JPH07172824A5 - - Google Patents
Info
- Publication number
- JPH07172824A5 JPH07172824A5 JP5-314791A JP31479193A JPH07172824A5 JP H07172824 A5 JPH07172824 A5 JP H07172824A5 JP 31479193 A JP31479193 A JP 31479193A JP H07172824 A5 JPH07172824 A5 JP H07172824A5
- Authority
- JP
- Japan
- Prior art keywords
- alumina gel
- aluminum chloride
- basic aluminum
- sulfate
- equipment
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP31479193A JP3194176B2 (ja) | 1993-12-15 | 1993-12-15 | 硫酸根含有高塩基性塩化アルミニウム溶液の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP31479193A JP3194176B2 (ja) | 1993-12-15 | 1993-12-15 | 硫酸根含有高塩基性塩化アルミニウム溶液の製造方法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH07172824A JPH07172824A (ja) | 1995-07-11 |
| JPH07172824A5 true JPH07172824A5 (enExample) | 1999-08-03 |
| JP3194176B2 JP3194176B2 (ja) | 2001-07-30 |
Family
ID=18057642
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP31479193A Expired - Lifetime JP3194176B2 (ja) | 1993-12-15 | 1993-12-15 | 硫酸根含有高塩基性塩化アルミニウム溶液の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP3194176B2 (enExample) |
Families Citing this family (10)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CA2229266C (en) * | 1995-09-18 | 2001-10-16 | Delta Chemical Corporation | Polyaluminum chlorides and polyaluminum chlorosulfates methods and compositions |
| JP2000264627A (ja) * | 1999-03-12 | 2000-09-26 | Kanto Denka Kogyo Co Ltd | 塩基性塩化アルミニウムの塩基度向上方法 |
| KR100402904B1 (ko) * | 2000-05-23 | 2003-10-30 | 동명화학공업 주식회사 | 폴리염화알루미늄의 불용성 침전물을 폴리염화알루미늄의제조에 이용하는 방법 |
| JP4953458B2 (ja) * | 2008-02-28 | 2012-06-13 | 多木化学株式会社 | 新規な塩基性塩化アルミニウム及びその製造方法並びにその用途 |
| JP5986448B2 (ja) * | 2012-07-25 | 2016-09-06 | 多木化学株式会社 | 硫酸根含有ポリ塩化アルミニウムの製造方法 |
| WO2015192044A1 (en) | 2014-06-13 | 2015-12-17 | Geo Specialty Chemicals, Inc. | Method for making sulfated polyaluminum chloride (pacs) or polyaluminum chloride (pac) and pacs of pac made by same |
| JP6277074B2 (ja) * | 2014-07-08 | 2018-02-07 | 水澤化学工業株式会社 | 硫酸根変性塩基性塩化アルミニウム水溶液及びその製造方法 |
| KR102175414B1 (ko) | 2016-03-31 | 2020-11-06 | 아사히 가가쿠 고교 가부시키가이샤 | 고 염기성 염화알루미늄 및 그 제조방법 |
| JP6814462B2 (ja) * | 2016-11-09 | 2021-01-20 | 大明化学工業株式会社 | 硫酸根含有塩基性塩化アルミニウム溶液の製造方法 |
| CN109734113B (zh) * | 2019-03-20 | 2021-08-31 | 湖南玖恪环境工程有限公司 | 高絮凝效果聚氯化铝的生产方法 |
-
1993
- 1993-12-15 JP JP31479193A patent/JP3194176B2/ja not_active Expired - Lifetime
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| AU710119B2 (en) | Process for purifying water | |
| JPS59116125A (ja) | 塩基性アルミニウムクロロサルフエ−トの製造方法 | |
| CA2001063C (en) | Method for producing aqueous solutions of basic poly aluminum sulphate | |
| JP3194176B2 (ja) | 硫酸根含有高塩基性塩化アルミニウム溶液の製造方法 | |
| JPH0692632A5 (enExample) | ||
| HU188227B (en) | Process for the production of cupric /ii/-hydroxide | |
| JP2000264627A (ja) | 塩基性塩化アルミニウムの塩基度向上方法 | |
| WO1996035647A1 (en) | A method of slowing the setting rate of magnesium phosphate cements | |
| JPH1053412A (ja) | 球状炭酸カルシウムの製造方法 | |
| JP2741137B2 (ja) | 鉄系凝集剤の製造方法 | |
| JP2991987B2 (ja) | 塩基性塩化アルミニウム及びその製造方法 | |
| KR900016048A (ko) | 마그네사이트의 제조방법, 그의 마그네슘 플루오라이드 제조에의 응용 및 이러한 방법으로 수득한 마그네슘 플루오라이드 | |
| US2783128A (en) | Process of producing cryolite from washing and waste liquors containing sodium fluoride | |
| KR920008517B1 (ko) | 수용성 스트론튬염으로부터 바륨의 분리방법 | |
| JPH05170772A5 (enExample) | ||
| JP2514389B2 (ja) | 変性セルロ―スエ―テルの製造方法 | |
| JPS61200103A (ja) | ホフマン分解されたアクリルアミド系ポリマ−の製法 | |
| JPS6111113A (ja) | 凝集剤の製造方法 | |
| JPH0681762B2 (ja) | 酸型カルボキシメチルセルロースの製造方法 | |
| JPH054342B2 (enExample) | ||
| JPS61205617A (ja) | 金属銅回収及びアルミニウム塩製造法 | |
| JP4209149B2 (ja) | 白色水酸化アルミニウムの製造方法 | |
| KR890003194B1 (ko) | 알루미늄 하이드록시 클로라이드의 제조방법 | |
| JP2000226213A (ja) | ポリ硫酸アルミニウムの製造方法 | |
| JPH10230102A (ja) | 鉄含有ポリ塩化アルミニウム水溶液の製造方法 |