JPS60128290A - 高耐食性亜鉛−アルミナ系複合電気めつき鋼板の製造方法 - Google Patents
高耐食性亜鉛−アルミナ系複合電気めつき鋼板の製造方法Info
- Publication number
- JPS60128290A JPS60128290A JP23677583A JP23677583A JPS60128290A JP S60128290 A JPS60128290 A JP S60128290A JP 23677583 A JP23677583 A JP 23677583A JP 23677583 A JP23677583 A JP 23677583A JP S60128290 A JPS60128290 A JP S60128290A
- Authority
- JP
- Japan
- Prior art keywords
- alumina
- zinc
- steel sheet
- cobalt
- corrosion resistance
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Electroplating And Plating Baths Therefor (AREA)
- Electroplating Methods And Accessories (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP23677583A JPS60128290A (ja) | 1983-12-15 | 1983-12-15 | 高耐食性亜鉛−アルミナ系複合電気めつき鋼板の製造方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP23677583A JPS60128290A (ja) | 1983-12-15 | 1983-12-15 | 高耐食性亜鉛−アルミナ系複合電気めつき鋼板の製造方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS60128290A true JPS60128290A (ja) | 1985-07-09 |
JPS6147919B2 JPS6147919B2 (de) | 1986-10-21 |
Family
ID=17005605
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP23677583A Granted JPS60128290A (ja) | 1983-12-15 | 1983-12-15 | 高耐食性亜鉛−アルミナ系複合電気めつき鋼板の製造方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS60128290A (de) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS63157900A (ja) * | 1986-12-19 | 1988-06-30 | Kawasaki Steel Corp | 亜鉛−クロム複合めつき鋼板の製造方法 |
-
1983
- 1983-12-15 JP JP23677583A patent/JPS60128290A/ja active Granted
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS63157900A (ja) * | 1986-12-19 | 1988-06-30 | Kawasaki Steel Corp | 亜鉛−クロム複合めつき鋼板の製造方法 |
Also Published As
Publication number | Publication date |
---|---|
JPS6147919B2 (de) | 1986-10-21 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
EP0277640B1 (de) | Mit einem Verbundwerkstoff auf der Grundlage von Zn beschichtetes metallisches Material und Verfahren zum Beschichten | |
US20010054557A1 (en) | Electroplating of metals using pulsed reverse current for control of hydrogen evolution | |
JPH01298A (ja) | 亜鉛系複合めっき金属材料およびめっき方法 | |
KR0175967B1 (ko) | 전기아연도금 강판과 그 방법 | |
JPS60125395A (ja) | 高耐食性Ζn−アルミナ系複合電気めっき鋼板 | |
JPH03138389A (ja) | めっき密着性および耐食性に優れたZn―Mg合金めっき鋼板およびその製造方法 | |
JPS60128290A (ja) | 高耐食性亜鉛−アルミナ系複合電気めつき鋼板の製造方法 | |
JP7400766B2 (ja) | 亜鉛系電気めっき鋼板およびその製造方法 | |
JP3499543B2 (ja) | 耐白錆性に優れる電気Znめっき鋼板およびその製造方法 | |
JPS60106996A (ja) | 耐食性Ζn−アルミナ複合めっき鋼板の製造方法 | |
JPH0447037B2 (de) | ||
JPS5928598A (ja) | 電気メツキ用Pb合金製不溶性陽極 | |
JPH025839B2 (de) | ||
US3898139A (en) | Process for surface treatment of zinc-plated steel plates | |
JPH04333593A (ja) | Al−Mn合金めっき鋼板の製造方法 | |
JPH09209108A (ja) | 鋼材加工品の浸漬めっき方法 | |
JP2584735B2 (ja) | A▲l▼合金めっき金属材とその製造法 | |
JPS6043498A (ja) | 高耐食性亜鉛系合金めっき鋼板およびその製造方法 | |
JPH0995795A (ja) | めっき密着性および化成処理性に優れたZn−Ni系合金電気めっき鋼板 | |
JPS61119694A (ja) | 電気メツキ鋼板の製造方法 | |
JPH0438837B2 (de) | ||
JPH052745B2 (de) | ||
JPH0633295A (ja) | 表面にMgO層を有するZn−Fe合金被覆鋼板の製造方法 | |
JPH06280083A (ja) | アルミニウム合金板への亜鉛系電気めっき方法 | |
JPH0772358B2 (ja) | 片面電気めっき鋼板の製造方法 |