JPH0215383B2 - - Google Patents
Info
- Publication number
- JPH0215383B2 JPH0215383B2 JP59092997A JP9299784A JPH0215383B2 JP H0215383 B2 JPH0215383 B2 JP H0215383B2 JP 59092997 A JP59092997 A JP 59092997A JP 9299784 A JP9299784 A JP 9299784A JP H0215383 B2 JPH0215383 B2 JP H0215383B2
- Authority
- JP
- Japan
- Prior art keywords
- film
- corrosion
- resins
- ion exchange
- forming
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Application Of Or Painting With Fluid Materials (AREA)
- Laminated Bodies (AREA)
- Chemical Treatment Of Metals (AREA)
Priority Applications (5)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP59092997A JPS60236746A (ja) | 1984-05-11 | 1984-05-11 | 耐食−親水性皮膜を形成する方法 |
GB08428144A GB2151641B (en) | 1983-11-11 | 1984-11-07 | Hydrophilic film-forming coating compositions |
CA000467532A CA1216695A (en) | 1983-11-11 | 1984-11-09 | Hydrophilic-film-forming preparation |
FR8417347A FR2554824B1 (fr) | 1983-11-11 | 1984-11-12 | Preparations pour la formation d'un film hydrophile, procede pour leur mise en oeuvre et articles ainsi revetus |
DE19843441275 DE3441275A1 (de) | 1983-11-11 | 1984-11-12 | Mittel zur herstellung hydrophiler filme |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP59092997A JPS60236746A (ja) | 1984-05-11 | 1984-05-11 | 耐食−親水性皮膜を形成する方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS60236746A JPS60236746A (ja) | 1985-11-25 |
JPH0215383B2 true JPH0215383B2 (enrdf_load_stackoverflow) | 1990-04-11 |
Family
ID=14070000
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP59092997A Granted JPS60236746A (ja) | 1983-11-11 | 1984-05-11 | 耐食−親水性皮膜を形成する方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS60236746A (enrdf_load_stackoverflow) |
Family Cites Families (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS604753B2 (ja) * | 1978-12-14 | 1985-02-06 | 新日本製鐵株式会社 | 高耐蝕性d&i缶の製造法 |
-
1984
- 1984-05-11 JP JP59092997A patent/JPS60236746A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS60236746A (ja) | 1985-11-25 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US5380374A (en) | Conversion coatings for metal surfaces | |
US4183772A (en) | Composition and method for coating metal surfaces | |
US4973359A (en) | Surface treatment chemical and bath for forming hydrophilic coatings and method of surface-treating aluminum members | |
US4650527A (en) | Hydrophilic surface-treating process for an aluminum article | |
JPH09502924A (ja) | アルミニウム表面の非磨耗性で、耐食性の親水性被覆、その被覆方法並びに被覆物 | |
NZ200958A (en) | Provision of corrosion-resistance on aluminium surfaces | |
US4775588A (en) | Metal substrates having hydrophilic resin paints containing finely divided ion exchange resins on its surface | |
KR20020017955A (ko) | 6가 크롬을 함유하지 않는 물계 금속표면 처리제 및그것으로써 처리한 표면처리 금속판 | |
JPH0348272B2 (enrdf_load_stackoverflow) | ||
EP0119608B1 (en) | Coating composite for extended corrosion resistance | |
US6294262B1 (en) | Composition and process for anticorrosive treatment of non-ferrous metal | |
JP2018070677A (ja) | 表面処理剤、皮膜及び表面処理方法 | |
CA1216695A (en) | Hydrophilic-film-forming preparation | |
JP3737168B2 (ja) | 高白色で塗装性に優れた電気亜鉛めっき鋼板の製造方法 | |
JPH0215383B2 (enrdf_load_stackoverflow) | ||
JP2017071720A (ja) | 表面処理剤、皮膜及び表面処理方法 | |
JPH04314872A (ja) | 耐食性およびスポット溶接性に優れた有機複合被覆鋼板 | |
JP2816559B2 (ja) | 黒色亜鉛めっき鋼板の製造方法 | |
JP3330423B2 (ja) | 陰極電解樹脂クロメート型金属表面処理方法 | |
JP6772943B2 (ja) | 塗装鋼板 | |
JP5000802B2 (ja) | 無機膜形成用塗布剤、その無機膜形成方法、そのものを用いて得られる無機膜被覆アルミニウム材及び無機膜被覆鋼材 | |
JPS63178873A (ja) | 耐食性および塗装性に優れたクロメ−ト処理メツキ鋼板の製造方法 | |
JP2000328259A (ja) | 熱交換器用プレコートフィン材 | |
JP2002225176A (ja) | 耐食性に優れた塗装冷延鋼板 | |
JPS6187878A (ja) | 親水性耐食皮膜を形成する方法 |