼板 | |
JP3563063B2 (ja) | 加工性及び耐食性に優れた潤滑被覆溶融Al−Zn合金めっき鋼板およびその製造方法 | |
JP2006097129A (ja) | 耐溶融金属脆化割れ性に優れたZn−Al−Mg合金めっき鋼板 | |
JP3009262B2 (ja) | 疲労特性に優れた溶融亜鉛アルミニウム合金めっき被覆物 | |
JPH11193452A (ja) | 溶融Zn−Mg−Alめっき鋼板の製造方法、溶融めっき浴、および溶融Zn−Mg−Alめっき鋼板 | |
JPS648703B2 (zh) | ||
JPH0414174B2 (zh) | ||
KR101629260B1 (ko) | 용융도금욕 조성물 | |
KR102453011B1 (ko) | 실러 접착성이 우수한 도금 강판 및 이의 제조방법 | |
JPS6310218B2 (zh) | ||
JP2006089787A (ja) | 耐溶融金属脆化割れ性に優れたZn−Al−Mg合金めっき鋼板の製造方法 | |
JP2964678B2 (ja) | Zn−Al合金めっき方法 |