JPH0519261B2 - - Google Patents
Info
- Publication number
- JPH0519261B2 JPH0519261B2 JP61124514A JP12451486A JPH0519261B2 JP H0519261 B2 JPH0519261 B2 JP H0519261B2 JP 61124514 A JP61124514 A JP 61124514A JP 12451486 A JP12451486 A JP 12451486A JP H0519261 B2 JPH0519261 B2 JP H0519261B2
- Authority
- JP
- Japan
- Prior art keywords
- polyvinyl alcohol
- cadmium
- slurry
- kneading
- aqueous solution
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/62—Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M4/621—Binders
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/24—Electrodes for alkaline accumulators
- H01M4/26—Processes of manufacture
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- General Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Manufacturing & Machinery (AREA)
- Battery Electrode And Active Subsutance (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP61124514A JPS62281267A (ja) | 1986-05-29 | 1986-05-29 | ニツケル・カドミウムアルカリ蓄電池用陰極活物質の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP61124514A JPS62281267A (ja) | 1986-05-29 | 1986-05-29 | ニツケル・カドミウムアルカリ蓄電池用陰極活物質の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS62281267A JPS62281267A (ja) | 1987-12-07 |
| JPH0519261B2 true JPH0519261B2 (cs) | 1993-03-16 |
Family
ID=14887369
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP61124514A Granted JPS62281267A (ja) | 1986-05-29 | 1986-05-29 | ニツケル・カドミウムアルカリ蓄電池用陰極活物質の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS62281267A (cs) |
Families Citing this family (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US5281495A (en) * | 1992-02-28 | 1994-01-25 | Sanyo Electric Co., Ltd. | Alkaline storage cell having a negative electrode comprising a cadmium active material |
| KR100590109B1 (ko) | 2004-12-03 | 2006-06-14 | 삼성에스디아이 주식회사 | 고출력 리튬 이차 전지 및 이의 제조방법 |
-
1986
- 1986-05-29 JP JP61124514A patent/JPS62281267A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS62281267A (ja) | 1987-12-07 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US4177157A (en) | Precoagulated PTFE-bound electrodes | |
| JPH0519261B2 (cs) | ||
| US3749605A (en) | Battery having zinc electrode containing tio2 | |
| JPS6298563A (ja) | ニツケル・カドミウムアルカリ蓄電池用陰極板の製造法 | |
| JP2701693B2 (ja) | アルカリ電池用ゲル状負極の製造方法 | |
| JPS5935360A (ja) | 亜鉛極 | |
| JP3276730B2 (ja) | アルカリ蓄電池の製造方法 | |
| JPH09147849A (ja) | ペースト式アルカリ蓄電池用負極とその製造方法 | |
| JP2942637B2 (ja) | ペースト式ニッケル極の製造方法 | |
| JP3146014B2 (ja) | ペースト式ニッケル極の製造方法 | |
| JPH0569264B2 (cs) | ||
| JPH0546061B2 (cs) | ||
| JPH03184261A (ja) | アルカリ蓄電池用陰極板の製造法 | |
| JPS61181061A (ja) | 非水電解液電池用正極の製造方法 | |
| JPS60151964A (ja) | アルカリ電池用正極板の製造法 | |
| JPS6273566A (ja) | 密閉形アルカリ蓄電池用陰極板の製造方法 | |
| JPS6269465A (ja) | ニツケル・カドミウムアルカリ蓄電池用陽極板 | |
| JPH0564421B2 (cs) | ||
| JPS60253156A (ja) | アルカリ蓄電池用ニツケル正極およびその製造法 | |
| JPS62243255A (ja) | アルカリ蓄電池用陰極板の製造方法 | |
| JPH08148149A (ja) | アルカリ蓄電池用非焼結式カドミウム負極 | |
| JPH02139855A (ja) | アルカリ蓄電池用亜鉛極の製造方法 | |
| JPS62113360A (ja) | スラリ−式カドミウム極板の製造法 | |
| JPS63119157A (ja) | 亜鉛極 | |
| JPH0935709A (ja) | ペースト式電極の製造方法 |