Prior art keywords
nickel
substrate
cobalt
electrode
hydroxide
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
JP60198119A
Other languages
English (en)
Japanese (ja)
Other versions
JPS6258566A (ja
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to JP60198119A priority Critical patent/JPS6258566A/ja
Publication of JPS6258566A publication Critical patent/JPS6258566A/ja
Publication of JPH0410179B2 publication Critical patent/JPH0410179B2/ja
Granted legal-status Critical Current

Links

Classifications

    • HELECTRICITY
    • H01ELECTRIC ELEMENTS
    • H01MPROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
    • H01M4/00Electrodes
    • H01M4/02Electrodes composed of, or comprising, active material
    • H01M4/24Electrodes for alkaline accumulators
    • H01M4/32Nickel oxide or hydroxide electrodes
    • HELECTRICITY
    • H01ELECTRIC ELEMENTS
    • H01MPROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
    • H01M4/00Electrodes
    • H01M4/02Electrodes composed of, or comprising, active material
    • H01M4/24Electrodes for alkaline accumulators
    • H01M4/26Processes of manufacture
    • H01M4/28Precipitating active material on the carrier
    • YGENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y02TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
    • Y02EREDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
    • Y02E60/00Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
    • Y02E60/10Energy storage using batteries

Landscapes

  • Chemical & Material Sciences (AREA)
  • Chemical Kinetics & Catalysis (AREA)
  • Electrochemistry (AREA)
  • General Chemical & Material Sciences (AREA)
  • Engineering & Computer Science (AREA)
  • Manufacturing & Machinery (AREA)
  • Battery Electrode And Active Subsutance (AREA)
JP60198119A 1985-09-06 1985-09-06 アルカリ蓄電池用水酸化ニツケル電極の製造方法 Granted JPS6258566A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP60198119A JPS6258566A (ja) 1985-09-06 1985-09-06 アルカリ蓄電池用水酸化ニツケル電極の製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP60198119A JPS6258566A (ja) 1985-09-06 1985-09-06 アルカリ蓄電池用水酸化ニツケル電極の製造方法

Publications (2)

Publication Number Publication Date
JPS6258566A JPS6258566A (ja) 1987-03-14
JPH0410179B2 true JPH0410179B2 (ko) 1992-02-24

Family

ID=16385773

Family Applications (1)

Application Number Title Priority Date Filing Date
JP60198119A Granted JPS6258566A (ja) 1985-09-06 1985-09-06 アルカリ蓄電池用水酸化ニツケル電極の製造方法

Country Status (1)

Country Link
JP (1) JPS6258566A (ko)

Families Citing this family (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS63216268A (ja) * 1987-03-03 1988-09-08 Sanyo Electric Co Ltd アルカリ蓄電池用水酸化ニツケル電極の製造方法
JPH02265165A (ja) * 1989-04-04 1990-10-29 Yuasa Battery Co Ltd アルカリ蓄電池用ニッケル電極

Also Published As

Publication number Publication date
JPS6258566A (ja) 1987-03-14

Similar Documents

Publication Publication Date Title
JPH0550099B2 (ko)
JPH0410179B2 (ko)
JP3412451B2 (ja) アルカリ蓄電池正極用ニッケル焼結基板とその製造法およびアルカリ蓄電池
JPH11339814A (ja) アルカリ蓄電池用電極の製造方法
US3779810A (en) Method of making a nickel positive electrode for an alkaline battery
JPH0410177B2 (ko)
JPH0410178B2 (ko)
JPH0570907B2 (ko)
JP3414184B2 (ja) アルカリ蓄電池用正極板の製造方法
JPH0475255A (ja) アルカリ蓄電池用水酸化ニッケル電極の製造方法
JP2951940B2 (ja) アルカリ蓄電池用電極とその製造方法、およびアルカリ蓄電池
JP2865391B2 (ja) アルカリ蓄電池用水酸化ニッケル電極の製造方法
JPH0589876A (ja) アルカリ蓄電池用ニツケル電極の製造方法
JP2898421B2 (ja) アルカリ二次電池用の焼結式ニッケル電極の製造方法
JP2639916B2 (ja) アルカリ蓄電池用焼結式ニツケル電極の製造方法
JPH1173957A (ja) アルカリ蓄電池とそのニッケル正極板の製造法
JP4356119B2 (ja) アルカリ蓄電池用焼結式ニッケル電極
JP3625681B2 (ja) アルカリ蓄電池用ニッケル電極の製造方法
JP2001351619A (ja) ニッケル正極板およびアルカリ蓄電池
JP3275594B2 (ja) アルカリ蓄電池用正極の製造法
JPS63114061A (ja) アルカリ蓄電池用焼結式ニツケル極の製法
JP5167681B2 (ja) アルカリ蓄電池用ニッケル正極の製造方法
JP3272009B2 (ja) アルカリ蓄電池用ニッケル電極の製造方法
JPS6266572A (ja) アルカリ蓄電池用電極の製造方法
JP2529308B2 (ja) アルカリ蓄電池用カドミウム負極の製造法

Legal Events

Date Code Title Description
EXPY Cancellation because of completion of term