JPS60236746A - 耐食−親水性皮膜を形成する方法 - Google Patents
耐食−親水性皮膜を形成する方法Info
- Publication number
- JPS60236746A JPS60236746A JP59092997A JP9299784A JPS60236746A JP S60236746 A JPS60236746 A JP S60236746A JP 59092997 A JP59092997 A JP 59092997A JP 9299784 A JP9299784 A JP 9299784A JP S60236746 A JPS60236746 A JP S60236746A
- Authority
- JP
- Japan
- Prior art keywords
- film
- corrosion
- forming
- resistant
- coating
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Chemical Treatment Of Metals (AREA)
- Application Of Or Painting With Fluid Materials (AREA)
- Laminated Bodies (AREA)
Priority Applications (5)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP59092997A JPS60236746A (ja) | 1984-05-11 | 1984-05-11 | 耐食−親水性皮膜を形成する方法 |
GB08428144A GB2151641B (en) | 1983-11-11 | 1984-11-07 | Hydrophilic film-forming coating compositions |
CA000467532A CA1216695A (en) | 1983-11-11 | 1984-11-09 | Hydrophilic-film-forming preparation |
DE19843441275 DE3441275A1 (de) | 1983-11-11 | 1984-11-12 | Mittel zur herstellung hydrophiler filme |
FR8417347A FR2554824B1 (fr) | 1983-11-11 | 1984-11-12 | Preparations pour la formation d'un film hydrophile, procede pour leur mise en oeuvre et articles ainsi revetus |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP59092997A JPS60236746A (ja) | 1984-05-11 | 1984-05-11 | 耐食−親水性皮膜を形成する方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS60236746A true JPS60236746A (ja) | 1985-11-25 |
JPH0215383B2 JPH0215383B2 (enrdf_load_stackoverflow) | 1990-04-11 |
Family
ID=14070000
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP59092997A Granted JPS60236746A (ja) | 1983-11-11 | 1984-05-11 | 耐食−親水性皮膜を形成する方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS60236746A (enrdf_load_stackoverflow) |
Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5582797A (en) * | 1978-12-14 | 1980-06-21 | Nippon Steel Corp | Preparation of high anticorrosive d and i can |
-
1984
- 1984-05-11 JP JP59092997A patent/JPS60236746A/ja active Granted
Patent Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5582797A (en) * | 1978-12-14 | 1980-06-21 | Nippon Steel Corp | Preparation of high anticorrosive d and i can |
Also Published As
Publication number | Publication date |
---|---|
JPH0215383B2 (enrdf_load_stackoverflow) | 1990-04-11 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US4183772A (en) | Composition and method for coating metal surfaces | |
EP3385405B1 (en) | Chromium-free surface-treated tinplate, production method and surface treating agent therefor | |
JPH09502924A (ja) | アルミニウム表面の非磨耗性で、耐食性の親水性被覆、その被覆方法並びに被覆物 | |
US4650527A (en) | Hydrophilic surface-treating process for an aluminum article | |
CN109321908A (zh) | 一种金属表面多功能环保型纳米陶化液及其制备方法和使用方法 | |
JPH0348272B2 (enrdf_load_stackoverflow) | ||
JPH05214266A (ja) | 自己析出型水性コーティング組成物 | |
JP2000248381A (ja) | アルミニウム材の親水性処理方法及びその下地処理剤並びに親水性塗料 | |
US2213263A (en) | Process of coating metals | |
CN101018888B (zh) | 在钢表面上形成非铬转化涂层的方法和组合物 | |
JP2018070677A (ja) | 表面処理剤、皮膜及び表面処理方法 | |
JPS5853960A (ja) | フツ素樹脂被覆用組成物 | |
JP3737168B2 (ja) | 高白色で塗装性に優れた電気亜鉛めっき鋼板の製造方法 | |
JPS60236746A (ja) | 耐食−親水性皮膜を形成する方法 | |
CA1216695A (en) | Hydrophilic-film-forming preparation | |
JP2780250B2 (ja) | 親水性表面処理剤、親水性表面処理浴及びアルミニウム材の表面処理方法 | |
JPH01108231A (ja) | 親水性表面処理剤及び処理方法 | |
JP2816559B2 (ja) | 黒色亜鉛めっき鋼板の製造方法 | |
JP3373801B2 (ja) | アルミニウム材の下地処理方法及び下地処理剤 | |
JPS63178873A (ja) | 耐食性および塗装性に優れたクロメ−ト処理メツキ鋼板の製造方法 | |
JPS6187878A (ja) | 親水性耐食皮膜を形成する方法 | |
JP7485533B2 (ja) | アルミニウム製フィン材 | |
JPH0348271B2 (enrdf_load_stackoverflow) | ||
JP2579487B2 (ja) | 表面特性の優れた白色クロメ−ト処理方法 | |
JPS61101798A (ja) | 熱交換器フイン材 |