JPH0582724B2 - - Google Patents
Info
- Publication number
- JPH0582724B2 JPH0582724B2 JP59212234A JP21223484A JPH0582724B2 JP H0582724 B2 JPH0582724 B2 JP H0582724B2 JP 59212234 A JP59212234 A JP 59212234A JP 21223484 A JP21223484 A JP 21223484A JP H0582724 B2 JPH0582724 B2 JP H0582724B2
- Authority
- JP
- Japan
- Prior art keywords
- cobalt
- chromium
- film
- magnetic
- oxidized
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Physical Vapour Deposition (AREA)
- Magnetic Record Carriers (AREA)
- Manufacturing Of Magnetic Record Carriers (AREA)
- Thin Magnetic Films (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP21223484A JPS6190405A (ja) | 1984-10-09 | 1984-10-09 | 垂直磁化膜の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP21223484A JPS6190405A (ja) | 1984-10-09 | 1984-10-09 | 垂直磁化膜の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6190405A JPS6190405A (ja) | 1986-05-08 |
| JPH0582724B2 true JPH0582724B2 (enExample) | 1993-11-22 |
Family
ID=16619178
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP21223484A Granted JPS6190405A (ja) | 1984-10-09 | 1984-10-09 | 垂直磁化膜の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6190405A (enExample) |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US20050244680A1 (en) * | 2004-05-03 | 2005-11-03 | Imation Corp. | Environmentally stable metal-evaporated recording media |
Family Cites Families (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS57197813A (en) * | 1981-05-29 | 1982-12-04 | Nippon Gakki Seizo Kk | Magnetic recording tape |
| JPS5917216A (ja) * | 1982-07-20 | 1984-01-28 | Ulvac Corp | 磁気記録体並にその製造法 |
| JPS59140629A (ja) * | 1983-01-31 | 1984-08-13 | Hitachi Ltd | 垂直磁気記録媒体の製造方法 |
-
1984
- 1984-10-09 JP JP21223484A patent/JPS6190405A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS6190405A (ja) | 1986-05-08 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CA1135411A (en) | Thin film head having negative magnetostriction | |
| JPH0773441A (ja) | 金属薄膜型磁気記録媒体とその製造方法 | |
| JPH0666087B2 (ja) | 磁気記録媒体 | |
| JPS6249722B2 (enExample) | ||
| CA1315612C (en) | Perpendicular magnetic storage medium | |
| US4587178A (en) | Magnetic recording medium | |
| US7105240B2 (en) | Perpendicular media with improved corrosion performance | |
| US4325733A (en) | Amorphous Co-Ti alloys | |
| US5316631A (en) | Method for fabricating a magnetic recording medium | |
| US5576099A (en) | Inductive head lamination with layer of magnetic quenching material | |
| Inagaki et al. | Ferrite thin films for high recording density | |
| JPH0582724B2 (enExample) | ||
| JPH056738B2 (enExample) | ||
| JPH01124108A (ja) | 薄膜磁気ヘツド | |
| JPS59178617A (ja) | 磁気記録媒体の製造方法 | |
| JPH0689422A (ja) | コバルト−鉄−ニッケル磁性膜の製造方法 | |
| JPH0323972B2 (enExample) | ||
| US20050057855A1 (en) | Magnetic recording medium and substrate for magnetic recording medium | |
| JP2005108407A (ja) | 磁気記録媒体及び磁気記録媒体用基板 | |
| Katori et al. | Wear and corrosion resistance of Fe-N based micrograin soft magnetic thin films | |
| JPS63124213A (ja) | 垂直磁気記録媒体 | |
| US20080085427A1 (en) | Amorphous soft magnetic layers for perpendicular magnetic recording media | |
| Shiomi et al. | Perpendicular anisotropy in electrodeposited Co-Pd alloy films | |
| JP2773477B2 (ja) | 磁気記録体の製造方法 | |
| JPS635505A (ja) | 垂直磁化膜およびその製法 |