JP2015534062A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2015534062A5 JP2015534062A5 JP2015533103A JP2015533103A JP2015534062A5 JP 2015534062 A5 JP2015534062 A5 JP 2015534062A5 JP 2015533103 A JP2015533103 A JP 2015533103A JP 2015533103 A JP2015533103 A JP 2015533103A JP 2015534062 A5 JP2015534062 A5 JP 2015534062A5
- Authority
- JP
- Japan
- Prior art keywords
- glass sheet
- temperature gradient
- tensile stress
- outer cylinder
- inner cylinder
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
- 239000011521 glass Substances 0.000 claims 25
- 238000000034 method Methods 0.000 claims 18
- 238000001514 detection method Methods 0.000 claims 5
- 230000007547 defect Effects 0.000 claims 2
- 230000003287 optical effect Effects 0.000 claims 1
- 238000005728 strengthening Methods 0.000 claims 1
- 230000000007 visual effect Effects 0.000 claims 1
Applications Claiming Priority (3)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US13/624,265 | 2012-09-21 | ||
| US13/624,265 US8960014B2 (en) | 2012-09-21 | 2012-09-21 | Methods of validating edge strength of a glass sheet |
| PCT/US2013/058967 WO2014046914A1 (en) | 2012-09-21 | 2013-09-10 | Methods of validating edge strength of a glass sheet |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JP2015534062A JP2015534062A (ja) | 2015-11-26 |
| JP2015534062A5 true JP2015534062A5 (enExample) | 2016-10-27 |
Family
ID=50337563
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2015533103A Pending JP2015534062A (ja) | 2012-09-21 | 2013-09-10 | ガラスシートの端部強度を検証する方法 |
Country Status (6)
| Country | Link |
|---|---|
| US (1) | US8960014B2 (enExample) |
| JP (1) | JP2015534062A (enExample) |
| KR (1) | KR20150054843A (enExample) |
| CN (1) | CN104769427B (enExample) |
| TW (1) | TW201418705A (enExample) |
| WO (1) | WO2014046914A1 (enExample) |
Families Citing this family (10)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| DE102014110855B4 (de) | 2014-07-31 | 2017-08-03 | Schott Ag | Verfahren und Vorrichtung zur Bestimmung der Bruchfestigkeit der Ränder dünner Bahnen sprödbrüchigen Materials |
| DE102014110856B4 (de) | 2014-07-31 | 2016-04-14 | Schott Ag | Verfahren und Vorrichtung zur Bestimmung der Kantenfestigkeit von scheibenförmigen Elementen aus sprödbrüchigem Material |
| WO2016149016A1 (en) * | 2015-03-13 | 2016-09-22 | Corning Incorporated | Edge strength testing methods and apparatuses |
| CN105973715A (zh) * | 2016-07-22 | 2016-09-28 | 江苏铁锚玻璃股份有限公司 | 一种飞机玻璃温差下压差强度性能及破坏强度试验装置 |
| KR102575017B1 (ko) * | 2016-11-17 | 2023-09-05 | 삼성디스플레이 주식회사 | 유리 기판의 결함 검출 방법 |
| WO2020036849A1 (en) | 2018-08-14 | 2020-02-20 | Corning Incorporated | Screen protector comprising a glass-based substrate and an adhesive |
| CN112823274A (zh) | 2018-08-14 | 2021-05-18 | 康宁股份有限公司 | 用于确定边缘的压碎强度的方法和设备 |
| JP7516422B2 (ja) * | 2019-05-15 | 2024-07-16 | コーニング インコーポレイテッド | 縁部強度試験方法及び装置 |
| WO2020231681A1 (en) * | 2019-05-15 | 2020-11-19 | Corning Incorporated | System and method for edge strength testing with real-time stress visualization in ultra-thin glass panels |
| DE102022127887A1 (de) * | 2022-10-21 | 2024-05-02 | Endress+Hauser Conducta Gmbh+Co. Kg | Verfahren zum Ermitteln eines Glasqualitätsindikators einer Glasbaugruppe sowie Glasbearbeitungsvorrichtung für eine Glasbaugruppe |
Family Cites Families (27)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US4395917A (en) * | 1981-10-26 | 1983-08-02 | Libbey-Owens-Ford Company | Apparatus for testing glass |
| US4440559A (en) * | 1982-06-30 | 1984-04-03 | Ppg Industries, Inc. | Apparatus for sensing a glass ribbon edge and method of use |
| US4711697A (en) * | 1985-11-21 | 1987-12-08 | The United States Of America As Represented By The Administrator Of The National Aeronautics And Space Administration | Method for investigating the formation of crystals in a transparent material |
| JPS6335945U (enExample) * | 1986-08-27 | 1988-03-08 | ||
| JPH01169343A (ja) * | 1987-12-25 | 1989-07-04 | Nippon Sheet Glass Co Ltd | ガラス板の切口欠点検出装置 |
| CH686304A5 (de) | 1994-07-08 | 1996-02-29 | Vetrotech Ag | Verfahren zum Herstellen von ebenen oder gewoelbten Glasplatten. |
| US6004655A (en) | 1994-10-26 | 1999-12-21 | Nippon Sheet Glass Co., Ltd. | Method of finishing edge of sheet glass, heat-tempered sheet glass using the method, and fire-resistant construction material using the heat-tempered sheet glass |
| JPH08271397A (ja) * | 1995-03-30 | 1996-10-18 | Hitachi Zosen Corp | 熱疲労試験方法および熱疲労試験装置 |
| DE19720330C1 (de) | 1997-05-15 | 1998-11-12 | Sekurit Saint Gobain Deutsch | Verfahren und Vorrichtung zur Messung von Spannungen in Glasscheiben mit Hilfe des Streulichtverfahrens |
| CA2317743A1 (en) * | 1998-12-11 | 2000-06-22 | Paul Mansky | Sensor array-based system and method for rapid materials characterization |
| US6515441B1 (en) * | 1999-09-07 | 2003-02-04 | Meritor Light Vehicle Systems, Inc. | Glass edge object detection sensor |
| FR2801302B1 (fr) * | 1999-11-22 | 2001-12-21 | Saint Gobain Vitrage | Procede de traitement de substrats en verre et substrats en verre pour la realisation d'ecrans de visualisation |
| US6501546B1 (en) | 2000-05-05 | 2002-12-31 | Photon Dynamics Canada Inc. | Inspection system for edges of glass |
| US6796144B2 (en) * | 2001-05-30 | 2004-09-28 | Battelle Memorial Institute | System and method for glass processing and temperature sensing |
| US20030076487A1 (en) | 2001-08-03 | 2003-04-24 | Cannon Bret D. | System and method for glass processing and stress measurement |
| AT8647U1 (de) * | 2005-08-08 | 2006-10-15 | Binder Co Ag | Verfahren zur detektion und sortierung von glas |
| CN101646524A (zh) | 2007-02-23 | 2010-02-10 | 康宁股份有限公司 | 热边缘精整 |
| TWI354153B (en) | 2007-11-19 | 2011-12-11 | Au Optronics Corp | Flat display panel having strength enhancing struc |
| JP5067223B2 (ja) * | 2008-03-24 | 2012-11-07 | 日本電気硝子株式会社 | 平面表示装置用板ガラスの評価方法 |
| US8656738B2 (en) | 2008-10-31 | 2014-02-25 | Corning Incorporated | Glass sheet separating device |
| WO2010135614A1 (en) | 2009-05-21 | 2010-11-25 | Corning Incorporated | Thin substrates having mechanically durable edges |
| JP2011112587A (ja) | 2009-11-30 | 2011-06-09 | Howa Mach Ltd | ガラス強度試験装置 |
| JP2011202991A (ja) * | 2010-03-24 | 2011-10-13 | Nippon Electric Glass Co Ltd | 板ガラスの端部検査方法及び端部検査装置 |
| US8571615B2 (en) * | 2010-09-10 | 2013-10-29 | California Institute Of Technology | Superconducting metallic glass transition-edge-sensors |
| JP2012078132A (ja) | 2010-09-30 | 2012-04-19 | Nippon Electric Glass Co Ltd | 板ガラス検査方法及び板ガラス検査装置 |
| CN102072918B (zh) | 2010-11-25 | 2012-08-22 | 中国科学技术大学 | 一种热载荷作用下玻璃破裂脱落封闭箱体实验装置 |
| US8607590B2 (en) | 2010-11-30 | 2013-12-17 | Corning Incorporated | Methods for separating glass articles from strengthened glass substrate sheets |
-
2012
- 2012-09-21 US US13/624,265 patent/US8960014B2/en not_active Expired - Fee Related
-
2013
- 2013-09-10 JP JP2015533103A patent/JP2015534062A/ja active Pending
- 2013-09-10 CN CN201380049070.XA patent/CN104769427B/zh not_active Expired - Fee Related
- 2013-09-10 KR KR1020157006846A patent/KR20150054843A/ko not_active Withdrawn
- 2013-09-10 WO PCT/US2013/058967 patent/WO2014046914A1/en not_active Ceased
- 2013-09-18 TW TW102133953A patent/TW201418705A/zh unknown
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN104769427B (zh) | 验证玻璃板的边缘强度的方法 | |
| Zhao et al. | Three-dimensional finite element analysis of thermal stress in single-pass multi-layer weld-based rapid prototyping | |
| TWI543858B (zh) | 退火方法、退火冶具及退火裝置 | |
| JP2015534915A5 (enExample) | ||
| JP2011173236A5 (enExample) | ||
| JP2011216832A5 (ja) | 基板接合装置、基板ホルダ、基板接合方法、デバイスの製造方法および位置合わせ装置 | |
| WO2014149428A3 (en) | Method and apparatus for reducing ply wrinkling of composite laminates during forming | |
| JP2017094706A5 (enExample) | ||
| MX384849B (es) | Método para producir un cristal compuesto para un vehículo de motor. | |
| MX2019009638A (es) | Metodos y sistemas para detectar defectos en materiales compuestos. | |
| WO2014121914A3 (de) | VERFAHREN ZUR FORMFREIEN HERSTELLUNG EINES GEFORMTEN GLASARTIKELS MIT VORBESTIMMTER GEOMETRIE, VERWENDUNG EINES VERFAHRENSGEMÄß HERGESTELLTEN GLASARTIKELS UND GEFORMTER GLASARTIKEL | |
| JP2018513093A5 (enExample) | ||
| Huang et al. | A dual-mesh method for efficient thermal stress analysis of large-scale welded structures | |
| JP2009015273A5 (enExample) | ||
| CN107530951A (zh) | 管子成型的方法和执行所述方法所使用的设备 | |
| JP2016531076A5 (enExample) | ||
| JP6021162B2 (ja) | 摺動式外側突出部を備えたマンドレル | |
| CN103862165B (zh) | 一种金属层合板激光协调弯曲的方法 | |
| CN104475928A (zh) | 锅炉钢架叠梁制作工艺 | |
| CN105710183A (zh) | 一种弯曲板激光成形技术 | |
| CN106050846B (zh) | 一种碳纤维加固铝合金榫卯结构的制备方法 | |
| CN115041855B (zh) | 一种超高强钢与高强钢焊接结构与焊接工艺 | |
| CN103624393B (zh) | 刚性拘束热自压连接方法 | |
| JP6579570B2 (ja) | コーティング層における剥離の非破壊検査方法および非破壊検査装置 | |
| FR2992889A1 (fr) | Procede de fixation par dilatation thermique d'un renfort metallique structurel sur une partie d'une aube de turbine a gaz en materiau composite et moule de collage pour la mise en oeuvre d'un tel procede |