JPH0379406B2 - - Google Patents

Info

Publication number
JPH0379406B2
JPH0379406B2 JP27541286A JP27541286A JPH0379406B2 JP H0379406 B2 JPH0379406 B2 JP H0379406B2 JP 27541286 A JP27541286 A JP 27541286A JP 27541286 A JP27541286 A JP 27541286A JP H0379406 B2 JPH0379406 B2 JP H0379406B2
Authority
JP
Japan
Prior art keywords
converter
repair
tap
tapping
time
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP27541286A
Other languages
English (en)
Japanese (ja)
Other versions
JPS63130708A (ja
Inventor
Sachoshi Isomura
Toshiharu Nonaka
Ryoichi Nojima
Toshitaka Inatomi
Kenji Ooya
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nippon Steel Corp
Original Assignee
Nippon Steel Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nippon Steel Corp filed Critical Nippon Steel Corp
Priority to JP27541286A priority Critical patent/JPS63130708A/ja
Publication of JPS63130708A publication Critical patent/JPS63130708A/ja
Publication of JPH0379406B2 publication Critical patent/JPH0379406B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Carbon Steel Or Casting Steel Manufacturing (AREA)
JP27541286A 1986-11-20 1986-11-20 転炉出鋼口の補修方法 Granted JPS63130708A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP27541286A JPS63130708A (ja) 1986-11-20 1986-11-20 転炉出鋼口の補修方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP27541286A JPS63130708A (ja) 1986-11-20 1986-11-20 転炉出鋼口の補修方法

Publications (2)

Publication Number Publication Date
JPS63130708A JPS63130708A (ja) 1988-06-02
JPH0379406B2 true JPH0379406B2 (enrdf_load_stackoverflow) 1991-12-18

Family

ID=17555138

Family Applications (1)

Application Number Title Priority Date Filing Date
JP27541286A Granted JPS63130708A (ja) 1986-11-20 1986-11-20 転炉出鋼口の補修方法

Country Status (1)

Country Link
JP (1) JPS63130708A (enrdf_load_stackoverflow)

Families Citing this family (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP5079444B2 (ja) * 2007-10-05 2012-11-21 新日本製鐵株式会社 転炉内壁面のスラグコーティング方法
DE102009056219A1 (de) * 2009-11-28 2011-06-01 Sms Siemag Ag Befestigungssystem für metallurgische Gefäße

Also Published As

Publication number Publication date
JPS63130708A (ja) 1988-06-02

Similar Documents

Publication Publication Date Title
US4434540A (en) Process for repairing or modifying refractory plates of ladle casting cassettes
JPH0379406B2 (enrdf_load_stackoverflow)
US5529729A (en) Process for producing the refractory lining of a casting ladle
JP2786832B2 (ja) 冷却パイプの鋳包み方法
JPH0445218A (ja) 転炉の出鋼孔の補修用治具および出鋼孔の補修方法
JP2544719Y2 (ja) 溶融金属容器のガス吹込みノズルの羽口構造
EP0519553B1 (en) Method of repair of the refractory lining of the wall of a shaft furnace
CN212864821U (zh) 一种矿热炉铁口泥套装置
JP3613815B2 (ja) 高炉炉壁の補修用ステーブによる補修方法
JPS6076253A (ja) 造塊用鋳型のクレ−ジング補修方法
JP2544720Y2 (ja) 溶融金属容器のガス吹込みノズルの羽口構造
JPH03134487A (ja) 不定形耐火物の施工方法
JPH08127812A (ja) 転炉内付着地金の除去方法
JP3613816B2 (ja) 高炉炉壁のステーブによる補修方法
JPH0140890B2 (enrdf_load_stackoverflow)
JPS6317571Y2 (enrdf_load_stackoverflow)
JPS5832211B2 (ja) 転炉出鋼口の簡易補修法
JPS5831006A (ja) 高炉の連続出湯作業方法
JPH01202349A (ja) 連続鋳造方法
JPS6058761B2 (ja) 底吹き羽口を有する転炉の炉底補修方法
JPS5837941Y2 (ja) 炉外精錬用上吹きランス
JPS6147630B2 (enrdf_load_stackoverflow)
JP2917848B2 (ja) 転炉吹錬兼炉口地金溶解用ランス
JP2710093B2 (ja) タンディッシュの連続使用方法
JP2000084645A (ja) タンディッシュの連続使用方法