Prior art keywords
monomer
residual
copolymer
maleic acid
diallyldimethylammonium chloride
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2009163820A
Other languages
English (en)
Japanese (ja)
Other versions
JP5464409B2 (ja
JP2010248460A (ja
Filing date
Publication date
Application filed filed Critical
Priority claimed from JP2009163820A external-priority patent/JP5464409B2/ja
Priority to JP2009163820A priority Critical patent/JP5464409B2/ja
Priority to EP20100755573 priority patent/EP2412736B1/en
Priority to PCT/JP2010/001182 priority patent/WO2010109766A1/ja
Priority to US13/254,423 priority patent/US8901266B2/en
Priority to CN201080013659.0A priority patent/CN102365305B/zh
Publication of JP2010248460A publication Critical patent/JP2010248460A/ja
Publication of JP2010248460A5 publication Critical patent/JP2010248460A5/ja
Publication of JP5464409B2 publication Critical patent/JP5464409B2/ja
Application granted granted Critical
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

JP2009163820A 2009-03-26 2009-07-10 ジアリルジアルキルアンモニウム塩とマレイン酸との共重合体の製造方法 Active JP5464409B2 (ja)

Priority Applications (5)

Application Number Priority Date Filing Date Title
JP2009163820A JP5464409B2 (ja) 2009-03-26 2009-07-10 ジアリルジアルキルアンモニウム塩とマレイン酸との共重合体の製造方法
CN201080013659.0A CN102365305B (zh) 2009-03-26 2010-02-23 用于生产二烯丙基二烷基铵盐/马来酸共聚物的方法
PCT/JP2010/001182 WO2010109766A1 (ja) 2009-03-26 2010-02-23 ジアリルジアルキルアンモニウム塩とマレイン酸との共重合体の製造方法
US13/254,423 US8901266B2 (en) 2009-03-26 2010-02-23 Method for producing diallyldialkylammonium salt/maleic acid copolymer
EP20100755573 EP2412736B1 (en) 2009-03-26 2010-02-23 Method for producing diallyldialkylammonium salt/maleic acid copolymer

Applications Claiming Priority (3)

Application Number Priority Date Filing Date Title
JP2009075391 2009-03-26
JP2009075391 2009-03-26
JP2009163820A JP5464409B2 (ja) 2009-03-26 2009-07-10 ジアリルジアルキルアンモニウム塩とマレイン酸との共重合体の製造方法

Publications (3)

Publication Number Publication Date
JP2010248460A JP2010248460A (ja) 2010-11-04
JP2010248460A5 true JP2010248460A5 (enExample) 2011-09-29
JP5464409B2 JP5464409B2 (ja) 2014-04-09

Family

ID=42780466

Family Applications (1)

Application Number Title Priority Date Filing Date
JP2009163820A Active JP5464409B2 (ja) 2009-03-26 2009-07-10 ジアリルジアルキルアンモニウム塩とマレイン酸との共重合体の製造方法

Country Status (5)

Country Link
US (1) US8901266B2 (enExample)
EP (1) EP2412736B1 (enExample)
JP (1) JP5464409B2 (enExample)
CN (1) CN102365305B (enExample)
WO (1) WO2010109766A1 (enExample)

Families Citing this family (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP5630672B2 (ja) * 2010-07-15 2014-11-26 日東紡績株式会社 金属の酸洗浄用腐食抑制剤、洗浄液組成物及び金属の洗浄方法
EP3004187A1 (en) * 2013-06-03 2016-04-13 General Electric Company Polymer coagulants
JP6350829B2 (ja) * 2015-10-15 2018-07-04 日東紡績株式会社 ジアリルアミン類と二酸化硫黄との共重合体、及びその製造方法。

Family Cites Families (10)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
DD274432A1 (de) 1988-07-28 1989-12-20 Akad Wissenschaften Ddr Verfahren zur herstellung neuer wasserloeslicher, thermisch vernetzbarer polyampholyte
JP2962816B2 (ja) 1990-11-27 1999-10-12 日東紡績株式会社 凝集剤
JP2766168B2 (ja) 1993-09-03 1998-06-18 日本碍子株式会社 消化汚泥の固液分離装置
JP3595995B2 (ja) * 1996-12-06 2004-12-02 日東紡績株式会社 インクジェット記録媒体
JP3903546B2 (ja) * 1997-10-03 2007-04-11 王子製紙株式会社 インクジェット記録体の製造方法
JP3659404B2 (ja) 1997-10-29 2005-06-15 日東紡績株式会社 N,n−ジアルキルアリルアミン系重合体の製造方法およびn,n−ジアルキルアリルアミン系重合体
EP1268214B1 (en) 2000-04-04 2006-06-07 Celanese International Corporation Ink receptive coating compositions containing poly(vinyl alcohol) grafted with amine functional groups
JP2004025773A (ja) * 2002-06-28 2004-01-29 Mitsui Chemicals Inc 記録媒体及びその製造方法
JP4468024B2 (ja) * 2004-03-15 2010-05-26 株式会社ワイヤーデバイス 衝突防止装置
JP4406882B2 (ja) * 2005-03-18 2010-02-03 ハリマ化成株式会社 填料内添紙及びその製造方法

Similar Documents

Publication Publication Date Title
Li et al. Desalination by membrane pervaporation: A review
JP2010510550A5 (enExample)
JP2017206509A5 (enExample)
JP2016034965A5 (enExample)
WO2007018783A3 (en) Polymerization of fluoropolymers using non-fluorinated surfactants
EP3196217B1 (en) Method for producing polyvinylamine crosslinked polymer particles
JP2016514753A5 (enExample)
RU2013155189A (ru) Улучшенная композиция
JP2010248460A5 (enExample)
BR112014015830A2 (pt) polímero adjuvante de processamento em emulsão em multi-estágio, formulação e processo de polimerização em emulsão em multi-estágio
WO2007149274A3 (en) Process for desactivating polymerization catalyst using phosphoric- or phosphonic acid salts and a catalyst deactivator
JP2008532751A5 (enExample)
JP2017171825A5 (enExample)
Li et al. How does alkali etching work on the polyamide membrane to obtain an m-phenylenediamine-based nf membrane?
JP6327003B2 (ja) イミノジ酢酸型キレート樹脂の製造方法
JP2009227979A5 (enExample)
JP2009300719A5 (enExample)
CN107922217B (zh) 净化水的方法
JP5522618B2 (ja) モノリス状有機多孔質アニオン交換体およびその製造方法
JP2010235536A5 (enExample)
JP6846773B2 (ja) 多孔質構造を有するポリビニルカルボン酸アミド架橋重合体球状粒子及びその製造方法
JP4971867B2 (ja) ポリビニルアルコール−ポリビニルピロリドングラフトコポリマーの製造方法
WO2015110096A8 (en) Method of preparation of a soluble block copolymer of styrene and olefines, and use thereof
JP2012526887A5 (enExample)
RU2016135946A (ru) Новые, легированные алюминием, содержащие группы иминодиуксусной кислоты хелатообразующие смолы