JPH0460696B2 - - Google Patents
Info
- Publication number
- JPH0460696B2 JPH0460696B2 JP59185445A JP18544584A JPH0460696B2 JP H0460696 B2 JPH0460696 B2 JP H0460696B2 JP 59185445 A JP59185445 A JP 59185445A JP 18544584 A JP18544584 A JP 18544584A JP H0460696 B2 JPH0460696 B2 JP H0460696B2
- Authority
- JP
- Japan
- Prior art keywords
- particles
- particle size
- particle
- mixing
- standard deviation
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Glanulating (AREA)
- Processes Of Treating Macromolecular Substances (AREA)
- Processing And Handling Of Plastics And Other Materials For Molding In General (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP18544584A JPS6164326A (ja) | 1984-09-06 | 1984-09-06 | 複合粒子の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP18544584A JPS6164326A (ja) | 1984-09-06 | 1984-09-06 | 複合粒子の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6164326A JPS6164326A (ja) | 1986-04-02 |
| JPH0460696B2 true JPH0460696B2 (cg-RX-API-DMAC7.html) | 1992-09-28 |
Family
ID=16170915
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP18544584A Granted JPS6164326A (ja) | 1984-09-06 | 1984-09-06 | 複合粒子の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6164326A (cg-RX-API-DMAC7.html) |
Families Citing this family (15)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0747118B2 (ja) * | 1985-03-05 | 1995-05-24 | 株式会社資生堂 | 複合粉体の製造方法 |
| JPH024330Y2 (cg-RX-API-DMAC7.html) * | 1985-03-22 | 1990-02-01 | ||
| JPH0775665B2 (ja) * | 1986-10-27 | 1995-08-16 | 日本合成ゴム株式会社 | マイクロカプセル化微粒子の製造方法 |
| JPH06102730B2 (ja) * | 1988-04-28 | 1994-12-14 | 鐘淵化学工業株式会社 | 分離材用バイモーダル粒子 |
| JPH0822377B2 (ja) * | 1990-03-02 | 1996-03-06 | 株式会社サンギ | カラム用充填剤 |
| JP4004470B2 (ja) * | 2001-11-02 | 2007-11-07 | 三洋化成工業株式会社 | 複合樹脂粒子 |
| KR100848023B1 (ko) | 2002-04-30 | 2008-07-23 | 카네카 코포레이션 | 중합체 입자 및 그 제조방법 |
| JP2006036841A (ja) * | 2004-07-23 | 2006-02-09 | Trial Corp | イオン交換樹脂で被覆された複合粒子 |
| JP4975275B2 (ja) * | 2005-06-13 | 2012-07-11 | 花王株式会社 | 複合化粒子の製造方法 |
| JP2008050592A (ja) * | 2006-07-28 | 2008-03-06 | Kyodo Printing Co Ltd | 粉体一体化樹脂粒子及びその造粒方法、並びに粒子含有成形体及び粒子含有シート材並びにこれらの成形方法 |
| WO2008013266A1 (en) * | 2006-07-28 | 2008-01-31 | Kyodo Printing Co., Ltd. | Resin particle with powder united thereto and method of forming the same, particle-containing molded object, particle-containing sheet material, and method of forming these, and functional sheet and process for producing functional sheet |
| JP2008093579A (ja) * | 2006-10-12 | 2008-04-24 | Kao Corp | 積層複合化粒子の製造方法 |
| JP4911762B2 (ja) * | 2006-10-16 | 2012-04-04 | 花王株式会社 | 複合化粒子の製造方法 |
| JP2011209040A (ja) * | 2010-03-29 | 2011-10-20 | Sekisui Medical Co Ltd | ヘモグロビン類測定用カラム充填剤、ヘモグロビンA1cの測定方法、並びに、ヘモグロビンA1c及び異常ヘモグロビン類の測定方法 |
| US9354242B2 (en) * | 2012-10-16 | 2016-05-31 | Ortho-Clinical Diagnostics, Inc. | Glass bead flow rates to facilitate immunodiagnostic test element manufacture |
Family Cites Families (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5120961B2 (cg-RX-API-DMAC7.html) * | 1971-10-19 | 1976-06-29 |
-
1984
- 1984-09-06 JP JP18544584A patent/JPS6164326A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS6164326A (ja) | 1986-04-02 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPH0460696B2 (cg-RX-API-DMAC7.html) | ||
| US4940734A (en) | Process for the preparation of porous polymer beads | |
| Senuma et al. | Alginate hydrogel microspheres and microcapsules prepared by spinning disk atomization | |
| DE3336235C2 (cg-RX-API-DMAC7.html) | ||
| JPH09509356A (ja) | 封入方法及びそれにより製造したマイクロカプセル | |
| JPH0581615B2 (cg-RX-API-DMAC7.html) | ||
| Fielden et al. | The influence of moisture content on spheronization of extrudate processed by a ram extruder | |
| JPH09507787A (ja) | 吸着材料および方法 | |
| EP1247831A4 (en) | POROUS PARTICLES AND METHOD FOR THE PRODUCTION THEREOF | |
| Cassignol et al. | Microstructure–conductivity relationship in conducting polypyrrole/epoxy composites | |
| JPH05505643A (ja) | 微細な重合体粒子および重合体封入粒子の形成方法 | |
| JPS619433A (ja) | 熱可塑性樹脂微小球体の製法 | |
| HU214982B (hu) | Vízoldható vagy vízben duzzasztható polimerszemcséket tartalmazó szilárd termék, eljárás előállítására és polimerizálási eljárás | |
| US8147783B2 (en) | Nickel hydroxide powder and method for producing same | |
| CA2143835C (en) | Method for manufacturing spherical particles | |
| KR101745017B1 (ko) | 초음파 고온 진동법을 이용한 열제어 소재용 마이크로 입자와, 이것의 제조 장치 및 방법 | |
| CN102884110B (zh) | 具有异质表面的复合微粒子的制造方法 | |
| JPH0457374B2 (cg-RX-API-DMAC7.html) | ||
| JP2001106793A (ja) | 充填材入りポリテトラフルオロエチレン粉末の造粒方法 | |
| JPH0459010B2 (cg-RX-API-DMAC7.html) | ||
| Wang et al. | Polymer/particle/water intermolecular interaction regulated freeze-dried Pickering emulsion morphology | |
| CN102085469B (zh) | 微纳米级粉体借助界面聚合制备大粒径颗粒的方法 | |
| JP3599536B2 (ja) | 架橋重合体からなる球状体及びその製造方法 | |
| WO2001064331A1 (de) | Verfahren zur herstellung von mikro- und/oder nanokapseln | |
| CN114377825B (zh) | 一种提高聚合物纳米复合材料中纳米粒子分散度的装置 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| LAPS | Cancellation because of no payment of annual fees |