Prior art keywords
nickel
sintered
slurry
substrate
porosity
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
JP59025395A
Other languages
English (en)
Japanese (ja)
Other versions
JPS60170167A (ja
Inventor
Masanori Endo
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Japan Storage Battery Co Ltd
Original Assignee
Japan Storage Battery Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Japan Storage Battery Co Ltd filed Critical Japan Storage Battery Co Ltd
Priority to JP59025395A priority Critical patent/JPS60170167A/ja
Publication of JPS60170167A publication Critical patent/JPS60170167A/ja
Priority to JP2069262A priority patent/JPH07120530B2/ja
Publication of JPH0324026B2 publication Critical patent/JPH0324026B2/ja
Granted legal-status Critical Current

Links

Classifications

    • HELECTRICITY
    • H01ELECTRIC ELEMENTS
    • H01MPROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
    • H01M4/00Electrodes
    • H01M4/02Electrodes composed of, or comprising, active material
    • H01M4/64Carriers or collectors
    • H01M4/70Carriers or collectors characterised by shape or form
    • H01M4/80Porous plates, e.g. sintered carriers
    • YGENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y02TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
    • Y02EREDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
    • Y02E60/00Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
    • Y02E60/10Energy storage using batteries

Landscapes

  • Chemical & Material Sciences (AREA)
  • Chemical Kinetics & Catalysis (AREA)
  • Electrochemistry (AREA)
  • General Chemical & Material Sciences (AREA)
  • Cell Electrode Carriers And Collectors (AREA)
JP59025395A 1984-02-13 1984-02-13 アルカリ電池用電極の製造方法 Granted JPS60170167A (ja)

Priority Applications (2)

Application Number Priority Date Filing Date Title
JP59025395A JPS60170167A (ja) 1984-02-13 1984-02-13 アルカリ電池用電極の製造方法
JP2069262A JPH07120530B2 (ja) 1984-02-13 1990-03-19 アルカリ電池用焼結式ニッケル基板の製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP59025395A JPS60170167A (ja) 1984-02-13 1984-02-13 アルカリ電池用電極の製造方法

Related Child Applications (2)

Application Number Title Priority Date Filing Date
JP2069262A Division JPH07120530B2 (ja) 1984-02-13 1990-03-19 アルカリ電池用焼結式ニッケル基板の製造方法
JP2069263A Division JPH0697610B2 (ja) 1990-03-19 1990-03-19 アルカリ電池用電極の製造方法

Publications (2)

Publication Number Publication Date
JPS60170167A JPS60170167A (ja) 1985-09-03
JPH0324026B2 true JPH0324026B2 (enrdf_load_stackoverflow) 1991-04-02

Family

ID=12164699

Family Applications (1)

Application Number Title Priority Date Filing Date
JP59025395A Granted JPS60170167A (ja) 1984-02-13 1984-02-13 アルカリ電池用電極の製造方法

Country Status (1)

Country Link
JP (1) JPS60170167A (enrdf_load_stackoverflow)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103229255A (zh) * 2011-11-28 2013-07-31 三菱电机株式会社 交流电磁铁构造

Families Citing this family (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH07120530B2 (ja) * 1984-02-13 1995-12-20 日本電池株式会社 アルカリ電池用焼結式ニッケル基板の製造方法
JP2567672B2 (ja) * 1987-07-08 1996-12-25 三洋電機株式会社 アルカリ蓄電池用焼結式カドミウム負極及びその製造方法
KR100362210B1 (ko) * 1995-03-27 2003-03-10 삼성전자 주식회사 니켈전극제조방법

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103229255A (zh) * 2011-11-28 2013-07-31 三菱电机株式会社 交流电磁铁构造

Also Published As

Publication number Publication date
JPS60170167A (ja) 1985-09-03

Similar Documents

Publication Publication Date Title
JP4514265B2 (ja) 電極及び非水電解液二次電池
JPH0324026B2 (enrdf_load_stackoverflow)
JPH0630248B2 (ja) アルカリ電池用ニッケル極
JPS62234867A (ja) アルカリ電池用ニッケル極の製造法
JP2615538B2 (ja) アルカリ蓄電池用ニツケル正極
JPS62222566A (ja) アルカリ電池用ニッケル極の製造法
JPH0837001A (ja) 鉛蓄電池用正極板及びその製造方法
JP2567672B2 (ja) アルカリ蓄電池用焼結式カドミウム負極及びその製造方法
JPS6264062A (ja) アルカリ蓄電池用正極板
JPS5931835B2 (ja) 電池用集電体の製造法
JPH03114143A (ja) アルカリ電池用電極の製造方法
JPH08203522A (ja) アルカリ蓄電池用ニッケル活物質及びその製法
JPH0619990B2 (ja) アルカリ電池用ニツケル電極の製造法
JP3691257B2 (ja) アルカリ蓄電池用焼結式カドミウム負極の製造方法
JPH0799690B2 (ja) 水素吸蔵電極の製造方法
JP2810460B2 (ja) アルカリ蓄電池用正極板
JPS63114061A (ja) アルカリ蓄電池用焼結式ニツケル極の製法
JP3073259B2 (ja) アルカリ蓄電池用ニッケル極
JP2015144057A (ja) アルカリ二次電池用正極及びその製造方法、アルカリ二次電池及びその製造方法
JPH07120530B2 (ja) アルカリ電池用焼結式ニッケル基板の製造方法
JPS60140656A (ja) アルカリ蓄電池用カドミウム陰極板の製造法
JPS6110864A (ja) 鉄電極およびその製造方法
JPS60216449A (ja) ペ−スト式カドミウム陰極板の製造方法
JPS61203566A (ja) アルカリ蓄電池用カドミウム負極板の製造法
JPH11102700A (ja) アルカリ蓄電池用ニッケル電極の製造方法