JPS594402A - 複合親水性膜 - Google Patents
複合親水性膜Info
- Publication number
- JPS594402A JPS594402A JP11147782A JP11147782A JPS594402A JP S594402 A JPS594402 A JP S594402A JP 11147782 A JP11147782 A JP 11147782A JP 11147782 A JP11147782 A JP 11147782A JP S594402 A JPS594402 A JP S594402A
- Authority
- JP
- Japan
- Prior art keywords
- membrane
- hydrophilic membrane
- ethylene
- composite
- film
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B01—PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL
- B01D—SEPARATION
- B01D67/00—Processes specially adapted for manufacturing semi-permeable membranes for separation processes or apparatus
- B01D67/0081—After-treatment of organic or inorganic membranes
Landscapes
- Chemical & Material Sciences (AREA)
- Inorganic Chemistry (AREA)
- Engineering & Computer Science (AREA)
- Manufacturing & Machinery (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Separation Using Semi-Permeable Membranes (AREA)
- Manufacture Of Macromolecular Shaped Articles (AREA)
- Treatments Of Macromolecular Shaped Articles (AREA)
- Laminated Bodies (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP11147782A JPS594402A (ja) | 1982-06-30 | 1982-06-30 | 複合親水性膜 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP11147782A JPS594402A (ja) | 1982-06-30 | 1982-06-30 | 複合親水性膜 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS594402A true JPS594402A (ja) | 1984-01-11 |
| JPH0347126B2 JPH0347126B2 (enExample) | 1991-07-18 |
Family
ID=14562243
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP11147782A Granted JPS594402A (ja) | 1982-06-30 | 1982-06-30 | 複合親水性膜 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS594402A (enExample) |
Cited By (9)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6171064A (ja) * | 1984-09-13 | 1986-04-11 | 日本赤十字社 | 血液成分の分離用器具 |
| US5204197A (en) * | 1990-03-26 | 1993-04-20 | Daiwabo Create Co., Ltd. | Separator material for storage batteries and method for making the same |
| US5215667A (en) * | 1991-08-20 | 1993-06-01 | Exxon Chemical Patents Inc. | Method for separating water soluble noble metal catalyst from a noble metal catalyzed hydroformylation reaction |
| US5288818A (en) * | 1991-08-20 | 1994-02-22 | Exxon Chemical Patents Inc. | Method for separating a water soluble noble metal catalyst from a noble metal catalyzed hydroformylation reaction |
| EP0842758A3 (en) * | 1996-11-19 | 1998-08-19 | Mitsui Chemicals, Inc. | Porous film of high molecular weight polyolefin and process for producing same |
| US6688477B2 (en) | 2001-05-03 | 2004-02-10 | Air Products And Chemicals, Inc. | Composite membranes |
| US6798316B2 (en) | 2001-09-06 | 2004-09-28 | Ngk Spark Plug.Co., Ltd. | Dielectric duplexer |
| CN104369509A (zh) * | 2014-12-11 | 2015-02-25 | 昆山加浦包装材料有限公司 | 可降解发泡共挤出pa阻隔薄膜 |
| CN108479403A (zh) * | 2018-04-13 | 2018-09-04 | 苏州凯虹高分子科技有限公司 | 一种超超亲水管式微滤膜及其制作方法 |
-
1982
- 1982-06-30 JP JP11147782A patent/JPS594402A/ja active Granted
Cited By (10)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6171064A (ja) * | 1984-09-13 | 1986-04-11 | 日本赤十字社 | 血液成分の分離用器具 |
| US5204197A (en) * | 1990-03-26 | 1993-04-20 | Daiwabo Create Co., Ltd. | Separator material for storage batteries and method for making the same |
| US5215667A (en) * | 1991-08-20 | 1993-06-01 | Exxon Chemical Patents Inc. | Method for separating water soluble noble metal catalyst from a noble metal catalyzed hydroformylation reaction |
| US5288818A (en) * | 1991-08-20 | 1994-02-22 | Exxon Chemical Patents Inc. | Method for separating a water soluble noble metal catalyst from a noble metal catalyzed hydroformylation reaction |
| EP0842758A3 (en) * | 1996-11-19 | 1998-08-19 | Mitsui Chemicals, Inc. | Porous film of high molecular weight polyolefin and process for producing same |
| US6688477B2 (en) | 2001-05-03 | 2004-02-10 | Air Products And Chemicals, Inc. | Composite membranes |
| US6798316B2 (en) | 2001-09-06 | 2004-09-28 | Ngk Spark Plug.Co., Ltd. | Dielectric duplexer |
| CN104369509A (zh) * | 2014-12-11 | 2015-02-25 | 昆山加浦包装材料有限公司 | 可降解发泡共挤出pa阻隔薄膜 |
| CN104369509B (zh) * | 2014-12-11 | 2016-09-21 | 昆山加浦包装材料有限公司 | 可降解发泡共挤出pa阻隔薄膜 |
| CN108479403A (zh) * | 2018-04-13 | 2018-09-04 | 苏州凯虹高分子科技有限公司 | 一种超超亲水管式微滤膜及其制作方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0347126B2 (enExample) | 1991-07-18 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US4670146A (en) | Composite hydrophilic membrane and method for manufacture thereof | |
| JP4824561B2 (ja) | 微孔性pvdfフィルムおよび製造方法 | |
| US7300984B2 (en) | Process for preparing graft copolymers and membranes formed therefrom | |
| US6130175A (en) | Integral multi-layered ion-exchange composite membranes | |
| CN103068473B (zh) | 离子交换膜及其制造方法 | |
| JP5057419B2 (ja) | 複合微多孔膜及びその製造方法並びに用途 | |
| JP2604734B2 (ja) | イオン透過性隔膜及びその製造方法 | |
| JP4857560B2 (ja) | 固体高分子型燃料電池用電解質膜の製造方法 | |
| EP0900249A1 (en) | Integral multi-layered ion-exchange composite membranes | |
| JP2005342718A (ja) | 部分要素からなる複合膜 | |
| WO2017098732A1 (ja) | 電解質膜及びその製造方法、並びに電解質膜を備えた燃料電池用の膜-電極接合体 | |
| JPS594402A (ja) | 複合親水性膜 | |
| EP4260390A1 (en) | Free-standing, ion-selective composite membranes | |
| JPS6069140A (ja) | イオン導電性の複合親水性膜 | |
| JPS59102404A (ja) | 複合親水性膜 | |
| JPS59203602A (ja) | 複合膜 | |
| JPS5984924A (ja) | 複合イオン交換膜 | |
| JPS59203607A (ja) | 異方性親水性膜及びその製造方法 | |
| JPS59203610A (ja) | 親水性樹脂複合膜の製造方法 | |
| JP2016015286A (ja) | 液体燃料電池用隔膜及びそれを備えた膜−電極接合体 | |
| WO2016002227A1 (ja) | 液体燃料電池用隔膜及びそれを備えた膜-電極接合体 | |
| JPS59219334A (ja) | 陰イオン交換膜 | |
| JPH10277373A (ja) | イオン交換性中空濾過膜およびその製法 | |
| JP2016015285A (ja) | アルカリ形液体燃料電池用隔膜及びそれを備えた膜−電極接合体 | |
| JPS6044334B2 (ja) | 親水性膜の製造方法 |