JPH0563546B2 - - Google Patents
Info
- Publication number
- JPH0563546B2 JPH0563546B2 JP2212889A JP2212889A JPH0563546B2 JP H0563546 B2 JPH0563546 B2 JP H0563546B2 JP 2212889 A JP2212889 A JP 2212889A JP 2212889 A JP2212889 A JP 2212889A JP H0563546 B2 JPH0563546 B2 JP H0563546B2
- Authority
- JP
- Japan
- Prior art keywords
- roll
- width
- snack
- steel strip
- snout
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
Landscapes
- Coating With Molten Metal (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP2212889A JPH02200759A (ja) | 1989-01-30 | 1989-01-30 | 溶融メッキ装置 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP2212889A JPH02200759A (ja) | 1989-01-30 | 1989-01-30 | 溶融メッキ装置 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPH02200759A JPH02200759A (ja) | 1990-08-09 |
JPH0563546B2 true JPH0563546B2 (enrdf_load_stackoverflow) | 1993-09-10 |
Family
ID=12074250
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP2212889A Granted JPH02200759A (ja) | 1989-01-30 | 1989-01-30 | 溶融メッキ装置 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPH02200759A (enrdf_load_stackoverflow) |
Families Citing this family (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2601040B2 (ja) * | 1991-02-13 | 1997-04-16 | 住友金属工業株式会社 | 合金化溶融亜鉛めっき鋼板の製造方法および装置 |
JPH04263056A (ja) * | 1991-02-18 | 1992-09-18 | Nippon Steel Corp | 溶融金属めっき鋼帯のめっき付着量制御方法 |
-
1989
- 1989-01-30 JP JP2212889A patent/JPH02200759A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPH02200759A (ja) | 1990-08-09 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
KR100502816B1 (ko) | 용융도금 금속스트립의 제조방법 및 그 장치 | |
KR100758240B1 (ko) | 용융금속 도금강판의 제조방법 | |
JP2848208B2 (ja) | 溶融金属めっき装置 | |
KR20180110043A (ko) | 연속 용융 금속 도금 장치 및 연속 용융 금속 도금 방법 | |
KR102405526B1 (ko) | 용융 금속 도금 강대의 제조 방법 및 연속 용융 금속 도금 설비 | |
KR102584645B1 (ko) | 용융 도금 장치 및 방법 | |
JPH0563546B2 (enrdf_load_stackoverflow) | ||
JP2017222923A (ja) | 溶融金属めっき鋼帯の製造方法及び連続溶融金属めっき設備 | |
US4958589A (en) | Continuous melt-plating apparatus | |
EP4176104B1 (en) | Correction apparatus for correcting the planarity of a metal strip and related correction method | |
JPH0263651A (ja) | 薄い金属製品の連続鋳造方法と装置 | |
JP3096166B2 (ja) | 連続溶融金属めっきラインのめっき装置 | |
JP5169089B2 (ja) | 連続溶融金属めっき方法 | |
JP2560662B2 (ja) | 表面欠陥の少ない溶融亜鉛めっき鋼板の製造装置 | |
JPH051357A (ja) | 溶融金属めつき方法 | |
JP2888318B2 (ja) | 金属帯の溶融めっき設備におけるボトムドロスの巻き上げ抑制装置 | |
JP2000273610A (ja) | 連続溶融めっき時の鋼帯幅反り制御方法及び装置 | |
JP4696428B2 (ja) | ストリップの連続溶融金属めっき設備 | |
JPH0941107A (ja) | 連続溶融金属めっき装置 | |
JP2560663B2 (ja) | 表面欠陥の少ない溶融亜鉛めっき鋼板の製造方法と装置 | |
JP2003073791A (ja) | 連続溶融金属めっき装置 | |
WO2025132891A1 (en) | A hot dip coating device and a method of coating a metal strip in a hot dip coating device | |
US2952568A (en) | Continuous hot dip galvanizing of metal strip | |
JP2732464B2 (ja) | 連続式溶融金属めっき鋼帯の製造方法 | |
JPH0120226B2 (enrdf_load_stackoverflow) |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
LAPS | Cancellation because of no payment of annual fees |