JP2011174167A5 JP2010170331A JP2010170331A JP2011174167A5 JP 2011174167 A5 JP2011174167 A5 JP 2011174167A5 JP 2010170331 A JP2010170331 A JP 2010170331A JP 2010170331 A JP2010170331 A JP 2010170331A JP 2011174167 A5 JP2011174167 A5 JP 2011174167A5
Authority
JP
Japan
Prior art keywords
oxide film
copper
niobium
atoms
less
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2010170331A
Other languages
English (en)
Japanese (ja)
Other versions
JP5641402B2 (ja
JP2011174167A (ja
Filing date
Publication date
Application filed filed Critical
Priority claimed from JP2010170331A external-priority patent/JP5641402B2/ja
Priority to JP2010170331A priority Critical patent/JP5641402B2/ja
Priority to PCT/JP2010/073700 priority patent/WO2011092993A1/ja
Priority to CN201080062959.8A priority patent/CN102741448B/zh
Priority to KR1020127020398A priority patent/KR20120112716A/ko
Priority to US13/576,567 priority patent/US20120301673A1/en
Publication of JP2011174167A publication Critical patent/JP2011174167A/ja
Publication of JP2011174167A5 publication Critical patent/JP2011174167A5/ja
Publication of JP5641402B2 publication Critical patent/JP5641402B2/ja
Application granted granted Critical
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Links

JP2010170331A 2010-02-01 2010-07-29 酸化物膜及びその製造方法、並びにターゲット及び酸化物焼結体の製造方法 Expired - Fee Related JP5641402B2 (ja)

Priority Applications (5)

Application Number Priority Date Filing Date Title
JP2010170331A JP5641402B2 (ja) 2010-02-01 2010-07-29 酸化物膜及びその製造方法、並びにターゲット及び酸化物焼結体の製造方法
US13/576,567 US20120301673A1 (en) 2010-02-01 2010-12-28 Oxide film, process for producing same, target, and process for producing sintered oxide
CN201080062959.8A CN102741448B (zh) 2010-02-01 2010-12-28 氧化物膜及其制造方法、与靶及氧化物烧结体的制造方法
KR1020127020398A KR20120112716A (ko) 2010-02-01 2010-12-28 산화물 막 및 그 제조 방법, 및 타겟 및 산화물 소결체의 제조 방법
PCT/JP2010/073700 WO2011092993A1 (ja) 2010-02-01 2010-12-28 酸化物膜及びその製造方法、並びにターゲット及び酸化物焼結体の製造方法

Applications Claiming Priority (3)

Application Number Priority Date Filing Date Title
JP2010020343 2010-02-01
JP2010020343 2010-02-01
JP2010170331A JP5641402B2 (ja) 2010-02-01 2010-07-29 酸化物膜及びその製造方法、並びにターゲット及び酸化物焼結体の製造方法

Publications (3)

Publication Number Publication Date
JP2011174167A JP2011174167A (ja) 2011-09-08
JP2011174167A5 true JP2011174167A5 (cg-RX-API-DMAC10.html) 2013-08-15
JP5641402B2 JP5641402B2 (ja) 2014-12-17

Family

ID=44318992

Family Applications (1)

Application Number Title Priority Date Filing Date
JP2010170331A Expired - Fee Related JP5641402B2 (ja) 2010-02-01 2010-07-29 酸化物膜及びその製造方法、並びにターゲット及び酸化物焼結体の製造方法

Country Status (5)

Country Link
US (1) US20120301673A1 (cg-RX-API-DMAC10.html)
JP (1) JP5641402B2 (cg-RX-API-DMAC10.html)
KR (1) KR20120112716A (cg-RX-API-DMAC10.html)
CN (1) CN102741448B (cg-RX-API-DMAC10.html)
WO (1) WO2011092993A1 (cg-RX-API-DMAC10.html)

Families Citing this family (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP5996227B2 (ja) * 2012-03-26 2016-09-21 学校法人 龍谷大学 酸化物膜及びその製造方法
KR20160017101A (ko) * 2014-05-08 2016-02-15 미쓰이금속광업주식회사 스퍼터링 타깃재
JP6503928B2 (ja) * 2015-06-29 2019-04-24 コニカミノルタ株式会社 電子写真感光体、画像形成装置および画像形成方法
JP7048193B2 (ja) * 2016-11-17 2022-04-05 日本化学工業株式会社 亜酸化銅粒子の製造方法
JP7172902B2 (ja) * 2019-07-29 2022-11-16 トヨタ自動車株式会社 酸素吸蔵材
CN111678927A (zh) * 2020-06-08 2020-09-18 首钢集团有限公司 一种钢铁表面氧化物的分析方法

Family Cites Families (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US6232542B1 (en) * 1996-11-15 2001-05-15 Citizen Watch Co., Ltd. Method of fabricating thermoelectric device
JP4446064B2 (ja) * 2004-07-07 2010-04-07 独立行政法人産業技術総合研究所 熱電変換素子及び熱電変換モジュール
US7657377B2 (en) * 2007-05-31 2010-02-02 Cbg Corporation Azimuthal measurement-while-drilling (MWD) tool
JP2009047969A (ja) * 2007-08-21 2009-03-05 Seiko Epson Corp プロジェクタおよび表示装置
JP2009246085A (ja) * 2008-03-31 2009-10-22 Hitachi Ltd 半導体装置およびその製造方法
JP2010031346A (ja) * 2008-07-02 2010-02-12 Central Glass Co Ltd 酸化亜鉛薄膜及び薄膜積層体

Similar Documents

Publication Publication Date Title
Qian et al. Enhanced thermoelectric performance in lead-free inorganic CsSn1–x Ge x I3 perovskite semiconductors
Cui et al. Thermochromic VO2 for energy-efficient smart windows
Yan et al. Enhanced thermoelectric figure of merit of p-type half-Heuslers
Guin et al. Cation disorder and bond anharmonicity optimize the thermoelectric properties in kinetically stabilized rocksalt AgBiS2 nanocrystals
Zhou et al. Significant enhancement in the thermoelectric performance of aluminum-doped ZnO tuned by pore structure
JP5884549B2 (ja) 透明酸化物膜およびその製造方法
Cao et al. Vertical SnSe nanorod arrays: from controlled synthesis and growth mechanism to thermistor and photoresistor
JP2010245299A (ja) 複合材熱電材料及びその製造方法
JP2019009307A5 (cg-RX-API-DMAC10.html)
WO2012043570A1 (ja) 酸化物焼結体及びその製造方法、スパッタリングターゲット、酸化物透明導電膜及びその製造方法、並びに太陽電池
Cheng et al. Enhancement of thermoelectric performance in Bi0. 5Sb1. 5Te3 particulate composites including ferroelectric BaTiO3 nanodots
TWI487687B (zh) Indium oxide sintered body and indium oxide transparent conductive film
Wu et al. TiOx/Ag/TiOx multilayer for application as a transparent conductive electrode and heat mirror
JP2013520394A (ja) ドープ化または非ドープ化ZnO材料の製造方法およびその材料
JP2011012341A5 (ja) 導電膜及び導電膜の作製方法
CN107394035A (zh) 一种Sb掺杂BiCuSeO热电材料及其制备方法
Salian et al. Evolution of high dielectric permittivity in low-temperature solution combustion-processed phase-pure high entropy oxide (CoMnNiFeCr) O for thin film transistors
Tan et al. Optimization of the thermoelectric properties of Bi2O2Se ceramics by altering the temperature of spark plasma sintering
Guo et al. Recent progresses on transparent electrodes and active layers toward neutral, color semitransparent perovskite solar cells
JP2015030896A (ja) スパッタリングターゲット及び酸化物透明導電膜
Zhao et al. Enhanced thermoelectric performance of Bi–Se Co-doped Cu1. 8S via carrier concentration regulation and multiscale phonon scattering
Park et al. Influence of SnO2 addition on the thermoelectric properties of Zn1− xSnxO (0.01≤ x≤ 0.05)
TWI360228B (cg-RX-API-DMAC10.html)
JP2015124145A5 (cg-RX-API-DMAC10.html)
JP2013001919A (ja) In2O3−ZnO系スパッタリングターゲット及び酸化物導電膜