JP5677358B2 - ルテニウム担持触媒の製造方法 - Google Patents
ルテニウム担持触媒の製造方法 Download PDFInfo
- Publication number
- JP5677358B2 JP5677358B2 JP2012091698A JP2012091698A JP5677358B2 JP 5677358 B2 JP5677358 B2 JP 5677358B2 JP 2012091698 A JP2012091698 A JP 2012091698A JP 2012091698 A JP2012091698 A JP 2012091698A JP 5677358 B2 JP5677358 B2 JP 5677358B2
- Authority
- JP
- Japan
- Prior art keywords
- ammonia
- ruthenium
- catalyst
- reaction tube
- supported catalyst
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Description
i)活性炭を塩化ルテニウム水溶液(ルテニウムとして10g/l)に8時間浸漬した後、同水溶液から取り出し、110℃で空気下で乾燥させた。
i)活性炭を塩化ルテニウム水溶液(ルテニウムとして10g/l)に8時間浸漬した後、同水溶液から取り出し、110℃で空気下で乾燥させた。
i)活性炭を塩化ルテニウム水溶液(ルテニウムとして10g/l)に8時間浸漬した後、同水溶液から取り出し、110℃で空気下で乾燥させた。
i)活性炭を塩化ルテニウム水溶液(ルテニウムとして10g/l)に8時間浸漬した後、同水溶液から取り出し、110℃で空気下で乾燥させた。
i)参考例3で得られたRu−Ba担持触媒を反応管に充填し、水素気流下で触媒充填層温度を450℃まで昇温し、450℃で2時間保持した後、温度を下げた。
i)参考例3で得られたRu−Ba担持触媒を反応管に充填し、アンモニアガス流中で充填層温度を450℃まで昇温し、450℃で2時間保持した後、温度を下げた。
i)活性炭を塩化ルテニウム水溶液(ルテニウムとして10g/l)に8時間浸漬した後、同水溶液から取り出し、110℃で空気下で乾燥させた。
i)活性炭を塩化ルテニウム水溶液(ルテニウムとして10g/l)に8時間浸漬した後、同水溶液から取り出し、110℃で空気下で乾燥させた。
i)参考例3で得られたRu−Ba担持触媒を反応管に充填し、水素気流下で触媒充填層温度を450℃まで昇温し、450℃で2時間保持した後、温度を下げた。
実施例、参考例および比較例で得られた各触媒のアンモニア分解活性を、図1に示す試験装置を用いて下記の試験条件で測定した。図1中、(1)はアンモニア分解用の反応器、(2)は反応器(1)に設けられた触媒充填層、(3)は反応器(1)のヒータ、(4)(5)は触媒充填層の上端および下端に配された熱電対、(6)は反応器(1)の頂部に供給されるアンモニア(+ヘリウム)の流量計、(7)は反応器(1)の下端から出るガス中の残存アンモニアを捕捉するトラップ、(8)(9)はアンモニア分解生成ガスの流量計およびガスクロマトクラフィである。
反応温度(℃) 400℃
圧力 常圧
入ロアンモニア濃度(%) 100%
空間速度(m3/h/m3−触媒) 5000
触媒 アンモニア分解率(%)
参考例1 20.3
実施例2 19.4
参考例3 60.1
実施例4 59.6
参考例5 60.0
参考例6 59.7
比較例1 5.3
比較例2 41.5
比較例3 28.5
(2) 触媒充填層
(3) ヒータ
(4)(5) 熱電対
(6) 流量計
(7) トラップ
(8) 流量計
(9)ガスクロマトクラフィ
Claims (4)
- 活性炭にルテニウムを担持してなる触媒の還元において、反応管内にてアンモニアガスで還元処理を行った後、引き続き同反応管にアンモニアガスを流通し、還元されたルテニウムにアンモニアを吸着させ、還元されたルテニウムの酸化活性を抑制することを特徴とするアンモニア分解用またはアンモニアからの水素製造用のルテニウム担持触媒の製造方法。
- 還元されたルテニウムにアンモニアを吸着させた後、促進剤であるバリウム化合物を担持させる、請求項1に記載の方法。
- 請求項1または2に記載の方法で製造された、アンモニア分解用またはアンモニアからの水素製造用のルテニウム担持触媒。
- 請求項3記載のアンモニア分解用またはアンモニアからの水素製造用のルテニウム担持触媒を用いるアンモニア分解方法またはアンモニアからの水素製造方法。