JP5183888B2 - 鉛蓄電池用極板の製造方法 - Google Patents
鉛蓄電池用極板の製造方法 Download PDFInfo
- Publication number
- JP5183888B2 JP5183888B2 JP2006163858A JP2006163858A JP5183888B2 JP 5183888 B2 JP5183888 B2 JP 5183888B2 JP 2006163858 A JP2006163858 A JP 2006163858A JP 2006163858 A JP2006163858 A JP 2006163858A JP 5183888 B2 JP5183888 B2 JP 5183888B2
- Authority
- JP
- Japan
- Prior art keywords
- paste
- active material
- electrode plate
- paper
- lead
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Description
まず、Pb−Ca系合金(合金組成がカルシウム0.1wt%、スズ0.5wt%、残部が鉛と不可避不純物)から成る連続鋳造基板に、主に金属鉛と一酸化鉛からなる活物質ペーストを充填した直後、極板両面にペースト紙を貼り、極板を横に水平に50枚重ねて1つの束とし、これを2束作製した。そして、夫々の極板束を断熱された熟成炉内に入れ、熟成初期段階で炉内温度が80℃、相対湿度が95%に到達するまでの時間が0.5時間になるよう温湿度を制御した。
同様に、熟成初期段階で炉内温度が80℃、相対湿度が95%に到達するまでの時間を1時間とした以外は本発明1と同様にして極板2を作製した(参考例2)。
熟成初期段階で炉内温度が80℃、相対湿度が95%に到達するまでの時間を1.5時間とした以外は本発明1と同様にして極板3を作製した(参考例3)。
熟成初期段階で炉内温度が80℃、相対湿度が95%に到達するまでの時間を3時間とし、ボイラーおよびヒータの所望の容量(参考例1記載のボイラーおよびヒータの1/3の容量)とした以外は本発明1と同様にして極板4を作製した(参考例4)。
また、参考例1、2、即ち4BSの生成量が50wt%以上であるものは、平均引張荷重も高く活物質とペースト紙の結着力が強固であり、ペースト紙が剥がれることは無かった。これに対し、参考例3、4は3BSの生成量が主となっており、活物質とペースト紙の結着力は低く参考例3で束上部の5枚、参考例4で束上部の11枚のペースト紙が剥がれる結果となった。
酸錬り時の冷却停止時間と酸練り時のペースト状活物質の最高温度を本発明規定値外とした以外は、実施例と同じ方法により極板を作製した(比較例1〜2)。
Claims (1)
- 鉛を主成分とする鉛合金の基板にペースト状活物質を充填し、その両面にペースト紙を貼り付けて作製される鉛蓄電池用極板の製造方法において、該ペースト状活物質のペースト練り工程終了時のペースト状活物質中に4塩基性硫酸鉛が5〜20質量%生成するように練り工程を行い、該ペースト状活物質を基板に充填し、その両面にペースト紙を貼り付けた後、4塩基性硫酸鉛の生成量が熟成終了後に50質量%以上となるように熟成工程を行うことを特徴とする鉛蓄電池用極板の製造方法。