JPH0565600B2 - - Google Patents
Info
- Publication number
- JPH0565600B2 JPH0565600B2 JP59247541A JP24754184A JPH0565600B2 JP H0565600 B2 JPH0565600 B2 JP H0565600B2 JP 59247541 A JP59247541 A JP 59247541A JP 24754184 A JP24754184 A JP 24754184A JP H0565600 B2 JPH0565600 B2 JP H0565600B2
- Authority
- JP
- Japan
- Prior art keywords
- colloid
- alumina
- plating
- silica
- sio
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Electroplating And Plating Baths Therefor (AREA)
- Electroplating Methods And Accessories (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP24754184A JPS61127900A (ja) | 1984-11-22 | 1984-11-22 | 複合めつき方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP24754184A JPS61127900A (ja) | 1984-11-22 | 1984-11-22 | 複合めつき方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS61127900A JPS61127900A (ja) | 1986-06-16 |
| JPH0565600B2 true JPH0565600B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | 1993-09-20 |
Family
ID=17165028
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP24754184A Granted JPS61127900A (ja) | 1984-11-22 | 1984-11-22 | 複合めつき方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS61127900A (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) |
Families Citing this family (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS63157900A (ja) * | 1986-12-19 | 1988-06-30 | Kawasaki Steel Corp | 亜鉛−クロム複合めつき鋼板の製造方法 |
| JPH01176095A (ja) * | 1987-12-29 | 1989-07-12 | Nippon Steel Corp | 高耐食性電気複合めっき鋼板 |
| JPH01176096A (ja) * | 1987-12-29 | 1989-07-12 | Nippon Steel Corp | 高耐食性電気複合めっき鋼板 |
| JPH01176099A (ja) * | 1987-12-29 | 1989-07-12 | Nippon Steel Corp | 高耐食性電気複合めっき鋼板 |
| JPH01176098A (ja) * | 1987-12-29 | 1989-07-12 | Nippon Steel Corp | 高耐食性電気複合めっき鋼板 |
| CN114867891A (zh) * | 2019-12-23 | 2022-08-05 | 迪普索股份公司 | 锌-镍-二氧化硅复合镀浴和使用该浴的镀覆方法 |
Family Cites Families (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6038480B2 (ja) * | 1978-06-08 | 1985-08-31 | 新日本製鐵株式会社 | 耐食性電気亜鉛複合めつき鋼材の製造方法 |
-
1984
- 1984-11-22 JP JP24754184A patent/JPS61127900A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS61127900A (ja) | 1986-06-16 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| KR20040030925A (ko) | 금속 표면 처리용 무전해 방법 및 이로부터 형성된 물품 | |
| CA1063966A (en) | Electroplating method | |
| DE3851425T2 (de) | Mit korrosionsbeständigem Verbundmaterial plattiertes Stahlblech und Verfahren zu seiner Herstellung. | |
| EP0277640B1 (en) | Zn-based composite-plated metallic material and plating method | |
| JPH0231519B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | ||
| US7030183B2 (en) | Surface treating method and surface treating agent | |
| JPS626760B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | ||
| US4086153A (en) | Method of producing a composite coated steel sheet | |
| JP5671210B2 (ja) | 金属表面処理方法 | |
| JPH01298A (ja) | 亜鉛系複合めっき金属材料およびめっき方法 | |
| JPH0565600B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | ||
| US6866896B2 (en) | Method for treating metallic surfaces and products formed thereby | |
| JP3573574B2 (ja) | 酸化チタン被覆金属材料の製造方法 | |
| US3227636A (en) | Method of bonding coatings | |
| US20040222105A1 (en) | Method for preparing and using silicate systems to treat electrically conductive surfaces and products obtained therefrom | |
| CN105039943A (zh) | 一种化学镀Ni-W-Zn-P合金镀层的镀液及其镀层工艺 | |
| JPH01246398A (ja) | 複合分散粒子の製造方法及び複合めっき方法 | |
| JPH0756080B2 (ja) | 塗料密着性に優れた有機高分子複合メツキ金属材の製造方法 | |
| CN100590225C (zh) | 制备和使用硅酸盐体系处理导电表面的方法和由此得到的产品 | |
| CN101831641B (zh) | 镁锂合金酸性浸锌溶液及浸锌方法 | |
| JP2015052168A (ja) | 表面処理金属材料 | |
| JPS59123796A (ja) | 高耐食性電気亜鉛めつき鋼板の製造方法 | |
| US20040188262A1 (en) | Method for treating metallic surfaces and products formed thereby | |
| JPH025839B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | ||
| JPS6154880B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) |