JPS61170577A - Al合金鋳物表面合金化層の形成方法 - Google Patents
Al合金鋳物表面合金化層の形成方法Info
- Publication number
- JPS61170577A JPS61170577A JP60010353A JP1035385A JPS61170577A JP S61170577 A JPS61170577 A JP S61170577A JP 60010353 A JP60010353 A JP 60010353A JP 1035385 A JP1035385 A JP 1035385A JP S61170577 A JPS61170577 A JP S61170577A
- Authority
- JP
- Japan
- Prior art keywords
- alloy
- alloy casting
- layer
- alloyed layer
- remelted
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Laser Beam Processing (AREA)
- Other Surface Treatments For Metallic Materials (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP60010353A JPS61170577A (ja) | 1985-01-22 | 1985-01-22 | Al合金鋳物表面合金化層の形成方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP60010353A JPS61170577A (ja) | 1985-01-22 | 1985-01-22 | Al合金鋳物表面合金化層の形成方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS61170577A true JPS61170577A (ja) | 1986-08-01 |
| JPH0480986B2 JPH0480986B2 (enExample) | 1992-12-21 |
Family
ID=11747817
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP60010353A Granted JPS61170577A (ja) | 1985-01-22 | 1985-01-22 | Al合金鋳物表面合金化層の形成方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS61170577A (enExample) |
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2005152925A (ja) * | 2003-11-25 | 2005-06-16 | Nissan Motor Co Ltd | レーザ肉盛り加工方法 |
| JP2009047026A (ja) * | 2007-08-16 | 2009-03-05 | Nissan Motor Co Ltd | バルブシート形成方法及びシリンダーヘッド |
| CN109454349A (zh) * | 2018-11-23 | 2019-03-12 | 安徽应流集团霍山铸造有限公司 | 一种降低铸钢件加工面焊缝硬度的热处理方法 |
| CN110756990A (zh) * | 2018-07-25 | 2020-02-07 | 株式会社东芝 | 焊接方法、焊接物的制造方法、以及焊接物 |
-
1985
- 1985-01-22 JP JP60010353A patent/JPS61170577A/ja active Granted
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2005152925A (ja) * | 2003-11-25 | 2005-06-16 | Nissan Motor Co Ltd | レーザ肉盛り加工方法 |
| JP2009047026A (ja) * | 2007-08-16 | 2009-03-05 | Nissan Motor Co Ltd | バルブシート形成方法及びシリンダーヘッド |
| CN110756990A (zh) * | 2018-07-25 | 2020-02-07 | 株式会社东芝 | 焊接方法、焊接物的制造方法、以及焊接物 |
| CN109454349A (zh) * | 2018-11-23 | 2019-03-12 | 安徽应流集团霍山铸造有限公司 | 一种降低铸钢件加工面焊缝硬度的热处理方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0480986B2 (enExample) | 1992-12-21 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP3049605B2 (ja) | 耐摩耗性アルミニウム−珪素合金被覆及びその製造方法 | |
| US4401726A (en) | Metal surface modification | |
| JPS56158871A (en) | Method for forming corrosion-resistant coating on metallic substrate | |
| JP2678804B2 (ja) | 鉄合金基材上に純Cu肉盛層を形成する方法 | |
| JPH1096037A (ja) | 耐摩耗性に優れた銅合金 | |
| JP2004263280A (ja) | 防蝕マグネシウム合金部材、マグネシウム合金部材の防蝕処理方法およびマグネシウム合金部材の防蝕方法 | |
| US4483286A (en) | Piston | |
| JPS6267182A (ja) | 金属表面再溶融合金化法 | |
| JPS62101392A (ja) | 高密度エネルギ源を利用した鋳鉄材料に対する盛金法 | |
| JPH0647187B2 (ja) | 肉盛用分散強化銅基合金 | |
| JPH0480986B2 (enExample) | ||
| JPH055585B2 (enExample) | ||
| US2911708A (en) | Babbitt-bronze-aluminum bonding process | |
| JPS6349744B2 (enExample) | ||
| JPH02205664A (ja) | レーザクラッディング法 | |
| JP3629578B2 (ja) | Ti系材料とCu系の接合方法 | |
| JPS6179783A (ja) | 部材表面への黒鉛化層の形成方法 | |
| JP3597709B2 (ja) | 耐高温溶射被覆部材 | |
| JP2000256822A (ja) | 表面改質アルミニウム合金及びその表面改質方法 | |
| JPS61170579A (ja) | 鋳鉄基材に対する表面合金化層の形成方法 | |
| JP2623605B2 (ja) | アルミニウム合金鋳物の表面メッキ層形成方法 | |
| JPH01205043A (ja) | 潤滑性に優れたCu基耐摩耗合金 | |
| JPH0387322A (ja) | アルミ部材の合金化方法 | |
| JPS6411073A (ja) | アルミニウム合金の耐摩耗処理方法 | |
| JPH04120280A (ja) | 表面硬化アルミニウム材の製造方法 |